Search NASA⌕ Search

SEARCH · Search NASA

Results for “surface characterization”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,135 records · Page 63

Reactivity of Au nanoparticles supported over SiO2 and TiO2 studiedby ambient pressure photoelectron spectroscopy

The influence of the metal cluster size and the identity of the support on the reactivity of gold based catalysts have been studied in the CO oxidation reaction. To overcome the structural complexity of the supported catalysts, gold nanoparticles synthesized from colloidal chemistry with precisely controlled size have been used. Those particles were supported over SiO{sub 2} and TiO{sub 2} and their catalytic activity was measured in a flow reactor. The reaction rate was dependent on the particle size and the support, suggesting two reaction pathways in the CO oxidation reaction. In parallel, ambient pressure photoelectron spectroscopy (APPS) has been performed under reaction conditions using bidimensional model catalysts prepared upon supporting the Au nanoparticles over planar polycrystalline SiO{sub 2} and TiO{sub 2} thin films by means of the Langmuir-Blodgett (LB) technique to mimic the characteristic of the powder samples. In this way, the catalytically active surface was characterized under true reaction conditions, revealing that during CO oxidation gold remains in the metallic state.

36 MATERIALS SCIENCE↗

Remarkable self-degradation of Cu/SAPO-34 selective catalytic reduction catalysts during storage at ambient conditions

A model Cu/SAPO-34 SCR catalyst with all Cu species maintained as isolated Cu(II) ions is synthesized herein. Following lengthy storage on the shelf under ambient conditions, this catalyst completely and irreversibly deactivates upon any heat treatments above ~100 °C. Via detailed characterizations with surface area/pore volume analysis, XRD, H 2 -TPR, and 27 Al, 29 Si and 31 P solid-state NMR, as well as continuous wave and pulsed EPR studies, it is concluded that over the course of storage, the SCR active sites [Cu(OH)] + and Brønsted acid sites ≡Si-O(H)-Al≡ are attacked by H 2 O molecules trapped in the SAPO-34 framework pores, and undergo hydrolysis to form copper hydroxide and terminal Al sites. Upon thermal treatment, these species interact with each other to form copper-aluminate-like species, leading to irreversible deactivation of this catalyst. This deactivation mechanism does not require or necessarily lead to extensive degradation (i.e., crystallinity loss) of the SAPO-34 support.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effect of PCEs with different structures on hydration and properties of cementitious materials with low water-to-binder ratio

Polycarboxylate ethers (PCEs) with different structures and densities of anchor groups in the backbone were synthesized and characterized. The surface tension of their solutions, their adsorption on cementitious particles and zeta potential of cement-silica fume pastes with PCEs were measured. Their effects on hydration and properties of cement-silica fume paste with low water-to-binder ratio were examined. Results indicated that the adsorption kinetics of theses PCEs on cementitious particles are fitted the pseudo-second-order model. The introduction of long silane chain on PCE decreased its electrostatic adsorption, while PCE was adsorbed onto the surface of particles via both chemical and electrostatic adsorption, when silicon hydroxyl is directly connected to its backbone. In the presence of PCE with higher adsorbed amount, pastes exhibited lower yield stress and higher flowability, and higher strength at 7 d and 28 d. The low plastic viscosity, autogenous and drying shrinkage were related to the low surface tension of PCE solution.

36 MATERIALS SCIENCE↗

Evaluation of HCF strength of Alloy 625 with non-optimum additive manufacturing process parameters

An extensive experimental program was undertaken to generate the process-structure-HCF property data for additive-manufactured Alloy 625. Round tensile and flat dog-bone HCF specimens were fabricated using a laser powder bed fusion process. Several builds were fabricated with different processing parameters. The fatigue strengths were determined using a step-test method and fracture surfaces were characterized to identify the critical microstructure feature associated with the formation of the fatigue crack. Finally, a fracture mechanics-based methodology using fatigue crack growth data measured on a wrought alloy is shown to provide conservative estimates of the HCF lives for the additive-manufactured alloy.

36 MATERIALS SCIENCE↗

Bulk single crystal growth and sample surface preparation of catalytic NaAu 2

Here in we have grown bulk single crystals of NaAu 2 for the first time to enable surface studies on the nature of the (111) bulk surface. This intermetallic compound exhibits surprisingly high catalytic activity for CO oxidation, a benchmark reaction. Theory predicts NaAu 2 to be the most thermodynamically stable composition in the Na-Au binary phase diagram and NaAu 2 has been seen to preferentially form in experiments containing Na and Au which supports this prediction. The (111) surface was also predicted to be the most stable and is nearly bulk-terminated making single crystal samples prepared with this crystallographic orientation a fitting choice. As a result, the crystal quality and surface composition of the metallographically prepared surface was determined by x-ray diffraction methods in addition to optical and electron microscopy.

