Search NASA⌕ Search

SEARCH · Search NASA

Results for “Joint strength”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 127 records · Page 7

A Statistical Analysis of Impact Ice Adhesion Strength Data Acquired with a Modified Lap Joint Test

Numerous methodologies have been utilized to measure the adhesion strength of impact ice, and the data reported in the literature varies significantly from method to method. In order to initiate an investigation to determine the cause of this disparity, a lap-joint shear test methodology that was recently developed was utilized in the Icing Research Tunnel at the NASA Glenn Research Center. Data was obtained while varying the temperature, test section velocity, liquid water content, and cloud droplet median volumetric diameter, among other parameters, over five campaigns. A new data set acquired using this new test method is presented. The results are analyzed with standard statistical methodologies and demonstrate a strong correlation between the apparent adhesion strength of ice and temperature, annealing time, and heating time. Observations during the test and analysis of the results suggest the presence of large residual stresses in the samples, which is in agreement with prior work. Due to the nature of the test methodology, and all known ice adhesion test methodologies, the measured, or apparent, adhesion strength is geometry dependent, a fact emphasized by the results presented here. The data was organized both cumulatively and independently by result code. Trends in the data are discussed in the context of causal physical mechanisms. The data shows the apparent adhesion strength was not linear with temperature, liquid water content, annealing time, and other variables. Short-term heating of the samples was shown to have negligible effect, and the apparent adhesion strength had a flat trend with velocity.

Ice Adhesion↗

Joining and Integration of Silicon Nitride Ceramics for Aerospace and Energy Systems

Light-weight, creep-resistant silicon nitride ceramics possess excellent high-temperature strength and are projected to significantly raise engine efficiency and performance when used as turbine components in the next-generation turbo-shaft engines without the extensive cooling that is needed for metallic parts. One key aspect of Si3N4 utilization in such applications is its joining response to diverse materials. In an ongoing research program, the joining and integration of Si3N4 ceramics with metallic, ceramic, and composite materials using braze interlayers with the liquidus temperature in the range 750-1240C is being explored. In this paper, the self-joining behavior of Kyocera Si3N4 and St. Gobain Si3N4 using a ductile Cu-based active braze (Cu-ABA) containing Ti will be presented. Joint microstructure, composition, hardness, and strength as revealed by optical microscopy, scanning electron microscopy (SEM), energy dispersive spectroscopy (EDS), Knoop microhardness test, and offset compression shear test will be presented. Additionally, microstructure, composition, and joint strength of Si3N4/Inconel 625 joints made using Cu-ABA, will be presented. The results will be discussed with reference to the role of chemical reactions, wetting behavior, and residual stresses in joints.

Singh, M.↗

Mechanically fastened joints in woven fabric composites

Strength analysis for composite bolted joints involves the mating of a stress analysis with an appropriate mode specific failure criterion for each of the primary failure modes. The stress analysis and failure criteria are independent of each other and can be manipulated separately in order to optimize the strength analysis package formed by their coupling. Material properties tests were conducted on rubber toughened graphite-epoxy material to measure the basic strength and stiffness in the warp and fill directions and in shear. Test matrices are summarized for investigations of laminate configuration, stacking sequence, fastener diameter, edge distance, fastener half spacing, laminate thickness, and fastener torque. A three dimensional finite element analysis computer program was written and failure criteria for net tension, shearout, and bearing were determined.

Wilson, D. W.↗

Room Temperature and Elevated Temperature Composite Sandwich Joint Testing

Testing of composite sandwich joint elements has been completed to verify the strength capacity of joints designed to carry specified running loads representative of a high speed civil transport wing. Static tension testing at both room and an elevated temperature of 350 F and fatigue testing at room temperature were conducted to determine strength capacity, fatigue life, and failure modes. Static tension test results yielded failure loads above the design loads for the room temperature tests, confirming the ability of the joint concepts tested to carry their design loads. However, strength reductions as large as 30% were observed at the elevated test temperature, where all failure loads were below the room temperature design loads for the specific joint designs tested. Fatigue testing resulted in lower than predicted fatigue lives.

Walker, Sandra P.↗

Static Strength Characteristics of Mechanically Fastened Composite Joints

The analysis of mechanically fastened composite joints presents a great challenge to structural analysts because of the large number of parameters that influence strength. These parameters include edge distance, width, bolt diameter, laminate thickness, ply orientation, and bolt torque. The research presented in this report investigates the influence of some of these parameters through testing and analysis. A methodology is presented for estimating the strength of the bolt-hole based on classical lamination theory using the Tsai-Hill failure criteria and typical bolthole bearing analytical methods.

