Search NASA⌕ Search

SEARCH · Search NASA

Results for “Dislocation structure”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,189 records · Page 66

Understanding the role of carbon atoms on microstructure and phase transformation of high Nb containing TiAl alloys

The microstructure and solidification behavior of high Nb containing TiAl alloys with the composition of Ti-46Al-8Nb-xC (x = 0.1, 0.7, 1.4, 2.5 at.%) prepared by arc-melting method have been investigated in this work. The results give evidence that the addition of carbon changes the solidification behavior from solidification via the β phase to the peritectic solidification. And carbon in solid solution enriches in the α{sub 2} phase and increases the microhardness. As the carbon content increases to 1.4 at.%, plate-shape morphology carbides Ti{sub 2}AlC (H phase) precipitate from the TiAl matrix which leads to the refinement microstructure. By aging at 1173 K for 24 h after quenching treatment, fine needle-like and granular shape Ti{sub 3}AlC (P phase) carbides are observed in the matrix of Ti-46Al-8Nb-2.5C alloy, which distribute along the lamellar structure or around the plate-shape Ti{sub 2}AlC. Transmission electron microscope observation shows that the Ti{sub 3}AlC carbides precipitate at dislocations. The phase transformation in-situ observations indicate that the Ti{sub 2}AlC carbides partly precipitate during the solid state phase transformation process. - Highlights: •Carbon changes the solidification behavior from β phase to peritectic solidification. •Dislocations in solution treated γ phase act as nucleation sites of Ti{sub 3}AlC precipitations. •Ti{sub 3}AlC precipitates as fine needle-like or granular shape in the solution treated matrix. •Ti{sub 2}AlC carbides precipitate during the solid state phase transformation process.

36 MATERIALS SCIENCE↗

Single-Particle Studies Reveal a Nanoscale Mechanism for Elastic, Bright, and Repeatable ZnS:Mn Mechanoluminescence in a Low-Pressure Regime

Mechanoluminescent materials, which emit light in response to elastic deformation, are demanded for use as in situ stress sensors. ZnS doped with Mn is known to exhibit one of the lowest reported thresholds for appearance of mechanoluminescence, with repeatable light emission under contact pressure <10 MPa. Here, the physical basis for such behavior remains as yet unclear. Here, reliable microscopic detection of mechanoluminescence of single ZnS:Mn microparticles, in combination with nanoscale structural characterization, provides evidence that the mechanoluminescent properties of these particles result from interplay between a non-centrosymmetric crystal lattice and its defects, viz., dislocations and stacking faults. Statistical analysis of the distributions of mechanoluminescence energy release trajectories reveals two distinct mechanisms of excitation: one attributable to a piezo-phototronic effect and the other due to dislocation motion. At pressures below 8.1 MPa, both mechanisms contribute to mechanoluminescent output, with a dominant contribution from the piezo-phototronic mechanism. In contrast, above 8.1 MPa, dislocation motion is the primary excitation source. For the piezo-phototronic mechanism, we propose a specific model that accounts for elastic ZnS:Mn mechanoluminescence under very low pressure. The charged interfaces in stacking faults lead to the presence of filled traps, which otherwise would be empty in the absence of the built-in electric field. Upon application of external stress, local enhancement of the piezoelectric field at the stacking faults’ interfaces facilitates release of the trapped carriers and subsequent luminescence. This field enhancement explains how <10 MPa pressure produces thousands of photons.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Laser-induced convection nanostructures on SiON/Si interface

The homogenized beam of an excimer KrF laser has been used to form rectangular millimeter-scale holes of vertical walls in the {approx}1 {mu}m thick silicon-oxynitride (SiON) thin film deposited on Si <111> wafer. The regular rectangular craters in SiON layer have the flat bottom surface reaching the SiON/Si interface. At the same time horizontal thermal gradient causes the formation of the nanoscale Marangoni convection structures at the SiON/Si interface. The inhomogeneous pattern of the roll structures can be divided into domains of regular, irregular, and chaotic organizations. The roll diameter is about 200 nm while their average wavelength, {lambda}, is, {approx}2 {mu}m, i.e., about ten times larger than the laser wavelength, and decreases with increasing number of pulses. Numerical simulation of the Marangoni domain roll structures based on the simple Swift-Hohenberg equation has reproduced all observed types of the roll organization, including those that show the evolution of dislocations from the Eckhause instability.

