High Thermal Conductivity of a Hydrogenated Amorphous Silicon Film

We measured the thermal conductivity {kappa} of an 80 {micro}m thick hydrogenated amorphous silicon film prepared by hot-wire chemical-vapor deposition with the 3{omega} (80-300 K) and the time-domain thermoreflectance (300 K) methods. The {kappa} is higher than any of the previous temperature dependent measurements and shows a strong phonon mean free path dependence. We also applied a Kubo based theory using a tight-binding method on three 1000 atom continuous random network models. The theory gives higher {kappa} for more ordered models, but not high enough to explain our results, even after extrapolating to lower frequencies with a Boltzmann approach. Our results show that this material is more ordered than any amorphous silicon previously studied.

14 SOLAR ENERGY↗

High Precision Detection of Change in Intermediate Range Order of Amorphous Zirconia-Doped Tantala Thin Films Due to Annealing

Understanding the local atomic order in amorphous thin film coatings and how it relates to macroscopic performance factors, such as mechanical loss, provides an important path towards enabling the accelerated discovery and development of improved coatings. High precision x-ray scattering measurements of thin films of amorphous zirconia-doped tantala (ZrO 2 -Ta 2 O 5 ) show systematic changes in intermediate range order (IRO) as a function of postdeposition heat treatment (annealing). Atomic modeling captures and explains these changes, and shows that the material has building blocks of metal-centered polyhedra and the effect of annealing is to alter the connections between the polyhedra. The observed changes in IRO are associated with a shift in the ratio of corner-sharing to edge-sharing polyhedra. These changes correlate with changes in mechanical loss upon annealing, and suggest that the mechanical loss can be reduced by developing a material with a designed ratio of corner-sharing to edge-sharing polyhedra.

36 MATERIALS SCIENCE↗

Thermodynamically stable Si{sub w}C{sub x}N{sub y}O{sub z} polymer-like, amorphous ceramics made from organic precursors.

This communication reports new results on the enthalpy of formation of pseudo-amorphous ceramic compounds constituted from silicon, carbon, oxygen, and nitrogen (SiCNO), made from the polymer route. Again, like the SiCO materials, although with one exception, the enthalpy of formation from crystalline components (SiO{sub 2} cristobalite, {beta}-Si{sub 3}N{sub 4}, SiC, and excess C) is negative. Some of the alloyed oxygen-nitrogen compositions yield enthalpies that are much more negative ({approx}100 kJ/g {center_dot} atom) in comparison with compositions that contain mainly oxygen or nitrogen ({approx}20 kJ/g {center_dot} atom). The exception, having a N/O ratio near 2, has a positive value for the enthalpy. This may reflect the presence of nanoclusters of stoichiometric Si{sub 2}N{sub 2}O instead of the pseudo-amorphous nanodomain structure seen for the other samples.

36 MATERIALS SCIENCE↗

Confirmation of the Dominant Defect Mechanism in Amorphous In-Zn-O Through the Application of In Situ Brouwer Analysis

The dominant point defect mechanism of amorphous (a-) indium zinc oxide (IZO) was probed through in situ electrical characterization of sputtered a-IZO thin films in response to changes in oxygen partial pressure (pO2) at 300 degrees C. The results yielded a power law dependence of conductivity (s) versus pOinline image of ~-1/6. This experimental method, known as Brouwer analysis, confirms doubly-charged oxygen vacancies as the dominant defect species in a-IZO. The success of this study suggests that Brouwer analysis is a viable method for studying the defect mechanisms of amorphous oxides.

