Metal-metal laminar composites for high-temperature applications.
A study was conducted to obtain indications of the potentialities of laminar metal-metal composites for elevated-temperature use. Most of the composites consisted of multiple layers or laminae of tungsten alternated with laminae of Nichrome V, a ductile, weaker, but oxidation-resistant alloy. Composites with 50 vol % of each phase made from 0.0025 cm, 0.0125 cm, or 0.050 cm laminae, were tested in tension and stress rupture at temperatures of 871 and 1093 C and in impact at 23 and 524 C. A tension and a short-time stress-rupture test was conducted on specimens of 77 vol % W-Re-Hf-C/23 vol % Inconel Alloy 600 at 1093 C.