Microstructural Development of Directionally Solidified Hg(1-x)Zn(x)Se Alloys

Hg(1-x)Zn(x)Se alloys have been studied as an alternative to Hg(1-x)Cd(x)Te for the detection of electromagnetic radiation, because the shorter ZnSe and HgSe bonds have been predicted to improve lattice stability. Several ingots with x = 0.1 were directionally solidified using a modified Bridgman-Stockbarger method; one was grown in an applied magnetic field, which greatly reduced radial compositional variations. A method was developed to reduce wetting. This, combined with the convex liquid-solid interface shape, produced boules that were single crystalline after growing about 3.5 cm. Observed surface features indicated ampoule wetting was eliminated using a graphite getter. Microstructural characteristics were greatly improved over HgCdTe alloys. In six boules, a total of only one twin was observed. A method for polishing and producing dislocation etch pits was developed for these alloys, revealing dislocation etch pit densities one to two orders of magnitude less than HgTe-based alloys. A kink in the thermal profile during processing of one boule generated more dislocations than did lattice mismatch due to compositional variations. This alloy has improved microstructural properties and resistance to dislocation formation compared with similar II-VI alloys.

Cobb, S. D.↗

Molecular-Dynamics Analysis of the Mechanical Behavior of Plasma-Facing Tungsten

We report a systematic computational analysis of the mechanical behavior of plasma-facing component (PFC) tungsten focusing on the impact of void and helium (He) bubble defects on the mechanical response beyond the elastic regime. Specifically, we explore the effects of porosity and He atomic fraction on the mechanical properties and structural response of PFC tungsten, at varying temperature and bubble size. We find that the Young modulus of defective tungsten undergoes substantial softening that follows an exponential scaling relation as a function of matrix porosity and He atomic content. Beyond the elastic regime, our high strain rate simulations reveal that the presence of nanoscale spherical defects (empty voids and He bubbles) reduces the yield strength of tungsten in a monotonically decreasing fashion, obeying an exponential scaling relation as a function of tungsten matrix porosity and He concentration. Our detailed analysis of the structural response of PFC tungsten near the yield point reveals that yielding is initiated by emission of dislocation loops from bubble/matrix interfaces, mainly 1/2<111> shear loops, followed by gliding and growth of these loops and reactions to form <100> dislocations. Furthermore, dislocation gliding on the <111>{211} twin systems nucleates 1/6<111> twin regions in the tungsten matrix. These dynamical processes reduce the stress in the matrix substantially. Subsequent dislocation interactions and depletion of the twin phases via nucleation and propagation of detwinning partials lead the tungsten matrix to a next deformation stage characterized by stress increase during applied straining. Furthermore, our structural analysis reveals that the depletion of twin boundaries (areal defects) is strongly impacted by the density of He bubbles at higher porosities. After the initial stress relief upon yielding, increase in the dislocation density in conjunction with decrease in the areal defect density facilitates the initiation of dislocation-driven deformation mechanisms in the PFC crystal.

36 MATERIALS SCIENCE↗

Effect of alloying elements on defect evolution in Ni-20X binary alloys

The effect of alloying elements on radiation-induced microstructural evolution in Ni and Ni-20X (X = Fe, Cr, Mn and Pd) binary alloys was investigated using ion irradiation and cross-sectional transmission electron microscopy. The three-dimensional migration mode is identified to be the dominating migration mechanism for interstitial clusters in these binary alloys, contrary to the one-dimensional mode that dominates in the well-studied dilute alloys. The results reveal that: (1) the average size of defect clusters decreases as the solute atomic volume size factor increases. Smaller void size in Ni-20Cr is attributed to faster vacancy mobility in the near surface region, and weaker vacancy binding energy beyond the irradiation peak than Ni-20Fe. The smaller voids observed in Ni-20Mn and Ni-20Pd beyond the damage peak are due to the stronger Mn/Pd-vacancy binding effect of largely oversized solute atoms. (2) Oversized solutes can act as strong trapping sites for interstitials. The larger the solute atomic volume factor, the stronger the trapping force. This leads to a more significantly sluggish interstitial migration and smaller dislocation loop size. The average dislocation loop size in Ni-20Fe was four times larger than Ni-20Pd (atomic volume factor being 10.6% and 41.3%) but an order of magnitude lower in density. The smaller dislocation loop size in Ni-20Cr is attributed to stronger interstitial binding of Cr-Ni. In conclusion, overall, the alloying effect on defects is more significant in concentrated binary alloys than in dilute binary alloys, due to the concentration difference of alloying atoms and the interstitial dominant migration mechanisms in the main irradiated region.

