Search NASA⌕ Search

SEARCH · Search NASA

Results for “Li-ion Cell Performance”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 127 records · Page 7

Novel architectures for stabilization of Mn-rich cathodes: a high-valent approach to interfaces

Lithium- and manganese-rich (LMR) layered oxides continue to generate significant interest as promising, earth-abundant cathode materials for next-generation Li-ion batteries. In spite of their attractive capacity and cost advantages, a few long-standing challenges still hamper their widespread adoption, with manganese dissolution being one of the most persistent and vexing issues. In the present study, we explore the incorporation of Sb5+ as a high-valent cation and exploit its ability to form unique lithium-rich surface and grain-boundary structures that can integrate directly with the LMR lattice. When synthesized under appropriate conditions, Sb5+ orders strongly with Li+ to form localized Li+–Sb5+ motifs, which play a key role in restructuring the surface and grain-boundary regions. These restructured regions act as protective, stabilizing entities that substantially suppress electrolyte-driven side reactions, reduce impedance growth, limit manganese dissolution, and help retain cyclable lithium during long-term electrochemical cycling. Further improvements of the electrochemical performance of Sb-treated LMR were achieved using a well-known additive to mitigate Mn dissolution and highlight the synergistic effects of combined strategies. Overall, this work showcases how high-valent elements such as Sb5+ can help tailor the surface and intergranular regions and work in synergy with other modifiers (e.g. electrolyte additives), enhancing the cycle life and practical viability of LMR cathodes for use in graphite-based full cells.

Mallick, Subhadip [Argonne National Laboratory (AN↗

In situ chamber for studying battery failure using high-speed synchrotron radiography

The investigation of lithium-ion battery failures is a major challenge for personnel and equipment due to the associated hazards (thermal reaction, toxic gases and explosions). To perform such experiments safely, a battery abuse-test chamber has been developed and installed at the microtomography beamline ID19 of the European Synchrotron Radiation Facility (ESRF). The chamber provides the capability to robustly perform in situ abuse tests through the heat-resistant and gas-tight design for flexible battery geometries and configurations, including single-cell and multi-cell assemblies. High-speed X-ray imaging can be complemented by supplementary equipment, including additional probes (voltage, pressure and temperature) and thermal imaging. Together with the test chamber, a synchronization graphical user interface was developed, which allows an initial interpretation by time-synchronous visualization of the acquired data. Enabled by this setup, new meaningful insights can be gained into the internal processes of a thermal runaway of current and future energy-storage devices such as lithium-ion cells.

25 ENERGY STORAGE↗

Quantifying the Impact of Charge Rate and Number of Cycles on Structural Degeneration of Li-Ion Battery Electrodes

A quantitative link between crack evolution in lithium-ion positive electrodes and the degrading performance on cells is not yet well established nor is any single technique capable of doing so widely available. Here, we demonstrate a widely accessible high-throughput approach to quantifying crack evolution within electrodes. The approach applies super-resolution scanning electron microscopy (SEM) imaging of cross-sectioned NMC532 electrodes, followed by segmentation and quantification of crack features. Crack properties such as crack intensity, crack width and length are quantified as a function of charge rate (1C, 6C, and 9C) and cycle number (25, 225, and 600 cycles). Hundreds of particles are characterized for statistical confidence in the quantitative crack measurements. The data on crack evolution is compared to electrochemical data from full cells and half cells with the NMC532 positive electrodes. We show that while crack evolution strongly correlates with capacity fade in the first 25 cycles, it does not correlate well for the following hundreds of cycles indicating that cracking may not be the dominant cause of capacity fade throughout the cycle-life of cells.

