At least 127 records · Page 7

A Review of Methodology Development for Controlling Loss of Alloying Elements During the Electroslag Remelting Process

Electroslag remelting (ESR) is an advanced secondary refining technology for the production of clean, fully dense, and homogeneous castings of steels and alloys by removal of undesirable elements and nonmetallic inclusions. However, because of some potential reactions between reactive elements, i.e., Al and Ti, in liquid metal and oxygen as well as weak oxides, such as FeO and SiO{sub 2}, in slag during the ESR process, it is impossible to hold those oxidative elements within specification or to maintain them uniformly from the bottom to top of the resultant ingot. According to a literature survey, recent fundamental research on the oxidation behaviors of Al and Ti in nickel-based alloy by ESR-type slag is scarce. Therefore, summarizing previous knowledge on the controlling loss reactive elements during ESR of Fe- and Ni-based alloys in view of thermodynamics and kinetics is in order to increase the basic understanding of the reaction mechanism between those elements and oxygen and weak oxides in the slag, which can guide the development of a new remelting technique that retards the oxidation of Al and Ti in Inconel 718 alloys during the ESR process. The presence of impurity elements, such as oxygen and sulfur, can also deteriorate the mechanical properties of metal products. Therefore, the inter-related literature about desulfurization during the ESR process is also reviewed in this article.

36 MATERIALS SCIENCE↗

Minimizing the diffusivity difference between vacancies and interstitials in multi-principal element alloys

Interstitial atoms usually diffuse much faster than vacancies, which is often the root cause for the ineffective recombination of point defects in metals under irradiation. Here, via ab initio modeling of single-defect diffusion behavior in the equiatomic NiCoCrFe(Pd) alloy, we demonstrate an alloy design strategy that can reduce the diffusivity difference between the two types of point defects. The two diffusivities become almost equal after substituting the NiCoCrFe base alloy with Pd. The underlying mechanism is that Pd, with a much larger atomic size (hence larger compressibility) than the rest of the constituents, not only heightens the activation energy barrier ( E a ) for interstitial motion by narrowing the diffusion channels but simultaneously also reduces E a for vacancies due to less energy penalty required for bond length change between the initial and the saddle states. Our findings have a broad implication that the dynamics of point defects can be manipulated by taking advantage of the atomic size disparity, to facilitate point-defect annihilation that suppresses void formation and swelling, thereby improving radiation tolerance.

36 MATERIALS SCIENCE↗

Tailoring planar slip to achieve pure metal-like ductility in body-centred-cubic multi-principal element alloys

Uniform tensile ductility (UTD) is crucial for the forming/machining capabilities of structural materials. Normally, planar-slip induced narrow deformation bands localize the plastic strains and hence hamper UTD, particularly in body-centred-cubic (bcc) multi-principal element high-entropy alloys (HEAs), which generally exhibit early necking (UTD < 5%). Here we demonstrate a strategy to tailor the planar-slip bands in a Ti-Zr-V-Nb-Al bcc HEA, achieving a 25% UTD together with nearly 50% elongation-to-failure (approaching a ductile elemental metal), while offering gigapascal yield strength. The HEA composition is designed not only to enhance the B2-like local chemical order (LCO), seeding sites to disperse planar slip, but also to generate excess lattice distortion upon deformation-induced LCO destruction, which promotes elastic strains and dislocation debris to cause dynamic hardening. Further, this encourages second-generation planar-slip bands to branch out from first-generation bands, effectively spreading the plastic flow to permeate the sample volume. Moreover, the profuse bands frequently intersect to sustain adequate work-hardening rate (WHR) to large strains. Our strategy showcases the tuning of plastic flow dynamics that turns an otherwise-undesirable deformation mode to our advantage, enabling an unusual synergy of yield strength and UTD for bcc HEAs.

36 MATERIALS SCIENCE↗

Hole Trapping at Acceptor Impurities and Alloying Elements in AlN

Hole localization is a root cause of difficulties in p-type doping of aluminum nitride. Herein, the stability of localized holes in AlN and their susceptibility to self-trapping within bulk material or in the presence of isovalent elements and acceptor impurities are calculated. It is found that self-trapped holes are metastable in bulk AlN, and also exhibit a very low barrier to detrapping. However, holes become trapped in the presence of acceptor impurities as well as isovalent elements such as B, In, and Sc, and may contribute to the broad luminescence observed in AlN alloys. It is also found that hole trapping contributes to the large ionization energies for acceptors in AlN. Most acceptors can also trap a second hole, becoming positively charged and further exacerbating difficulties in doping aluminum nitride p type. Furthermore, the stability of trapped holes is found to scale with atomic size mismatch to Al.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Influence of alloying elements on the oxidation behavior of NbAl3

