Characterization of Fe-6Si Soft Magnetic Alloy Produced by Laser-Directed Energy Deposition Additive Manufacturing

Abstract Commercial electrical steels, Fe-Si alloys with < 4 wt.% Si, are inexpensive and efficient materials for electrical power conversion. Further efficiency improvements require increasing the silicon concentration to 6 wt.%, at which point the material becomes brittle and difficult to form by conventional rolling and sheet fabrication methods. Additive manufacturing stands to overcome challenges with commercial manufacturing techniques by leveraging near-net-shape fabrication. The wide array of process conditions provides additive manufacturing with increased flexibility, enabling control over the microstructure and mechanical properties. This work explores the microstructures and magnetic properties of ring-shaped Fe-Si alloys produced using concentric and cross-hatch tool paths on a laser-directed energy deposition additive manufacturing system. Concentric-built samples exhibit elongated grain structures while cross-hatch-built samples comprise lower aspect ratio grain structures. Thermal finite element analysis simulations model the stress conditions produced by the different scan path geometries. Microhardness measurements probe the mechanical properties as a function of anneal temperature, providing a qualitative understanding of the intergranular defect density. Soft magnetic properties measured under quasistatic and AC conditions show frequency- and microstructure-dependent coercivity and permeability. Finally, analysis of the core loss quantifies how the build strategies and thermal treatments influence efficiency in electrical power conversion applications. Understanding the influences of scan path geometry and thermal treatment provides a pathway towards application of additively manufactured soft magnetic materials.

Adamczyk, Jesse M.↗

Microstructure evolution and mechanical properties of nano-SiCp/AZ91 composite processed by extrusion and equal channel angular pressing (ECAP)

Nano-SiCp/AZ91 magnesium matrix composite was fabricated by stir casting. The as-cast ingots were extruded at 350 °C, then processed by equal channel angular pressing (ECAP) at various temperatures (250 °C, 300 °C and 350 °C). Grains are significantly refined after the extrusion and the ECAP. A basal fibre texture was detected by neutron diffraction after the extrusion, which inclines about 45° to the extrusion direction (ED) after the ECAP. Nano-scaled SiC particles agglomerate in the as-cast composite. After the extrusion, the agglomeration tends to form continuous or discontinuous strips along the extrusion direction. By application of the ECAP, the agglomerated SiC particles are partly dispersed and the strips formed during the extrusion tend to be thinner and broken with the increasing pass number. The yield tensile strength (YTS) and the ultimate tensile strength (UTS) of the composite are dramatically increased after the extrusion. ECAP for one pass at various temperatures further increases the strength, however, the YTS decreases with the increasing ECAP temperature and the pass number. The Orowan equations predict the maximum YTS of the composite may be up to 400 MPa providing SiC particles are homogenously distributed in the matrix. - Highlights: •Nano-scaled SiC particles were successfully added into AZ91 by stirring casting. •Agglomeration of nano-particles were improved by extrusion and ECAP. •Yield strength of the composite is 328 MPa after one pass of ECAP. •Further ECAP process with optimized parameters may fully disperse nano-particles. •Yield strength is predicted to up to 400 MPa when particles are fully dispersed.

36 MATERIALS SCIENCE↗

Heterogeneous microstructure of yttrium hydride and its relation to mechanical properties

Here, the goal of this study is to investigate the properties of yttrium hydride materials in relation to the microstructure, especially its homogeneity. High-throughput nanoindentation mapping was used to evaluate hardness distribution. Raman spectral imaging demonstrated its sensitivity to the presence of YH2 and impurities. Raman peak position maps were correlated with residual stress in the specimens. Electron backscatter diffraction mapping provided phase distributions with correlation to high-energy X-ray diffraction analysis. The experimental mapping data were combined and analyzed using unsupervised machine learning cluster procedures. The machine learning analysis revealed that yttrium hydride specimens contained a major δ-YH2 – x phase component and minor α-Y and δ-YH2 – x components with significant residual stress. The minor phase fraction decreased with increasing nominal H/Y ratio, which affected the nanoindentation and Vickers hardness. The multimodal mapping procedures described herein affect developing important microstructure–property relationships, as well as correlations in heterogeneity and mechanical properties.

