Search NASA⌕ Search

SEARCH · Search NASA

Results for “electron backscattered diffraction”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,135 records · Page 63

The influence of power spinning and annealing temperature on microstructures and properties of Cu-Sn alloy

Highlights: • The strengthening effect of power spinning is mainly achieved by strengthening fine grains and dislocations. • Twins formed by the aggregation and overlapping of stacking faults grow and widen • In power spinning of Cu-Sn alloy, plastic deformation is primarily powered by dislocation sliding. - Abstract: Electron back scatter diffraction pattern (EBSD), metallographic microscope (OM) and transmission electron microscope (TEM) are used to analyze the microstructural state of the Cu-Sn alloy before and after power spinning and annealing. The results show that after power spinning, the α phase grains are refined and gradually evolve into small and fine α{sub II} and deformed α{sub III} crystal grains, with an average grain size of about 2.2 μm. Work hardening results in massive network-like subgrain boundaries distributed in power spinning microstructure. Annealing at 400 °C contributes to the formation of dislocation cells and stacking faults, and high-angle grain boundaries (HABS) start to migrate and slide. After the formation of less defective equiaxed grains at 500 °C, twins continue to grow and widen based through continuous accumulation of stacking faults. Further testing of mechanical properties reveals that power spinning is conducive to the improvement of mechanical properties of Cu-Sn alloy.

36 MATERIALS SCIENCE↗

Structure and properties of solid surfaces

Difficulties in experimental studies of crystalline surfaces are related to the fact that surface atoms have an intrinsic tendency to react with their environment. A second problem is connected with the effective thickness of surfaces, which ranges from one to several atom layers. The phenomenology of surface interactions with gases are considered, taking into account physical adsorption, chemisorption, and the oxidation of surfaces. Studies of the surface structure are discussed, giving attention to field emission microscopy, field-ion microscopy, electron diffraction techniques, Auger spectroscopy, scanning electron microscopy, electron probe microanalysis, ion microprobe methods, and low-energy backscattering spectroscopy. Investigations of semiconductor surfaces are also described.

Gatos, H. C.↗

Epitaxial growth of rock salt MgZrN 2 semiconductors on MgO and GaN

Ternary nitride compound semiconductors have attracted recent attention as electronic materials since their properties can be tuned by cation stoichiometry and ordering. A recently discovered example is MgZrN 2 , a ternary analog to the rock salt semiconductor ScN. MgZrN 2 has a larger bandgap and stronger dielectric response than the binary compound. Polycrystalline thin films of MgZrN 2 have been studied, but demonstration of high-quality growth is still required to establish its suitability for technological applications. Here, we report on epitaxial growth of MgZrN 2 thin films on (100) and (111) MgO substrates and (001) GaN templates. The MgZrN 2 composition is confirmed by Rutherford backscattering spectrometry, showing no oxygen in the film except for a thin surface oxide layer. Epitaxial growth results in MgZrN 2 with x-ray diffraction rocking curves with a full-width at half-maximum in the range of 0.3–3.0°, depending on the substrate. Transmission electron microscopy analysis of the MgZrN 2 film grown on a (111) MgO substrate confirms epitaxial growth and shows a sharp film/substrate interface. In-plane temperature-dependent Hall effect measurements show that the material is an n-type semiconductor with a relatively high concentration ( n 300K ≈ 10 19 –10 20 cm -3 ) of thermally activated electrons. Room-temperature transport measurements show a conductivity of 25 S cm -1 and a Seebeck coefficient of -80 μ V K -1 . Overall, these results provide an important step toward integration of rock salt MgZrN 2 with other technological nitrides for device applications.

36 MATERIALS SCIENCE↗

Simulation Kinetics of Austenitic Phase Transformation in Ti+Nb Stabilized IF and Microalloyed Steels

