Search NASA⌕ Search

SEARCH · Search NASA

Results for “FRICTION STIR WELDING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 127 records · Page 7

Neutron diffraction measurements of residual stresses in friction stir welding: a review

Significant amounts of residual stresses are often generated during welding and result in critical degradation of the structural integrity and performance of components. Neutron diffraction has become a well established technique for the determination of residual stresses in welds because of the unique deep penetration, three-dimensional mapping capability, and volume averaged bulk measurements characteristic of the scattering neutron beam. Friction stir welding has gained prominence in recent years. The authors reviewed a number of neutron diffraction measurements of residual stresses in friction stir welds and highlighted examples addressing how the microstructures and residual stresses are correlated with each other. An example of in situ neutron diffraction measurement result shows the evolution of the residual stresses during welding.

36 MATERIALS SCIENCE↗

Effect of the surface preparation techniques on the EBSD analysis of a friction stir welded AA1100-B{sub 4}C metal matrix composite

Aluminum based metal matrix composites (MMCs) have been used in various automobile, aerospace and military industries. Yet characterization of the microstructure in these materials remains a challenge. In the present work, the grain structure in the matrix of B{sub 4}C particulate reinforced MMCs and their friction stir welds is characterized by using optical metallography and the electron backscatter diffraction (EBSD) technique. Optical metallography can partially reveal the grain structure in the matrix of AA1100-16 vol.% B{sub 4}C composite. The EBSD technique has been successfully applied to characterize the grain structure in the AA1100-16 vol.% B{sub 4}C friction stir welds, which provides a powerful tool to follow the microstructural evolution of MMC materials during friction stir welding (FSW). Both mechanical polishing and ion beam polishing are used for the EBSD sample preparation. The effect of the sample preparation on the EBSD data acquisition quality is studied. Some typical examples, such as the identification of grains and subgrains, grain size distribution, deformation fields and the texture components are given. - Highlights: {yields} EBSD has been used to characterize the grain structure of Al-B{sub 4}C MMCs. {yields} Mechanical and ion beam polishing are compared for EBSD sample preparation of MMCs. {yields} EBSD shows great advantages over optical microscopy for microtexture analysis of MMCs.

36 MATERIALS SCIENCE↗

Interfacial microstructure and properties of copper clad steel produced using friction stir welding versus gas metal arc welding

A preliminary study compares the feasibility and microstructures of pure copper claddings produced on a pressure vessel A516 Gr. 70 steel plate, using friction stir welding versus gas metal arc welding. A combination of optical and scanning electron microscopy is used to characterize the grain structures in both the copper cladding and heat affected zone in the steel near the fusion line. The friction stir welding technique produces copper cladding with a grain size of around 25 μm, and no evidence of liquid copper penetration into the steel. The gas metal arc welding of copper cladding exhibits grain sizes over 1 mm, and with surface microcracks as well as penetration of liquid copper up to 50 μm into the steel substrate. Transmission electron microscopy reveals that metallurgical bonding is produced in both processes. Increased diffusion of Mn and Si into the copper cladding occurs when using gas metal arc welding, although some nano-pores were detected in the FSW joint interface. - Highlights: • Cladding of steel with pure copper is possible using either FSW or GMAW. • The FSW yielded a finer grain structure in the copper, with no evidence of cracking. • The FSW joint contains some evidence of nano-pores at the interface of the steel/copper. • Copper cladding by GMAW contained surface cracks attributed to high thermal stresses. • The steel adjacent to the fusion line maintained a hardness value below 248 HV.

36 MATERIALS SCIENCE↗

Improving Joint Formation and Tensile Properties of Dissimilar Friction Stir Welding of Aluminum and Magnesium Alloys by Solving the Pin Adhesion Problem

Friction stir welding (FSW), as a solid-state welding technology invented by TWI in 1991, has potential to join dissimilar Al/Mg alloys. In this study, the pin adhesion phenomenon affecting joint quality during FSW of 6061-T6 aluminum and AZ31B magnesium alloys was investigated. The adhesion phenomenon induced by higher heat input easily transformed the tapered-and-screwed pin into a tapered pin, which greatly reduced the tool’s ability to drive the plasticized materials and further deteriorated joint formation. Under the condition without the pin adhesion, the complex intercalated interlayer at the bottom of stir zone was beneficial to mechanical interlocking of Al/Mg alloys, improving tensile properties. However, the formation of intermetallic compounds was still the main reason of the joint fracture, significantly deteriorating tensile properties. Under the welding speed of 60 mm/min without the pin adhesion phenomenon, the maximum tensile strength of 107 MPa and elongation of 1.2% were achieved.

