Design of heterogeneous structured Al alloys with wide processing window for laser-powder bed fusion additive manufacturing

Required microstructural attributes of an alloy vary with structural applications. The microstructural fine-tuning capability of laser-powder bed fusion (L-PBF) additive manufacturing (AM) enables application specific manufacture of the components. Such manufacture with L-PBF AM requires alloys that exhibit wide processing window and are amenable to multiple deformation mechanisms. However, high hot cracking susceptibility of Al alloys poses a barrier to such printability-performance synergy. In this work we show that an integration of, a) grain refinement through heterogeneous nucleation, and b) eutectic solidification, leads to crack-free parts at wide range of process parameters, microstructural heterogeneity, and hierarchy in the Al-Ni-Ti-Zr alloy. Such an integration targets hot cracking at multiple stages of solidification in L-PBF as opposed to the contemporary alloy design strategies that target hot-cracking at only specific stages of solidification. The Al-Ni-Ti-Zr alloy exhibits excellent printability and a high as-built tensile performance. Due to the wide processing window and amenability to multiple deformation mechanisms, the alloy microstructure and subsequently the performance, can be fine-tuned. Here, such strategy opens the gateway for application-specific manufacture of Al alloys with L-PBF AM and establishes a fundamental shift in current methodologies for design of these alloys for L-PBF AM.

36 MATERIALS SCIENCE↗

Effect of different grain boundary diffusion alloys on magnetic properties of Dy-free sintered NdFeB magnet

Dy-free sintered magnets were fabricated by blending Neo powder with different grain boundary diffusion alloy powders. Cu, CeAl and CeAlCu have a negative effect on H cj of magnets, while PrAlCu and AlCuGa have a positive effect. The PrAlCu-added magnet achieves the best magnetic properties among all magnets with the additions of different diffusion alloys. With increasing PrAlCu from 0-10 wt.%, H cj of the magnets gradually increases from the original 14.5 kOe to 19.2 kOe. The magnet with 7.5 wt.% PrAlCu obtains a H cj of 18 kOe and (BH) max of 39.1 MGOe. It is found that Pr and Cu in PrAlCu alloy is mainly distributed at grain boundary and triple junctions, leading to a reduced coupling among grains, thus an enhanced H cj . Here, the grain boundary engineering by adding an appropriate alloy is an effective method to improve H cj of Dy-free NdFeB magnets.

36 MATERIALS SCIENCE↗

Effect of Zr and Sc additions on coarsening- and creep resistance of AlSi10Mg fabricated by laser powder bed fusion

Microstructure and creep properties are studied in a eutectic AlSi10Mg alloy modified with Zr and Sc additions (Al-9.8Si-0.32Mg-0.70Zr-0.23Sc, wt%) manufactured through laser powder-bed fusion (L-PBF). Three types of Zr/Sc-bearing powders - elemental, master-alloy, and pre-alloyed - are employed in the fabrication process, with the pre-alloyed powders providing the highest incorporation of Zr and Sc in the Al matrix. Here, the as-printed alloy exhibits a fine cellular Al-Si eutectic structure which fragments and coarsens into micron-sized Si particles during aging at 300 ºC, leading to a steady drop in alloy microhardness between 0.1 and 1000 h. Coarsening of the eutectic Si phase during aging is not measurably affected by Zr and Sc in solid solution, which precipitate during aging and increases strength, compensating weakening from Si coarsening between 1 and 200 h at 300 ºC. Atom-probe analysis in the peak-aged condition (96 h/300 °C) confirms the presence of Al 3 (Sc,Zr) secondary nano-precipitates with an average radius of 1.0 nm and some Si solubility. Micron-sized grains are present throughout the alloy, with ultra-fine-grained regions at the melt pool boundaries, neither of which coarsen during long-term aging at 300 ºC. Under creep conditions at 300 °C, the Zr/Sc-bearing alloy with Al 3 (Sc,Zr) nano-precipitates exhibits power-law behavior, with a high apparent stress exponent (n a = 9) and a high threshold stress (σ th = 43 MPa), exhibiting nearly double the strength of a Zr/Sc-free AlSi10Mg control alloy (σ th = 22 MPa).