36 MATERIALS SCIENCE↗

Microstructure Investigation and Mechanical Properties of Coated Zircaloy Cladding

Accident Tolerant Fuel concepts have been developed and tested in diverse research programs presently around the world. Industry teams have developed proprietary coating compositions and geometries, but significant knowledge gaps exist in terms of the resulting properties of the coating and the cladding and how those components impact each other in reactor conditions. Furthermore, the national laboratory and university teams currently studying the industry concepts are limited in their ability to freely disseminate and discuss results obtained on commercial coatings. The Advanced Fuels Campaign is therefore working to develop an understanding of ‘generic’ coatings applied to commercial nuclear cladding alloys free of these constraints. This milestone report provides insights in the microstructure of a 7-micrometer Cr coating on Zircaloy-2 and a 5- micrometer coating on Zry-4 as reference materials. SEM and TEM methods were utilized to describe and identify the interface, while nanoindentation was used to determine hardness and E-Moduli of coating and cladding material. This milestone summarizes the acquired knowledge to build a necessary verified foundation for future simulation and qualification efforts.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Enhancing Formability of AA2219 Aluminum Alloy Friction Stir Welded Blanks with Preheating Treatment

The deformation behaviors of FSW blank are complicated due to the incompatibility of the mechanical property and microstructure for the weld and base material. In order to improve the formability of friction stir welded (FSW) blanks, the weld and base material in this paper were subjected to preheating treatments of 250, 300, 350, 400, and 450 °C, plus a solution treatment of 535 °C. The deformation behavior of the AA2219 FSW blank was characterized using uniaxial tension, microhardness test, hydro-bulging test and electron backscattered diffraction to determine the relationship of the deformation property and microstructure for the FSW blanks. Full strain fields of the tensile and bulging specimens were used to analyze the deformation uniformity of the weld and base material under uniaxial tension and biaxial tension stress states. With the limiting bulging height under various preheating temperatures, the formability behavior of the weld and base material was analyzed during the whole bulging process. The optimum preheating temperature can increase the formability and refrain from abnormal grain growth of the weld on the premise of maintaining the weld strength. The limiting bulging height of FSW blank is obviously improved by the lower preheating temperature from 300 to 350 °C. Additionally, the weld position has a significant impact on the deformation of the whole FSW blanks.

36 MATERIALS SCIENCE↗

60 keV Ar⁺-ion induced modification of microstructural, compositional, and vibrational properties of InSb

Room temperature irradiation of InSb(111) by 60 keV Ar⁺-ions at normal (0°) and oblique (60°) angles of incidence led to the formation of nanoporous structure in the high fluence regime of 1×10¹⁷ to 3×10¹⁸ ions cm⁻². While a porous layer comprising of a network of interconnected nanofibers was generated by normal ion incidence, evolution of plate-like structures was observed for obliquely incident ions. Systematic studies of composition and structure using energy dispersive x-ray spectroscopy, Raman spectroscopy, x-ray photoelectron spectroscopy, Raman mapping, grazing incidence x-ray diffraction, and cross-sectional transmission electron microscopy revealed a high degree of oxidation of the ion-induced microstructures with the presence of In₂O₃ and Sb₂O₃ phases and presence of nanocrystallites within the nanoporous structures. The observed structural evolution was understood in terms of processes driven by ion-induced defect accumulation within InSb.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Microstructure and Hard Magnetic Properties of Sm 1-x Zr x (Fe,Co) 11.3-y Ti 0.7 By Ingots and Thick Melt-Spun Ribbons