(111) catalytic surface↗

Effect of high temperature preoxidation treatment on the oxidation behavior of MoSi 2 - and WSi 2 –Al 2 O 3 composites

Composites of 30 vol% MoSi 2 -70 vol% Al 2 O 3 and 30 vol% WSi 2 -70 vol% Al 2 O 3 were prepared via sintering at 1600 °C in argon. The high-temperature preoxidation treatments were applied at 1000°-1200 °C for 10–120 min in air. The non-isothermal oxidation tests were conducted in air at temperatures ranging between 50° and 870 °C to study and understand the influence of the alumina phase and preoxidation process on the low-temperature oxidation behavior. The optical and scanning electron microscopy, X-ray diffraction, X-ray photoelectron and Raman spectroscopy were used to characterize the surface layers formed. The oxidation-induced mass gains were substantially reduced by 82.1–99.8%, implying their enhanced oxidation resistance. This was due to the formation of highly dense, protective surface layers with a sufficient thickness (3.1–14.2 μm). The structural and surface analyses revealed their complex chemistries, since the ternary (Mo–Si–Al, W–Si–Al) intermetallic, mullite, alumina and silica phases with high oxidation resistances were identified within these surface features. In addition, the high-temperature electrical properties of the composites were highly preserved after the preoxidation treatment, and their electrical conductivities were measured as 45.1–78.6 S/cm at 800 °C and 40.1–69.1 S/cm at 900 °C.

36 MATERIALS SCIENCE↗

Oxide structure of air-passivated U-6Nb alloy thin films

U-6Nb is a uranium alloy containing 6 wt% niobium that possesses high corrosion resistance. The structure and composition of the passivating oxide layer formed on air-aged U-6Nb, which gives the material its corrosion resistant properties, was characterized using surface scattering techniques. Stable oxide layers formed on the surface of a set of U-6Nb alloy thin films under ambient conditions were investigated using neutron reflectometry (NR), x-ray reflectometry (XRR) and grazing incidence x-ray diffraction (GIXD). The passivating oxide was composed of approximately 27% U, 5% Nb, and 68% O, primarily consisting of a thin niobium oxide layer (5.5 ± 0.4 nm) separating a thicker UO2 layer (27.1 ± 2.3 nm) from the underlying U-6Nb alloy. A critical density of enriched niobium oxide at the metal-oxide interface is hypothesized to limit oxygen diffusion and confer high corrosion resistance to the alloy.

36 MATERIALS SCIENCE↗

Characterization of modeling and experimental data inconsistencies from burst testing for high-burnup commercial fuel rod applications

Fuel fragmentation, relocation, and dispersal are some of the largest issues remaining in the nuclear industry before rod-average burnup can be increased beyond 62 GWd/tU. The issue is primarily related to the potential for fuel to be dispersed into the reactor primary system, which may increase public risk. One way to prevent dispersal is to avoid cladding burst. The objective of this work is to support the high burnup safety case by evaluating cladding burst under high-burnup, full-length fuel rods and to identify uncertainties that could improve model predictions. The results of this analysis will evaluate realistic, prototypic loss-of-coolant accident (LOCA) conditions; support future cladding burst test designs; and inform the development of mechanistic material models. Realistic high-burnup operating conditions were implemented in the BISON fuel performance code to simulate steady-state and LOCA transient fuel rod evolution to the point at which cladding burst occurred. Parametric studies are performed to assess code response to changes in rod internal pressures and heating rates. Results were compared with simulated LOCA experiments to identify inconsistencies between commercial fuel rod analysis and experimental validation. The representative full-length fuel rod LOCA simulation results did not agree with cladding burst tests. Cladding burst tests indicated burst occurring well below (100–150 °C) those calculated in the full-length fuel rod LOCA analysis. Further investigation indicated that the cladding burst tests do not appear to be representative for full-length fuel rods. The inconsistency investigated in this work showed that the differences between the BISON simulation and the experiment's cladding burst conditions arise from an incomplete characterization of the cladding surface temperature, detailed rodlet characterization, lack of cladding strain measurements, and uncertainty in the cladding creep and failure models.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Impact of corrosion layer composition and thermal pretreatment on the radiolytic generation of molecular hydrogen from aluminum alloys

To fully evaluate the feasibility of extending the dry storage of aluminum-clad spent nuclear fuel (ASNF) in helium-backfilled cannisters, the amount of radiation-induced molecular hydrogen (H 2 ) generated and the impact of absorbed radiation dose on the ASNF corrosion layer composition must be accurately assessed. Here, in this study, we report a slowing in the rate of radiolytic H 2 generation for pre-corroded AA1100 and AA6061 aluminum alloy coupons irradiated to up to 53 MGy of absorbed cobalt-60 gamma dose. By exploring a variety of thermal pretreatment conditions for AA6061 coupons, we find that the “steady-state” yield of H 2 depends more on the aluminum alloy used than on the treatments applied prior to dry storage. Scanning electron microscopy and positron annihilation lifetime spectroscopy techniques also provided evidence for gamma radiation-induced defects in the corrosion layers of the investigated aluminum alloy coupons for high absorbed doses (~50 MGy), the consequences of which on cladding integrity and H 2 generation should be explored in future works.