36 MATERIALS SCIENCE↗

Evaluation of AlGaN/GaN high electron mobility transistors grown on ZrTi buffer layers with sapphire substrates

Here, AlGaN/GaN high electron mobility transistors (HEMTs) have been grown on sapphire substrates, using ZrTi buffer layers to provide in-plane lattice-matching to hexagonal GaN. X-ray diffraction (XRD) as well as cross-section transmission electron microscopy (TEM) were used to assess the quality of the HEMT structure. The XRD 2θ scans showed full-width-at-half-maximum values of 0.16°, 0.07°, and 0.08° for ZrTi alloy, GaN buffer layer, and the entire HEMT structure, respectively. TEM studies of the GaN buffer layer and the AlN/ZrTi/AlN stack showed the importance of growing thin AlN buffer layers on the ZrTi layer prior to growth of the GaN buffer layer. The density of threading dislocations in the GaN channel layer of the HEMT structure was estimated to be in the 10 8 cm –2 range. The HEMT device exhibited a saturation drain current density of 820 mA/mm, and the channel of the fabricated HEMTs could be well modulated. A cutoff frequency (f T ) of 8.9 GHz and a maximum frequency of oscillation (f max ) of 17.3 GHz were achieved for HEMTs with gate dimensions of 1 × 200 μm.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Evolution of extended defects in UO 2 during high temperature annealing

The evolution of thermophysical characteristics of uranium oxide (UO 2 ) under irradiation is a critical aspect of nuclear fuel performance of light water reactors. This study examines the effect of high-temperature annealing at 1000 °C - 1600 °C on defect evolution in krypton irradiated UO 2 at room temperature. Transmission electron microscopy analysis reveals that the size of irradiation-induced bubbles and dislocation loops increases but their density decreases with annealing temperatures. Perfect dislocation loops with = <110> dominate, regardless of the annealing temperature. A rate theory model for extended defect evolution is applied to conclude that current understanding of dynamical loop and bubble evolution at high-temperature annealing is governed by defect coalescence.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Enhanced void swelling in NiCoFeCrPd high-entropy alloy by indentation-induced dislocations

The role of dislocations on ion irradiation-induced void formation is studied in a high-entropy alloy (HEA) NiCoFeCrPd. Despite previous observations that show high-entropy alloys are swelling resistant due to a high defect recombination rate, the swelling is enhanced with increasing density of pre-existing dislocations at low strain levels that shortened transient duration before the onset of void swelling. Under certain irradiation conditions, a high density of dislocations may carry the material closer to the sink-dominated regime. Finally, compared to another HEA NiCoFeCrMn, NiCoFeCrPd has a smaller loop size and higher loop density due to the stronger lattice distortion.

36 MATERIALS SCIENCE↗

Stress relaxation in vanadium under shock and shockless dynamic compression

Evolutions of elastic-plastic waves have been recorded in three series of plate impact experiments with annealed vanadium samples under conditions of shockless and combined ramp and shock dynamic compression. The shaping of incident wave profiles was realized using intermediate base plates made of different silicate glasses through which the compression waves were entered into the samples. Measurements of the free surface velocity histories revealed an apparent growth of the Hugoniot elastic limit with decreasing average rate of compression. The growth was explained by “freezing” of the elastic precursor decay in the area of interaction of the incident and reflected waves. A set of obtained data show that the current value of the Hugoniot elastic limit and plastic strain rate is rather associated with the rate of the elastic precursor decay than with the local rate of compression. The study has revealed the contributions of dislocation multiplications in elastic waves. It has been shown that independently of the compression history the material arrives at the minimum point between the elastic and plastic waves with the same density of mobile dislocations.

36 MATERIALS SCIENCE↗

On the electronic properties of a single dislocation

A detailed knowledge of the electronic properties of individual dislocations is necessary for next generation nanodevices. Dislocations are fundamental crystal defects controlling the growth of different nanostructures (nanowires) or appear during device processing. We present a method to record electric properties of single dislocations in thin silicon layers. Results of measurements on single screw dislocations are shown for the first time. Assuming a cross-section area of the dislocation core of about 1 nm{sup 2}, the current density through a single dislocation is J = 3.8 × 10{sup 12} A/cm{sup 2} corresponding to a resistivity of ρ ≅ 1 × 10{sup −8} Ω cm. This is about eight orders of magnitude lower than the surrounding silicon matrix. The reason of the supermetallic behavior is the high strain in the cores of the dissociated dislocations modifying the local band structure resulting in high conductive carrier channels along defect cores.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effect of Interface Shape and Magnetic Field on the Microstructure of Bulk Ge:Ga