Fox, D. E.↗

Development of the weldbond process for joining titanium

High quality resistance spot welds were produced by welding through epoxy adhesive on titanium alloys. Weldbond joints were consistently stronger than those of either mechanical fasteners, structural adhesive bonds, or mechanical fasteners with adhesive at the joint interface. Weldbond joints and/or spot weld joints showed superior strength at all temperature ranges as compared to other joints tested.

Fields, D.↗

Equivalent Properties of Interfacial Void Defects at the CFRTP-adhesive Interface and Their Detrimental Effects on the Bonding Performance of Metal-CFRTP Dissimilar Joints

This paper revealed the detrimental effects of micro-scale air interfacial voids on the debonding at the interface of carbon-fiber-reinforced polyphthalamide (CFRPPA) and thermoset adhesive, representing a weak adherend-adhesive interface, within a dissimilar joint made of an aluminum alloy and a CFRPPA. The reduced lap shear strength of the joint, due to different void area fractions at the CFRPPA-adhesive interface, can be computationally described by using equivalent interfacial properties in the modeling to avoid the explicit modeling of the micro-scale interfacial voids. Such equivalent interfacial properties (e.g., interfacial normal strength, etc.) was found to have a non-linear relationship with respect to interfacial void area fraction as well as lap shear strength. This work has practical applications by utilizing equivalent interfacial properties for the analytical and/or computational design(s) of adhesively bonded joints.

Qiao, Yao↗

Study of gas tungsten arc welding procedures for tantalum alloy T-111 (Ta-8 W-2Hf) plate

Methods of eliminating or reducing underbread cracking in multipass GTA welds in thick T-111 plate were studied. Single V butt welds prepared using experimental filler metal compositions and standard weld procedures resulted in only moderate success in reducing underbread cracking. Subsequent procedural changes incorporating manual welding, slower weld speeds, and three or fewer fill passes resulted in crack-free single V welds only when the filler metal was free of hafnium. The double V joint design with successive fill passes on opposite sides of the joint produced excellent welds. The quality of each weld was determined metallographically since the cracking, when present, was very slight and undetectable using standard NDT techniques. Tensile and bend tests were performed on selected weldments. The inherent filler metal strength and the joint geometry determined the strength of the weldment. Hardness and electron beam microprobe traverses were made on selected specimens with the result that significant filler metal-base metal dilution as well as hafnium segregation was detected. A tentative explanation of T-111 plate underbread cracking is presented based on the intrinsic effects of hafnium in the weldment.

Gold, R. E.↗

Effect of stitching on the strength of bonded composite single lap joints

An experimental investigation has been conducted to determine the effect of stitching on the static and fatigue failure load of bonded composite single lap joints. The variables considered in the static tests included adherend thickness, overlap length, stitch spacing, and number of rows of stitches. A limited fatigue program was conducted for one configuration to compare the fatigue life of stitched and unstitched joints. Up to a 38 percent improvement in static failure load and an order of magnitude increase in fatigue life compared with unstiffened results are obtained by a single row of stitches near the end of the overlap. Additional rows of stitching or different stitch spacing has little effect on static joint failure load. Thicker adherends and larger overlap length result in larger improvements in static failure load with stitching. Further research is needed to refine the stitching process in order to obtain the maximum improvements in joint failure load.

Sawyer, J. W.↗

Effect of Rivet Pitch upon the Fatigue Strength of Single-row Riveted Joints of 0.025- to 0.025-inch 24S-T Alclad

S-N curves at the range ratio of 0.2 were experimentally obtained for each of the following values of rivet pitch P as used in a single-row lap joint of 0.025- to 0.025-inch 24S-T alclad with one-eight AN430 round-head rivets: p=0.5, 0.75, 1.0, 1.5. Families of constant rivet pitch curves, which define the fatigue life for specimens studied, were developed. Curves showing the variation of the effective stress concentration factor in fatigue with rivet pitch and maximum load per rivet were also established.