36 MATERIALS SCIENCE↗

Influence of clinostat rotation on fertilized amphibian egg pattern specification

Pattern specification in fertile Xenopus eggs rotated on horizontal clinostats was monitored with respect to primary embryonic axis formation, subsequent morphogenesis, and compartmentalization of the cytoplasm. At the speeds of 1 to 24 rpm (which are believed to simulate microgravity) a large percentage of eggs developed normal axial structures. Eggs clinostated at 12 rpm showed a randomization of dorsal/ventral polarity. The cytoplasmic compartments showed some clinostat effects but no abnormal mixing, disruption or dislocation of compartments. It is predicted that Xenopus eggs fertilized and allowed to develop in space will retain normal cytoplasmic density compartments, establish primary axes and undergo normal morphogenesis in space. Their dorsal/ventral polarity may not, however, be determined by the sperm entrance site (as is the case for 1 g eggs).

Neff, A. W.↗

Pinning, flow and plastic deformation of flux vortices in high T(sub c) superconductors

In high temperature superconductor (HTSC) materials the vortices are highly mobile and flexible. This is reflected in different models of melt of a vortex lattice. Another aspect of the problem is stressed: an easy nucleation and high mobility of dislocations in the vortex lattice. Some models of plastic deformation of vortex lattice are considered as a result of its interaction with a real crystal structure. Depinning is interpreted as yield of plastic flow is vortex medium. Effect of macroscopic defects in crystal structures (pores, inclusions, grain and domain boundaries) is being considered in detail. Available experimental facts on magnetization and a critical current in HTSC and conventional superconductors are discussed from the points of view of depinning to vortices vs. plastic flow of vortices vs. plastic flow of vortices medium.

Roytburd, A.↗

Topological Defects in Graphite under Irradiation using Molecular Dynamics

Graphite is the preferred material for moderating elements and structural components in a Very High Temperature Reactor (VHTR). It has a layered structure with basal planes constituted by carbon atoms arranged in a hexagonal lattice. Graphite accommodates a wide variety of defects such as vacancies, interstitials, and dislocation loops; a detailed description can be found in a review paper by Telling and Heggie. The layered configuration in graphite engenders energetic conditions that favor the formation of topological defects. Unlike the interlayer defects, which often are sp{sup 3} hybridized, topological defects maintain their sp{sup 2} bond connectivity. Several types of topological defects are known to arise in graphite; one of the most recognizable defects corresponds to a 5-7 Stone-Wales (SW) configuration that arises by a simple rotation of bonds. While the bond rotations result in a defected configuration, each carbon atom is still bonded to three other carbon atoms in the SW configuration, albeit with different bond lengths. Topological defects are expected to arise in irradiated graphite. A recent investigation with Raman and XPS spectroscopy have concluded that a large number of such defects are generated under neutron irradiation; an earlier ab-initio investigation has also arrived at the same conclusion. While several molecular dynamics (MD) simulations have been reported on irradiated graphite in the past, none have characterized the evolution of defects that are topological in nature. Using MD simulations, the current investigation quantifies the evolution and the distribution of topological defects under irradiation. Using MD simulations, we establish the presence of 5 and 7 membered topological defects in graphite following radiation. There is a greater probability for the formation of a 7 member ring relative to that of a 5 member ring. Since a heptagon causes a lower distortion to the 120 deg. bond angle of the sp{sup 2} hybridized orbital than a pentagon it is plausible to expect a larger number of 7 member rings following a radiation perturbation. Using a spatial distribution analysis, we have verified that 7 member rings tend to stay adjacent to 5 member rings as in Stone-Wales (SW) configuration. Since there are unequal number of 5 and 7 member rings, it follows that there are several isolated 7 member topological defects in graphite following radiation, possibly connected to dangling bonds or non-planar (sp{sup 3}) defects.

36 MATERIALS SCIENCE↗

Damage Detection and Electrical Performance Impact of Flat-Flexible Circuits

Flat-flexible circuits or ‘flex circuits’ have varied applications in electronics and in explosive detonation systems. They pose advantages over conventional coaxial cables in their ability to fit into small mechanical envelopes and routings. A typical flex circuit is composed of a laminated assembly of multiple layers of conductor and dielectric materials. Copper, because of its high electrical conductivity, is one of the primary materials used in flex circuit conductors. The conductor must maintain structural integrity and electrical continuity when the flexible circuit is bent during processing or to fit an application envelope. Under some strain conditions a cable may have degraded electrical performance even though visible damage may not be evident. Dislocation density can increase by mechanisms such as dislocation forest hardening, where gliding dislocations in primary slip planes get pinned at obstacles and form Frank-Read sources. Dislocation density increases within the conductor layers may impact electrical resistivity but would not necessarily result in visible mechanical failure. In some detonation applications, such as for building implosion for demolition, the time for signal transmission and voltage used for firing detonators can be critical. If the resistance in a single flex cable within a building demolition array is too high, the resultant demolition shape may be asymmetric, leading to unplanned damage to nearby structures and potential hazards to public safety. This study will apply non-destructive evaluation techniques to evaluate the detectability of damage accumulation in flat, flexible copper-conductor cables and discuss potential implications to their practical use.