Permanent magnets made from Sm(Fe,Co) 12 -based compounds are being actively pursued through nanostructuring and powder metallurgy. This study was aimed at the development of hard magnetic properties in bulk as-cast alloys and in melt-spun alloys for very low wheel speeds. Slower solidification rates and alloying with Zr promote the tetragonal ThMn 12 -type crystal structure, whereas higher solidification rates and alloying with B replace the ThMn 12 structure type with the TbCu 7 structure type. When introduced simultaneously, Zr and B dramatically reduce the alloy solidification rates required for both the refinement of the 1:12 crystallites and their replacement with the 1:7 phase. In bulk arc-melted alloys, this allowed for a microstructure of separated 1:12 crystallites 1–3 μm in size, although, because of the ferromagnetic nature of a minority phase, the coercivity of these fine-grained alloys reached only 0.73 kOe. A moderately accelerated solidification further refined the 1:12 crystallites and increased the coercivity; a Sm 0.7 Zr 0.4 (Fe,Co) 10.8 Ti 0.7 B 0.5 alloy exhibited a coercivity of 1.5 kOe and a maximum energy product of 3.4 MGOe when it was melt-spun into a 0.26-mm-thick ribbon. A more rapid solidification suppressed the 1:12 phase and after annealing at 800–850 °C, the alloys modified with Zr and B developed reasonably high coercivity and maximum energy product even when melt-spun at a wheel speed of 6 m/s. For the above-mentioned alloy, these values were 4.1 kOe and 7.8 MGOe, respectively. Further, a similarly processed very-Sm-lean Sm 0.5 Zr 0.6 (Fe,Co) 10.6 Ti 0.7 B 0.7 alloy exhibited a remanence of 8.8 kG and an energy product of 7.4 MGOe.

36 MATERIALS SCIENCE↗

Microstructure characterisation and mechanical properties of a functionally-graded NbC/high chromium white cast iron composite

Highlights: • A functionally-graded NbC – white cast iron composite was centrifugally cast. • Primary NbC particle distribution follows Stokes' Law, with 30 vol% at the surface. • Presence of primary NbC particles refined eutectic M{sub 7}C{sub 3} morphology at the surface. • The surface layer was hard and wear resistant, while the interior was tougher. • NbC and M{sub 7}C{sub 3} carbides form independent eutectic structures within the interior. - Abstract: A functionally graded NbC – high chromium white cast iron composite was successfully fabricated by centrifugal casting for high wear applications. The migration of primary NbC particles to the outer periphery, as predicted by Stokes' law, resulted in an extremely hard outer layer at the surface of a softer bulk material. Microstructural characterisation showed that both the volume fraction and the morphology of the carbides varies along the thickness of the specimen. At the outer surface, the NbC was present as primary carbides while Chinese-script NbC was found in the bulk of the material. Hardness, sliding wear and three-point bending tests confirmed that the outer layer was harder and more wear resistant than the rest of the material, which was correspondingly tougher. The study of the fracture surface of the specimens showed that there is a strong bond between NbC and the matrix such that delamination between the reinforcements and the matrix did not occur during fracture. If Chinese-script NbC can be reduced or prevented in the bulk material, further improvements to toughness could be achieved.

36 MATERIALS SCIENCE↗

Microstructural Development and Mechanical Properties for Reactive Air Brazing of ZTA to Ni Alloys using Ag-CuO Braze Alloys

Reactive air brazing (RAB) is a potential joining technique to join metal alloys to ceramics for a variety of applications. In the current study, nickel (Ni) alloys were heat treated to form an oxide layer prior to RAB joining to zirconia toughened alumina (ZTA). The Ni alloys evaluated were Nicrofer 6025 HT, Inconel 600, Inconel 693, Haynes 214 and Inconel 601. The ZTA studied had compositions of 0 to 15 wt% zirconia and 0 to 14 wt% glass. Four point-bend tests were performed to evaluate the joint strength of ZTA/ZTA and ZTA/nickel alloys brazed with Ag-2wt% CuO braze alloys. It was determined that the joint strength is not a function of the ZTA composition, but that the strength is a strong function of the chemistry and microstructure of the oxide layer formed on the nickel alloy. It was determined that an increase in the aluminum content of the Ni alloy resulted in an increase of the thickness of alumina in the oxide layer and was directly proportional to the bond strength with the exception of Inconel 601 which exhibited relatively high joint strengths even though it had a relatively low aluminum content.

