Search NASA⌕ Search

SEARCH · Search NASA

Results for “SINTERING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,171 records · Page 65

Hybrid additive manufacturing methods using hybrid additively manufactured features for hybrid components

A hybrid additive manufacturing method comprises building an additive structure on a pre-sintered preform base, wherein building the additive structure comprises iteratively fusing together a plurality of layers of additive material with at least a first layer of additive material joined to the pre-sintered preform base, and wherein the pre-sintered preform base comprises an initial shape. The hybrid additive manufacturing method further comprises modifying the initial shape of the pre-sintered preform base comprising the additive structure into a modified shape comprising the additive structure, and, joining the pre-sintered preform base in its modified shape to a component.

36 MATERIALS SCIENCE↗

Ceramic assembly with a stabilizer layer

In one embodiment, the method of producing a ceramic assembly includes: disposing an electrode precursor on an electrolyte precursor having an electrolyte sintering shrinkage, disposing a stabilizer precursor having a stabilizer sintering shrinkage on the electrode precursor on a side opposite the electrolyte precursor to form a precursor assembly, and sintering the precursor assembly to form the ceramic assembly comprising a stabilizer layer, electrode, and electrolyte. The difference between the electrolyte sintering shrinkage and the stabilizer sintering shrinkage is less than or equal to ±1% and a surface of the ceramic assembly has less than or equal to about 5.0 degrees camber, as measured from the horizontal plane.

36 MATERIALS SCIENCE↗

Observations of Oxygen Ion Behavior in the Lithium-Based Electrolytic Reduction of Uranium Oxide

Parametric studies were performed on a lithium-based electrolytic reduction process at bench-scale to investigate the behavior of oxygen ions in the reduction of uranium oxide for various electrochemical cell configurations. Specifically, a series of eight electrolytic reduction runs was performed in a common salt bath of LiCl – 1 wt% Li2O. The variable parameters included fuel basket containment material (i.e., stainless steel wire mesh and sintered stainless steel) and applied electrical charge (i.e., 75 – 150% of the theoretical charge for complete reduction of uranium oxide in a basket to uranium metal). Samples of the molten salt electrolyte were taken at regular intervals throughout each run and analyzed to produce a time plot of Li2O concentrations in the bulk salt over the course of the runs. Following each run, the fuel basket was sectioned and the fuel was removed. Samples of the fuel were analyzed for the extent of uranium oxide reduction to metal and for the concentration of salt constituents, i.e., LiCl and Li2O. Extents of uranium oxide reduction ranged from 43 – 70% in stainless steel wire mesh baskets and 8 – 33 % in sintered stainless steel baskets. The concentrations of Li2O in the salt phase of the fuel product from the stainless steel wire mesh baskets ranged from 6.2 – 9.2 wt%, while those for the sintered stainless steel baskets ranged from 26 – 46 wt%. Another series of tests was performed to investigate the dissolution of Li2O in LiCl at 650 °C across various cathode containment materials (i.e., stainless steel wire mesh, sintered stainless steel and porous magnesia) and configurations (i.e., stationary and rotating cylindrical baskets). Dissolution of identical loadings of Li2O particulate reached equilibrium within one hour for stationary stainless steel wire mesh baskets, while the same took several hours for sintered stainless steel and porous magnesia baskets. Rotation of an annular cylindrical basket of stainless steel wire mesh accelerated the Li2O dissolution rate by more than a factor of six.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Microstructure Evolution During Controlled Solidification of “Fe{sub 2}O{sub 3}”-CaO-SiO{sub 2} Liquids in Air