In the present study, the influence of cooling rates (low to ultrafast) on diffusion controlled and displacive transformation of Ti-Nb IF and microalloyed steels has been thoroughly investigated. Mechanisms of nucleation and formation of non-equiaxed ferrite morphologies (i.e., acicular ferrite and bainitic ferrite) have been analyzed in details. The continuous cooling transformation behavior has been studied in a thermomechanical simulator (Gleeble 3800) using the cooling rates of 1-150 °C/s. On the basis of the dilatometric analysis of each cooling rate, continuous cooling transformation (CCT) diagrams have been constructed for both the steels to correlate the microstructural features at each cooling rate in different critical zones. In the case of the IF steel, massive ferrite grains along with granular bainite structures have been developed at cooling rates > 120 °C/s. On the other hand, a mixture of lath bainitic and lath martensite structures has been formed at a cooling rate of ~ 80 °C/s in the microalloyed steel. A strong dependence of the cooling rates and C content on the microstructures and mechanical properties has been established. The steel samples that were fast cooled to a mixture of bainite ferrite and martensite showed a significant improvement of impact toughness and hardness (157 J, for IF steel and 174 J for microalloyed steel) as compared to that of the as-received specimens (133 J for IF steel and 116 J for microalloyed steel). Thus, it can be concluded that the hardness and impact toughness properties are correlated well with the microstructural constituents as indicated by the CCT diagram. Transformation mechanisms and kinetics of austenitic transformation to different phase morphologies at various cooling rates have been discussed in details to correlate microstructural evolution and mechanical properties.

36 MATERIALS SCIENCE↗

Expanding the Zinc Precursor Toolbox: A Comparative Study of Precursors for Thermal ALD of ZnO Thin Films

Atomic layer deposition (ALD) of zinc oxide (ZnO) has been widely researched using diethyl zinc (DEZ)-based methods. The significant importance of thin films of ZnO as transparent conductive oxides (TCO) in optoelectronic devices and photovoltaics warrants examining alternative Zn precursors for ZnO ALD as potential replacements for the pyrophoric DEZ. In this study, we investigated three alternative Zn precursors: Zn(EEKI)2, Zn(DMP)2, ZnEt(HMDS), in the process development for high-quality ZnO thin films and compared them to DEZ. The ALD processes were studied using in situ spectroscopic ellipsometry. The properties of the ALD ZnO films were characterized using ex situ X-ray photoelectron spectroscopy (XPS), Rutherford backscattering spectrometry and nuclear reaction analysis (RBS/NRA), X-ray diffraction (XRD), atomic force microscopy (AFM), transmission electron microscopy (TEM), and ultraviolet-visible (UV/Vis) spectrophotometry. These measurements confirmed the formation of pure, stoichiometric, and polycrystalline ZnO films using all four Zn precursors. Although the selected precursors are chemically diverse Zn compounds, they all yielded saturating ALD processes and high-quality ZnO thin films at 200 °C. This study highlights the potential benefits of alternative zinc precursors in designing ALD processes for ZnO thin films.

Obenlüneschloß, Jorit↗

Dopant activation in ion implanted silicon by microwave annealing

Microwaves are used as a processing alternative for the electrical activation of ion implanted dopants and the repair of ion implant damage within silicon. Rutherford backscattering spectra demonstrate that microwave heating reduces the damage resulting from ion implantation of boron or arsenic into silicon. Cross-section transmission electron microscopy and selective area electron diffraction patterns demonstrate that the silicon lattice regains nearly all of its crystallinity after microwave processing of arsenic implanted silicon. Sheet resistance readings indicate the time required for boron or arsenic electrical activation within implanted silicon. Hall measurements demonstrate the extent of dopant activation after microwave heating of implanted silicon. Physical and electrical characterization determined that the mechanism of recrystallization in arsenic implanted silicon is solid phase epitaxial regrowth. The boron implanted silicon samples did not result in enough lattice damage to amorphize the silicon lattice and resulted in low boron activation during microwave annealing even though recrystallization of the Si lattice damage did take place. Despite low boron activation levels, the level of boron activation in this work was higher than that expected from traditional annealing techniques. The kinetics of microwave heating and its effects on implanted Si are also discussed.

36 MATERIALS SCIENCE↗

Crystal defects and related stress in Y{sub 2}O{sub 3} thin films: Origin, modeling, and consequence on the stability of the C-type structure

We study the impact that the crystal defects have on the C-type structure of rare earth sesquioxide thin films grown by ion-beam sputtering, through the example of Y{sub 2}O{sub 3}. By monitoring the energy of the argon beam used in the sputter deposition process (between 600 and 1200 eV), we show that it is possible to control the microstructure (defects concentration, stress state and phase) in the oxide layer. Two main types of defects, ascribed to the 'atomic peening effect', are evidenced by high-resolution transmission electron microscopy, Rutherford backscattering spectroscopy, and nuclear reaction analysis experiments: anti-Frenkel pairs, leading to a disorder on the oxygen-vacancy network, and oxygen-vacancy dislocations loops, to accommodate the strong nonstoichiometry. From a macroscopic measurement of the residual stresses in the as-deposited and the annealed layers, through x-ray diffraction and the sin{sup 2}{Psi} method, we have modeled the related stress state using an enhanced triaxial stress model. In the as-grown films, we evidence the coexistence of a biaxial and a hydrostatic stress, due to inclusions of atomic size defects. Quantitative information of the concentration and the nature of each type of defect (size effect) have also been determined, in good agreement with experiments. Interestingly, in the most energetic growth conditions corresponding to the highest degree of disorder on the oxygen-vacancy network and to the highest stress field in the film, we demonstrate that it is possible to stabilize an unexpected and metastable non equilibrium fluorite-like phase (X-type).

