Search NASA⌕ Search

SEARCH · Search NASA

Results for “FIBER STRENGTH”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 127 records · Page 7

Factors affecting miniature Izod impact strength of tungsten-fiber-metal-matrix

The miniature Izod and Charpy impact strengths of copper, copper-nickel, and nickel-base superalloy uniaxially reinforced with continuous tungsten fibers were studied. In most cases, impact strength was increased by increasing fiber or matrix toughness, decreasing fibermatrix reaction, increasing test temperature, hot working, or heat treating. Notch sensitivity was reduced by increasing fiber content or matrix toughness. An equation relating impact strength to fiber and matrix properties and fiber content was developed. Program results imply that tungsten alloy-fiber/superalloy matrix composites can be made with adequate impact resistance for turbine blade or vane applications.

Winsa, E. A.↗

Pyrolysis Rate and Yield Strength Reduction Incarbon Fiber and Glass Fiber Composites Underreentry Heating Conditions

The behavior of composite materials, specifically carbon fiber reinforced plastic (CFRP) and glass fiber reinforced plastic (GFRP), under reentry conditions poses a problem for space debris reentry risk modeling. Since these materials pyrolyze rather than melt and their different components demise at different rates, modeling their destruction to determine ground impact risk is complex. Modern spacecraft are using these materials in ever-greater quantities owing to their superior strength-to-weight characteristics, and this has required that the orbital debris community improve its understanding of how these materials demise on reentry. The NASA Orbital Debris Program Office undertook an extensive test campaign to better understand the rate at which several types of GFRP and CFRP materials pyrolyze under reentry heating conditions and how that pyrolysis affects the ultimate strength of the material. GFRP with a polyester resin (G10/FR-4) and CFRP with epoxy, cyanate ester, vinyl ester, and phenolic resins were tested. The test campaign was carried out at the Inductively Coupled Plasma (ICP) Torch Facility at the University of Texas at Austin. Because the ICP facility operates in a shirt-sleeve environment, test samples can be changed within seconds or minutes, allowing many samples to be tested in a short period. Two heat flux rates, 20 W/m2 and 30W/m2, and two oxygen concentration conditions, 0% and 2% of atmospheric, were applied to all five types of material. To measure both the char rate and the effect of pyrolysis on the ultimate material strength, two types of test were carried out for each material: a char rate test on a ~10 mm thick sample of material and an in-situ bending stress test of a ~2 mm thick sample of material. Measurements of the char rate showed very similar average pyrolysis front velocity in epoxy resin CFRP as in G10 at 3.6 mm/min and 3.4 mm/min, respectively. However, the total mass loss rate in theG10 was nearly double that of the CFRP at 3.8 g/min and 2.2 g/min, respectively. This result represented a slow ablation rate of carbon fibers in the CFRP at the temperatures encountered in low Earth orbit reentry and a comparatively rapid removal of the glass fibers in G10 due to melting and spallation. Pyrolysis front velocity was more significantly affected by the type of plastic than the type of fiber, with the cyanate ester CFRP samples displaying an average pyrolysis front velocity of only 1.9 mm/min. Similarly, the effect of thermal exposure on the ultimate strength of the material depended heavily on the type of plastic and very little on the type of fiber in the material. Epoxy, vinyl ester, and polyester resins all behaved very similarly, with complete structural failure at between 400 J/g and 600 J/g of specific absorbed heat. Phenolic and cyanate ester resins, on the other hand, displayed a change in structural properties that was only barely measurable with the current apparatus even after the maximum exposure time tested. These data are being incorporated into a numerical model of the ablation and demise of composite materials that will be used to more accurately calculate the ground casualty risk of future spacecraft.