42 ENGINEERING↗

Enhancing fatigue life by ductile-transformable multicomponent B2 precipitates in a high-entropy alloy

Catastrophic accidents caused by fatigue failures often occur in engineering structures. Thus, a fundamental understanding of cyclic-deformation and fatigue-failure mechanisms is critical for the development of fatigue-resistant structural materials. Here we report a high-entropy alloy with enhanced fatigue life by ductile-transformable multicomponent B2 precipitates. Its cyclic-deformation mechanisms are revealed by real-time in-situ neutron diffraction, transmission-electron microscopy, crystal-plasticity modeling, and Monte-Carlo simulations. Multiple cyclic-deformation mechanisms, including dislocation slips, precipitation strengthening, deformation twinning, and reversible martensitic phase transformation, are observed in the studied high-entropy alloy. Its improved fatigue performance at low strain amplitudes, i.e., the high fatigue-crack-initiation resistance, is attributed to the high elasticity, plastic deformability, and martensitic transformation of the B2-strengthening phase. This study shows that fatigue-resistant alloys can be developed by incorporating strengthening ductile-transformable multicomponent intermetallic phases.

36 MATERIALS SCIENCE↗

Effect of Heat Treatment on Microstructure and Mechanical Property of 316L Stainless Steel Produced by Laser Powder Bed Fusion

The advanced non-light water reactor designs (Gen IV reactors), including molten salt/ very high temperature/ sodium-cooled and lead-cooled fast reactors, typically operate at higher temperatures and more extreme radiation conditions than light water reactors. An intrinsic part of the deployment and progress of Gen IV reactor designs is selecting the most suitable structural material for a specific application. Additive manufacturing (AM), a fairly new process of making physical, three-dimensional objects from a computer design file, is going to completely change the way of design, build and certify nuclear systems. It offers a range of opportunities to produce complex geometries from existing materials, offers new routes for processing of previously difficult to process materials, allows for design of new high-performance materials, and finally facilitates hybridization of dissimilar materials. This emerging technology has successfully produced cars, wind turbine blade molds and even live cells. It could also open up big opportunities for the nuclear industry to quickly deploy technologies at a fraction of the cost. So far, AM techniques have been preliminarily applied in the field of nuclear reactors, including the classical parts such as the pressure vessel of a small reactor with 508-III steel, the bottom nozzle of a fuel assembly with 304L steel, the fuel cladding with zirconium alloy and the integrated impeller of a pump and the multi-channel valve body with 316L steel [6,7]. The AM applications for operating nuclear reactors started in auxiliary plant components and have slowly migrated to metallic reactors and core components, but many of these are not safety critical components. Although many parts used for nuclear reactors have been fabricated by AM techniques, practical applications in engineering are still a long way off due to the uncertainty factors focused on the processing, material properties, analysis methods and application standards, which feeds the safety and life-cycle of the nuclear reactor. Due to rapid, repeated heating and cooling during production, a high dislocation density was present in the AM material. This microstructure feature is unstable at elevated temperature while high temperature is one of the typical operation environments for nuclear reactors. Thus, it is important to understand the thermal effect on the microstructure of AM material. The objectives of this study are to investigate the effect of heat treatment on the microstructure and mechanical properties of 316L stainless steel produced by laser powder bed fusion additive manufacturing, and to determine an appropriate heat treatment practice that will be applied to the lightweight AM lattice-structured material with the same chemistry. The heat treatment study consisted of annealing the samples at a temperature range of 800 to 1200 oC with a 50 oC increment for different times (1-24 hours), followed by vacuum or air cooling. Microstructural characterization was carried out by Scanning Electron Microscope (SEM). Grain size and crystallographic orientation were investigated by Electron Backscatter Diffraction (EBSD). Vickers hardness tests with a 0.5 kg load were employed to determine the hardness of samples after different heat treatments. After heat treatment, the random crystallographic orientation was preserved, and the volume fraction of high-angle grain boundaries (grain boundary misorientation =15 oC) remained the same. The dislocation density decreased with annealing temperature due to recovery. The fine subgrain structures in the as-printed specimen were quite stable up to 1200 oC. Minimal recrystallization was observed up to 1200 oC. Recrystallization initiated only after 8.5 hours at 1200 oC. The SEM images did not show obvious dependence of microstructure on cooling rate. The hardness of the specimens decreased with increasing annealing temperature as a result of the decrease in dislocation density. It is interesting to note that the AM material showed very similar hardness to the wrought material when annealing at similar temperature, although the microstructures are very different. Annealing at 1050 oC for 1 hour followed by air cooling was selected as the heat treatment procedure for the lattice designed lightweight AM 316L material.