Ag-CuO↗

Novel preparation of Al-5%Cu / BN and Si3N4 composites with analyzing microstructure, thermal and mechanical properties

Highlights: • The novel MMCs Al5Cu-Si{sub 3}N{sub 4}/BN successfully produced by squeeze casting techniques • Squeeze casting technique improves the wettability between the matrix and nitrides. • XRD analysis showing the presence of new AlN and AlB{sub 2} phases • The hardness curves of the MMCs exhibited the increasing trend till reaching peak. • BN reinforcements significantly accelerate precipitation behavior of Al-5%Cu alloy. - Abstract: The purpose of this research is to develop and characterize composites of Al-5%Cu alloy reinforced by silicon and boron nitride (Si{sub 3}N{sub 4}, BN). The developing of this type of composites gives a new trend of metal matrix composite synthesizing, especially in the case of boron nitride. The stir cast composites showed large areas of porosity and agglomeration. On the other hand, the squeezed cast composites exhibited a fairly uniform particles distribution throughout the matrix alloy. The microstructure and XRD results of the composites confirmed a reaction occurred at the interface between the particles and alloy. AlN and AlB{sub 2} phases were identified in Al5%Cu-Si{sub 3}N{sub 4} and Al5%Cu-BN composites respectively. The ageing results showed that the time to reach peak hardness decreased with addition of the particles. Also, the ageing kinetics was significantly accelerated due to the presence of BN particulates. The coefficient of thermal expansion (CTE) results of the matrix alloy and its composites were practically and theoretically determined. Difference between experimental and calculated values of CTE was less than 8%. Increasing the concentration of Si{sub 3}N{sub 4} increased YS from 215 MPa in the matrix alloy to 285 MPa in the Al-5%Cu-7%Si{sub 3}N{sub 4} composites at a testing temperature of 20 °C.

36 MATERIALS SCIENCE↗

Micro- and macro-scale characterization of nano-SiO2 reinforced alkali activated slag composites

Highlights: • Combined advanced micro-scale measurements were used to predict properties of NS AASC. • NS enhances both the macro- and micro-mechanical properties of AASC. • Combination of MIP and XCT facilitates a complete characterization of pore structure. • Combined tools at multi-scale provide efficient approaches to optimize material design. - Abstract: The effect of nano-SiO{sub 2} on the micromechanical properties and microstructure of alkali-activated slag cement (AASC) composites was investigated. The investigation involved the use of: (i) nanoindentation to determine the elastic properties of the constituent phases using statistical deconvolution; (ii) scanning electron microscopy equipped with energy-dispersive X-ray spectroscopy and backscattered electrons to identify and characterize the solid phases in the microstructure; and (iii) X-ray computed tomography microscopy to determine the morphology of microscale pores and mercury intrusion porosimetry to measure the volume fraction of the nanoscale pores. The combined use of micro- and macro-scale characterization tools can establish a logical link between the macro-mechanics, microstructure, and micromechanical properties, which provides valuable information aiding the material design of AASC with nanoparticles.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Microstructural Characteristics and Mechanical Properties in the Laser Beam Welded Joints of High-Strength Microalloyed Steel

The laser beam welded joints of the high-strength microalloyed steel consist of the base metal (BM), the partially transformed heat-affected zone I (PTHAZ-I), the partially transformed heat-affected zone II (PTHAZ-II), the fully transformed heat-affected zone (FTHAZ) and the fusion zone (FZ). The martensite/austenite (M/A) islands of the bainites in the PTHAZ-II are dense versus those in the PTHAZ-I, and the martensites exist in the FTHAZ and the FZ together with the bainites under the slow welding speed. The M/A islands of the bainites and/or the martensites in the PTHAZ become denser under the high welding speed, and the martensites in the FTHAZ and the FZ predominate. The low-angle boundary density and the high local misorientation proportion are used to identify the constituents roughly, consistent with the microstructural characteristics in the welded joints. The misorientation angle distributions are employed to evaluate the degree of the phase transformation, reflecting the change law of the degree of the phase transformation in the welded joints. The hardness and the tensile tests indicate that the HAZ and the FZ are stronger than the BM, dependent on the microstructures in the welded joints. The strengthening in the HAZ and the FZ is mainly attributed to the products of non-equilibrium phase transformation with the high dislocation density.

