Search NASA⌕ Search

SEARCH · Search NASA

Results for “CASTING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 127 records · Page 7

Supplemental Immobilization of Hanford Low-Activity Waste: Cast Stone Augmented Formulation Matrix Tests

More than 56 million gallons of radioactive and hazardous waste are stored in 177 underground storage tanks at the U.S. Department of Energy’s (DOE’s) Hanford Site in Washington State. The HLW will be vitrified in the HLW facility for ultimate disposal at an offsite federal repository. A portion (~35%) of the LAW will be vitrified in the LAW vitrification facility for disposal onsite at the Integrated Disposal Facility (IDF). The pretreatment and HLW vitrification facilities will have the capacity to treat and immobilize all of the wastes destined for those facilities. However, a second facility will be needed for the expected volume of LAW requiring immobilization. Cast Stone, a cementitious waste form, is being considered to provide the required additional LAW immobilization capacity. The Cast Stone waste form must be acceptable for disposal in the IDF. The Cast Stone waste form and immobilization process must be tested to demonstrate that the final Cast Stone waste form can comply with the waste acceptance criteria for the disposal facility and that the immobilization processes can be controlled to consistently provide an acceptable waste form product. A testing program was developed in fiscal year (FY) 2012 describing in detail the work needed to develop and qualify Cast Stone as a waste form for the solidification of Hanford LAW. A statistically designed test matrix was used to evaluate the effects of key parameters on the properties of the Cast Stone as it is initially prepared and after curing. For the processing properties, the water-to-dry-blend mix ratio was the most significant parameter in affecting the range of values observed for each property. The single shell tank (SST) Blend simulant also showed differences in measured properties compared to the other three simulants tested. A review of the testing matrix and results indicated that an additional set of tests would be beneficial to improve the understanding of the impacts noted in the Screening Matrix tests. A set of Cast Stone formulations were devised to augment the original screening test matrix and focus on the range of the test conditions. Fly ash and blast furnace slag were limited to either northwest or southeast and the salt solutions were narrowed to the Average and the SST Blend at the 7.8M Na concentration. To fill in the matrix, a mix ratio of 0.5 was added. In addition, two admixtures, Xypex Admix C-500 and Rheomac SF100 (silica fume), were added as an additional dry material binder in select compositions. As in the Screening Matrix, both fresh and cured properties were evaluated for the formulations. In this study, properties that were influenced by the W/DM ratio in the Screening Matrix; flow diameter, plastic viscosity, density, and compressive strength, showed consistent behavior with respect to W/DM. The leach index for highly soluble components, sodium and nitrate, were not influenced by changes in formulation or the admixtures. The leach index for both iodine and Tc-99 show an influence from the addition of the admixture, Xypex Admix C-500. Additional testing should be performed to further evaluate the influence of Xypex Admix C-500 on the leach index over a range of admixture concentrations, Cast Stone formulations, and curing and storage conditions.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Evaluation of Technetium Getters to Improve the Performance of Cast Stone

Cast Stone has been selected as the preferred waste form for solidification of aqueous secondary liquid effluents from the Hanford Tank Waste Treatment and Immobilization Plant (WTP) process condensates and low-activity waste (LAW) melter off-gas caustic scrubber effluents. Cast Stone is also being evaluated as a supplemental immobilization technology to provide the necessary LAW treatment capacity to complete the Hanford tank waste cleanup mission in a timely and cost effective manner. One of the major radionuclides that Cast Stone has the potential to immobilize is technetium (Tc). The mechanism for immobilization is through the reduction of the highly mobile Tc(VII) species to the less mobile Tc(IV) species by the blast furnace slag (BFS) used in the Cast Stone formulation. Technetium immobilization through this method would be beneficial because Tc is one of the most difficult contaminants to address at the U.S. Department of Energy (DOE) Hanford Site due to its complex chemical behavior in tank waste, limited incorporation in mid- to high-temperature immobilization processes (vitrification, steam reformation, etc.), and high mobility in subsurface environments. In fact, the Tank Closure and Waste Management Environmental Impact Statement for the Hanford Site, Richland, Washington (TC&WM EIS) identifies technetium-99 ( 99 Tc) as one of the radioactive tank waste components contributing the most to the environmental impact associated with the cleanup of the Hanford Site. The TC&WM EIS, along with an earlier supplemental waste-form risk assessment, used a diffusion-limited release model to estimate the release of different contaminants from the WTP process waste forms. In both of these predictive modeling exercises, where effective diffusivities based on grout performance data available at the time, groundwater at the 100-m down-gradient well exceeded the allowable maximum permissible concentrations for 99 Tc. (900 pCi/L). Recent relatively short-term (63 day) leach tests conducted on both LAW and secondary waste Cast Stone monoliths indicated that 99 Tc diffusivities were at or near diffusivities where the groundwater at the 100-m down-gradient well would exceed the allowable maximum permissible 99 Tc concentrations. There is, therefore, a need and an opportunity to improve the retention of Tc in the Cast Stone waste form. One method to improve the performance of the Cast Stone waste form is through the addition of “getters” that selectively sequester Tc inside Cast Stone.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Development of a new casting method to fabricate U–Zr alloy containing minor actinides