36 MATERIALS SCIENCE↗

Evaluation of Directed Energy Deposition and Laser Powder Bed Fusion Nickel-Based Alloys Process Application Envelopes Based on Performance, Process Economics, Supply Chain Risks, and Reactor-Specific Targeted Components

The goal of the Advanced Materials and Manufacturing Technologies (AMMT) program is to accelerate the deployment of new materials and manufacturing technologies into advanced nuclear-related systems. Although 316H stainless steel fabricated by laser powder bed fusion (LPBF) has already been identified as an alloy that could have a significant effect on various reactor technologies, many other materials and manufacturing techniques are being evaluated. Nickel-based alloys typically offer higher-temperature capabilities compared with advanced stainless steels, and previous reports looked at three Ni-based alloy categories: low-Co alloys with a potential use close to the reactor core; high-temperature, high-strength alloys; and molten salt–compatible alloys. Due to the increasing interest in the low Co 625 alloy for nuclear applications, the alloy was compared at the Oak Ridge National Laboratory (ORNL) with 617, 230, two high-temperature, high-strength solution-strengthened alloys. Hot cracking could not be suppressed for alloy 230, and it was shown that these cracks, which were elongated along the build direction (BD), had a drastic effect on the ductility of alloy 230 at room temperature when specimens were machined perpendicular to the BD. Cracking was not as significant for alloy 617, but still led to significant variation in ductility at room temperature along the build direction. On the contrary, LPBF printing of crack-free alloy 625 was achieved using similar printing parameters, and the alloy looks like a very promising candidate for various reactor technologies.

36 MATERIALS SCIENCE↗

Microstructural and Hall–Petch Analysis of Additively Manufactured Ferritic Alloy Using 2507 Duplex Stainless Steel Powder

The powder bed fusion–laser beam (PBF-LB) process, a method of additive manufacturing (AM), was used to print duplex stainless steel (DSS) using commercial-grade 2507 powders. While conventionally processed DSS has a two-phase microstructure consisting of 50% austenite and 50% ferrite, the PBF-LB-printed 2507 alloy was nearly 100% ferrite. Optimal processing conditions that minimized porosity were determined to be 290 W laser power and 1000 mm/s scan speed, and grain size, texture, and phases were characterized as a function of laser power and scan speed. Grain size increased with increasing laser power but decreased with increasing scan speed. A <100> texture diminished with increasing scan speed from 1000 mm/s to 1400 mm/s. No austenite phase was detected. Transmission electron microscopy (TEM) and scanning transmission electron microscopy (STEM) characterization revealed nanoscale chromium nitride precipitates in the ferritic matrix (incoherent hexagonal close-packed (HCP) precipitates at grain boundaries and coherent body-centered cubic (BCC) precipitates within the grains) and a high density of tangled dislocations. Tensile tests of as-printed alloys showed a yield strength of 570 MPa, an ultimate tensile strength of 756 MPa, and an elongation to failure of 10%. The tensile properties were analyzed based on the observed microstructure considering grain size, nanoscale precipitates, and the high density of dislocations.

Crystallography↗

Chemistry effects on ODS steel consolidated via laser powder bed fusion from GARS powder

Oxide Dispersion Strengthened (ODS) steels are promising candidate alloys for structural and cladding applications in extreme environments. They contain a high density of nanoscale oxides for high temperature mechanical strength and radiation resistance. In this work, gas atomization reaction synthesis (GARS) was used to produce powders that were used for additive manufacturing (AM) Laser Powder Bed Fusion consolidation of ODS steels, in order to skip the traditional mechanical alloying of blended yttria and alloy powders. Powder containing iron, chromium, and tungsten with varying amounts of yttrium, titanium, oxygen and zirconium were used to produce ODS steel samples. AM consolidated specimens and powder samples were characterized with transmission electron microscopy. TEM imaging, diffraction patterns, and energy dispersive X-ray spectroscopy (EDS) was used to identify phases present before and after consolidation across chemistries. The effect of the controlled oxygen input (from GARS) and the oxide-forming additions (Y, Ti, Zr) on precipitate size distribution and composition is substantiated and discussed.

36 MATERIALS SCIENCE↗

Comparison of powder bed fusion and directed energy deposition for tailoring mechanical properties of traditionally brittle alloys

The mechanical performance of an Fe-Co intermetallic alloy processed by laser powder bed fusion (L-PBF) and laser directed energy deposition (L-DED) additive manufacturing is compared. L-PBF material was characterized by high strength (500–550 MPa) and high ductility (35%) in tension, corresponding to a ~250% increase in strength and an order-of-magnitude improvement in ductility relative to conventional material. Conversely, L-DED material exhibited similarly poor tensile properties to the conventional wrought alloy, with low strength (200–300 MPa) and low ductility (0–2.7%). Finally, the disparity in properties between L-PBF and L-DED material is discussed in the context of the fundamental differences between manufacturing methods.