36 MATERIALS SCIENCE↗

Complete Status Report Documenting Development of Friction Stir Welding for Joining Thin Wall Tubing of ODS Alloys

The development of friction stir welding (FSW) for joining thin sections of the advanced oxide dispersion strengthened (ODS) 14YWT ferritic alloy was initiated in Fuel Cycle Research and Development (FCRD), now the Nuclear Technology Research and Development (NTRD), in 2015. The first FSW experiment was conducted in late FY15 and successfully produced a bead-on-plate stir zone (SZ) on a 1 mm thick plate of 14YWT (SM13 heat). The goal of this research task is to ultimately demonstrate that FSW is a feasible method for joining thin wall (0.5 mm thick) tubing of 14YWT.

36 MATERIALS SCIENCE↗

Stability of Y–Ti–O precipitates in friction stir welded nanostructured ferritic alloys

Nanostructured ferritic alloys, which have complex microstructures which consist of ultrafine ferritic grains with a dispersion of stable oxide particles and nanoclusters, are promising materials for fuel cladding and structural applications in the next generation nuclear reactor. This paper evaluates microstructure of friction stir welded nanostructured ferritic alloys using electron microscopy and atom probe tomography techniques. Atom probe tomography results revealed that nanoclusters are coarsened and inhomogeneously distributed in the stir zone and thermomechanically affected zone. Three hypotheses on coarsening of nanoclusters are presented. Finally, the hardness difference in different regions of friction stir weld has been explained.

36 MATERIALS SCIENCE↗

Interfacial Microstructure and Mechanical Properties of Friction Stir Welded Joints of Commercially Pure Aluminum and 304 Stainless Steel

In the present investigation, friction stir welding of commercially pure aluminum and 304 stainless steel was carried out at varying tool rotational speeds from 200 to 1000 rpm in steps of 200 rpm using 60 mm/min traverse speed at 2 (degree) tool tilt angle. Microstructural characterization of the interfacial zone was carried out using optical microscope and scanning electron microscope. Energy-dispersive spectroscopy indicated the presence of FeAl{sub 3} intermetallic phase. Thickness of the intermetallic layer increased with the increase in tool rotational speed. X-ray diffraction studies indicated the formation of intermetallic phases like FeAl{sub 2}, Fe{sub 4}Al{sub 13}, Fe{sub 2}Al{sub 5}, and FeAl{sub 3}. A maximum tensile strength of ~ 90% that of aluminum along with ~ 4.5% elongation was achieved with the welded sample at tool rotational speed of 400 rpm. The stir zone showed higher hardness as compared to base metals, heat affected zone, and thermo-mechanically affected zone due to the presence of intermetallics. The maximum hardness value at the stir zone was achieved at 1000 rpm tool rotational speed.

36 MATERIALS SCIENCE↗

FRICTION STIR WELDING AND PRELIMINARY CHARACTERIZATION OF IRRADIATED 304 STAINLESS STEEL

The mitigation of helium induced cracking in the heat affected zone (HAZ), a transition metallurgical zone between the weld zone and base metal, during repair welding is a great challenge in nuclear industry. Successful traditional fusion welding repairs are limited to metals with a maximum of a couple of atomic parts per million (appm) helium, and structural materials helium levels in operating nuclear power plants are generally exceed a couple of appm after years of operations. Therefore, fusion welding is very limited in nuclear power plants structural materials repairing. Friction stir welding (FSW) is a solid-state joining technology that reduces the drivers (temperature and tensile residual stress) for helium-induced cracking. This paper will detail initial procedural development of FSW weld trials on irradiated 304L stainless steel (304L SS) coupons utilizing a unique welding facility located at one of Oak Ridge National Laboratory’s hot cell facilities. The successful early results of FSW of an irradiated 304L SS coupon containing high helium are discussed. Helium induced cracking was not observed by scanning electron microscopy in the friction stir weld zone and the metallurgical zones between the weld zone and base metal, i.e. thermal mechanical affected zone (TMAZ) and HAZ. Characterization of the weld, TMAZ and HAZ regions are detailed in this paper.

Tang, Wei↗

On the solid-state-bonding mechanism in friction stir welding

This study is a critical assessment of various solid-state-bonding mechanisms is established for friction stir welding (FSW) processes of engineering alloys. The commonly assumed sintering-like diffusional-bonding hypothesis is criticized in this work as not the dominant mechanism. For the wide spectrum of material constitutive laws and FSW processing conditions examined and employed in realistic applications, the thermomechanical history on the workpiece–workpiece interface traverses in the creep-dominated regime for the growth/shrinkage of interfacial cavities. The evolution of the bonding fraction relies mainly on the creep strain rate in the adjourning workpieces, weakly on stress triaxiality, and negligibly on interfacial diffusion.