Seliger, Victor↗

Joining and Testing Composite Plates to Ti Tubes

The joining of metal tubes to composite plates is required for heat-rejection components in several space applications. Currently a number of different braze compositions are being evaluated as to their effectiveness. Such tube-plate configurations cannot be represented by traditional methods of testing, e.g., lap joints. The joined region is not between two flat surfaces, but rather between a flat surface and a curved surface. Therefore, several tests have been employed to ascertain the effectiveness of the different braze approaches in tension that are both simple and representative of the actual system and relatively straightforward in analysis. The results of these "tube-tests" will be discussed for the three different braze compositions, Cu-ABA, Ti-Cu-Sil, and Ti-Cu-Ni. In addition, fracture analysis of the failed joints was performed and offers insights into the cause of joint failure and the distinctions which need to be made between the "strength" of a joint versus the "load carrying ability" of a joint.

Morscher, Gregory N.↗

Mechanical Characterization of Reactively Brazed Metal-Composite Joints for Heat Rejection Systems

The joining of metal tubes to composite plates is required for heat-rejection components in several space applications. Currently a number of different braze compositions are being evaluated as to their effectiveness. Such tube-plate configurations cannot be represented by traditional methods of testing, e.g., lap joints. The joined region is not between two flat surfaces, but rather between a flat surface and a curved surface. Therefore, several tests have been employed to ascertain the effectiveness of the different braze approaches in tension and in shear that are both simple and representative of the actual system and relatively straightforward in analysis. The results of these "tube tests" will be discussed for the three different braze compositions, Cu-ABA, Ti-Cu-Sil, and Ti-Cu-Ni. In addition, fracture analysis of the failed joints was performed and offers insights into the cause of joint failure and the distinctions which need to be made between the "strength" of a joint versus the "load carrying ability" of a joint.

Morscher, Gregory N.↗

Effect of preforming adherends on static and fatigue strength of bonded composite single-lap joints

An analytical and experimental investigation was conducted on bonded composite single-lap joints with the adherends performed to reduce the angle between the line of action of the applied in-plane force and the bondline. A classical closed-form solution was used to analyze the composite joints with various preform angles and overlap lengths. The adherends of the test specimens were preformed before bonding, during the layup and curing process. Static tests were conducted for preform angles of 0, 5, 10, and 15 deg and overlap lengths of 0.75, 1.75, 2.75, and 3.75 in. A limited fatigue study was conducted for specimens with a 2.75-in. overlap and a preform angle of 5 deg. Results of the analysis showed that preforming the adherends of bonded composite single-lap joints significantly reduced the shear and peel stress concentrations in the adhesive. Experimental results showed that preforming the adherends significantly increased their static and fatigue strength and thus increased the load level for which bonded composite single-lap joints can be designed.

Sawyer, J. W.↗

The Adhesion Strength of Impact Ice Measured Using a Modified Lap Joint Test

Numerous methodologies have been utilized to measure the adhesion strength of impact ice, and the data reported in the literature varies significantly from test to test. In order to initiate an investigation to determine the cause of this disparity, a new test methodology has been developed and utilized in the Icing Research Tunnel at the NASA Glenn Research Center. Data was obtained while varying the temperature, test section velocity, and cloud droplet mean volumetric diameter. The first data set acquired using this new test method is presented. New trends demonstrate the effect of annealing ice samples, with temperature being a key variable. Observations during the test and analysis of the results suggest the presence of large residual stresses in the samples.

Work, Andrew H., Jr.↗

Experimental data on single-bolt joints in quasi isotropic graphite/polyimide laminates

Sixteen ply, quasi-isotropic laminates of Celanese Celion 6000/PMR-15 and Celion 6000/LARC-160 with a fiber orientation of (0/45/90/-45) sub 2S were evaluated. Tensile and open hole specimens were tested at room temperature to establish laminate tensile strength and net tensile strength at an unloaded bolt hole. Double lap joint specimens with a single 4.83-mm (0.19 in.) diameter bolt torqued to 1.7 N-m (15 lbf-in.) were tested in tension at temperatures of 116 K (-250F), 297 K (75F), and 589 K (600F). The joint ratios of w/d (specimen width to hole diameter) and e/d (edge distance to hole diameter) were varied from 4 to 6 and from 2 to 4, respectively. The effect of joint geometry and temperature on failure mode and joint stresses are shown. Joint stresses calculated at maximum load for each joint geometry and test temperature are reported. Joint strength in net tension, bearing, and shear out at 116 K (-250F), 297 K (75F), and 589 K (600F) are given for the Celion 6000/PMR-15 and Celion 6000/LARC-160 laminates.

Wichorek, G. R.↗