36 MATERIALS SCIENCE↗

A macro-micro approach for identifying crystal plasticity parameters for necking and failure in nickel-based alloy haynes 282

Here, this work develops a two-scales macro-micro approach to address the challenge in calibrating crystal plasticity microstructural models when samples undergo necking prior to fracture. The crystal plasticity models are crucial for predicting the materials’ plastic deformation and failure at the microstructure level, identifying the materials’ intrinsic properties as well as investigating the microstructure-properties relationships. However, after necking occurs, the experimentally measured stress-strain curves fail to reflect the materials ‘true’ stress-strain behavior and cannot be directly fitted into crystal plasticity models. The proposed macro-micro approach employs a top-down strategy to address this challenge, which has been studied with experimental tests on precipitation-strengthened Ni-based superalloy Haynes® 282®. In this approach, a macro rate-dependent anisotropic plasticity model with Voce-type hardening and Rice-Tracey damage law is first utilized to model the deformation and failure of the tensile bar, and calibrated by matching the stress-strain curves, necking strain, and reduction of area. Especially, to match the testing results under different applied strain rates, the rate-sensitivity parameter m and saturation stress in the elasticity model are modified to incorporate dependence on the local strain rate. Then, the ‘true’ stress-strain behaviors are extracted from the necking zone of the macro-model, which are used to calibrate a micro-model with explicit microstructures and governed by an extended crystal plasticity law. The consistency between the micro-model and macro-model are enforced during calibration. The calibration outcomes from the crystal plasticity model elucidate the materials intrinsic properties for slip, hardening, and failure, which is vital for further investigations into the microstructure-properties relationship and for accurate prediction of the material behavior under various test and service conditions.

36 MATERIALS SCIENCE↗

Microstructural Analysis and Transport Properties of Thermally Sprayed Multiple-Layer Ceramic Coatings

In this paper, multilayer, graded ceramic/metal coatings were prepared by an air plasma spray method on Ti-6Al-4V, 4140 steel and graphite substrates. The coatings were designed to provide thermal barriers for diesel engine pistons to operate at higher temperatures with improved thermal efficiency and cleaner emissions. A systematic, progressive variation in the mixture of yttria-stabilized zirconia and bondcoat alloys (NiCoCrAlYHfSi) was designed to provide better thermal expansion match with the substrate and to improve thermal shock resistance and cycle life. Heat transfer through the layers was evaluated by a flash diffusivity technique based on a model of one-dimensional heat flow. The aging effect of the as-sprayed coatings was captured during diffusivity measurements, which included one heating and cooling cycle. The hysteresis of thermal diffusivity due to aging was not observed after 100-h annealing at 800 °C. The measurements of coatings on substrate and freestanding coatings allowed the influence of interface resistance to be evaluated. Finally, the microstructure of the multilayer coating was examined using scanning electron microscope and electron probe microanalysis.

36 MATERIALS SCIENCE↗

Directly obtained τ-phase MnAl, a high performance magnetic material for permanent magnets

The metastable tetragonal τ-phase has been directly obtained from casting Mn{sub 0.54}Al{sub 0.46} and (Mn{sub 0.55}Al{sub 0.45}){sub 100}C{sub 2} using the drop synthesis method. The as-casted samples were ball milled to decrease the particle size and relaxed at 500 °C for 1 h. The phase composition, crystallographic parameters, magnetic properties and microstructure were systematically studied. The results reveal that the τ-phase could be directly obtained from drop synthesis. The highest M{sub s} of 117 emu/g was achieved in the (Mn{sub 0.55}Al{sub 0.45}){sub 100}C{sub 2} where the τ-phase was stabilized by doping with carbon. Carbon doping increased the c/a ratio of the τ-phase as it occupies specific interstitial positions (½, ½, 0) in the structure. Furthermore, ball milling increases the coercivity (H{sub c}) at the expense of a decrease in magnetic saturation (M{sub s}). The increase in coercivity is explained by a decrease of grain size in conjunction with domain wall pinning due to defects introduced during the ball milling process. - Graphical abstract: The tetragonal τ-phase has been directly obtained from casting Mn{sub 0.54}Al{sub 0.46} and (Mn{sub 0.55}Al{sub 0.45}){sub 100}C{sub 2} using the drop synthesis method. The phase composition, crystallographic parameters, magnetic properties and microstructure were systematically studied. The highest M{sub s} of 117 emu/g was achieved for (Mn{sub 0.55}Al{sub 0.45}){sub 100}C{sub 2} ball milling increases the coercivity (H{sub c}) at the expense of a decrease in magnetic saturation (M{sub s}). - Highlights: • The ferromagnetic τ-phase has been directly obtained from casting. • The highest M{sub s} of 117 emu/g was achieved for (Mn{sub 0.55}Al{sub 0.45}){sub 100}C{sub 2}. • Ball milling increases the coercivity but decreases the magnetic saturation.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effect of isochronal annealing on the microstructure, texture and mechanical properties of a cold-rolled high manganese steel