36 MATERIALS SCIENCE↗

Effect of Rotation Speed on the Microstructure and Mechanical Properties of Friction-Stir-Welded CuSn6 Tin Bronze

Four-mm-thick CuSn6 tin bronze plates were friction stir welded at a constant tool traverse speed of 100 mm min{sup −1}. Favorable joints could be obtained with rotation speeds ranging from 600 to 1000 rev min{sup −1}, and groove was found on the surface of the joint under 400 rev min{sup −1}. The microstructure of the weld nugget zone was characterized by equiaxed recrystallized grains with heterogeneity along the thickness direction. Moreover, the grain size of the thermo-mechanically affected zone and stir zone increased with the increase in rotation speed. Hardness of the stir zone was higher than that of other zones due to microstructural refinement. There was little change in tensile properties of the defect-free welded joints. During tensile test, all of the defect-free joints were fractured at heat-affected zone with typical plastic fracture.

36 MATERIALS SCIENCE↗

Microstructural characterisation of friction stir welding joints of mild steel to Ni-based alloy 625

In this study, 6-mm-thick mild steel and Ni-based alloy 625 plates were friction stir welded using a tool rotational speed of 300 rpm and a travel speed of 100 mm·min{sup −1}. A microstructural characterisation of the dissimilar butt joint was performed using optical microscopy, scanning and transmission electron microscopy, and energy dispersive X-ray spectroscopy (XEDS). Six different weld zones were found. In the steel, the heat-affected zone (HAZ) was divided into three zones and was composed of ferrite, pearlite colonies with different morphologies, degenerated regions of pearlite and allotriomorphic and Widmanstätten ferrite. The stir zone (SZ) of the steel showed a coarse microstructure consisting of allotriomorphic and Widmanstätten ferrite, degenerate pearlite and MA constituents. In the Ni-based alloy 625, the thermo-mechanically affected zone (TMAZ) showed deformed grains and redistribution of precipitates. In the SZ, the high deformation and temperature produced a recrystallised microstructure, as well as fracture and redistribution of MC precipitates. The M{sub 23}C{sub 6} precipitates, present in the base material, were also redistributed in the stir zone of the Ni-based alloy. TMAZ in the steel and HAZ in the Ni-based alloy could not be identified. The main restorative mechanisms were discontinuous dynamic recrystallisation in the steel, and discontinuous and continuous dynamic recrystallisation in the Ni-based alloy. The interface region between the steel and the Ni-based alloy showed a fcc microstructure with NbC carbides and an average length of 2.0 μm. - Highlights: • Comprehensive microstructural characterisation of dissimilar joints of mild steel to Ni-based alloy • Friction stir welding of joints of mild steel to Ni-based alloy 625 produces sound welds. • The interface region showed deformed and recrystallised fcc grains with NbC carbides and a length of 2.0 μm.

36 MATERIALS SCIENCE↗

Effect of Tool Offset and Rotational Speed in Dissimilar Friction Stir Welding of AISI 304 Stainless Steel and Mild Steel

In the present study, dissimilar friction stir welding was carried out between stainless steel (UNS S30400) and mild steel (UNS G10080) plates of 4 mm thickness using a tungsten carbide tool. The influence of tool rotational speeds (600, 875 rpm) and tool offsets (0.6, 1.2 mm) on mechanical properties, i.e., hardness, tensile strength, and impact toughness of welded joints was investigated. Maximum tensile strength of the joint was about 107.6% of the mild steel under rotational speed of 875 rpm and tool offset of 1.2 mm. The maximum hardness reached in the stir zone was about 281 HV{sub 0.5} due to the phase transformations and grain refinement. Charpy’s notch toughness of the welded joints was observed lower than the base materials. The microstructural characterizations were carried by using an optical microscope, and FESEM–EDS analysis which revealed the complex material mixing and material movement during the welding. Tungsten-rich bands were observed in the weld micrograph especially toward the advancing side. During this study, various wear mechanisms like oxidation wear, abrasive wear, and adhesion wear were responsible for the degradation of tungsten carbide tool.