14 SOLAR ENERGY↗

Self-bias voltage diagnostics for the amorphous-to-microcrystalline transition in a-Si:H under a hydrogen-plasma treatment

The authors demonstrate the possibility of using self-bias voltage on the radio-frequency electrode of a capacitively coupled deposition system as a diagnostic tool to detect the amorphous-to-microcrystalline silicon transition during the exposure of a-Si:H thin films to a hydrogen plasma. This is achieved by combining self-bias voltage (V{sub dc}) and kinetic-ellipsometry measurements, which provide real-time information on the film properties. On intrinsic and n-type a-Si:H films, the hydrogen-plasma exposure results in the formation of a hydrogen-modified layer, which is accompanied with a decrease in the absolute values of V{sub dc}, until a plateau corresponding to the nucleation and the growth of the microcrystalline layer occurs. On p-type a-Si:H, the amorphous-to-microcrystalline transition is characterized by a rapid increase in the absolute values of V{sub dc}. This particular trend is ascribed to the effects of boron on both the solid and plasma phases.

36 MATERIALS SCIENCE↗

Low-temperature growth of low friction wear-resistant amorphous carbon nitride thin films by mid-frequency, high power impulse, and direct current magnetron sputtering

The potential of different magnetron sputtering techniques for the synthesis of low friction and wear resistant amorphous carbon nitride (a-CN{sub x}) thin films onto temperature-sensitive AISI52100 bearing steel, but also Si(001) substrates was studied. Hence, a substrate temperature of 150 °C was chosen for the film synthesis. The a-CN{sub x} films were deposited using mid-frequency magnetron sputtering (MFMS) with an MF bias voltage, high power impulse magnetron sputtering (HiPIMS) with a synchronized HiPIMS bias voltage, and direct current magnetron sputtering (DCMS) with a DC bias voltage. The films were deposited using a N{sub 2}/Ar flow ratio of 0.16 at the total pressure of 400 mPa. The negative bias voltage, V{sub s}, was varied from 20 to 120 V in each of the three deposition modes. The microstructure of the films was characterized by high-resolution transmission electron microscopy and selected area electron diffraction, while the film morphology was investigated by scanning electron microscopy. All films possessed an amorphous microstructure, while the film morphology changed with the bias voltage. Layers grown applying the lowest substrate bias of 20 V exhibited pronounced intercolumnar porosity, independent of the sputter technique. Voids closed and dense films are formed at V{sub s} ≥ 60 V, V{sub s} ≥ 100 V, and V{sub s} = 120 V for MFMS, DCMS, and HiPIMS, respectively. X-ray photoelectron spectroscopy revealed that the nitrogen-to-carbon ratio, N/C, of the films ranged between 0.2 and 0.24. Elastic recoil detection analysis showed that Ar content varied between 0 and 0.8 at. % and increased as a function of V{sub s} for all deposition techniques. All films exhibited compressive residual stress, σ, which depends on the growth method; HiPIMS produces the least stressed films with values ranging between −0.4 and −1.2 GPa for all V{sub s}, while CN{sub x} films deposited by MFMS showed residual stresses up to −4.2 GPa. Nanoindentation showed a significant increase in film hardness and reduced elastic modulus with increasing V{sub s} for all techniques. The harder films were produced by MFMS with hardness as high as 25 GPa. Low friction coefficients, between 0.05 and 0.06, were recorded for all films. Furthermore, CN{sub x} films produced by MFMS and DCMS at V{sub s} = 100 and 120 V presented a high wear resistance with wear coefficients of k ≤ 2.3 × 10{sup −5} mm{sup 3}/Nm. While all CN{sub x} films exhibit low friction, wear depends strongly on the structural and mechanical characteristics of the films. The MFMS mode is best suited for the production of hard CN{sub x} films, although high compressive stresses challenge the application on steel substrates. Films grown in HiPIMS mode provide adequate adhesion due to low residual stress values, at the expense of lower film hardness. Thus, a relatively wide mechanical property envelope is presented for CN{sub x} films, which is relevant for the optimization of CN{sub x} film properties intended to be applied as low friction and wear resistant coatings.