36 MATERIALS SCIENCE↗

Do voids nucleate at grain boundaries during ductile rupture? [Do voids initiate at grain boundaries during ductile rupture?]

In the absence of pre-existing failure-critical defects, the fracture or tearing process in deformable metals loaded in tension begins with the nucleation of internal cavities or voids in regions of elevated triaxial stress. While ductile rupture processes initiate at inclusions or precipitates in many alloys, nucleation in pure metals is often assumed to be associated with grain boundaries or triple junctions. This study presents ex situ observations of incipient, subsurface void nucleation in pure tantalum during interrupted uniaxial tensile tests using electron channeling contrast (ECC) imaging, electron backscatter diffraction (EBSD), transmission Kikuchi diffraction (TKD) and transmission electron microscopy (TEM). Instead of forming at grain boundaries, voids initiated at and grew along dislocation cell and cell block boundaries created by plastic deformation. Most of the voids were associated with extended, lamellar deformation-induced boundaries that run along the traces of the {110} or {112} planes, though a few voids initiated at low-angle dislocation subgrain boundaries. In general, a high density of deformation-induced boundaries was observed near the voids. TEM and TKD demonstrate that voids initiate at and grow along cell block boundaries. Two mechanisms for void nucleation in pure metals, vacancy condensation and stored energy dissipation, are discussed in light of these results. In conclusion, the observations of the present investigation suggest that voids in pure materials nucleate by vacancy condensation and subsequently grow by consuming dislocations.

36 MATERIALS SCIENCE↗

Roles of V-shaped pits on the improvement of quantum efficiency in InGaN/GaN multiple quantum well light-emitting diodes

The roles of V-shaped pits on the improvement of quantum efficiency in InGaN/GaN multiple quantum well (MQW) light-emitting diodes are investigated by numerical simulation. The simulation results show that V-shaped pits cannot only screen dislocations, but also play an important role on promoting hole injection into the MQWs. It is revealed that the injection of holes into the MQW via the sidewalls of the V-shaped pits is easier than via the flat region, due to the lower polarization charge densities in the sidewall structure with lower In concentration and (10–11)-oriented semi-polar facets.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Controlling Deformation in Al/Ti: How Interface Roughness and Orientation Drive Bimetal Mechanics

The microstructural characteristics and morphology of interfaces in metals can be crucial in governing the initiation of plasticity and early deformation mechanisms under extreme conditions. During high-strain-rate deformation, these interfaces significantly affect dislocation nucleation, twinning, and other mechanisms that directly impact material strength and failure. Despite their importance, a substantial knowledge gap remains between the observed macroscopic material behavior and the underlying role of bimetal interfaces in plasticity initiation. Here, to address this gap, large-scale molecular dynamics simulations are performed on Al/Ti bimetal structures to examine the effect of interface characteristics on the onset of plasticity under uniaxial compression. Specifically, this study investigates how interface roughness (flat vs waveform interfaces) modifies the initiation of plastic events in the microstructure. Atomistic simulations indicate that interface roughness (a microscopic behavior) reduces the stress required for dislocation nucleation, thereby reducing the peak stress relative to a flat interface. For the square interface, the step height strongly influences plasticity initiation by setting the separation of locally flat regions. Varying the interface rotation relative to the loading direction (macroscopic behavior) reveals that the peak stress for both flat and waveform interfaces initially decreases and then increases with rotation, accompanied by a shift in dominant mechanisms—from Al twinning (flat) to interface sliding and Ti-dominated phase transformation and twinning at lower angles. The change in the stress-strain slope during initial compression reflects how rotation alters the resolved shear stress and activates different slip systems. Overall, the study provides valuable insights into the role of bimetal interfaces in controlling plasticity initiation and early deformation pathways for Al/Ti under extreme loading conditions.