36 MATERIALS SCIENCE↗

Effect of laser power on roughness and porosity in laser powder bed fusion of stainless steel 316L alloys measured by X-ray tomography

The quality of metal objects fabricated via laser powder bed fusion are highly affected by process parameters, and their influence on final products is yet to be fully explored. In this work, pyrometry signals of the melt pool were collected from a set of stainless-steel samples during manufacturing and the effect of laser power on porosity and roughness of final printed parts was analyzed. Results show that the melt pool pyrometry signal of contours increases with higher laser power, whereas it is lower and decreases for the infilled part. Post-built X-ray computed tomography imaging reveals that porosity decreases while sample roughness increases upon increasing laser power. The decrease in porosity with increasing laser power is attributed to the larger size of the contour welds that were printed first, leading to an increase in dimension of the final products.

36 MATERIALS SCIENCE↗

Developing ductile and isotropic Ti alloy with tailored composition for laser powder bed fusion

Laser powder bed fusion (LPBF) is an advanced technology to create metallic components with complex geometry. Ti-6Al-4V (Ti64) is one of the most frequently used materials for LPBF. The intrinsic high cooling rates and ultra-high directional thermal gradient of melt, however, lead to a hierarchical structure composed of fine martensitic alpha' within columnar prior-beta grains in LPBF Ti64. This microstructure results in poor ductility and strong mechanical anisotropy in as-built Ti64 components, which largely limit their applications. Here, we report that the above shortcomings can be overcome by tailoring the alloy composition. Specifically, by reducing the aluminum content from 6 wt% to 4 wt%, the resultant LPBF Ti-4Al-4V (Ti44) alloy exhibits substantially improved ductility and mechanical isotropy. These improvements are attributed to grain refinement during solidification and the activation of multiple slip modes and twinning in the as-built material during deformation. This work offers a simple strategy to design new titanium alloys for LPBF with significantly improved ductility and isotropy.

36 MATERIALS SCIENCE↗

SA508 low alloy steel to 316L stainless steel dissimilar metal joint made by powder metallurgy hot isostatic pressing

Joining ferritic SA508 low alloy steel (LAS) and austenitic 316 L stainless steel (SS) via powder metallurgy hot isostatic pressing (PM-HIP) was evaluated as an alternative method to welding. This study investigated the mechanical and microstructural evolutions of the bimetallic interface under different joint designs and heat treatments. Here, the direct joining of dissimilar metal alloys by PM-HIP method resulted in two designs: 1) powder SA508 to solid bar 316 L (P508–B316L) and 2) powder 316 L solid bar SA508 (P316L-B508). In both cases, P508–B316L and P316L-demonstrated satisfactory tensile strength, however, high hardness and severe depreciation in toughness were located on the bimetallic interface. The mechanisms responsible for the detrimental mechanical properties were verified. Large oxides were observed in P508–B316L due to the prior powder boundary (PPB) oxides present in SA508 powder. The intense sensitization occurred from the formation of M 23 C 6 carbides, consequently from the slow cooling after PM-HIP in P316L-B508. Post-HIP heat treatments were explored to reduce the distance of carbide formation; however, the heat treatment could not eliminate the carbides. The experimental results were compared to the diffusion couple simulation as a function of carbide formation with distance. The analysis also showed the high hardness at the bimetallic interface was primarily contributed by solid solution strengthening. In conclusion, the direct joining of P316L-B508 and P508–B316L via PM-HIP was deemed to be unfeasible, and a transitional material is necessary to impede the diffusion of carbon.

316L stainless Steel↗

Local atomic configurations in mechanically alloyed amorphous (FeCoNi) 70 Ti 10 B 20 powders

Here, the atomic structure of amorphous (FeCoNi) 70 Ti 10 B 20 alloy synthesized by mechanical alloying was investigated using high energy synchrotron X-ray diffraction and inverse Monte Carlo simulations of pair distribution functions. Empirical potential structure refinement indicates a chemical short-range order at the length scales of 2.1–2.5 Å via local atomic arrangements forming deformed bcc-like clusters. The structural model obtained was described by bond lengths, coordination numbers, and bond angle distribution functions determined for the first neighbor atoms by x-ray scattering supplemented with 3D Monte Carlo simulations.