The principal chemical components in iron ore sintering are Fe{sub 2}O{sub 3}, CaO, and SiO{sub 2}. This sintering process consists of three key steps: heating, holding at peak temperature, and cooling. During the cooling stage, a liquid oxide solidifies to form the final sinter microstructures. To investigate the fundamental processes taking place during the cooling of sinters, a new experimental technique has been developed that allows the stages of solidification to be determined in isolation, rather than inferred from the final microstructures. Fe{sub 2}O{sub 3}-CaO-SiO{sub 2} oxide samples of a bulk composition having a CaO/SiO{sub 2} mass ratio of 3.46 and 73.2 wt pct Fe{sub 2}O{sub 3} were cooled in air from 1623 K (1350 °C) at 2 K/s, quenched at 5 K temperature intervals from 1533 K to 1453 K (1260 °C to 1180 °C), and analyzed using Electron Probe Micro X-Ray Analysis (EPMA). During cooling, four distinct stages were observed, consisting of the phase assemblages Liquid + Hematite (I), Liquid + Hematite + C{sub 2}S(II), Liquid + C{sub 2}S + CF{sub 2}(III), and C{sub 2}S + CF{sub 2} + CF (IV). This solidification sequence differs from that predicted under equilibrium and Scheil–Gulliver Cooling. Importantly, no Silico-Ferrite of Calcium (SFC) phase was observed to form on solidification of the liquid. Based on the microstructures formed and liquid compositions, measured by EPMA, it was demonstrated that kinetic factors play a major role in determining the phases and microstructures formed under the conditions investigated.

36 MATERIALS SCIENCE↗

In situ measurement of temperature and reduction of rutile titania using energy dispersive x-ray diffraction

Using in situ energy dispersive x-ray diffraction (EDXRD) the average specimen temperature of TiO 2 in the steady state of flash is experimentally determined. Comparison of the microstructure for flash sintering and conventional sintering in addition to the temperature determined from calibration of the unit cell expansion indicates that rapid Joule heating during flash sintering causes densification and grain growth comparable with conventional sintering. An average temperature approximation model is proposed to account for greybody radiation and thermal conduction. In conclusion, the inhomogeneity of the grain growth across the sample length is confirmed to correlate with inhomogeneity in temperature distribution and this suggests a current induced Peltier effect in n-type TiO 2 .

36 MATERIALS SCIENCE↗

High Temperature Integrated Thermoelectric Ststem and Materials

The final goal of this project is to produce, by the end of Phase II, an all ceramic high temperature thermoelectric module. Such a module design integrates oxide ceramic n-type, oxide ceramic p-type materials as thermoelectric legs and oxide ceramic conductive material as metalizing connection between n-type and p-type legs. The benefits of this all ceramic module are that it can function at higher temperatures (> 700 C), it is mechanically and functionally more reliable and it can be scaled up to production at lower cost. With this all ceramic module, millions of dollars in savings or in new opportunities recovering waste heat from high temperature processes could be made available. A very attractive application will be to convert exhaust heat from a vehicle to reusable electric energy by a thermoelectric generator (TEG). Phase I activities were focused on evaluating potential n-type and p-type oxide compositions as the thermoelectric legs. More than 40 oxide ceramic powder compositions were made and studied in the laboratory. The compositions were divided into 6 groups representing different material systems. Basic ceramic properties and thermoelectric properties of discs sintered from these powders were measured. Powders with different particles sizes were made to evaluate the effects of particle size reduction on thermoelectric properties. Several powders were submitted to a leading thermoelectric company for complete thermoelectric evaluation. Initial evaluation showed that when samples were sintered by conventional method, they had reasonable values of Seebeck coefficient but very low values of electrical conductivity. Therefore, their power factors (PF) and figure of merits (ZT) were too low to be useful for high temperature thermoelectric applications. An unconventional sintering method, Spark Plasma Sintering (SPS) was determined to produce better thermoelectric properties. Particle size reduction of powders also was found to have some positive benefits. Two composition systems, specifically 1.0 SrO - 0.8 x 1.03 TiO2 - 0.2 x 1.03 NbO2.5 and 0.97 TiO2 - 0.03 NbO2.5, have been identified as good base line compositions for n-type thermoelectric compositions in future module design. Tests of these materials at an outside company were promising using that company's processing and material expertise. There was no unique p-type thermoelectric compositions identified in phase I work other than several current cobaltite materials. Ca3Co4O9 will be the primary p-type material for the future module design until alternative materials are developed. BaTiO3 and rare earth titanate based dielectric compositions show both p-type and n-type behavior even though their electrical conductivities were very low. Further research and development of these materials for thermoelectric applications is planned in the future. A preliminary modeling and optimization of a thermoelectric generator (TEG) that uses the n-type 1.0 SrO - 1.03 x 0.8 TiO2 - 1.03 x 0.2 NbO2.5 was performed. Future work will combine development of ceramic powders and manufacturing expertise at TAM, development of SPS at TAM or a partner organization, and thermoelectric material/module testing, modeling, optimization, production at several partner organizations.