36 MATERIALS SCIENCE↗

Five-second STEM dislocation tomography for 300 nm thick specimen assisted by deep-learning-based noise filtering

Scanning transmission electron microscopy (STEM) is suitable for visualizing the inside of a relatively thick specimen than the conventional transmission electron microscopy, whose resolution is limited by the chromatic aberration of image forming lenses, and thus, the STEM mode has been employed frequently for computed electron tomography based three-dimensional (3D) structural characterization and combined with analytical methods such as annular dark field imaging or spectroscopies. However, the image quality of STEM is severely suffered by noise or artifacts especially when rapid imaging, in the order of millisecond per frame or faster, is pursued. Here we demonstrate a deep-learning-assisted rapid STEM tomography, which visualizes 3D dislocation arrangement only within five-second acquisition of all the tilt-series images even in a 300 nm thick steel specimen. The developed method offers a new platform for various in situ or operando 3D microanalyses in which dealing with relatively thick specimens or covering media like liquid cells are required.

47 OTHER INSTRUMENTATION↗

GaN-Ready Aluminum Nitride Substrates for Cost-Effective, Very Low Dislocation Density III-Nitride LED's

The objective of this project was to develop and then demonstrate the efficacy of a costeffective approach for a low defect density substrate on which AlInGaN LEDs can be fabricated. The efficacy of this “GaN-ready” substrate would then be tested by growing high efficiency, long lifetime InxGa1-xN blue LEDs. The approach used to meet the project objectives was to start with low dislocation density AlN single-crystal substrates and grow graded AlxGa1-xN layers on top. Pseudomorphic AlxGa1-xN epitaxial layers grown on bulk AlN substrates were used to fabricate light emitting diodes and demonstrate better device performance as a result of the low defect density in these layers when benched marked against state-of-the-art LEDs fabricated on sapphire substrates. The pseudomorphic LEDs showed excellent output powers compared to similar wavelength devices grown on sapphire substrates, with lifetimes exceeding 10,000 hours (which was the longest time that could reliably be estimated). In addition, high internal quantum efficiencies were demonstrated at high driving current densities even though the external quantum efficiencies were low due to poor photon extraction. Unfortunately, these pseudomorphic LEDs require high Al content so they emit in the ultraviolet. Sapphire based LEDs typically have threading dislocation densities (TDD) > 108 cm-2 while the pseudomorphic LEDs have TDD ≤ 105 cm-2. The resulting TDD, when grading the AlxGa1-xN layer all the way to pure GaN to produce a “GaN-ready” substrate, has varied between the mid 108 down to the 106 cm-2. These inconsistencies are not well understood. Finally, an approach to improve the LED structures on AlN substrates for light extraction efficiency was developed by thinning and roughening the substrate.

72 PHYSICS OF ELEMENTARY PARTICLES AND FIELDS↗

Grain boundary softening from stress assisted helium cavity coalescence in ultrafine-grained tungsten

The formation of helium cavities in coarse-grained materials produces hardening proportional to the number density and size of the cavities and due to the interaction of dislocations with intragranular helium defects. In nanostructured metals containing a high density of interfacial sinks, preferential cavity formation in the grain boundaries instead produces softening that is often attributed to enhanced interfacial plasticity. Here, employing two grades of ultrafine-grained tungsten, we explore this effect using targeted implantation studies to map cavity evolution as a function of the irradiation conditions and quantify its impact on the mechanical response through nanoindentation. Softening is reported at implantation temperatures above the threshold for preferential grain boundary cavity formation but at a sufficiently low fluence prior to the growth of intragranular cavities. Collective changes in the mean cavity size, density, and morphology beneath a residual impression on an implanted surface indicate that cavity coalescence accompanied the reduction in hardness. Complementary atomistic simulations demonstrate that, in tungsten grain structures exhibiting softening, grain boundary bubble coalescence is driven by stress concentrations that further act to localize strain in the grain boundaries through cooperative deformation processes involving local atomic shuffling and sliding, dislocation emission, and even the nucleation of unstable twinning events.

36 MATERIALS SCIENCE↗

Electrical Impact of SiC Structural Crystal Defects on High Electric Field Devices (Invited)

As illustrated by the invited paper at this conference and other works, SiC wafers and epilayers contain a variety of crystallographic imperfections, including micropipes, closed-core screw dislocations, grain boundaries, basal plane dislocations, heteropolytypic inclusions, and surfaces that are often damaged and contain atomically rough features like step bunching and growth pits or hillocks. Present understanding of the operational impact of various crystal imperfections on SiC electrical devices is reviewed, with an emphasis placed on high-field SiC power devices and circuits.