36 MATERIALS SCIENCE↗

Room temperature corrosion behaviour of plastically deformed AISI 304 stainless steel by friction stir welding in neutral and acidified chloride solutions

Severe plastic deformation of 304L stainless steel plate was carried out by friction stirring under an isothermal tool temperature at 825°C. The friction stirred zone showed extensive grain refinement, high fraction of low angle grain boundaries due to dislocation rearrangement, Σ3 and Σ9 special grain boundaries and discrete Fe–Cr–Mn-rich particles. Electrochemical polarisation measurements were done on the base metal (BM) and friction stir welded (FSW) specimens in the neutral and acidified 3.5% NaCl solutions. The BM showed marginally better pitting resistance in the neutral chloride solution than the FSW because of a larger fraction of special grain boundaries, and larger grain size. Whereas in acidified 3.5% NaCl solution, the FSW showed better corrosion resistance than the BM. Furthermore, the surface film of the FSW had a lower impedance and a lower defect concentration than the BM indicating higher diffusivity of point defects in the FSW.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of Friction Stir Welded Q235 Low-Carbon Steel

Three-millimeter-thick Q235 steel plates were friction stir welded using a tool made of tungsten-rhenium alloy in the present study. The microstructure and mechanical properties of welded joints at various traverse speeds from 50 to 150 mm/min were analyzed. It was demonstrated that traverse speed had great impacts on microstructure and mechanical properties of the joints. Phase transformation accompanied with recrystallization occurred during FSW process which resulted in different microstructures in the WNZ, and the grain size in other zones was significantly affected by traverse speed. The highest hardness was located in the nugget zone, while the lowest hardness was found in the heat-affected zone. The transverse tensile test suggested that all the joints showed slightly lower tensile strength than that of the base material, and the tensile strength increased with increasing traverse speed. All the joints fractured in the heat-affected zone with ductile fracture mode. The impact test showed that the impact toughness decreased with the increasing traverse speed and the impact fracture surface could be divided into shear lip zone and fibrous zone which showed a typical ductile fracture.

36 MATERIALS SCIENCE↗

Polishing-assisted galvanic corrosion in the dissimilar friction stir welded joint of AZ31 magnesium alloy to 2024 aluminum alloy

Galvanic corrosion of a dissimilar friction stir welded 2024-T3 Al/AZ31B-H24 Mg joint prepared using a water-based and a non-water-based polishing solution was characterized. Microstructure and the distribution of chemical elements were analyzed using optical microscopy, scanning electron microscopy and energy dispersive X-ray spectroscopy. The stir zone polished using water-based solution was observed to be much more susceptible to galvanic corrosion attack than that obtained using non-water-based polishing solution. The location of corrosion attack was observed in the narrow regions of AZ31 Mg alloy adjacent to Al2024 regions in the stir zone. The occurrence of galvanic corrosion was due to the formation of Mg/Al galvanic couples with a small ratio of anode-to-cathode surface area. The corrosion product was primarily the porous magnesium hydroxide with characteristic microcracks and exhibited a low microhardness value.

36 MATERIALS SCIENCE↗

Friction Stir Welding of Low-Carbon AISI 1006 Steel: Room and High-Temperature Mechanical Properties

Friction stir welding (FSW) is an ecologically benign solid-state joining process. In this work, FSW of low-carbon AISI 1006 steel was carried out to study the microstructure and mechanical properties of the resulting joints at both room temperature (RT) and 200 °C. In the parameter space investigated here, a rotational tool speed and translation feed combination of 1200 rpm and 60 mm/min produced a defect-free weld with balanced mechanical properties and a superior Vickers microhardness profile compared to all other conditions and to base metal (BM). At faster translation feeds (100 and 150 mm/min), wormhole defects were observed in the weld microstructure and were attributed to higher strain rate experienced by the weld zone. Under tensile loading, welded material exhibited yield strength that was up to 86 and 91% of the BM at RT and 200 °C, respectively. On the other hand, tensile strength of welded material was nearly similar to that of the base metal at both RT and 200 °C. However, at both temperatures the tensile ductility of the welded joints was observed to be significantly lower than the BM. Annealing of the 1200 rpm and 60 mm/min FSW specimen resulted in tensile strength of 102% compared to base material and 47% increase in the strain at failure compared to the as-welded specimen. The Charpy impact values revealed up to 62 and 53% increase in the specific impact energy for the 1200 rpm and 60 mm/min welded joints as compared with the BM.