25 ENERGY STORAGE↗

Outside Mainstream Electronic Databases: Review of Studies Conducted in the USSR and Post-Soviet Countries on Electric Current-Assisted Consolidation of Powder Materials

This paper reviews research articles published in the former USSR and post-soviet countries on the consolidation of powder materials using electric current that passes through the powder sample and/or a conductive die-punch set-up. Having been published in Russian, many of the reviewed papers are not included in the mainstream electronic databases of the scientific articles and thus are not known to the scientific community. The present review is aimed at filling this information gap. In the paper, the electric current-assisted sintering techniques based on high- and low-voltage approaches are presented. The main results of the theoretical modeling of the processes of electromagnetic field-assisted consolidation of powder materials are discussed. Sintering experiments and related equipment are described and the major experimental results are analyzed. Sintering conditions required to achieve the desired properties of the sintered materials are provided for selected material systems. Tooling materials used in the electric current-assisted consolidation set-ups are also described.

powder materials↗

NUMERICAL MODELING OF CATHODE CONTACT MATERIAL DENSIFICATION

Numerical modeling was used to simulate the constrained sintering process of the cathode contact layer during assembly of solid oxide fuel cells (SOFCs). A finite element model based on the continuum theory for sintering of porous bodies was developed and used to investigate candidate low-temperature cathode contact materials. Constitutive parameters for various contact materials under investigation were estimated from dilatometry screening tests, and the influence of processing time, processing temperature, initial grain size, and applied compressive stress on the free sintering response was predicted for selected candidate materials. The densification behavior and generated stresses within a 5-cell planar SOFC stack during sintering, high temperature operation, and room temperature shutdown were predicted. Insufficient constrained densification was observed in the stack at the proposed heat treatment, but beneficial effects of reduced grain size, compressive stack preload, and reduced thermal expansion coefficient on the contact layer densification and stresses were observed.

30 DIRECT ENERGY CONVERSION↗

Synthesis, Processing and Properties of Calcium- and Nickel-Doped Yttrium Chromates(III) Y{sub 0.8}Ca{sub 0.2}Cr{sub 1−x}Ni{sub x}O{sub 3} (x = 0-0.3) and Studies on Their Potential Application as Coatings for SOFC Interconnects

In the present study, a calcium- and nickel-doped yttrium chromates (YCCN)-based, conductive–protective layers for metallic interconnects used in the intermediate-temperature solid oxide fuel cells (IT-SOFCs) were investigated. Synthesis of Y{sub 0.8}Ca{sub 0.2}Cr{sub 1−x}Ni{sub x}O{sub 3} (x = 0; 0.15 and 0.3) powders was performed using a wet chemistry method with two different complexing agents: ethylenediaminetetraacetic acid and glycine. Based on the result of thermal analysis of obtained precursors, optimal conditions of the calcination process were determined. Powders were then milled, compacted and sintered at different temperatures using free sintering method, into series of dense, polycrystalline sinters. The use of glycine precursor allowed obtaining a single-phase material in all cases. Based on the electrical and sintering properties, the Y{sub 0.8}Ca{sub 0.2}Cr{sub 0.85}Ni{sub 0.15}O{sub 3} material was selected for further studies. It was deposited using cost-effective screen-printing method on the Crofer 22APU ferritic stainless steel. To investigate properties and suitability of the resulting layer/steel system for IT-SOFCs applications, the high-temperature, dual-atmosphere studies were carried out for the first time for ceramic/metallic system, in conditions as close as possible to actual working conditions of the fuel cell. The layer exhibited high stability and good protective properties. The area-specific resistance of the studied ceramic layer/metallic substrate composite was determined, with the obtained value of 0.0366 Ω cm{sup 2} being within the arbitrary limit set for these materials (0.1 Ω cm{sup 2}). The results show that the investigated materials are suitable for the projected application.