36 MATERIALS SCIENCE↗

Methods of producing a titanium alloy product

A method for producing a particulate titanium alloy product can include preparing a composite particulate oxide mixture with TiO2 powder and at least one alloying element powder. The composite particulate oxide mixture can be co-reduced using a metallic reducing agent under a hydrogen atmosphere at a reduction temperature for a reduction time sufficient to produce a hydrogenated titanium alloy product. The hydrogenated titanium alloy product can then be heat treated under a hydrogen atmosphere and a heat treating temperature to reduce pore size and specific surface area to form a heat treated hydrogenated titanium product. The heat treated hydrogenated titanium product can be deoxygenated to reduce residual oxygen to less than 0.2 wt % to form a deoxygenated hydrogenated titanium product as a particulate. The deoxygenated hydrogenated titanium product can optionally be dehydrogenated to form the titanium alloy product as a particulate.

Fang, Zhigang Zak↗

Laser powder bed fusion of oxide dispersion-strengthened IN718 alloys: A complementary study on microstructure and mechanical properties

In this study, two new grades of oxide dispersion strengthened (ODS) Inconel 718 (IN718) alloys were designed by the thermochemical CALPHAD method and produced by laser powder bed fusion (LPBF) technique. Alloys designated as IN718-YF and IN718-YFH, that consist Y 2 O 3 –FeO and Y 2 O 3 –FeO–Hf, respectively, were fabricated with >99.9 % densification using optimized process parameters. CALPHAD calculations were highly consistent with experimental findings, highlighting the formation of Al-containing Y–Ti–O and Y–Hf–O nano-oxides in both alloy types. Texture analyzes revealed no significant texture development in as-built (AB) or heat-treated (HT) alloys. Heat treatment was applied at 1050 °C for 1 h to enhance nano-oxide density. Further, the nano-oxide number density remained similar in IN718-YF while it decreased in IN718-YFH alloy as a result of carbide formation after the heat treatment. Besides, formation of secondary γ' particles was observed in the IN718-YFH/HT alloy. Even though the yield strengths of IN718-YF and IN718-YFH alloys in both AB and HT conditions were similar, the ductility of IN718-YFH was ~50 % less in almost all conditions compared to the ductility of IN718-YF. This has been shown to be as a result of irregular shaped micron-sized Y-Hf-O oxides, martensite formation in AB condition, increased amount of carbides and existence of secondary γ' particles in HT condition in IN718-YFH. High density of stacking faults (SF) forming at the interface of the nano-oxides have been detected in IN718-YF alloys. Besides dislocation/nanoparticle interactions, SFs which are responsible for the delocalization of the deformation improve the ductility of IN718-YF alloys. Overall, high temperature mechanical tests exhibit that both alloys have higher strength with improved ductility compared to the standard IN718 alloys, indicating the contribution of the nano-oxides.

36 MATERIALS SCIENCE↗

Boosting the Strength and Electrical Conductivity of Aluminum Alloys

It is common practice to use pure copper as the material of choice in applications requiring adequate strength and high electrical conductivity (EC). However, the overwhelming increase in the cost and worldwide demand for copper is becoming a major concern. As the move towards electrification throughout the world is occurring, so is a parallel move to make aluminum (Al) and Al alloys suitable as a replacement for copper. To make this goal a reality, exploration into enhancements in the strength and EC of high conductivity Al alloys is necessary. This study compiles strength and EC data for current Al powder metallurgy (PM) alloys to better understand existing data and target future research. Also highlighted are reviews of completed research projects, including studies relating to liquid metallurgy, by industry professionals and academia, noting both shortcomings and successes.