25 ENERGY STORAGE↗

Electrochemical Formation of Li-M-(M')-Si Phases Using Multivalent Electrolyte Salt Additives

Lithium-rich silicides (Li 15 Si 4 ), formed during the electrochemical lithiation of silicon, show high reactivity with electrolyte components that contribute to capacity decay, formal lithium loss, and low coulombic efficiency. Recently, the reactivity of lithium silicides was found to be suppressed by substituting a multivalent cation (i.e. Mg, Ca) for lithium that results in the room temperature formation of a ternary Li-M-Si phase. In this study, we explored a range of multivalent electrolyte salt additives (M = Ni, Cu, La, Ce, Sr, Ba, and Ca-Mg mixed salt) in a lithium-ion cell configuration and identified a room temperature electrochemical route to the formation of new ternary and quaternary lithium silicides. Using this method, both nickel and copper salts were found to plate onto the silicon electrode surface upon lithiation. Further, based on refined synchrotron XRD data, multivalent cations with an ionic radius similar to Na (~1.03 Å) or smaller can be inserted electrochemically into a formally cation-deficient Li 15 Si 4 host lattice to form new ternary (or quartenary) phases. The electrochemical synthesis of a new quaternary Li-M-M’-Si phase represents a facile route to preparing and scaling materials isostructural to the Heusler phase and electron-precise Li 14 MgSi 4 phase that results in enhanced cycling and calendar life performance.

25 ENERGY STORAGE↗

Transition from Vogel-Fulcher-Tammann to Arrhenius Ion-Conducting Behavior in Poly(Ethyl Acrylate)-Based Solid Polymer Electrolytes via Succinonitrile Plasticizer Addition

Solid polymer electrolytes (SPEs) offer potential advantages over liquid electrolytes, including flexibility, safety, and processability. However, they suffer from low room-temperature ionic conductivity. Recently, it has been reported a poly(ethyl acrylate) based (polyEA) SPE, by incorporating 50 wt% of succinonitrile (SN) solid plasticizer, 30 wt% of lithium salt and 5 wt% of fluoroethylene carbonate additive, which achieves a high room-temperature ionic conductivity of 1.01 × 10 −3 S cm −1 (Nat. Nanotechnol, 2022, 17, 768-776). This novel SPE exhibits stability against Li 0 and anodic stability up to 4.9 V vs Li + /Li. However, the specific mechanism responsible for its high ionic conductivity remains elusive. In this work, by adjusting the weight ratio of SN in the SPE, a transition from Vogel-Fulcher-Tammann to Arrhenius ion-conducting behavior is observed. It is demonstrated that the addition of SN leads to the gradual decoupling of Li-ion from the polymer backbone and its coordination with SN, as revealed by 6 Li solid-state nuclear magnetic resonance spectroscopy. As a result, Li-ion migration primarily occurs through SN rather than the segmental motion of the polymer backbone. Performances of the SPE in Cu||Li, Li||Li and a LiFePO 4 ||Li pouch cells are shown to demonstrate the commercial viability of this SPE in Li 0 -anode solid-state batteries.

Electrochemistry↗

Characterization of Cycle-Aged Commercial NMC and NCA Lithium-ion Cells: I. Temperature-Dependent Degradation

Lithium-ion batteries are widely used in applications from consumer electronic devices to stationary energy storage. Appropriate management of batteries is challenging due to limited data on their performance and materials degradation. Previous studies have focused on characterization of single cells under specific operating conditions. In the present work, commercial 18650 lithium-ion cells with LiNi x Mn y Co 1-x-y O 2 (NMC) and LiNi x Co y Al 1-x-y O 2 (NCA) positive electrodes were characterized by a wide range of electrochemical and materials techniques after cycling at 15, 25, or 35 °C to ∼80% capacity. The NCA cells exhibit weak temperature dependence in their cycle aging and materials degradation. The NMC cells exhibited increased capacity fade and materials degradation as ambient temperature decreased. All cells exhibited loss of lithium inventory as their primary degradation mode. However, the NCA cells only showed evidence of solid electrolyte interphase (SEI) growth whereas the NMC cells showed signs of Li plating at 15 °C, transitioning to SEI growth at 35 °C. The NMC cells displayed signs of loss of active material at the positive electrode at lower temperatures, suggesting that Li plating is correlated to additional processes that increase the rate of degradation. These results highlight the importance of avoiding broad generalizations about Li-ion battery temperature dependence.