36 MATERIALS SCIENCE↗

Enhanced Mechanical, Tribological, and Thermal Properties of Fe{sub 3}Al Composites with Carbon Nanotubes

In this work, Fe{sub 3}Al-based composites reinforced with carbon nanotubes were fabricated by a hot-press sintering process under various sintering pressures. The effects of sintering pressure and additives (alumina and lanthanum) on both the physical and the mechanical properties were systematically investigated. Results showed that with the sintering pressure of 15 MPa and incorporation of carbon nanotubes (CNTs), the microhardness of Fe{sub 3}Al composite exhibited a peak value at 1038.1 HV, which was ~ 60% higher than those without the addition of carbon nanotubes (644.9 HV). Also, both the compressive yield strength and the thermal conductivity of Fe{sub 3}Al composite were also significantly improved. Results of wear test showed the Fe{sub 3}Al composite exhibited a low wearing rate (10{sup −6}-10{sup −5} order of magnitude) and a friction coefficient (0.53-0.67).

36 MATERIALS SCIENCE↗

Manufacturing and characterization of Ni-free N-containing ODS austenitic alloys

Ni-free N-containing oxide dispersion strengthened (ODS) austenitic alloys were manufactured by mechanical alloying (MA) followed by spark plasma sintering (SPS). The phase evolutions during milling under a nitrogen atmosphere and after sintering were studied by X-ray diffraction (XRD). Transmission electron microcopy (TEM) and contrast variation analysis (ACV), including small-angle neutron scattering (SANS) and ultra-small X-ray scattering (USAXS), revealed the existence of nanoparticles with a diameter of 3-51 nm for the samples sintered at 950 ºC. Sintering at 1000 ºC for 5 and 15 min caused slight growth and a significant coarsening of the nanoparticles, up to 70 nm and 128 nm, respectively. The ACV analysis indicated the existence of two populations of Y2O3, ε-martensite and MnO. The dispersive X-ray spectrometry (EDS) confirmed two kinds of nanoparticles, Y2O3 and MnO. The material was characterized by superior micro-hardness, of above 500 HV0.1.

36 MATERIALS SCIENCE↗

Preparation and thermoelectric properties of AgPb{sub m}SbSe{sub m+2} materials

Hydrothermally synthesized AgPb{sub m}SbSe{sub m+2} (m=10, 12, 16, 18) nanoparticles with diameters of 20-50 nm were compacted by pressureless sintering. The Seebeck coefficient and electrical conductivity of the samples were measured from room temperature up to {approx}750 K. The samples show large and positive values of the Seebeck coefficient and moderate electrical conductivity. The thermoelectric properties of Ag{sub x}Pb{sub 18}SbSe{sub 20} (x=0.8, 0.85) and AgPb{sub 18}SbSe{sub 20-y}Te{sub y} (y=1, 3) samples have also been studied. It has been found that Ag{sub 0.85}Pb{sub 18}SbSe{sub 20} sample has a higher thermoelectric power factor. A significant difference in thermoelectric properties has also been observed for the AgPb{sub 18}SbSe{sub 20} samples prepared with pressureless sintering and spark plasma sintering. - Graphical abstract: SEM image of the fracture surface of an Ag{sub 0.85}Pb{sub 18}SbSe{sub 20} nano/micron composite material prepared by spark plasma sintering of hydrothermally synthesized nanopowders.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

The Li{sup +} conducting composite based on LiTi{sub 2}(PO{sub 4}){sub 3} and Li{sub 3}BO{sub 3} glass

Highlights: • Addition of the LBO glass enhance total ion conductivity up to four orders of magnitude. • Transport of Li{sup +} could be attributed to two media: grains and grain boundaries. • Sintering temperature is the most influential factor affecting the σ{sub tot}. • Melting of the LBO above 700 °C supports the sintering process. - Abstract: The LiTi{sub 2}(PO{sub 4}){sub 3} based composites containing amorphous Li{sub 3}BO{sub 3} were formed and investigated by means of X–ray diffractometry, thermogravimetry, scanning electron microscopy, impedance spectroscopy and density methods. The study shows that when a polycrystalline LiTi{sub 2}(PO{sub 4}){sub 3} material is sintered with Li{sub 3}BO{sub 3} glass, the resultant ceramics exhibit very high total ion conductivity. The maximum conductivity of 1.43 × 10{sup −4} S cm{sup −1} at 30 °C was achieved for the LTP–0.3LBO material sintered at 900 °C compared to 5.15 × 10{sup −8} S cm{sup −1} of the ceramic LiTi{sub 2}(PO{sub 4}){sub 3}.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Thermal behavior of SrSO{sub 4}-SrCO{sub 3} and SrSO{sub 4}-SrCO{sub 3}-Al{sub 2}O{sub 3} mixtures