Metal fuel slugs of U–Zr alloys for a sodium-cooled fast reactor (SFR) have conventionally been fabricated using an injection casting method. However, casting alloys containing volatile radioactive constituents, such as Am, are problematic in a conventional injection casting method. As an alternative fabrication method, low pressure gravity casting has been developed. Casting soundness, microstructural characteristics, alloying composition, density, and fuel losses were evaluated for the following as-cast fuel slugs: U–10 wt% Zr, U–10 wt% Zr–5 wt% RE, and U–10 wt% Zr–5 wt% RE–5 wt% Mn. The U and Zr contents were uniform throughout the matrix, and impurities such as oxyen, carbon, and nitrogen satisfied the specification of total impurities less than 2,000 ppm. The appearance of the fuel slugs was generally sound, and the internal integrity was shown to be satisfactory based on gamma-ray radiography. In a volatile surrogate casting test, the U–Zr–RE–Mn fuel slug showed that nearly all of the manganese was retained when casting was done under an inert atmosphere.

99 GENERAL AND MISCELLANEOUS↗

URANIUM ACCUMULATIONS IN CASTING OPERATIONS

In December 2017, unexpected accumulations of uranium were discovered in several locations throughout the casting process area at the Y-12 National Security Complex that subsequently placed casting operations on hold. The Y-12 uranium casting process takes place in enclosures and hoods, many of which are open to a large floor surface area that has limited visibility and access. At the time of discovery, there were no Nuclear Criticality Safety (NCS) analyses or limits for material accumulations in the casting processing areas. Due to changes in the operation of the casting process and invalid assumptions in the criticality safety evaluation, significant material accumulations were occurring inside the enclosures. The material accumulations were identified as a result of an extent of condition review from another process, and an occurrence report was filed. The NCS organization worked with Production and Operations personnel to identify additional areas of uranium accumulation in the casting area, which resulted in several iterations of cleaning and material collection. Following material recovery, a causal analysis was performed that identified several contributing factors that allowed the accumulations to go unnoticed. In order to resume operations, the criticality safety evaluation was revised to analyze and control uranium accumulations in the casting area. Additionally, improvements in nuclear material control and accountability (NMC&A) controls were required. Casting operations have since resumed with frequently required material collections, which have limited the amount of uranium material accumulation.

42 ENGINEERING↗

URANIUM ACCUMULATIONS IN CASTING OPERATIONS

In December 2017, unexpected accumulations of uranium were discovered in several locations throughout the casting process area at the Y-12 National Security Complex that subsequently placed casting operations on hold. The Y-12 uranium casting process takes place in enclosures and hoods, many of which are open to a large floor surface area that has limited visibility and access. At the time of discovery, there were no Nuclear Criticality Safety (NCS) analyses or limits for material accumulations in the casting processing areas. Due to changes in the operation of the casting process and invalid assumptions in the criticality safety evaluation, significant material accumulations were occurring inside the enclosures. The material accumulations were identified as a result of an extent of condition review from another process, and an occurrence report was filed. The NCS organization worked with Production and Operations personnel to identify additional areas of uranium accumulation in the casting area, which resulted in several iterations of cleaning and material collection. Following material recovery, a causal analysis was performed that identified several contributing factors that allowed the accumulations to go unnoticed. In order to resume operations, the criticality safety evaluation was revised to analyze and control uranium accumulations in the casting area. Additionally, improvements in nuclear material control and accountability (NMC&A) controls were required. Casting operations have since resumed with frequently required material collections, which have limited the amount of uranium material accumulation.