25 ENERGY STORAGE↗

Effects of Trigger Method on Fire Propagation during the Thermal Runaway Process in Li-ion Batteries

Lithium-ion batteries are prone to fire hazards due to the possibility of thermal runaway propagation. During battery product development and subsequent safety tests for design validation and safety certification, the thermal runaway onset is triggered by various test methods such as nail penetration, thermal ramp, or external short circuit. This failure initiation method affects the amount of heat contributions and the composition of gas generations. This study compares two such trigger methods, external heating and using a thermally-activated internal short circuit device (ISCD). The effects of the trigger method on total heat generation are experimentally investigated within 18650 cylindrical cells at single cell level as well as at multiple cell configuration level. The severity of failure was observed to be worse for cells with ISCDs at single cell level, whereas quite the opposite results were observed at multiple cell configuration level. A preliminary numerical analysis was performed to better understand the battery safety performance with respect to thermal runaway trigger methods and heat transfer conditions.

25 ENERGY STORAGE↗

Multiscale approaches for optimizing the impact of strain on Na-ion battery cycle life

Abstract The high costs and geopolitical challenges inherent to the lithium-ion (Li-ion) battery supply chain have driven a rising interest in the development of sodium-ion (Na-ion) batteries as a potential alternative. Unfortunately, the larger ionic radius of Na limits the reversibility of cycling because of the extensive atomic rearrangements that accompany Na-ion insertion, which in turn limit diffusion and charging speed, and lead to rapid degradation of the electrodes. The Center for Strain Optimization for Renewable Energy (STORE) was established to address these challenges and develop new electrode materials for Na-ion cells. This article discusses the current state-of-the-art materials used in Na-ion cells and several directions that STORE believes are critical to understand and control the structural and volumetric changes during the reversible (de)insertion of large cations. Graphical abstract Highlights Understanding the fundamental way materials respond to localized strains at the atomic length-scale is a critical first step in the development of highly reversible, long cycle life, Na-ion insertion hosts. This perspective explores a variety of methods that can be employed to mitigate the detrimental effects of large strain. The insights gained from these investigations should help lay the foundation for the creation of more economical and sustainable batteries that could have immediate impact on global energy infrastructure. Discussion Although there is near universal agreement that electrochemical energy storage must be an integral part of a green-energy future, there is less agreement about how to reduce the cost of energy storage. Replacing high-cost lithium-ion cells with lower-cost sodium-ion batteries is one option frequently considered in future energy models, but the details of what can be achieve with optimized sodium cell performance remains unclear. Here we posit that developing methods to mitigating strain on the electrode particle length scale is a key factor for achieving long-cycle-life sodium-ion batteries. Mitigating strain on the atomic scale suppress electrode-level volume change. Allowing for fast cycling in materials without the problems of electrode cracking or delamination. We further posit that understanding volume change in sodium-ion electrodes at a fundamental level will lead to the designing new sodium-ion electrode materials that will allow for efficient, stable, lower-cost energy storage.

Brady, Michael J.↗

Highly Loaded Sulfur Cathode, Coated Separator and Gel Electrolyte for High Rate Li-Sulfur Batteries