36 MATERIALS SCIENCE↗

Amorphous sulfide heterostructure precursors prepared by radio frequency sputtering

Two-dimensional sulfides and their heterostructures have emerged as potentially useful materials for technological applications. Controllable self-assembly of interleaved crystalline heterostructures from designed thin-film precursors has been demonstrated in selenide and telluride chemical systems, but not yet in sulfide chemistries. Preparing such amorphous sulfide heterostructure precursors is a necessary first step toward this goal. Here, deposition of thin-film amorphous precursors for layered sulfide heterostructures by RF sputtering is presented on the example of SnS-MoS 2 . Here, a calibration process specific to the mechanisms of RF sputtering from sulfide and disulfide compound targets is established. Precursor film structure and composition are confirmed via x-ray reflectivity and Rutherford backscattering measurements. Local nanostructure and composition are also examined by electron microscopy and electron energy loss spectroscopy.

14 SOLAR ENERGY↗

Optical functions of crystalline and amorphous TeO2

The optical functions of crystalline paratellurite (α-TeO2) and amorphous TeO2 were determined using several optical techniques: (1) standard spectroscopic two-modulator generalized ellipsometry (2-MGE) of paratellurite (200–850 nm, 6.2–1.46 eV), (2) near-normal-incidence two-modulator generalized ellipsometry microscopy (2-MGEM) of paratellurite (577 nm, 2.15 eV), (3) Mueller matrix transmission of paratellurite (320–798 nm, 3.87–1.55 eV), and (4) polarized transmission of paratellurite (323.6–334.3 nm, 3.83–3.71 eV). The 2-MGE measurements yielded highly accurate values of the dielectric functions and error estimates from 1.46 to 6.2 eV for both paratellurite and amorphous TeO2, whereas the polarization-dependent transmission yielded more accurate values of the absorption coefficient below the band edge of paratellurite. The 2-MGEM measured the diattenuation of paratellurite, which is related to the birefringence. Mueller matrix transmission measurements of paratellurite of a (001) cut crystal as a function of angle of incidence were used to determine both the birefringence and the rotary power as a function of photon energy.

Jellison Jr, Gerald [ORNL]↗

Off-axis dose response characteristics of an amorphous silicon electronic portal imaging device

Amorphous silicon (a-Si) electronic portal imaging devices (EPIDs) have typically been calibrated to dose at central axis (CAX). Division of acquired images by the flood-field (FF) image that corrects for pixel sensitivity variation as well as open field energy-dependent off-axis response variation should result in a flat EPID response over the entire matrix for the same field size. While the beam profile can be reintroduced to the image by an additional correction matrix, the CAX EPID response to dose calibration factor is assumed to apply to all pixels in the detector. The aim of this work was to investigate the dose response of the Varian aS500 amorphous silicon detector across the entire detector area. First it was established that the EPID response across the panel became stable (within {approx}0.2%) for MU settings greater than {approx}200 MU. The EPID was then FF calibrated with a high MU setting of {approx}400 for all subsequent experiments. Whole detector images with varying MU settings from 2-500 were then acquired for two dose rates (300 and 600 MU/min) for 6 MV photons for two EPIDs. The FF corrected EPID response was approximately flat or uniform across the detector for greater than 100 MU delivered (within 0.5%). However, the off-axis EPID response was greater than the CAX response for small MU irradiations, giving a raised EPID profile. Up to 5% increase in response at 20 cm off-axis compared to CAX was found for very small MU settings for one EPID, while it was within 2% for the second (newer) EPID. Off-axis response nonuniformities attributed to detector damage were also found for the older EPID. Similar results were obtained with the EPID at 18 MV energy and operating in asynchronous mode (acquisition not synchronized with beam pulses), however the profiles were flatter and more irregular for the small MU irradiations. By moving the detector laterally and repeating the experiments, the increase in response off-axis was found to depend on the pixel position relative to the beam CAX. When the beam was heavily filtered by a phantom the off-axis response variation was reduced markedly to within 0.5% for all MU settings. Independent measurements of off-axis point doses with ion chamber did not show any change in off-axis factor with MUs. Measurements of beam quality (TMR{sub 20-10}) for MU settings of 2, 5, and 100 at central axis and at 15 cm off-axis could not explain the effect. The response change is unlikely to be significant for clinical IMRT verification with this imaging/acclerator system where MUs are of the order of 100-300, provided the detector does not exhibit radiation damage artifacts.