61 RADIATION PROTECTION AND DOSIMETRY↗

Lost Foam Thin Wall: Feasibility of Producing Lost Foam Castings in Aluminum and Magnesium Based Alloys

With the increased emphasis on vehicle weight reduction, production of near-net shape components by lost foam casting will make significant inroad into the next-generation of engineering component designs. The lost foam casting process is a cost effective method for producing complex castings using an expandable polystyrene pattern and un-bonded sand. The use of un-bonded molding media in the lost foam process will impose less constraint on the solidifying casting, making hot tearing less prevalent. This is especially true in Al-Mg and Al-Cu alloy systems that are prone to hot tearing when poured in rigid molds partially due to their long freezing range. Some of the unique advantages of using the lost foam casting process are closer dimensional tolerance, higher casting yield, and the elimination of sand cores and binders. Most of the aluminum alloys poured using the lost foam process are based on the Al-Si system. Very limited research work has been performed with Al-Mg and Al-Cu type alloys. With the increased emphasis on vehicle weight reduction, and given the high-strength-to-weight-ratio of magnesium, significant weight savings can be achieved by casting thin-wall (≤ 3 mm) engineering components from both aluminum- and magnesium-base alloys.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Achieving Metallurgical Bonding in Aluminum/Steel Bimetallic Castings

Abstract Aluminum castings are increasingly being used in automotive powertrain and structural applications for vehicle lightweighting. Cast aluminum parts often need to be machined and joined to steel components in multi-material systems. Bimetallic components produced by casting aluminum over steel substrate are advantageous due to the elimination of machining and traditional dissimilar material joining processes. However, forming a strong metallurgical bonding during overcasting process has been challenging. In this paper, the effects of processing conditions such as substrate surface preparation, pre-heating temperature, melt conditions as well as casting design were studied by investigating the bimetallic interfaces for aluminum A319 casting alloy and a high alloy steel substrate in a sand-casting process. Zn and Al-based substrate coatings were evaluated. The experimental results suggest a metallurgical bond between aluminum and steel can be formed during the sand-casting process via high temperature diffusion with or without coatings. Al-based substrate coating prior to overcasting results in the formation of a continuous layer of intermetallics at the bimetallic interface, with large Al–Si–Fe intermetallics penetrating the cast aluminum.

Moodispaw, Michael P. (ORCID:0000000267635882)↗

Freeze Tape Cast Thick Mo Doped Li 4 Ti 5 O 12 Electrodes for Lithium-Ion Batteries

Lithium titanate (Li 4 Ti 5 O 12 ) powders with and without molybdenum doping (LTO and MoLTO respectively) were synthesized by a solid-state method and used to fabricate electrodes on Cu foil using a normal tape-cast method and a novel freeze-tape-cast method. Modest molybdenum doping produces a significant electronic conductivity increase (e.g. 1 mS cm -1 for MoLTO vs 10 -7 mS cm -1 for LTO) that is thought to reflect a partial Ti 4+ reduction to Ti 3+ with charge compensation by the Mo 6+ dopant, producing a stable mixed-valent Ti 4+/3+ state. Freeze-tape-cast electrodes were fabricated by a variant of the normal tape-cast method that includes a rapid freezing step in which the solvent in the Cu-foil-supported slurry is rapidly frozen on a cold finger then subsequently sublimed to create unidirectional columnar macropores in the electrode. The resulting electrodes exhibit high porosity and low tortuosity which enhances electrolyte accessibility throughout the full electrode thickness. Freeze-tape-cast electrodes subjected to galvanostatic charge-discharge testing as cathodes in cells vs. a lithium metal anode exhibit higher specific capacity and lower capacity loss at high discharge rates compared with normal-tape-cast electrodes of the same mass loading, despite the fact that the freeze-tape-cast electrodes are nearly twice as thick as the normal tape cast electrodes.