As one of DOE Battery 500 Seedling projects, Cornell University and EIC Labs investigated and developed i) highly loaded sulfur cathodes (> 3 mg/cm 2 ), ii) hybrid separators, and iii) gel ceramic electrolytes (GCE) to mitigate the low rate capability, shuttling effect and limited cycle life in high performance Li-Sulfur batteries. Scalable nanomanufacturing processes such as air-controlled electrospray (ACES) and gas-assisted electrospinning (GAES) have been utilized to develop directly deposited electrodes and polymer/ceramic hybrid separators. First, in the development of highly loaded cathodes, alternating layers of sulfur impregnated mesoporous carbon and graphene were fabricated via ACES and the resulting layered cathodes and coated separators exhibit higher capacity and capacity retention (about 1,000 mAh/g capacity with less than 0.02% fade/cycles) than single layer cathode or cathode prepared by conventional slurry cast. Alternating layer approach via ACES has been applied to high loading systems (3 - 5 mg S/cm 2 ), demonstrating the potential to increase sulfur utilization and capacity retention. We have also incorporated iron oxides (Fe 3 O 4 ) into S/mesoporous carbon/graphene cathodes to enhance sulfur utilization and mitigation of polysulfide shuttling. and the effect of Fe 3 O 4 in mesoporous carbon and Gr is highly pronounced at high C rates of 1C and 2C cycling performance. To further improve the cathodes at high rates, graphene nanoribbons (GNR) which can promote ion transport were incorporated in the cathode, resulting in 550 mAh/g at 5C/5C rates. Hybrid Li-ion/Li-S cathodes has also been explored to better engage unreacted polysulfides during charge/discharge. S/LFP hybrid cathodes offer higher sulfur utilization and enhanced rate capability, as well as higher areal loading. This study suggests inclusion of iron phosphide (Fe2P) which can chemically interact with polysulfides can further enhance sulfur utilization and mitigation of soluble polysulfides at high rates. Secondly, in the development of hybrid separators, we first employed graphene coating on the commercial polyolefin separators, which exhibits higher capability, better capacity retention and enhanced rate capability. To improve the rate capability with enhanced safety features such as thermal stability and nonflammability, we developed polymer/ceramic hybrids based on thermally stable polyimide (PI) and room temperature curable ceramic precursors such as organopolysilazane (OPSZ) or polysilsesquioxanes (PSSQ), which exhibit no shrinkages up to 300 ºC and non-flammability. To improve mechanical properties and electrochemical stability, polybenzimidazole (PBI) and alumina have been incorporated in polymer/ceramic hybrid separator, replacing PI and OPSZ/PSSQ, respectively. Finally, the gel ceramic electrolyte (GCE) based on ceramic cross linkers have been applied to make Li-S cells even safer and also to mitigate the polysulfide shuttling further. The resulting gel ceramic electrolyte offers improved capacity retention and rate capability, and also effectively mitigates polysulfide shuttling which was also confirmed by modeling. Inclusion of high ion conducting additives into GCE together with polymer/ceramic hybrid separators exhibit the higher ionic conductivity than liquid electrolyte with commercial polyolefin separator. We demonstrated that the developed highly loaded sulfur cathodes, polymer/ceramic hybrid separators and gel ceramic electrolyte can effectively mitigate the low rate capability, shuttling effect and limited cycle life in high performance Li-Sulfur batteries with improved safety.

25 ENERGY STORAGE↗

Performance of Lithium-Ion Batteries with 3D Printed Anodes and Compressible Carbon Structures

Carbon scaffolds have been shown to improve the performance of Li metal anodes in Li-ion batteries by acting as conductive hosts for Li metal plating and stripping. The scaffolds provide a more uniform electric field, and their 3D geometry enables smaller diffusion paths for the Li ions. In this project, several different types of carbon lattices were 3D printed, mechanically tested, and analyzed in coin cells. Planar and 3D printed graphite coatings were evaluated as the baseline, since graphite is a common anode material. The results showed that implementing a 3D graphite lattice into a coin cell improved the Li plating and stripping efficiency compared to the planar coating. However, since graphite can intercalate Li ions, other carbon materials were also explored that should act as better hosts for Li plating/stripping. To improve the compressibility of these non-graphite carbon scaffolds, five different carbon ink formulations were 3D printed in lattice configurations. SEM imaging and compression testing showed that both the final dimensions and the compressibility of the carbon lattices depended on the type of carbon precursors used. The two most suitable compositions were found to be those made with graphene oxide-resorcinol formaldehyde and graphene oxide-ammonium hydroxide. In the future, these formulations will be further refined to increase their mechanical strength, and their performance as scaffold hosts for Li metal anodes will be evaluated in coin cells.