62 RADIOLOGY AND NUCLEAR MEDICINE↗

Testing the GLAaS algorithm for dose measurements on low- and high-energy photon beams using an amorphous silicon portal imager

The GLAaS algorithm for pretreatment intensity modulation radiation therapy absolute dose verification based on the use of amorphous silicon detectors, as described in Nicolini et al. [G. Nicolini, A. Fogliata, E. Vanetti, A. Clivio, and L. Cozzi, Med. Phys. 33, 2839-2851 (2006)], was tested under a variety of experimental conditions to investigate its robustness, the possibility of using it in different clinics and its performance. GLAaS was therefore tested on a low-energy Varian Clinac (6 MV) equipped with an amorphous silicon Portal Vision PV-aS500 with electronic readout IAS2 and on a high-energy Clinac (6 and 15 MV) equipped with a PV-aS1000 and IAS3 electronics. Tests were performed for three calibration conditions: A: adding buildup on the top of the cassette such that SDD-SSD=d{sub max} and comparing measurements with corresponding doses computed at d{sub max}, B: without adding any buildup on the top of the cassette and considering only the intrinsic water-equivalent thickness of the electronic portal imaging devices device (0.8 cm), and C: without adding any buildup on the top of the cassette but comparing measurements against doses computed at d{sub max}. This procedure is similar to that usually applied when in vivo dosimetry is performed with solid state diodes without sufficient buildup material. Quantitatively, the gamma index ({gamma}), as described by Low et al. [D. A. Low, W. B. Harms, S. Mutic, and J. A. Purdy, Med. Phys. 25, 656-660 (1998)], was assessed. The {gamma} index was computed for a distance to agreement (DTA) of 3 mm. The dose difference {delta}D was considered as 2%, 3%, and 4%. As a measure of the quality of results, the fraction of field area with gamma larger than 1 (%FA) was scored. Results over a set of 50 test samples (including fields from head and neck, breast, prostate, anal canal, and brain cases) and from the long-term routine usage, demonstrated the robustness and stability of GLAaS. In general, the mean values of %FA remain below 3% for {delta}D equal or larger than 3%, while they are slightly larger for {delta}D=2% with %FA in the range from 3% to 8%. Since its introduction in routine practice, 1453 fields have been verified with GLAaS at the authors' institute (6 MV beam). Using a DTA of 3 mm and a {delta}D of 4% the authors obtained %FA=0.9{+-}1.1 for the entire data set while, stratifying according to the dose calculation algorithm, they observed: %FA=0.7{+-}0.9 for fields computed with the analytical anisotropic algorithm and %FA=2.4{+-}1.3 for pencil-beam based fields with a statistically significant difference between the two groups. If data are stratified according to field splitting, they observed %FA=0.8{+-}1.0 for split fields and 1.0{+-}1.2 for nonsplit fields without any significant difference.

62 RADIOLOGY AND NUCLEAR MEDICINE↗

A field-shaping multi-well avalanche detector for direct conversion amorphous selenium

Purpose: A practical detector structure is proposed to achieve stable avalanche multiplication gain in direct-conversion amorphous selenium radiation detectors. Methods: The detector structure is referred to as a field-shaping multi-well avalanche detector. Stable avalanche multiplication gain is achieved by eliminating field hot spots using high-density avalanche wells with insulated walls and field-shaping inside each well. Results: The authors demonstrate the impact of high-density insulated wells and field-shaping to eliminate the formation of both field hot spots in the avalanche region and high fields at the metal-semiconductor interface. Results show a semi-Gaussian field distribution inside each well using the field-shaping electrodes, and the electric field at the metal-semiconductor interface can be one order-of-magnitude lower than the peak value where avalanche occurs. Conclusions: This is the first attempt to design a practical direct-conversion amorphous selenium detector with avalanche gain.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Amorphous In–Ga–Zn–O thin-film transistor active pixel sensor x-ray imager for digital breast tomosynthesis