25 ENERGY STORAGE↗

Extended Leach Testing of Simulated LAW Cast Stone Monoliths

This report describes the results from long-term laboratory leach tests performed at Pacific Northwest National Laboratory (PNNL) for Washington River Protection Solutions (WRPS) to evaluate the release of key constituents from monoliths of Cast Stone prepared with four simulated low-activity waste (LAW) liquid waste streams. Specific objectives of the Cast Stone long-term leach tests described in this report focused on four activities: 1. Extending the leaching times for selected ongoing EPA-1315 tests on monoliths made with LAW simulants beyond the conventional 63-day time period up to 609 days reported herein (with some tests continuing that will be documented later) in an effort to evaluate long-term leaching properties of Cast Stone to support future performance assessment activities. 2. Starting new EPA-1315 leach tests on archived Cast Stone monoliths made with four LAW simulants using two leachants (deionized water [DIW] and simulated Hanford Integrated Disposal Facility (IDF) Site vadose zone pore water [VZP]). 3. Evaluating the impacts of varying the iodide loading (starting iodide concentrations) in one LAW simulant (7.8 M Na Hanford Tank Waste Operations Simulator (HTWOS) Average) by manufacturing new Cast Stone monoliths and repeating the EPA-1315 leach tests using DIW and the VZP leachants. 4. Evaluating the impacts of using a non-pertechnetate form of Tc that is present in some Hanford tanks. In this activity one LAW simulant (7.8 M Na HTWOS Average) was spiked with a Tc(I)-tricarbonyl gluconate species and then solidified into Cast Stone monoliths. Cured monoliths were leached using the EPA-1315 leach protocol with DIW and VZP. The leach results for the Tc-Gluconate Cast Stone monoliths were compared to Cast Stone monoliths pertechnetate.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Getter Incorporation into Cast Stone and Solid State Characterizations

Washington River Protection Solutions (WRPS) is collecting relevant available data on waste forms for use as a supplemental immobilization technology, to provide the additional capacity needed to treat low-activity waste (LAW) in Hanford Site tanks and complete the tank waste cleanup mission in a timely and cost-effective manner. One candidate supplemental waste form, fabricated using a low-temperature process, is a cementitious grout called Cast Stone. Cast Stone has been under investigation for this application at Pacific Northwest National Laboratory (PNNL) since initial screening tests in FY13. This report is the culmination of work to lower the diffusivities of Tc and I from Cast Stone using getters. Getters are compounds added to a system designed to selectively sequester a species of interest to provide increased stability to the species. The work contained within this report is related to waste form development and testing, and does not directly support the 2017 integrated disposal facility (IDF) performance assessment. However, this work contains valuable information which may be used in performance assessment maintenance past FY17, and in future waste form development. This report on performance characterization of Tc and I getters in Cast Stone fabricated with simulated LAW covers several areas of interest and major findings to WRPS: investigating performance of potassium metal sulfide (KMS-2-SS) and tin (II) apatite (Sn-A) as Tc getters when incorporated into Cast Stone; investigating performance of silver exchanged zeolite (Ag-Z) and argentite (Arg) as I getters when incorporated into Cast Stone; utilizing sequential addition of Tc and I getters to overcome any deleterious interactions between the getters in solution; determining, for the first time, Tc distribution within the cured Cast Stone and its evolution during leaching; and performing solid state characterization of getters and Cast Stone samples to support leach test findings and develop a mechanistic understanding of the processes that control Tc and I release into solution.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Effects of casting conditions and deformation processing on A356 aluminum and A356-20 vol. pct SiC composites

The effects of casting conditions and deformation processing on the mechanical properties of unreinforced A356 aluminum and A356-20 vol pct SiC composite were investigated by tensile properties in these compounds fabricated by either sand casting or squeeze casting techniques followed by hot working to 33, 50, 90, and 95 percent reductions. The evolution of the microstructure and values of tensile properties were evaluated for the cast materials in each of the hot worked conditions. It was found that, while the deformation processing of the sand-cast composite resulted in banding of the Al and SiC particles within the microstructure, such features were not observed in the squeeze-cast microstructure. The tensile strengths of the squeeze cast materials was found to be higher than those of the sand cast materials, for both the unreinforced and composite samples, while increased amounts of deformation were found to improve the ductility of the composite.

Rozak, G. A.↗

Processing of IN-718 Lattice Block Castings

Recently a low cost casting method known as lattice block casting has been developed by JAM Corporation, Wilmington, Massachusetts for engineering materials such as aluminum and stainless steels that has shown to provide very high stiffness and strength with only a fraction of density of the alloy. NASA Glenn Research Center has initiated research to investigate lattice block castings of high temperature Ni-base superalloys such as the model system Inconel-718 (IN-718) for lightweight nozzle applications. Although difficulties were encountered throughout the manufacturing process , a successful investment casting procedure was eventually developed. Wax formulation and pattern assembly, shell mold processing, and counter gravity casting techniques were developed. Ten IN-718 lattice block castings (each measuring 15-cm wide by 30-cm long by 1.2-cm thick) have been successfully produced by Hitchiner Gas Turbine Division, Milford, New Hampshire, using their patented counter gravity casting techniques. Details of the processing and resulting microstructures are discussed in this paper. Post casting processing and evaluation of system specific mechanical properties of these specimens are in progress.