25 ENERGY STORAGE↗

High-Performance Low-Cobalt Cathode Materials for Li-ion Batteries

The layer-structured Li[Ni x Co y Mn 1-x-y ]O 2 (NCM) cathode materials have been the best choice for increasing electric vehicle driving distance per charge. The high Ni layered oxide represents successfully commercialized NCM cathodes (such as NCM622 and NCA) in lithium-ion batteries (LIBs) for EV applications due to their high energy density and acceptable cycling stability. However, the price of cobalt, the key element within LIBs for stability, has nearly tripled over the past few years due to increased demand from the cell phone industry. As mentioned in the DOE Funding Opportunity Announcement, the current materials shortage will also cause speculation for a future global shortage. Therefore, to meet the requirement and sustainability of the next-generation long-range and low-cost EVs, developing cathode materials with low-Co content to achieve higher energy density and lower cost is both essential and urgent. The overarching objective of this work is to develop stabilized NCM cathode materials with low Co content (namely LiNi x Co y Mn 1-x-y O 2 , y ≤ 0.04) to meet DOE’s goal of reducing Co loading below 50 mg Wh -1 while maintaining energy density greater than 600 Wh kg -1 based on cathode material. Via various dopings and coatings scalable methods, we explored and enhanced the cycling performance of low-cobalt cathodes. The final obtained NCM cathodes paired with graphite anode aim to deliver batteries with a high initial specific energy density of over 240 Wh kg -1 and a low capacity fading rate of less than 20% in 1000 cycles under a C/3 discharge rate. To accomplish this goal, a multidisciplinary team with several co-investigators has been formed from three organizations: The Pennsylvania State University (PSU), Oak Ridge National Laboratory (ORNL), and Pacific Northwest National Laboratory (PNNL). The PI and co-investigators are Dr. Donghai Wang (PI) from PSU with expertise in the synthesis of nanostructured materials and manipulation of interfacial properties of electrochemically active materials, Dr. Jagjit Nanda, with substantial knowledge of and expertise in state-of-the-art cathodes from ORNL, Dr. Chao-Yang Wang with significant experience in advanced cell design and fabrication and cell diagnostics from PSU, and Dr. Chongmin Wang with world-wide known expertise of advance atomic scale characterization of electrode materials from PNNL. Furthermore, this project will leverage and synergistically work with the current DOE-funded programs on battery materials at PSU and ORNL and electrode materials characterization at PNNL. During this funded period, we have accomplished milestones stated as follows: • Scale up production of LiFePO 4 (LFP) coated NCM811 with a production of 300g/batch. Fifteen (≥2 Ah) pouch cells with LFP-coated NCM811 cathode are delivered. Self-evaluated pouch cells in PSU show superior over 80% capacity retention performance even after 1500 cycles at C/3 rate. • Various cations (Al, Ti, Zr, and Mo) substitute cobalt in low-cobalt partially and Co-free cathodes. Their effects on crystal structure and electrochemical behavior are explored. • Phosphate compounds as coating materials represent promising surface protection precursors for low-cobalt cathode materials. Therefore, several metal phosphates were selected for improving the NMC cycling performance and are regarded as effective approaches for a scalable and practical surface protection method. • Production of NCM92, where Nickel content is 92% among transition metals, is scaled up from synthesis to coating and heat treatment procedures. Fifteen 2.7Ah pouch cells with Ti-doped NCM92 cathodes and industrial graphite anode are delivered to Idaho National Lab for testing.

25 ENERGY STORAGE↗

CRADA Number NFE-21-08827 with DayLyte, Inc. (CRADA Final Report)

DayLyte Batteries is developing an aqueous Sodium-Air battery made with abundant materials while being half to a third the weight of Li-ion to power electric aircraft, electric vehicles and provide renewable energy on demand. To make this battery practical, DayLyte is developing a thin film ceramic Nasicon solid electrolyte amenable to rapid scaleup as well as a protective coating that will protect the solid electrolyte from 50wt% NaOH during the battery’s end-of-discharge while still allowing Na-ions to pass back and forth. If the thin film solid electrolyte and stable coating can be developed it will open the world to step change in battery performance all while not sacrificing the environment on the way. The project was designed to first focus on making and characterizing the Nasicon membrane followed by measuring its electrochemical performance, then assembling a full cell, optimizing its NaOH stability and then optimize the overall prototype design. Over the past two years, we have significantly improved the Nasicon film uniformity, demonstrated protective ligands that are stable in 50wt% NaOH by measuring no mass change with a quartz crystal microbalance, tested different heating methods like tube furnace and rapid heating and developed glassy carbon coatings on the current collector to prevent Nasicon-current collector alloying. We have found that getting film uniformity as measured by electrochemical impedance spectroscopy (EIS) is difficult because of different factors like surface roughness, deposition uniformity and heat treatment time and uniformity. The glassy carbon coating should significantly reduce the surface roughness and by tuning the coating conditions the film deposition uniformity improves and using an automated heating method should lead to much improved film uniformity.