The high temperature behavior of SrSO{sub 4}, SrCO{sub 3} and Al{sub 2}O{sub 3} mixtures was studied. A mixture of 1:1 mole of SrSO{sub 4} and mechanically activated SrCO{sub 3} was mixed and characterized using thermal gravimetric analysis. Some samples were uniaxially pressed and sintered at 1100, 1200 and 1300 deg. C for 8 h and then analyzed using X-ray diffraction and scanning electron microscopy. Additionally, a mixture of SrSO{sub 4}:SrCO{sub 3}:Al{sub 2}O{sub 3} was uniaxially pressed and sintered at 1500 deg. C. The decomposition temperature of SrCO{sub 3} was decreased 18 deg. by milling for 180 min. Samples sintered at 1300 deg. C showed a microstructure free of porosity. X-ray diffraction analysis showed the presence of SrO and SrSO{sub 4} after sintering at 1100, 1200 and 1300 deg. C. The mixture containing alumina showed the formation of a strontium aluminum oxide sulfate compound in addition to strontium aluminate.

36 MATERIALS SCIENCE↗

Synthesis of nanocrystalline yttrium iron garnet by low temperature solid state reaction

In this work, nanocrystalline yttrium iron garnet powders were produced by low temperature solid state reaction. The phase evolution during the procedure was determined from the thermogravimetric and differential thermal analysis, and the x-ray diffraction patterns. The results of transmission electron microscopy indicated that the prepared powders exhibited grain size at the nano-level of 20 {approx} 40 nm. Dense ceramics with a theoretical density of around 98% were obtained from the prepared powders after sintering at 1280 deg. C, a relative low sintering temperature compared with conventional ceramic processes, and the saturation magnetizations of sintered samples were also determined. - Research Highlights: {yields}No sol or gel form during the synthesis processing using nitrates and citric acid as raw materials. {yields}The synthesis method needs a low heating temperature (700 deg. C) compared with conventional solid state reaction. {yields}The product is a single phase with homogeneous size distribution and nano grains (20 {approx} 40 nm) confirmed by TEM. {yields}Dense YIG ceramic can be sintered at a low temperature (1280 deg. C) compared with that in conventional processing.

36 MATERIALS SCIENCE↗

Characterization of 430L porous supports obtained by powder extrusion moulding for their application in solid oxide fuel cells

The characterization of 430L stainless steel planar porous supports obtained by powder extrusion moulding was performed in this work. A thermoplastic multicomponent binder based on high density polyethylene and paraffin wax was selected for the process. Green supports were shaped by extrusion moulding, and subsequently the binder was removed by a thermal cycle previously optimized. Sintering was carried out at different temperatures in low vacuum. Density of sintered parts was measured by Archimedes' method and porosity was also evaluated through a microstructural analysis by optical microscopy. The porosity degree of samples sintered at low temperature was close to 35% which is a very suitable value for their application in SOFCs. Tensile tests were carried out in order to determine mechanical strength as a function of porosity degree. Based on these results, the best feedstock composition and processing parameters were selected. The oxidation behaviour in static air at high temperature was studied, and formed oxides were characterized in a scanning electron microscope equipped with energy dispersive analysis of X-rays. X-ray diffraction experiments were performed in order to identify the formed oxides based on formula Fe{sub 2−x}Cr{sub x}O{sub 3}. The results of these studies showed that this kind of ferritic stainless steel would be more suitable to be used as anodic supports where a rich hydrogen atmosphere is employed. Preliminary deposition tests allowed obtaining a homogeneous Ni–YSZ anode layer with a thickness of 10 μm on the porous metallic substrates. - Highlights: • 430L stainless steel porous supports were obtained by powder extrusion moulding. • Porosity degree was controlled sintering at different temperatures in low vacuum. • Tensile tests allowed determining mechanical strength of porous supports. • A study about its oxidation behaviour in static air at high temperature was realized. • After oxidation, formed oxides were characterized by EDS–SEM and XRD.