Hebsur, Mohan G.↗

Aluminum-Silicon Alloy Having Improved Properties At Elevated Temperatures and Process for Producing Cast Articles Therefrom

A process for making a cast article from an aluminum alloy includes first casting an article from an alloy having the following composition, in weight percent: Silicon 11.0-14.0, Copper 5.6-8.0, Iron 0-0.8, Magnesium 0.5-1.5, Nickel 0.05-0.9, Manganese 0-1.0, Titanium 0.05-1.2, Zirconium 0.12-1.2, Vanadium 0.05-1.2, Zinc 0.05-0.9, Strontium 0.001-0.1, Aluminum balance . In this alloy the ratio of silicon to magnesium is 10 to 25, and the ratio of copper to magnesium is 4 to 15. After an article is cast from the alloy, the cast article is aged at a temperature within the range of 400F to 500F for a time period within the range of four to 16 hours. It has been found especially advantageous if the cast article is first exposed to a solutionizing step prior to the aging step. This solutionizing step is carried out by exposing the cast article to a temperature within the range of 900F to 1000F for a time period of fifteen minutes to four hours. It has also been found to be especially advantageous if the solutionizing step is followed directly with a quenching step, wherein the cast article is quenched in a quenching medium such as water at a temperature within the range of 120F to 300F. The resulting cast article is suitable in a number of high temperature applications, such as heavy-duty pistons for internal combustion engines.

Lee, Jonathan A.↗

Process for Producing a Cast Article from a Hypereutectic Aluminum-Silicon Alloy

A process for making a cast article from an aluminum alloy includes first casting an article from an alloy having the following composition, in weight percent: Silicon (Si) 14.0-25.0, Copper (CU) 5.5-8.0, Iron (Fe) 0-0.8, Magnesium (Mg) 0.5-1.5, Nickel (Ni) 0.05-1.2, Manganese (Mn) 0-1.0, Titanium (Ti) 0.05-1.2, Zirconium (Zr) 0.12-1.2, Vanadium (V) 0.05-1.2, Zinc (Zn) 0-0.9, Phosphorus (P) 0.001-0.1, Aluminum, balance. In this alloy the ration of Si:Mg is 15-35, and the ratio of Cu:Mg is 4-15. After an article is cast from the alloy, the cast article is aged at a temperature within the range of 400 F to 500 F for a time period within the range of four to 16 hours. It has been found especially advantageous if the cast article is first exposed to a solutionizing step prior to the aging step. This solutionizing step is carried out by exposing the cast article to a temperature within the range of 875 F to 1025 F for a time period of fifteen minutes to four hours. It has also been found to be especially advantageous if the solutionizing step is followed directly with a quenching step, wherein the cast article is quenched in a quenching medium such as water at a temperature within the range of 120 F to 300 F. The resulting cast article is highly suitable in a number of high temperature applications, such as heavy-duty pistons for internal combustion engines.

Jonathan A Lee↗

Effect of Friction Stir Processing on Fatigue Behavior of an Investment Cast Al-7Si-0.6 Mg Alloy

Cast aluminum alloys in general show poor fatigue performance due to presence of defects. Friction stir processing (FSP) can be used as a tool for enhancing mechanical properties of cast alloys by eliminating such defects. In the present study FSP led to a five times improvement in fatigue life of an investment cast Al-7Si-0.6Mg hypoeutectic alloy. The reason for such enhancement was linked to closure of casting porosity which acted as crack nucleation sites in the as-cast condition. Porosity acted as notches in the as-cast alloy and led to an order of magnitude higher crack growth rate. As FSP eliminated the porosity and refined Si particles, crack growth rate dropped due to the elimination of the notch effect together with increased crack path tortuosity. Finally, short crack behavior was noted in both cast and FSP specimens. The critical crack length where transition from short crack to long crack behavior took place is related to respective microstructural characteristic dimensions.