Benton R. Greene↗

A Quantitative Damage Tolerance Comparison of High Strength and High Modulus Carbon Fiber Sandwich Structure

This study presents experimental results of the compression after impact (CAI) testing of sandwich structure with face sheets made either with IM7/8552 high strength fiber or HM63/8552 high modulus fiber. While the HM63/8552 face sheet sandwich specimens would not be as damage tolerant as the IM7/8552 face sheet sandwich specimens, a quantitative measure of how much more damage tolerant the IM7/8552 face sheets were than the HM63/8552 face sheets was sought. Due to the IM7/8552 face sheets being 28% thicker than the HM63/8552 face sheets, the impact energies used needed to be adjusted for a fair comparison. The results show that the modulus is 35% lower for the IM7/8552 face sheet sandwich structure while the CAI strength

High modulus carbon fiber↗

Measurement of interfacial shear strength in SiC-fiber/Si3N4 composites

An indentation method for measuring shear strength in brittle matrix composites was applied to SiC-fiber/Si3N4-matrix samples. Three methods were used to manufacture the composites: reaction bonding of a Si/SiC preform, hot-pressing, and nitrogen-overpressure sintering. An indentation technique developed by Marshall for thin specimens was used to measure the shear strength of the interface and the interfacial friction stresses. This was done by inverting the sample after the initial push through and retesting the pushed fibers. SEM observations showed that the shear strength was determined by the degree of reaction between the fiber and the matrix unless the fiber was pushed out of its (well-bonded) sheath.

Laughner, James W.↗

Studies of fiber-matrix adhesion on compression strength

A study was initiated on the effect of the matrix polymer and the fiber matrix bond strength of carbon fiber polymer matrix composites. The work includes tests with micro-composites, single ply composites, laminates, and multi-axial loaded cylinders. The results obtained thus far indicate that weak fiber-matrix adhesion dramatically reduces 0 degree compression strength. Evidence is also presented that the flaws in the carbon fiber that govern compression strength differ from those that determine fiber tensile strength. Examination of post-failure damage in the single ply tests indicates kink banding at the crack tip.

Bascom, Willard D.↗

Moisture effects on the high-temperature strength of fiber-reinforced resin composites.

Under NAS 8-27435, the Convair Aerospace Division of General Dynamics and their subcontractor, Hercules Incorporated, have conducted studies on the effects of moisture on the properties of fiber-reinforced resin composites and on the epoxy resins presently used in advanced composites. Data are presented on the resins and composites subjected to varying time/temperature/humidity or time/temperature/water-boil exposures. The effects of moisture on matrix, reinforcement, and fiber/resin interface are discussed and supported by experimental test data.

Hertz, J.↗

Environmental effects on the tensile strength of chemically vapor deposited silicon carbide fibers

The room temperature and elevated temperature tensile strengths of commercially available chemically vapor-deposited (CVD) silicon carbide fibers were measured after 15 min heat treatment to 1600 C in various environments. These environments included oxygen, air, argon and nitrogen at one atmosphere and vacuum at 10/9 atmosphere. Two types of fibers were examined which differed in the SiC content of their carbon-rich coatings. Threshold temperature for fiber strength degradation was observed to be dependent on the as-received fiber-flaw structure, on the environment and on the coating. Fractographic analyses and flexural strength measurements indicate that tensile strength losses were caused by surface degradation. Oxidation of the surface coating is suggested as one possible degradation mechanism. The SiC fibers containing the higher percentage of SiC near the surface of the carbon-rich coating show better strength retention and higher elevated temperature strength.

Bhatt, R. T.↗

Tensile properties of PRD-49 fiber in epoxy matrix.

Recently a high-modulus and high-strength organic fiber, identified as PRD-49-III by the manufacturer, became commercially available. To assess the fiber performance and its potential as a reinforcement for fiber composites, the tensile properties of the fiber in an epoxy matrix were determined. During this study over 6000 fiber/epoxy strands were made using the filament winding process; these strands were representative samples taken from over 60 lb of single-end fiber. The fiber uniformity, its strength distribution at room and LN2 temperature, stress-strain characteristics, and the strain rate effect on the fiber strength were evaluated.