Thermal and compositional gradients induced during the growth process contribute significantly to the development of defects in the solidified boule. Thermal gradients and the solid-liquid interface shape can be greatly effected by ampoule material. Compositional gradients are strongly influenced by interface curvature and convective flow in the liquid. Results of this investigation illustrate the combined influences of interface shape and convective fluid flow. An applied magnetic field was used to reduce the effects of convective fluid flow in the electrically conductive melt during directional solidification. Several 8 mm diameter boules of Ga-doped Ge were grown at different field strengths, up to 5 Tesla, in four different ampoule materials. Compositional profiles indicate mass transfer conditions ranged from completely mixed to diffusion controlled. The influence of convection in the melt on the developing crystal microstructure and defect density was investigated as a function of field strength and ampoule material. Chemical etching and electron backscattered electron diffraction were used to map the crystal structure of each boule along the center plane. Dislocation etch pit densities were measured for each boule. Results show the influence of magnetic field strength and ampoule material on overall crystal quality.

Cobb, S. D.↗

THERMAL ANNEALING OF IRRADIATED PREHYDRIDED ZIRCALOY-4 MATERIALS

Hydrogen-assisted irradiation growth is an important issue for reliability and performance of nuclear materials in nuclear fuel cladding and fuel assembly components. The mechanisms of irradiation growth are not entirely clear and the role of hydrogen and hydrides are less so. There is evidence that breakaway irradiation growth is strongly influenced by the formation and dynamics of dislocation loops that vary with alloy composition, heat treatment and hydrogen content. Thermal annealing of eight Zircaloy-4 specimens irradiated in the Advanced Test Reactor (ATR) at the Idaho National Laboratory as part of the joint EPRI Nuclear Fuels Industry Research (NFIR) and Fuel Reliability Program (FRP) AsTeR irradiation growth study were performed by hot-stage transmission electron microscopy (TEM), differential scanning calorimetry (DSC), and dilatometry via NSUF RTE 17-1093. Two fluence levels (6.7 and 12.3 dpa) and three hydrogen contents (~10, 40, 120 ppm) were investigated. TEM with a hot stage was used for the quantification of "a" and "c" dislocation loop population densities and size distributions at a range of temperatures from 25 to 800oC. DSC and dilatometry were performed by dynamically heating and cooling from 30 to 750ºC at rates of 5, 10, and 20 oC/min to determine the behavior of dislocation loop annealing. Dynamic temperature DSC tests were able to detect the temperature ranges and enthalpies of "a" and "c" loop annihilation, hydride dissolution and precipitation, secondary particle precipitation, and a?a + ß phase transformations upon heating and cooling. Dilatometry tests showed that all of the test showed initial linear expansion followed by a decrease in expansion rate from about 400 to 600 ºC associated with annihilation of "a" and "c" loops and showed evidence for the thermal stabilizing effect of hydrogen on dislocation loops. The results are discussed in the context of the larger AsTeR program that will include higher exposure (~20 dpa) and different alloys when they become available in 2021.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

TEM investigation of beta-SiC grown epitaxially on Si substrate by CVD

A transmission electron microscopy study is being conducted on the microstructure of beta-SiC films grown epitaxially on 001-plane silicon by chemical vapor deposition. Observations have been made in plain view and in cross-section. A high density of stacking faults has been found in the bulk of the epilayer which are bounded by partials of the Shockley type with Burgers vectors 1/6 211-line. Cross-sectional high resolution electron microscopy of the interface has shown it to be semicoherent with misfit dislocations to accommodate the lattice parameter difference between the substrate and the epilayer. In addition to misfit dislocations, a high density of twins and some stacking faults are present in the SiC near the interface. Mechanisms for the nucleation and growth of these defects are discussed.