Purpose: The breast cancer detection rate for digital breast tomosynthesis (DBT) is limited by the x-ray image quality. The limiting Nyquist frequency for current DBT systems is around 5 lp/mm, while the fine image details contained in the high spatial frequency region (>5 lp/mm) are lost. Also today the tomosynthesis patient dose is high (0.67–3.52 mGy). To address current issues, in this paper, for the first time, a high-resolution low-dose organic photodetector/amorphous In–Ga–Zn–O thin-film transistor (a-IGZO TFT) active pixel sensor (APS) x-ray imager is proposed for next generation DBT systems. Methods: The indirect x-ray detector is based on a combination of a novel low-cost organic photodiode (OPD) and a cesium iodide-based (CsI:Tl) scintillator. The proposed APS x-ray imager overcomes the difficulty of weak signal detection, when small pixel size and low exposure conditions are used, by an on-pixel signal amplification with a significant charge gain. The electrical performance of a-IGZO TFT APS pixel circuit is investigated by SPICE simulation using modified Rensselaer Polytechnic Institute amorphous silicon (a-Si:H) TFT model. Finally, the noise, detective quantum efficiency (DQE), and resolvability of the complete system are modeled using the cascaded system formalism. Results: The result demonstrates that a large charge gain of 31–122 is achieved for the proposed high-mobility (5–20 cm{sup 2}/V s) amorphous metal-oxide TFT APS. The charge gain is sufficient to eliminate the TFT thermal noise, flicker noise as well as the external readout circuit noise. Moreover, the low TFT (<10{sup −13} A) and OPD (<10{sup −8} A/cm{sup 2}) leakage currents can further reduce the APS noise. Cascaded system analysis shows that the proposed APS imager with a 75 μm pixel pitch can effectively resolve the Nyquist frequency of 6.67 lp/mm, which can be further improved to ∼10 lp/mm if the pixel pitch is reduced to 50 μm. Moreover, the detector entrance exposure per projection can be reduced from 1 to 0.3 mR without a significant reduction of DQE. The signal-to-noise ratio of the a-IGZO APS imager under 0.3 mR x-ray exposure is comparable to that of a-Si:H passive pixel sensor imager under 1 mR, indicating good image quality under low dose. A threefold reduction of current tomosynthesis dose is expected if proposed technology is combined with an advanced DBT image reconstruction method. Conclusions: The proposed a-IGZO APS x-ray imager with a pixel pitch <75 μm is capable to achieve a high spatial frequency (>6.67 lp/mm) and a low dose (<0.4 mGy) in next generation DBT systems.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Amorphization in extreme deformation of the CrMnFeCoNi high-entropy alloy

Ever-harsher service conditions in the future will call for materials with increasing ability to undergo deformation without sustaining damage while retaining high strength. Prime candidates for these conditions are certain high-entropy alloys (HEAs), which have extraordinary work-hardening ability and toughness. By subjecting the equiatomic CrMnFeCoNi HEA to severe plastic deformation through swaging followed by either quasi-static compression or dynamic deformation in shear, we observe a dense structure comprising stacking faults, twins, transformation from the face-centered cubic to the hexagonal close-packed structure, and, of particular note, amorphization. The coordinated propagation of stacking faults and twins along {111} planes generates high-deformation regions, which can reorganize into hexagonal packets; when the defect density in these regions reaches a critical level, they generate islands of amorphous material. These regions can have outstanding mechanical properties, which provide additional strengthening and/or toughening mechanisms to enhance the capability of these alloys to withstand extreme loading conditions.