36 MATERIALS SCIENCE↗

Modeling of Dendritic Evolution of Continuously Cast Steel Billet with Cellular Automaton

In order to predict the dendritic evolution during the continuous steel casting process, a simple mechanism to connect the heat transfer at the macroscopic scale and the dendritic growth at the microscopic scale was proposed in the present work. As the core of the across-scale simulation, a two-dimensional cell automaton (CA) model with a decentered square algorithm was developed and parallelized. Apart from nucleation undercooling and probability, a temperature gradient was introduced to deal with the columnar-to-equiaxed transition (CET) by considering its variation during continuous casting. Based on the thermal history, the dendritic evolution in a 4 mm × 40 mm region near the centerline of a SWRH82B steel billet was predicted. The influences of the secondary cooling intensity, superheat, and casting speed on the dendritic structure of the billet were investigated in detail. The results show that the predicted equiaxed dendritic solidification of Fe-5.3Si alloy and columnar dendritic solidification of Fe-0.45C alloy are consistent with in situ experimental results [Yasuda et al. Int J Cast Metals Res 22:15–21 (2009); Yasuda et al. ISIJ Int 51:402–408 (2011)]. Moreover, the predicted dendritic arm spacing and CET location agree well with the actual results in the billet. The primary dendrite arm spacing of columnar dendrites decreases with increasing secondary cooling intensity, or decreasing superheat and casting speed. Meanwhile, the CET is promoted as the secondary cooling intensity and superheat decrease. However, the CET is not influenced by the casting speed, owing to the adjusting of the flow rate of secondary spray water. Compared with the superheat and casting speed, the secondary cooling intensity can influence the cooling rate and temperature gradient in deeper locations, and accordingly exerts a more significant influence on the equiaxed dendritic structure.

36 MATERIALS SCIENCE↗

Integrated System of Thermal/Dimensional Analysis for Quality Control of Metallic Melt and Ductile Iron Casting Solidification

The main objective of the present work is to introduce a specific experimental instrument and technique for simultaneously evaluating cooling curves and expansion or contraction of cast metals during solidification. Contraction/expansion analysis illustrates the solidification parameters progression, according to the molten cast iron characteristics, which are dependent on the melting procedure and applied metallurgical treatments, mold media rigidity and thermal behavior [heat transfer parameters]. The first part of the paper summarizes the performance of this two-mold device. Its function is illustrated by representative shrinkage tendency results in ductile cast iron as affected by mold rigidity (green sand and furan resin sand molds) and inoculant type (FeSi-based alloys), published in part previously. The second part of the paper illustrates an application of this equipment adapted for commercial foundry use. It conducts thermal analysis and volume change measurements in a single ceramic cup so that mold media as well as solidification conditions are constants, with cast iron quality as the variable. Experiments compared gray and ductile cast iron solidification patterns. Gray iron castings are characterized by higher undercooling at the beginning and at the end of solidification and lower graphitic expansion. Typically, ductile cast iron exhibits higher graphitic, initial expansion, conducive for shrinkage formation in soft molds.

36 MATERIALS SCIENCE↗

Secondary Waste Cast Stone Waste Form Qualification Testing Plan (Rev.1)

The Hanford Tank Waste Treatment and Immobilization Plant (WTP) is being constructed to treat the 56 million gallons of radioactive waste stored in 177 underground tanks at the Hanford Site. The WTP includes a pretreatment facility to separate the wastes into high-level waste (HLW) and low-activity waste (LAW) fractions for vitrification and disposal. The LAW will be converted to glass for final disposal at the Integrated Disposal Facility (IDF). Cast Stone – a cementitious waste form, has been selected for solidification of this secondary waste stream after treatment in the ETF. The secondary-waste Cast Stone waste form must be acceptable for disposal in the IDF. This secondary waste Cast Stone waste form qualification testing plan outlines the testing of the waste form and immobilization process to demonstrate that the Cast Stone waste form can comply with the disposal requirements. Specifications for the secondary-waste Cast Stone waste form have not been established. For this testing plan, Cast Stone specifications are derived from specifications for the immobilized LAW glass in the WTP contract, the waste acceptance criteria for the IDF, and the waste acceptance criteria in the IDF Permit issued by the State of Washington. This testing plan outlines the testing needed to demonstrate that the waste form can comply with these waste form specifications and acceptance criteria. The testing program must also demonstrate that the immobilization process can be controlled to consistently provide an acceptable waste form product. This testing plan also outlines the testing needed to provide the technical basis for understanding the long-term performance of the waste form in the disposal environment. These waste form performance data are needed to support performance assessment analyses of the long-term environmental impact of the secondary-waste Cast Stone waste form in the IDF

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