Chorey, C. M.↗

Orbital processing of high-quality CdTe compound semiconductors

CdZnTe crystals were grown in one-g and in micro-g for comparative analysis. The two micro-g crystals were grown in the Crystal Growth Furnace during the First United States Microgravity Laboratory mission (USML-1). The samples were analyzed for chemical homogeneity, structural perfection, and optoelectronic performance (infrared transmission). Fourier Transform Infrared (FTIR) transmission of both ground and flight materials showed that the infrared transmission was close to theoretical, 63% versus 66%, suggesting that the material was close to the stochiometric composition during both the ground and flight experiments. Infrared microscopy confirmed that the principal precipitates were Te and their size (1-10 microns) and density suggested that the primary flight and ground base samples experienced similar cooling rates. Macrosegregation was predicted, using scaling analysis, to be low even in one-g crystals and this was confirmed experimentally, with nearly diffusion controlled growth achieved even in the partial mixing regime on the ground. Radial segregation was monitored in the flight samples and was found to vary with fraction solidified, but was disturbed due to the asymmetric grvitational and thermal fields experienced by the flight samples. The flight samples, however, were found to be much higher in structural perfection than the ground samples produced in the same furnace under identical growth conditions except for the gravitational level. Rocking curve widths were found to be substantially reduced, from 20/35 (one-g) to 9/20 (micro-g) for the best regions of the crystals. The full width at half maximum (FWHM) of 9 arc seconds is as good as the best reported terrestrially for this material. The ground samples were found to have a fully developed mosaic structure consisting of subgrains, whereas the flight sample dislocations were discrete and no mosaic substructure was evident. The defect density was reduced from 50-100,000 (one-g) to 500-25000 EPD (micro-g). These results were confirmed using rocking curve analysis, synchrotron topography, and etch pit analysis. The low dislocation density is thought to have resulted from the near-absence of hydrostatic pressure which allowed the melt to solidify with minimum or no wall contact, resulting in very low stress being exerted on the crystal during growth or during post-solidification cooling.

Larson, David J., Jr.↗

Influence of interfacial dislocations on hysteresis loops of ferroelectric films

We investigated the influence of dislocations, located at the interface of a ferroelectric film and its underlying substrate, on the ferroelectric hysteresis loop including the remanent polarization and coercive field using phase-field simulations. We considered epitaxial ferroelectric BaTiO3 films and found that the hysteresis loop is strongly dependent on the type and density of interfacial dislocations. The dislocations that stabilize multiple ferroelectric variants and domains reduce the coercive field, and consequently, the corresponding remanent polarization also decreases.

36 MATERIALS SCIENCE↗

Dislocation loop evolution during in-situ ion irradiation of model FeCrAl alloys

Model FeCrAl alloys of Fe-10%Cr-5%Al, Fe-12%Cr-4.5%Al, Fe-15%Cr-4%Al, and Fe-18%Cr-3%Al (in wt %) were irradiated with 1 MeV Kr++ ions in-situ with transmission electron microscopy to a dose of 2.5 displacements per atom (dpa) at 320 °C. In all cases, the microstructural damage consisted of dislocation loops with ½< 111 > and <100 > Burgers vectors. The proportion of ½< 111 > dislocation loops varied from ~50% in the Fe-10%Cr-5%Al model alloy and the Fe-18Cr%-3%Al model alloy to a peak of ~80% in the model Fe-15%Cr-4.5%Al alloy. The dislocation loop volume density increased with dose for all alloys and showed signs of approaching an upper limit. The total loop populations at 2.5 dpa had a slight (and possibly insignificant) decline as the chromium content was increased from 10 to 15 wt %, but the Fe-18%Cr-3%Al alloy had a dislocation loop population ~50% smaller than the other model alloys. As a result, the largest dislocation loops in each alloy had image sizes of close to 20 nm in the micrographs, and the median diameters for all alloys ranged from 6 to 8 nm. Nature analysis by the inside-outside method indicated most dislocation loops were interstitial type.

36 MATERIALS SCIENCE↗

Emulation of neutron-irradiated microstructure of austenitic 21Cr32Ni model alloy using dual-ion irradiation

Here, in this study, the capability of heavy-ion irradiation to emulate neutron irradiation was demonstrated on an austenitic 21Cr32Ni type ternary model alloy. The model alloy used in this study is chemically analogous but compositionally simpler than of alloy 800H, which is a candidate austenitic Ni alloy which has been proposed for use in Generation IV reactors. The microstructure of the 21Cr32Ni model alloy irradiated in the BOR-60 fast reactor to 17.1 dpa and 35 dpa at ~380°C was characterized using transmission electron microscopy (TEM). The 17.1 dpa BOR-60 irradiated microstructure was then compared with the microstructure of the same material developed under dual-ion (DI) irradiation using various He/dpa ratios between 0.1 and 16.6 appm He/dpa in the temperature range of 430°C-500°C. The results showed that both neutron and DI irradiation of 21Cr32Ni model alloy produced dislocations in the form of a dislocation network as well as {111}-type faulted dislocation loops, cavities, and radiation-induced Ni enrichment at radiation-induced sinks. When the dose and the He/dpa ratio were kept similar to those in neutron irradiation, DI irradiation of the 21Cr32Ni model alloy at 460°C resulted in over-nucleation of small cavities and in a high density of faulted dislocation loops compared to those observed in the fast-neutron irradiated alloy of the same heat irradiated at ~380°C. The optimal condition for reproducing the neutron-irradiated microstructure was DI irradiation at 460°C and 0.1 appm He/dpa. In that case, the faulted loop and cavity size distributions in the BOR-60 irradiated 21Cr32Ni model alloy samples closely matched with those measured in the DI irradiated 21Cr32Ni model alloy sample. The fact that the He/dpa is an order of magnitude smaller than the helium generation rate for fast neutron irradiation, stops over nucleation and allows for the development of a similar microstructure as for neutron irradiation.