36 MATERIALS SCIENCE↗

Variation of lattice constant and cluster formation in GaAsBi

We investigate the structural properties of GaAsBi layers grown by molecular beam epitaxy on GaAs at substrate temperatures between 220–315 °C. Irrespective of the growth temperature, the structures exhibited similar Bi compositions, and good overall crystal quality as deduced from X-Ray diffraction measurements. After thermal annealing at temperatures as low as 500 °C, the GaAsBi layers grown at the lowest temperatures exhibited a significant reduction of the lattice constant. The lattice variation was significantly larger for Bi-containing samples than for Bi-free low-temperature GaAs samples grown as a reference. Rutherford backscattering spectrometry gave no evidence of Bi diffusing out of the layer during annealing. However, dark-field and Z-contrast transmission electron microscopy analyses revealed the formation of GaAsBi clusters with a Bi content higher than in the surrounding matrix, as well as the presence of metallic As clusters. The apparent reduction of the lattice constant can be explained by a two-fold process: the diffusion of the excess As incorporated within As{sub Ga} antisites to As clusters, and the reduction of the Bi content in the GaAs matrix due to diffusion of Bi to GaAsBi clusters. Diffusion of both As and Bi are believed to be assisted by the native point defects, which are present in the low-temperature as-grown material.

36 MATERIALS SCIENCE↗

Growth of ordered silver nanoparticles in silica film mesostructured with a triblock copolymer PEO-PPO-PEO

Elaboration of mesostructured silica films with a triblock copolymer polyethylene oxide-polypropylene oxide-polyethylene oxide, (PEO-PPO-PEO) and controlled growth of silver nanoparticles in the mesostructure are described. The films are characterized using UV-visible optical absorption spectroscopy, TEM, AFM, SEM, X-ray diffraction (XRD) and Rutherford backscattering spectrometry (RBS). Organized arrays of spherical silver nanoparticles with diameter between 5 and 8 nm have been obtained by NaBH{sub 4} reduction. The size and the repartition of silver nanoparticles are controlled by the film mesostructure. The localization of silver nanoparticles exclusively in the upper-side part of the silica-block copolymer film is evidenced by RBS experiment. On the other hand, by using a thermal method, 40 nm long silver sticks can be obtained, by diffusion and coalescence of spherical particles in the silica-block copolymer layer. In this case, migration of silver particles toward the glass substrate-film interface is shown by the RBS experiment. - Graphical abstract: Growth of silver nanoparticles in a mesostructured block copolymer F127-silica film is performed either by a chemical route involving NaBH{sub 4} reduction or by a thermal method. An array of spherical silver nanoparticles with 10 nm diameter on the upper-side of the mesostructured film or silver sticks long of 40 nm with a preferential orientation are obtained according to the method used. a: TEM image of the Fag5SiNB sample illustrating the silver nanoparticles array obtained by the chemical process; b: HR-TEM image of the Fag20Sid2 sample illustrating the silver nanosticks obtained by the thermal process.

36 MATERIALS SCIENCE↗

Evaluation of the interface of thin GaN layers on c- and m-plane ZnO substrates by Rutherford backscattering

Lattice distortion at the interfaces between thin GaN layers with {approx}400 nm in thickness and ZnO substrates with non-polar m-plane (10-10) and polar c-plane (0001) is studied using Rutherford backscattering/ion channeling techniques. The interface between GaN/m-plane ZnO is aligned clearly to m-axis, indicating no lattice distortion, while between GaN/c-plane ZnO causes the lattice distortion in the GaN layer due to the piezoelectric field. The range of distortion exceeds {approx}90 nm from the interface of GaN/c-plane ZnO. These results are confirmed by x-ray diffraction and reflection high energy electron diffraction studies.