Imbrogno, Peter↗

LPBF Processability of NiTiHf Alloys: Systematic Modeling and Single-Track Studies

Research into the processability of NiTiHf high-temperature shape memory alloys (HTSMAs) via laser powder bed fusion (LPBF) is limited; nevertheless, these alloys show promise for applications in extreme environments. This study aims to address this limitation by investigating the printability of four NiTiHf alloys with varying Hf content (1, 2, 15, and 20 at. %) to assess their suitability for LPBF applications. Solidification cracking is one of the main limiting factors in LPBF processes, which occurs during the final stage of solidification. To investigate the effect of alloy composition on printability, this study focuses on this defect via a combination of computational modeling and experimental validation. To this end, solidification cracking susceptibility is calculated as Kou’s index and Scheil–Gulliver model, implemented in Thermo-Calc/2022a software. An innovative powder-free experimental method through laser remelting was conducted on bare NiTiHf ingots to validate the parameter impacts of the LPBF process. The result is the processability window with no cracking likelihood under diverse LPBF conditions, including laser power and scan speed. This comprehensive investigation enhances our understanding of the processability challenges and opportunities for NiTiHf HTSMAs in advanced engineering applications.

36 MATERIALS SCIENCE↗

Variations in GARS powder microstructure as a function of powder chemistry and particle size

The properties of metal produced through powder metallurgy depends on the feedstock used. Powders produced via gas atomization reaction synthesis (GARS) are used to produce oxide dispersion strengthened alloys. The desired powder size range can vary for each consolidation technique. However, powder microstructure also can vary with powder particle size, which in turn can impact the microstructure and properties of the consolidated parts. In this study, GARS powders are characterized via inductively coupled plasma mass spectroscopy, inert gas fusion, and high-resolution x-ray diffraction to determine variations in elemental and phase compositions. Transmission electron microscopy was used to understand microstructure variations as a function of chemistry and size. Across the three batches tested intermetallic content was 0.73–1.35 wt% in the 0-20 μm powder batch and increased to 2.46–3.80 wt% in the coarse 45-106 μm batch. Across all batches, volume percent of surface oxidation decreased with powder diameter, with volume percents within the range of 0.75–1.2 % across 10 μm powder particles, and below 0.4 % across coarse powder particles approximately 100 μm in diameter. These observations were supported by inert gas fusion measurements. However, the oxide layer was thicker in coarse powder particles due to a slower cooling rate. Increasing oxygen content in atomization gas to 2000 ppm and adding yttrium increased both the surface oxidation content and yttrium intermetallic content. Lastly, intermetallic phases within the powder coarsened with powder size. Intermetallic morphology changed from fine spherical intermetallic and columnar dendritic growth to a cellular structure with finer spherical intermetallic, to coarse irregular intermetallic and intermetallic along grain boundaries as a result of slower cooling rate and solidification rate in coarse powder particles. Furthermore, the addition of zirconium does not appear to significantly change intermetallic morphology, but the composition changed from a Y-Fe rich intermetallic to a Y-Zr-Fe intermetallic.

42 ENGINEERING↗

Solving Recent Challenges for Wrought Ni-Base Superalloys

This paper reviews the status of technology in design and manufacture of new wrought 21 polycrystalline Ni-base superalloys for critical engineering applications. There is a strong 22 motivation to develop new alloys that are capable of operating at higher temperatures to 23 realise improvements in thermal efficiency, which are necessary to achieve environmental 24 targets for reduced emissions of harmful green-house gases. From the aerospace sector, 25 the development of new powder metallurgy and ingot metallurgy alloys are discussed for 26 disk rotor and static applications. New compositions for powder metallurgy contain about 27 50-55% of gamma prime (γ') strengthening precipitates to ensure components operate 28 successfully at temperatures up to 788°C (1450°F). In contrast, new compositions for ingot 29 metallurgy aim to occupy a design space in temperature capability between Alloy 718 and 30 current powder alloys that are in-service, and show levels of γ' of about 30-44%. The focus 31 in developing these alloys was design for manufacturability. To complement the aerospace 32 developments, a review of work to understand the suitability of candidate alloys for multiple 33 applications in Advanced-Ultra Supercritical (AUSC) power plants has been undertaken by 34 Detrois, Jablonski and Hawk from the National Energy Technology Laboratory. In these 35 power plants, steam temperatures are required to reach 700-760°C. The common thread is 36 to develop alloys that demonstrate a combination of high temperature properties, which are 37 reliant on both the alloy composition and microstructure and can be produced readily at the 38 right price. For the AUSC applications, the emphasis is on high temperature strength, long 39 term creep life, phase stability, oxidation resistance and robust welding for fabrications. 40 Whereas for powder disk rotors in aircraft engines, the priority is enhanced resistance to 41 time dependent crack growth, phase stability and resistance to environmental damage, while 42 extending the current strength levels, which are shown by existing alloys, to higher 43 temperatures.

36 MATERIALS SCIENCE↗