21Cr32Ni model alloy↗

Structural Characterization of Lateral-grown 6H-SiC am-plane Seed Crystals by Hot Wall CVD Epitaxy

The performance of commercially available silicon carbide (SiC) power devices is limited due to inherently high density of screw dislocations (SD), which are necessary for maintaining polytype during boule growth and commercially viable growth rates. The NASA Glenn Research Center (GRC) has recently proposed a new bulk growth process based on axial fiber growth (parallel to the c-axis) followed by lateral expansion (perpendicular to the c-axis) for producing multi-faceted m-plane SiC boules that can potentially produce wafers with as few as one SD per wafer. In order to implement this novel growth technique, the lateral homoepitaxial growth expansion of a SiC fiber without introducing a significant number of additional defects is critical. Lateral expansion is being investigated by hot wall chemical vapor deposition (HWCVD) growth of 6H-SiC am-plane seed crystals (0.8mm x 0.5mm x 15mm) designed to replicate axially grown SiC single crystal fibers. The post-growth crystals exhibit hexagonal morphology with approximately 1500 m (1.5 mm) of total lateral expansion. Preliminary analysis by synchrotron white beam x-ray topography (SWBXT) confirms that the growth was homoepitaxial, matching the polytype of the respective underlying region of the seed crystal. Axial and transverse sections from the as grown crystal samples were characterized in detail by a combination of SWBXT, transmission electron microscopy (TEM) and Raman spectroscopy to map defect types and distribution. X-ray diffraction analysis indicates the seed crystal contained stacking disorders and this appears to have been reproduced in the lateral growth sections. Analysis of the relative intensity for folded transverse acoustic (FTA) and optical (FTO) modes on the Raman spectra indicate the existence of stacking faults. Further, the density of stacking faults is higher in the seed than in the grown crystal. Bundles of dislocations are observed propagating from the seed in m-axis lateral directions. Contrast extinction analysis of these dislocation lines reveals they are edge type basal plane dislocations that track the growth direction. Polytype phase transition and stacking faults were observed by high-resolution TEM (HRTEM), in agreement with SWBXT and Raman scattering.

Single Crystal↗

Microstructure Evolution during Cold Rolling in a Nanocrystalline Ni-Fe Alloy Determined by Synchrotron X-ray Diffraction

Stress softening after cold rolling is observed in an electrodeposited nanocrystalline Ni-Fe alloy. The grain-size distribution becomes much broader after the cold rolling. Microstructure changes, though moderate, such as simultaneously decreased dislocation and twin densities with grain growth during cold rolling, are systematically proved by synchrotron high-energy X-ray diffraction, and transmission-electron microscopy and differential-scanning calorimetry (DSC). The amorphous fractions in the form of grain boundaries are evidenced by the diffuse-background scatterings and large DSC values. Partial dislocation separation calculation, a dislocation mean free path and annihilation model, and texture development together reveal that the current nanocrystalline Ni-Fe alloy exhibits the combined behavior of perfect dislocation slip and grain-boundary mediated deformation.

43 PARTICLE ACCELERATORS↗

The potential for ductility enhancement from surface and interface dislocation sources in NiAl

Limited ductility and toughness of NiAl and related aluminides near room temperature pose major problems in their potential application as structural materials. An analysis of these problems is presented as part of a review of the flow and fracture behavior of binary NiAl. Following this discussion is a demonstration that conditions of elastic and plastic constraint associated with phase boundaries afforded by surface films, internal lamellae, or precipitates may introduce sufficient densities of mobile dislocations to enhance the ductility of NiAl-based materials by significant amounts. Examples of this behavior are presented for several model materials, including 001- and 123-oriented single crystals of oxide-coated NiAl, directionally solidified beta-gamma-prime (Ni70Al30) and beta-gamma (Ni50Fe30Al20) in situ composites, and several NiAl/precipitate systems. The nature of the resulting dislocation substructures and the effects of several materials variables are described.

Noebe, R. D.↗