Highlights: • Recrystallised γ grains have similar orientations to reverted/recovered γ grains. • After reversion, γ orientations are correlated to ε and α′-martensite orientations. • γ nucleation at the boundary of reverted/recovered γ grains - Abstract: A Fe-17Mn-3Al-2Si-1Ni-0.06C wt.% steel was subjected to cold-rolling to 42% thickness reduction and isochronally annealed for 300 s between 500 and 850 °C. The high Mn steel was characterised via electron back-scattering diffraction, transmission electron microscopy and uniaxial tensile testing. The reversion of deformation-induced ε and α′-martensite to austenite (γ) was witnessed with the formation of fine twins in reverted/recovered γ grains after annealing to 650 °C. The nucleation of new γ grains at the boundary of reverted/recovered γ grains was also noted. Upon reversion, the γ orientations originated from the ε and α′-martensite orientations by phase transformation via the Shoji-Nishiyama and Kurdjumov-Sachs orientation relationships, respectively. Upon segmenting the γ grains, the recrystallised γ grains were observed to nucleate with orientations similar to those of the reverted/recovered γ grains. Uniaxial tension on a fully recrystallised γ microstructure showed that the initial γ grain size has a more significant effect on the yield strength than the ε and α′-martensite fractions. On the other hand, the initial ε and α′-martensite fractions affect the total elongation.

36 MATERIALS SCIENCE↗

Effect of annealing temperature on the contact properties of Ni/V/4H-SiC structure

A sandwich structure of Ni/V/4H-SiC was prepared and annealed at different temperatures from 650 °C to 1050 °C. The electrical properties and microstructures were characterized by transmission line method, X-ray diffraction, Raman spectroscopy and transmission electron microscopy. A low specific contact resistance of 3.3 × 10{sup -5} Ω·cm{sup 2} was obtained when the Ni/V contact was annealed at 1050 °C for 2 min. It was found that the silicide changed from Ni{sub 3}Si to Ni{sub 2}Si with increasing annealing temperature, while the vanadium compounds appeared at 950 °C and their concentration increased at higher annealing temperature. A schematic diagram was proposed to explain the ohmic contact mechanism of Ni/V/4H-SiC structure.

36 MATERIALS SCIENCE↗

Microstructural, optical and electrical properties of LaFe{sub 0.5}Cr{sub 0.5}O{sub 3} perovskite nanostructures

Perovskite nanocrystalline powder of LaFe{sub 0.5}Cr{sub 0.5}O{sub 3} was synthesized by sol-gel combustion route and characterized by x-ray diffractometer (XRD), scanning electron microscopy (SEM) equipped with EDS, UV-visible and LCR meter at room temperature Rietveld refinement of the XRD data confirms that the sample is in single phase-rhombohedral structure with space group R-3C. SEM micrograph shows clear nanostructure of the sample and EDS ensures the presence of all elements in good stoichiometric. The optical absorption indicates the maximum absorption at 315 nm and optical band gap of 2.94 eV was estimated using Tauc’s relation. Dielectric constant (ε’) and loss were found to decrease with increase in frequencies. The dielectric behavior was explained on the basis of Maxwell-Wagner’s two layer model.

77 NANOSCIENCE AND NANOTECHNOLOGY↗