Chiao, T. T.↗

Thermomechanical Characterization of SiC Fiber Tows and Implications for CMC

In order to better understand SiC fiber behavior within CMC microstructures, mechanical tests were performed on multifilament tows consisting of different types of as produced and pretreated fibers. Tensile strengths of tows and single fibers were measured at room temperature for nonstoichiometric Hi-Nicalon and ZMI fibers and for stoichiometric Hi-Nicalon-S, Tyranno SA. and Sylramic fibers. Based on simple bundle theory, measured strengths for as-produced and sized tows were in general agreement with the single fiber results. However, after sizing removal under inert conditions, tow strengths for the coarser grained stoichiometric fibers were typically lower than those predicted from individual fiber data. This effect is attributed to enhanced fiber-fiber mechanical interaction caused by sizing removal from the rough surfaces of these fibers. In support of this, tow strengths remained high for those fiber types with fine grains or excess surface carbon; and, when re-coated with a BN interphase coating, tow strengths for the coarser grained fibers returned to their as-produced values. When the tows were pretreated in air at intermediate temperatures, tow strengths decreased in a manner that could be correlated with the oxidation characteristics of each fiber type as measured by thermogravimetric analysis. The creep and rupture properties of Hi-Nicalon and Sylramic tows were also measured in air and argon from 1200 to 1400 C. Although displaying transient and environmental effects similar to single fibers, the tows crept faster at short times and slower at long times. This resulted in the tow rupture strengths at long time being much greater than the rupture strengths of single fibers. The CMC implications of the tow results are discussed, as well as the benefits and limitations of tow testing.

Yun, H. M.↗

High strength high modulus ceramic fiber

Low cost method was developed for producing high strength, high modulus, continuous ceramic oxide fibers. Process transforms inexpensive metallic salts into syrup-like liquids that can be fiberized at room temperatures. Resulting salt fibers are then converted to oxides by calcination at relatively low temperatures.

Fetterolf, R. N.↗

Application of advanced flywheel technology for energy storage on space station

In space power applications where solar inputs are the primary thermal source, energy storage is necessary to provide a continuous power supply during the eclipse portion of the orbit. Because of their potentially high storage density, flywheels are being considered for use as the storage system on the proposed orbiting space station. During the past several years, graphite fiber technology has advanced, leading to significant gains in flywheel storage density. Use of these improved fibers in experimental flywheel rims has resulted in ultimate storage densities of 878 kJ/kg. With these high strength graphite fibers, operational storage densities for flywheel storage modules applicable to the space station power storage could reach 200 kJ/kg. This module would also be volumetrically efficient occupying only about 1 cu m. Because the size and mass of the flywheel storage module are controlled by the storage density, improvements in fiber strength can have a significant impact on these values. With the improvements anticipated within the next five years, operational storage density on the order of 325 kJ/kg may be possible for the flywheel module.

Olszewski, Mitchell↗

PMR polyimide/graphite fiber composite fan blades

Ultrahigh speed fan blades, designed in accordance with the requirements of an ultrahigh tip speed blade axial flow compressor, were fabricated from a high strength graphite fiber tow and a PMR polyimide resin. The PMR matrix was prepared by combining three monomeric reactants in methyl alcohol, and the solution was applied directly to the reinforcing fiber for subsequent in situ polymerization. Some of the molded blades were completely finished by secondary bonding of root pressure pads and an electroformed nickel leading edge sheath prior to final machining. The results of the spin testing of nine PMR fan blades are given. Prior to blade fabrication, heat resin tensile properties of the PMR resin were examined at four formulated molecular weight levels. Additionally, three formulated molecular weight levels were investigated in composite form with both a high modulus and a high strength fiber, both as-molded and postcured, in room temperature and 232 C transverse tensile, flexure and short beam shear. Mixed fiber orientation panels simulating potential blade constructions were also evaluated. Flexure tests, short beam shear tests, and tensile tests were conducted on these angle-plied laminates.

Cavano, P. J.↗

Improving the interlaminar shear strength of carbon fiber-epoxy composites through carbon fiber bromination

The use of bromine to improve the interlaminar shear strength of PAN-based carbon fibers was investigated. Composite test specimens fabicated from brominated T-300 fibers and a MY720 matrix exhibited on average a 30% improvement in ILSS over their pristine counterparts. Mass, electrical resistivity, density, contact angle, and scanning Auger microscopy results suggested a mechanism in which the bromine was covalently bonded to the surface of the fiber, and this resulted in an increased van der Waal's adhesion between fiber and matrix.

Jaworske, Donald A.↗