36 MATERIALS SCIENCE↗

Electron back scattered diffraction characterization of Sm(CoFeCuZr){sub z} magnets

In permanent magnets based on the Sm{sub 2}Co{sub 17} phase, the high coercivity depends on the presence of a complex microstructure, consisting of a Sm{sub 2}(Co,Fe){sub 17} cell phase, a cell boundary phase Sm(Co,Cu){sub 5}, and a Zr-rich platelet or lamellae phase. The aim of this work is to use electron back scatter diffraction (EBSD) in order to identify the different phases present in the isotropic magnets produced from cast alloys with the composition of Sm(Co{sub bal}Fe{sub 0.2}Cu{sub 0.1}Zr{sub x}){sub 8}, where x = 0, 0.02, or 0.06, and correlate them with the different phases observed in scanning electron microscopy (SEM) images. Due to the combination of careful surface preparation and high resolution microscopy, it was possible to observe the cellular structure characteristic of the 2:17 magnets in the SEM images. Until now, only transmission electron microscopy (TEM) had been used. Composition maps, energy dispersive spectroscopy (EDS), and EBSD measurements were used for doing the phase identification.

36 MATERIALS SCIENCE↗

Particle stimulated nucleation during dynamic and metadynamic recrystallisation of Ni-30%Fe-Nb-C alloy

For the first time, a combination of scanning transmission electron microscopy and electron back-scattering diffraction is used to elucidate the early stages of particle stimulated recrystallisation at Nb carbides in Ni-30wt.%Fe alloy subjected to high temperature plane strain compression. While particles with sizes even below 1 μm were found to induce dynamic or metadynamic recrystallisation, only a small fraction of coarse particles served as nucleation sites. - Highlights: • The early stages of particle stimulated recrystallisation at Nb carbides are elucidated • A combination of transmission electron microscopy and electron back scattering diffraction used • Particles below 1 μm size could induce dynamic or metadynamic recrystallization.

36 MATERIALS SCIENCE↗

Influence of Thermomechanically Controlled Processing on Microstructure and Hydrogen Induced Cracking Susceptibility of API 5L X70 Pipeline Steel

The effect of different thermomechanical controlled processing routes on susceptibility of X70 pipeline steel to hydrogen induced cracking (HIC) have been studied. Two X70 pipeline steel specimens labelled WE and WD were investigated. These specimens have the same chemical composition, but they were processed with seperate thermomechanical treatments parameters. Microstructural examinations showed that WE consists of mainly acicular ferrite and polygonal ferrite, while WD consists of acicular ferrite and bainitic ferrite. After subjecting both specimens to hydrogen charging for 12 and 16 h in 0.2 M sulfuric acid and 3 g/L ammonium thiocyanate, early onset of HIC was observed in specimen WD. Post-hydrogen charging microstructural evaluation showed the nucleation of discontinuous cracks in WD after 12 h of charging. However, extended charging for up to 16 h resulted in HIC along the mid-thickness region of both specimens. Hydrogen diffusion across specimen WE was better than that of specimen WD. Therefore, hydrogen trapping at grain boundaries, banded deformed grains, inclusions and secondary phases such as martensite and cementite aided initiation and propagation of HIC in specimens. Nevertheless, the adverse effect of these features on HIC risks was more prominent in specimen WD compared to specimen WE. The Vickers microhardness values measured in WD (349.6 HV) and WE (307.4 HV) suggest that WD is harder than WE; and higher kernel average misorientation of 0.66° in WD than in WE (0.58°) shows higher dislocation density in WD. The results from slow strain rate tensile test confirmed that specimen WD was stronger and more susceptible to HIC than specimen WE. It was concluded that microstructural phases developed during thermomechanical processing improved strength in WD at the expense of its crack resistance, while WE with lower strength showed more ductility and higher resistance to HIC.

36 MATERIALS SCIENCE↗

Mechanical Properties of Laser Heat Treated 6 mm Thick UHSS-Steel

In this work abrasion resistant (AR) steel with a sheet thickness of 6 mm was heat treated by a 4 kW Nd:YAG and a 4 kW Yb:Yag-laser, followed by self-quenching. In the delivered condition, test material blank (B27S) is water quenched from 920 deg. C. In this condition, fully martensitic microstructure provides excellent hardness of over 500 HB. The test material is referred to AR500 from now onwards. Laser heat treatment was carried out only on top surface of the AR500 sheet: the achieved maximum temperature in the cross-section varies as a function of the depth. Consequently, the microstructure and mechanical properties differ between the surfaces and the centre of the cross-section (layered microstructure). For better understanding, all layers were tested in tensile tests. For a wide heat treatment track, the laser beam was moved by scanning. Temperatures were measured using thermographic camera and thermocouples. Laser heat treated AR500 samples were tested in hardness tests and by air bending using a press brake machine. Microstructures were studied using a light microscope and FE-SEM/SEM-EBSD. At least three kind of microstructure layers were observed: 1) Dual-Phase ferritic/martensitic (T = A{sub C1}-A{sub C3}), 2) ferritic (T{approx}A{sub C3}) and 3) bainitic/martensitic (T>A{sub C3}).