36 MATERIALS SCIENCE↗

Effect of tool pin features on process response variables during friction stir welding of dissimilar aluminum alloys

In this article, the effect of pin features and orientation/placement of the materials on advancing side were investigated for friction stir welding (FSW) of dissimilar aluminum alloys AA2050 and AA6061. Pins for FSW were produced with a 2.12 mm pitch thread having three flats/flutes. Three sets of rotational speed/welding speed were used to perform a series of welds in a butt joint arrangement. The results show that, joint quality, process response variables and welding temperature are highly affected by pin features and material orientation in FSW. Defect free joints with effective material transportation in the weld nugget zone were obtained when welding was performed with AA2050 on the advancing side. The tool also encounters less in-plane reaction force for welding with 2050 on the advancing side. Pin with thread+3 flats produces quality welds at low rotational and travel speed regardless of the location of alloys on advancing or retreating side.

36 MATERIALS SCIENCE↗

Complete Status Report Documenting the Development of Friction Stir Welding for Producing a Butt Joint in Thin Wall Tubing of ODS Alloys

A challenging attempt using friction stir welding to produce a butt joint between two 1.0 mm thick plates of 14YWT was nearly successful. The modified tool pin mostly penetrated the thickness of the adjoined thin plate samples resulting in a small blunt notch on the bottom surface of the butt joint. A bend occurred in the thin plate sample due to formation of stresses from clamping the thin plate sample during FSW. The peak displacement of the bend occurred along the center line of the butt joint. The weld zone showed good microstructure mixing with some flashing mostly on the retreating side that suggested excess heat input by friction between the traveling and spinning tool pin and thin plates of 14YWT. Neutron diffraction experiments were performed on the bent sample of 14YWT to measure the residual stresses in the butt joint on the HB-2B beam line at the Neutron Residual Stress Facility at HFIR. However, the neutron scattering to background noise ratio was very low during data acquisition. Measurements of lattice strains were obtained in the rolling (RD) and normal (ND) directions but not in the extrusion direction (ED) of the thin plate sample. Unfortunately, the quality of the data was not sufficient for determining the residual stresses in the butt joint. From the previous neutron scattering experiments conducted on four hot rolled plates (R1, R2, R3 and R4) of 14YWT, the residual stresses were calculated from lattice strain data and plotted in 2-D color contour maps for ED, RD and ND. The results showed variations in the magnitude and spatial position of residual stresses in the microstructure of the four plates. The magnitude in residual stresses in ED and RD increased gradually with increasing rolling deformation for R1 (50%) to R2 (76%), followed by larger increases in R3 (89%) and R4 (95%). The maximum peaks in residual stresses for R4 was ~710-730 MPa in ED and RD. The residual stresses in ND were below ~300 MPa for each of the 4 rolled plates, with a maximum residual stress in R4 (95%) of ~400 MPa. These results indicated that significant residual stresses representing ~57% of the yield stress of 14YWT (SM13) had accumulated in the 14YWT plate after hot rolling to the 1 mm thickness, which was used in the FSW experiments. The microstructure analysis of the 1.0 mm thick plate of 14YWT containing the butt joint produced by FSW revealed significant changes in the grain structure and texture between the unaffected zone (UZ) of the rolled plate and the butt joint weld. In the UZ, the grains were severely elongated after 95% deformation and mainly possessed the {101} texture component in the ED. Two predominant grain misorientation angles were observed: one consisting of small misorientations of <5º between highly elongated grains and the other consisting of large misorientations of >15º in pockets of small grains that might have formed by dynamic recrystallization processes during rolling of the plate at 1000ºC. The morphology and texture of grains in the heat affected zone (HAZ) were similar to those in UZ, except the grains had coarsened due to excess heat input during FSZ. A population of pores formed and the grains both coarsened and changed to isotropic morphology in the microstructure of the butt joint on both the advancing and retreating sides. The texture of grains in both regions were randomly orientated between the 3 poles {001}, {101} and {111}. The main difference in texture of grains between the advancing side and retreating side was with the misorientation angles of neighboring grains. Most of the grains in the advancing side had misorientation angles of >5º indicating that these grains experienced recrystallization. On the retreating side, areas containing larger grains showed high misorientation angles of >15º compared to areas appearing as bands of grains with misorientation angles of <5º and between 5º-15º. Numerous small pockets of grains with low misorientation angles of <5º were distributed in the microstructure among the grains showing high misorientation angles of >15º. It was determined that the grains associated with low misorientation angles contained sub-grain structures, which was consistent with both recrystallization and recovery mechanisms for grains located on the retreating side of the butt joint. These results demonstrate the complex microstructure that evolves in the microstructure of 14YWT resulting from the input of high temperatures and severe deformations during FSW.

36 MATERIALS SCIENCE↗