36 MATERIALS SCIENCE↗

Amorphization mechanism of SrIrO 3 electrocatalyst: How oxygen redox initiates ionic diffusion and structural reorganization

The use of renewable electricity to prepare materials and fuels from abundant molecules offers a tantalizing opportunity to address concerns over energy and materials sustainability. The oxygen evolution reaction (OER) is integral to nearly all material and fuel electrosyntheses. However, very little is known about the structural evolution of the OER electrocatalyst, especially the amorphous layer that forms from the crystalline structure. Here, we investigate the interfacial transformation of the SrIrO 3 OER electrocatalyst. The SrIrO 3 amorphization is initiated by the lattice oxygen redox, a step that allows Sr 2+ to diffuse and O 2− to reorganize the SrIrO 3 structure. This activation turns SrIrO 3 into a highly disordered Ir octahedral network with Ir square-planar motif. The final Sr y IrO x exhibits a greater degree of disorder than IrO x made from other processing methods. Our results demonstrate that the structural reorganization facilitated by coupled ionic diffusions is essential to the disordered structure of the SrIrO 3 electrocatalyst.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

The crystallization kinetics of nanothin amorphous TlGa{sub 1-x}Ge{sub x}Se{sub 2} films

The kinetics of phase transformations of amorphous Ge-doped TlGaSe{sub 2} films has been investigated by kinematic electron diffraction. It is shown that the crystallization of 30-nm-thick amorphous films obtained both in the absence of external effects and in an external electric field occurs according to the regularities established by Avrami and Kolmogorov and described by the analytical expression V{sub t} = V{sub 0}[1 - exp(-kt{sup m})]. The activation energies of nucleation and the further growth of nuclei have been determined from the kinetic curves of phase transformations.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

An observation of amorphous-crystalline phase transitions at severe plastic deformation of the Ti{sub 50}Ni{sub 25}Cu{sub 25} alloy

The features of structural and phase transitions during severe plastic deformation (in Bridgman anvils) of the amorphous Ti{sub 50}Ni{sub 25}Cu{sub 25} alloy have been studied by X-ray diffraction and transmission electron microscopy. Application of successively increasing deformation has revealed three cycles of successive phase transitions from amorphous to crystalline state and vice versa. The results obtained are explained in terms of the superposition of the different channels of elastic energy dissipation, which are activated during severe plastic deformation.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Specific features of sample preparation from amorphous aluminum alloys for transmission electron microscopy

An aluminum amorphous alloy doped with transition (Fe and Ni) and rare earth (La) metals has been used as an object of systematic study of the structural transformations that are characteristic of different methods of sample preparation for transmission electron microscopy (the mechanical tearing of ribbons, electrochemical thinning, and Ar{sup +}-ion etching under different conditions). The results of X-ray diffraction analysis and a calorimetric study of the structure in comparison with electron microscopy data made it possible to determine the optimal method of sample preparation, which ensures minimum distortions in the structure of metastable amorphous alloys with a low crystallization temperature.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Relaxation of bending stresses and the reversibility of residual stresses in amorphous soft magnetic alloys

The reversibility of residual bending stresses is revealed in ribbon samples of cobalt- and iron-based amorphous alloys Co{sub 69}Fe{sub 3.7}Cr{sub 3.8}Si{sub 12.5}B{sub 11} and Fe{sub 57}Co{sub 31}Si{sub 2.9}B{sub 9.1}: the ribbons that are free of applied stresses and bent under the action of residual stresses become completely or incompletely straight upon annealing at the initial temperatures. The influence of annealing on the relaxation of bending stresses is studied. Preliminary annealing is found to sharply decrease the relaxation rate of bending stresses, and the initial stage of fast relaxation of these stresses is absent. Complete straightening of preliminarily annealed ribbons is shown to occur at significantly higher temperatures than that of the initial ribbons. Incomplete straightening of the ribbons is explained by the fact that bending stresses relaxation at high annealing temperatures proceeds due to both reversible anelastic deformation and viscous flow, which is a fully irreversible process. Incomplete reversibility is also caused by irreversible processes, such as the release of excess free volume and clustering (detected by small-angle X-ray scattering). The revealed differences in the relaxation processes that occur in the cobalt- and iron-based amorphous alloys are discussed in terms of different atomic diffusion mobilities in these alloys.