36 MATERIALS SCIENCE↗

Epitaxial growth of high purity cubic InN films on MgO substrates using HfN buffer layers by pulsed laser deposition

Cubic InN films have been grown on MgO substrates with HfN buffer layers by pulsed laser deposition (PLD). It has been found that the use of HfN (100) buffer layers allows us to grow cubic InN (100) films with an in-plane epitaxial relationship of [001]{sub InN}//[001]{sub HfN}//[001]{sub MgO}. X-ray diffraction and electron back-scattered diffraction measurements have revealed that the phase purity of the cubic InN films was as high as 99%, which can be attributed to the use of HfN buffer layers and the enhanced surface migration of the film precursors by the use of PLD. - Graphical abstract: Cubic InN films have been grown on MgO substrates with HfN buffer layers by pulsed laser deposition (PLD). It has been revealed that the phase purity of the cubic InN films was as high as 99 %, which can be attributed to the use of HfN buffer layers and the enhanced surface migration of the film precursors by the use of PLD.

36 MATERIALS SCIENCE↗

Characterization of high-temperature mechanical properties of plasma-cladded coatings with thermo-mechanical coupling

High temperature mechanical properties was detected here to study the failure and strengthening mechanism of the coating-substrate (cobalt-based coatings were fabricated on FV520B substrate) integral structure with thermo-mechanical coupling effects. Microstructure, phase composition, element distribution of the coatings was characterized by optical microscopy (OM), scanning electron microscopy (SEM), transmission electron microscope (TEM), electron back scattering diffraction (EBSD), X-ray diffraction (XRD), electron probe microanalysis (EPMA) and energy dispersive X-ray analysis (EDS). Results elucidate that fracture occurs in the coating for Co50 coating-substrate structure from 300 °C to 700 °C, but failure position transfer to substrate from coating at elevated temperatures with the addition of niobium and cerium oxide. Throughout, there is no crack originated from the interface. Fracture mechanism: the dislocation pile-up causes great stress concentration in the grain boundary, which results in the nucleation of the crack, and then the crack extends along the hard brittle Fe-Cr phase until the material fails. HRTEM shows the high density dislocation and the severe lattice distortion was formed during tensile deformation. On the macro level, the fracture tends to occur in the coarse dendrites region.

36 MATERIALS SCIENCE↗

In-situ stoichiometry determination using x-ray fluorescence generated by reflection-high-energy-electron-diffraction

A major challenge in the stoichiometric growth of complex oxide compounds is the control of the relative compositions of the constituent materials. A potential avenue for compositional analysis during growth is the use of x-ray fluorescence generated during reflection high energy electron diffraction measurements. Using this technique, relative compositions of Y and Mn in molecular beam epitaxy grown YMnO{sub 3} samples were studied. Comparing the results with Rutherford back scattering spectroscopy suggests that the technique has the potential for real-time analysis of elemental fluxes and stoichiometry control during sample growth.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

X-ray Diffraction Spectra in Cu-Implanted SiO{sub 2} Films on Si(100) Substrates

Cu-implanted SiO{sub 2} films on Si(100) have been studied using x-ray methods and x-ray diffraction pattern processing. The x-ray results indicate the presence of a preferred orientation for Cu {l_brace}111{r_brace} planes parallel to the substrate surface without directional orientation for Cu-implanted SiO{sub 2}/Si(100) and nano-crystalline-Cu/SiO{sub 2}/Si(100)(ie. after implanted and annealed Cu). The x-ray diffraction spectra of the Cu-implanted and nano-crystalline-Cu phases were analyzed (ie. in terms of peak search, profile fit, crystallite size) and compared to data from complimentary techniques (RBS, TEM). Results are discussed with respect to x-ray spectral lines shapes derived from XRD spectra processing and the nanostructure problem.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