36 MATERIALS SCIENCE↗

Microstructure and mechanical properties of bulk highly faulted fcc/hcp nanostructured cobalt microstructures

Nanostructured cobalt powders with an average particle size of 50 nm were synthesized using a polyol method and subsequently consolidated by spark plasma sintering (SPS). SPS experiments performed at 650 °C with sintering times ranging from 5 to 45 min under a pressure of 100 MPa, yielded to dense bulk nanostructured cobalt (relative density greater than 97%). X-ray diffraction patterns of the as-prepared powders showed only a face centered cubic (fcc) crystalline phase, whereas the consolidated samples exhibited a mixture of both fcc and hexagonal close packed (hcp) phases. Transmission electron microscopy observations revealed a lamellar substructure with a high density of nanotwins and stacking faults in every grain of the sintered samples. Room temperature compression tests, carried out at a strain rate of 10{sup −3} s{sup −1}, yielded to highest strain to fracture values of up to 5% for sample of holding time of 15 min, which exhibited a yield strength of 1440 MPa, an ultimate strength as high as 1740 MPa and a Young's modulus of 205 GPa. The modulus of elasticity obtained from the nanoindentation tests, ranges from 181 to 218 GPa. The lowest modulus value of 181 GPa was obtained for the sample with the highest sintering time (45 min), which could be related to mass density loss as a consequence of trapped gases releasing. - Highlights: • Co nanopowder (50 nm) was prepared by reduction in polyol medium. • SPS was used to process bulk nanostructured Co specimens. • Microstructures were made of intricate fcc/hcp, along with nanotwins and SFs. • High strengths and moderate compressive ductility were obtained. • Deformation mechanisms related to complex interplay of different length scales.

36 MATERIALS SCIENCE↗

Mechanically induced self-propagating reaction and consequent consolidation for the production of fully dense nanocrystalline Ti{sub 55}C{sub 45} bulk material

We employed a high-energy ball mill for the synthesis of nanograined Ti{sub 55}C{sub 45} powders starting from elemental Ti and C powders. The mechanically induced self-propagating reaction that occurred between the reactant materials was monitored via a gas atmosphere gas-temperature-monitoring system. A single phase of NaCl-type TiC was obtained after 5 h of ball milling. To decrease the powder and grain sizes, the material was subjected to further ball milling time. The powders obtained after 200 h of milling possessed spherical-like morphology with average particle and grain sizes of 45 μm and 4.2 nm, respectively. The end-products obtained after 200 h of ball milling time, were then consolidated into full dense compacts, using hot pressing and spark plasma sintering at 1500 and 34.5 MPa, with heating rates of 20 °C/min and 500 °C/min, respectively. Whereas hot pressing of the powders led to severe grain growth (∼ 436 nm in diameter), the as-spark plasma sintered powders maintained their nanograined characteristics (∼ 28 nm in diameter). The as-synthesized and as-consolidated powders were characterized, using X-ray diffraction, high-resolution electron microscopy, and scanning electron microscopy. The mechanical properties of the consolidated samples obtained via the hot pressing and spark plasma sintering techniques were characterized, using Vickers microhardness and non-destructive testing techniques. The Vickers hardness, Young's modulus, shear modulus and fracture toughness of as-spark plasma sintered samples were 32 GPa, 358 GPa, 151 GPa and 6.4 MPa·m{sup 1/2}, respectively. The effects of the consolidation approach on the grain size and mechanical properties were investigated and are discussed. - Highlights: • Room-temperature synthesizing of NaCl-type TiC • Dependence on the grain size on the ball milling time • Fabrication of equiaxed nanocrystalline grains with a diameter of 4.2 nm • Fabrication of nanocrystalline bulk TiC material by SPS with minimal grain growth • Dependence of improved mechanical properties on the consolidation techniques.

36 MATERIALS SCIENCE↗