38 - RADIATION CHEMISTRY, RADIOCHEMISTRY, AND NUCL↗

Plasma exposures of a high-conductivity graphitic foam for plasma facing components

The plasma-surface interactions from samples of high-conductivity graphitic foam biased to 120 V and placed in 6–8 eV deuterium plasmas with densities as high as 10 19 m -3 were investigated at the PSI-2 linear plasma device in Jülich. Graphitic foam-plasma interactions were also studied at the Wendelstein 7-X (W7-X) stellarator in Greifswald by exposure to hydrogen and helium plasmas using the Jülich multi-purpose manipulator. The purpose was to explore the possibility of using the material in a plasma facing component, and initial results were encouraging. In W7-X, no measurable erosion or cracking was observed. The PSI-2 samples received a deuterium fluence of 5 × 10 25 m -2 resulting in an average erosion of 43 µm or about 5 mg per sample. Residual gas analysis (RGA) data were acquired to monitor sample outgassing. Laser-induced Breakdown Spectroscopy (LIBS) was used to measure deuterium retention in the porous foam. After exposure, the surfaces were characterized with scanning electron microscopy, energy dispersive x-ray analysis and time-of-flight secondary ion mass spectrometry (ToF-SIMS). The graphitic foam has a thermal conductivity as high as 287 W/mK and is considered as a replacement to more exotic carbon fiber composites such as SepCarb NB31 or isotropic graphites like ATJ that are no longer produced but used in present-day tokamak experiments. Actively cooled monoblocks were made from the foam and underwent extensive materials characterization including infrared response studies at Oak Ridge National Laboratory. This material is under consideration for the proposed actively-cooled W7-X divertor scraper element.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Framework for Predicting the Photodegradation of Adhesion of Silicone Encapsulants

We developed a framework to predict and model the photodegradation of adhesion and cohesion of a silicone encapsulant for concentrator photovoltaic applications. Silicone encapsulant specimens were artificially weathered under narrow band UV filters to determine the effects of individual wavelengths within the UV spectrum on the photodegradation of the cohesion of encapsulant material and its adhesion with adjacent interfaces. The threshold wavelength, signifying the upper bound of the damaging action spectrum for the silicone, was identified from the results. In addition, specimens were artificially weathered with different relative humidities to understand the effects of moisture on the rate of photodegradation. The adhesion energy was measured using a fracture mechanics approach. The complementary delaminated surfaces were characterized to determine the failure pathway and chemistry changes resulting from photodegradation. A previously developed model was modified to account for the effects of damaging wavelengths in the terrestrial solar spectrum and reciprocity law failure due to varying UV intensity during weathering. With these modifications, the model showed good agreement with the behavior of the silicone encapsulant exposed in an outdoor solar concentrator simulating concentrator photovoltaics operating conditions. Similar studies can be adopted to develop models that can have high predictive accuracies based on accelerated aging studies.

14 SOLAR ENERGY↗

The effect of current and lambda on white-etch-crack failures

White etching cracks (WECs) have been associated with premature failure of wind turbine roller bearings. Various drivers for the generation of WECs have been identified such as loading conditions, slip, steel quality, lubrication, hydrogen embrittlement, corrosion fatigue cracking, and stray electrical currents passing through the surface. Here, in this work, a benchtop test rig utilizing a three-ring-on-roller test configuration was used to investigate the effect of electrical current and operation in different lubricating regimes, defined by lambda (λ), on high-quality bearing steel samples tested in a commercially available power transmission EP gear lubricant. It was observed that there is an inverse correlation between the magnitude of electric current applied to the ring/ roller system and time-to-failure. Higher current magnitudes lead to shorter time-to-failure than lower current magnitudes, with macropitting as the main failure mode. Sub-surface investigation revealed the presence of WECs in all cases. For the same current magnitude, tests conducted in boundary and mixed lubrication regimes showed that time-to-failure increased as lambda increased, and the tests resulted in WEC related macropits, whereas tests conducted in near-hydrodynamic regime resulted in surface damage with no macropit. It was also noted that a shift toward near-hydrodynamic lubrication resulted in a distinct surface distress on the roller surface. Furthermore, there seems to be a transition in the mixed regime during which the surface distress occurred. The damage on the surface of the test samples resembled non-spatially, periodic, groove-like corrugations and, in some cases, crater-like depressions. Sub-surface imaging, performed by sequential sectioning, revealed the presence of WECs in all cases, and broad, branching cracks that were more prevalent under the more severe boundary conditions.

17 WIND ENERGY↗