Neudeck, Philip G.↗

Microstructural evolution in a precipitate-hardened (Fe 0.3 Ni 0.3 Mn 0.3 Cr 0.1 ) 94 Ti 2 Al 4 multi-principal element alloy during high-pressure torsion

Multi-principal element alloys demonstrate high strength, thermal stability, and irradiation resistance, making them excellent candidate materials for applications in nuclear reactors and other harsh environments. Some studies have examined the use of high-pressure torsion to strengthen MPEAs through grain size reduction and strain hardening. However, no studies have investigated the effect of HPT on secondary phases (precipitates) within an MPEA. Two alloys, (Fe 0.3 Ni 0.3 Mn 0.3 Cr 0.1 ) 94 Ti 2 Al 4 containing Ni(Ti, Al) B2 phase, and CrFe σ phase, and single-phase Fe 0.3 Ni 0.3 Mn 0.3 Cr 0.1 , were fabricated by casting and heat treatment. Both alloys were then processed with HPT to study microstructural evolution. Scanning electron microscopy (SEM) and transmission electron microscopy (TEM) were used to characterize the alloys before and after HPT processing. HPT processing produced a nanocrystalline structure in both alloys, but (Fe 0.3 Ni 0.3 Mn 0.3 Cr 0.1 ) 94 Ti 2 Al 4 exhibited a significantly smaller grain size and higher dislocation density than Fe 0.3 Ni 0.3 Mn 0.3 Cr 0.1 , with corresponding higher hardness. Before HPT, the (Fe 0.3 Ni 0.3 Mn 0.3 Cr 0.1 ) 94 Ti 2 Al 4 alloy consisted of large grain (~ 400 μm) and precipitates, including B2 of ~ 38 μm average size, B2 of ~ 0.7 μm average size, and small amounts of σ of ~ 1.5 μm average size. After HPT, the larger B2 precipitates were decreased in size and volume fraction, while the smaller B2 precipitates were completely dissolved; the σ precipitates appeared unaffected by HPT, likely due to their much higher hardness. Finally, observation of the B2 precipitate distribution along radial distance indicates that the strain caused the precipitates to fracture at intermediate strain (γ = 125) and dissolve at high strain (γ = 280).

36 MATERIALS SCIENCE↗

Atomistic modeling of interface strengthening in Al-Si eutectic alloys

Al-Si cast alloys are usually composed of α-Al and Al-Si eutectic. Si flakes and Al matrix generally hold cube-on-cube orientation relationship with the primary interface (111) Al ∥(111) Si . Extensive experimental studies demonstrated that Si flakes cannot significantly improve mechanical properties of Al-Si cast alloys. We hypothesize that the weak strengthening effect associated with Si flakes might be attributed to thermomechanical properties of Al-Si interfaces besides their morphologies. To characterize Al-Si interfaces with a large lattice mismatch (> 30%), we proposed the quasi-coincident site lattice (Q-CSL) as reference lattice, and demonstrated that the Q-CSL Al-Si coherent interface has three characteristic coherent structures, one stable and low energy structure and two metastable and high energy structures. The translation vectors for the same type of coherent Q-CSL structures are consistent with three displacement shift complete (DSC) vectors. The two metastable structures can be obtained by shifting the low energy structure with three partial DSC vectors. Semi-coherent interface is composed of the low energy Q-CSL patches and three sets of interface misfit dislocations with Burgers vectors same as the DSC vectors. Atomistic simulations revealed that Al-Si interface exhibits low shear resistance. Ideal shear strength of the Q-CSL coherent interface is 110 MPa and semi-coherent interface is 20 MPa. The low shear resistance is attributed to the glide of interface misfit dislocations. Al-Si interface also exhibits low formation and migration energies of point defects. Owing to low shear strength and low formation and migration energies of point defects, interface sliding or shear readily happen under mechanical loading or during dislocation-interface interactions. Lattice dislocations can cross slip onto or climb along Al-Si interfaces. These reactions decrease the number of accumulated dislocation loops around Si flakes and promote nucleation and emission of lattice dislocations from Al-Si interfaces to matrix, consequently reduce the repulsive force on approaching dislocations and weaken Si flakes strengthening effect. In situ tension and compression tests in a scanning electron microscope reveal relatively weak strengthening effect due to Si flakes, consistent with the computed dislocation interaction with interfaces and shear behavior of interfaces.

36 MATERIALS SCIENCE↗