NbAL3 is one candidate material for advanced aeropropulsion systems because of its high melting point, low density, and good oxidation resistance. Although NbAl3 has the lowest oxidation rate among the binary Nb-Al alloys, it does not form exclusive layers of protective Al2O3 scales. Recently Perkin et al., have shown the feasibility of forming alumina scales on Nb-Al alloys at greatly reduced Al contents. However, the objective was to maintain the high Al content, and hence low density, while achieving the capability of growing protective alumina scales. Alloy development followed approaches similar to those used successfully for superalloys and oxidation resistant MCrAlY coatings. Among the three elements examined (Ti, Si, and Cr) as ternary additions to Nb-Al3, Cr was the most effective in favoring the selective oxidation of Al. Nb-41Al-8Cr formed exclusive layers of alumina and had a k sub p value of 0.22 mg squared/cm (sup 4)/hr at 1200 C. The addition of 1 wt percent Y to this alloy was also beneficial, resulting in nearly an order of magnitude decrease in K sub p at 1200 C. Further improvements were achieved by adding about 1 wt percent Si to the quaternary alloy. The k sub p value of 0.012 mg squared/cm (sup 4)/hr for Nb-40Al-8Cr-1Y-1Si at 1200 C was identical to the best NiAl + Zr alloys. These NbAl3 alloys also exhibited excellent cyclic oxidation resistance for 100 hr at 1200 C, being nearly equivalent to NiAl + Zr.

Hebsur, M. G.↗

Influence of alloying elements on the oxidation behavior of NbAl3

NbAl3 is one candidate material for advanced aeropropulsion systems because of its high melting point, low density, and good oxidation resistance. Although NbAl3 has the lowest oxidation rate among the binary Nb-Al alloys, it does not form exclusive layers of protective Al203 scales. Recently Perkin et al., have shown the feasibility of forming alumina scales on Nb-Al alloys at greatly reduced Al contents. However, the objective was to maintain the high Al content, and hence low density, while achieving the capability of growing protective alumina scales. Alloy development followed approaches similar to those used successfully for superalloys and oxidation resistant MCrAly coatings. Among the three elements examined (Ti, Si, and Cr) as ternary additions to Nb-Al3, Cr was the most effective in favoring the selective oxidation of Al. Nb-41Al-8Cr formed exclusive layers of alumina and had a k sub p value of 0.22 mg squared/cm (sup 4)/hr at 1200 C. The addition of 1 wt percent Y to this alloy was also beneficial, resulting in nearly an order of magnitude decrease in K sub p at 1200 C. Further improvements were achieved by adding about 1 wt percent Si to the quaternary alloy. The k sub p value of 0.012 mg squared/cm (sup 4)/hr for Nb-40Al-8Cr-1Y-1Si at 1200 C was identical to the best NiAl + Zr alloys. These NbAl3 alloys also exhibited excellent cyclic oxidation resistance for 100 hr at 1200 C, being nearly equivalent to NiAl + Zr.

Hebsur, M. G.↗

Oxidation Behavior of Candidate NiCr Alloys for Engine Exhaust Valves: Part I—Effect of Minor Alloying Elements

Oxidation-induced degradation of structural materials employed as exhaust valves within internal combustion engines (ICEs) will be a relevant life-limiting mechanism, in addition to creep and mechanical fatigue, due to ever-increasing severity of operating temperatures and pressures. Ni–Cr-based alloys, which form external chromia-based scales at the relevant operating temperatures are being considered as suitable candidate materials. Thermal cycling of these alloys in water vapor-containing atmospheres, such as those present during hydrocarbon fuel combustion within ICEs, can considerably influence their oxidation behavior. Here, the role of typical alloying additions such as Mn, Si, Al and Ti on the cyclic oxidation behavior of model NiCr–X (X = Mn,Si,Al,Ti) alloys exposed in dry air and air + 10% H 2 O at 800°C and 950°C was investigated. Combined additions of Mn and Si reduced scaling rates compared to binary Ni–22Cr alloys. The presence of water vapor possibly suppressed formation of NiMnCr spinel and thereby the Cr depletion in the alloy. Combined Al and Ti additions mainly resulted in accelerated oxidation kinetics due to the Ti doping of chromia scales. More porous external scales were observed in water vapor leading to a much deeper depth of nitridation in the Ni–22Cr–Al–Ti alloys.

36 MATERIALS SCIENCE↗