25 ENERGY STORAGE↗

CRADA Final Report: Ultralong Cycle Life and Ultrafast Charging Batteries to Electrify High Duty-Cycle, Mobile Platforms

As part of the Cyclotron Road program, Tyfast Energy Corp. aimed to investigate the Li 3 V 2 O 5 (LVO) anode material for next generation lithium batteries. State of the art and fast charging lithium-ion batteries are based on the lithium titanate or Li 4 Ti 5 O 12 (LTO) anode chemistry. LTO cells demonstrate fast charging times (<6 mins), long cycle life (>20,000 cycles), but at the expense of very low energy density (<200Wh/L, <80Wh/kg). Silicon anodes have the promise of achieving fast charging times, however, issues with cycling stability in combination with fast charging is unknown. LVO has unique properties that enable new performance window for lithium batteries. First, LVO operates at an average potential of 0.6V vs. Li/Li + , well above the Li-metal plating region allowing ultrafast charge capability without sacrificing safety. Second, the LVO has a high specific capacity of 250 mAh/g making battery pack energy density equivalent with current high-energy Li-ion chemistries.

25 ENERGY STORAGE↗

Novel One-Step Production of Carbon-Coated Sn Nanoparticles for High-Capacity Anodes in Lithium-Ion Batteries

Lithium-ion batteries offer the highest energy density of any currently available portable energy storage technology. By using different anode materials, these batteries could have an even greater energy density. One material, tin, has a theoretical lithium capacity (994 mAh/g) over three-times higher than commercial carbon anode materials. Unfortunately, to achieve this high capacity, bulk tin undergoes a large volume expansion, and the material pulverizes during cycling, giving a rapid capacity fade. To mitigate this issue, tin must be scaled down to the nano-level to take advantage of unique micromechanics at the nanoscale. Synthesis techniques for Sn nanoparticle anodes are costly and overly complicated for commercial production. A novel one-step process for producing carbon-coated Sn nanoparticles via spark plasma erosion (SPE) shows great promise as a simple, inexpensive production method. The SPE method, characterization of the resulting particles, and their high-capacity reversible electrochemical performance as anodes are described. With only a 10% addition of these novel SPE carbon-coated Sn particles, one anode composition demonstrated a reversible capacity of ~460 mAh/g, achieving the theoretical capacity of that particular electrode formulation. These SPE carbon-coated Sn nanoparticles are drop-in ready for present commercial lithium-ion anode processing and would provide a ~10% increase in the total capacity of current commercial lithium-ion cells.

25 ENERGY STORAGE↗

Effect of Si Content on Extreme Fast Charging Behavior in Silicon–Graphite Composite Anodes

Commercial Li-ion batteries typically incorporate a small amount of high-capacity silicon (Si)-based materials in the composite graphite-based anode to increase the energy density of the battery. However, very little is known about the effects of Si on the fast-charging behavior of composite anodes. Herein, we examine the effects of the Si/graphite ratio in the composite anode on the fast-charging behavior of full cells. We show that addition of Si increases the rate capability from 1C to 8C and improves the capacity retention in early cycles at 6C due to reduced overpotential in constant current charging cycles. The impacts of Si content on fast-charging aging were identified by Post-Test characterization. Despite realizing benefits of available capacity and reduced Li plating at 6C, silicon–electrolyte interactions lead the time-dependent cell performance to fade quickly in the long term. The Post-Test analysis also revealed the thickening of the electrode and nonuniform distribution of electrolyte decomposition products on the Si-containing anodes, as well as the organic-rich solid electrolyte interphase (SEI), which are the factors behind cell degradation. Our study sheds insight on the advantages and disadvantages of Si/graphite composite anodes when they are used in fast-charging applications and guides further research in the area by designing an optimized composition of Si incorporated in a mature graphite matrix.

25 ENERGY STORAGE↗

One-Step Spark Plasma Erosion Processing of Carbon-Coated Sn-Si Nanoparticles for Lithium-Ion Battery Anodes

High density portable energy storage is desirable owing to the energy requirements of portable electronics and electric vehicles. The Li-ion battery’s high energy density could be even further improved through the utilization of alternative materials (instead of carbon) for the anode, such as Sn or Si. Nonetheless, the large volume expansion upon lithiation, up to ~300% for Li 22 Si 5 , causes pulverization and rapid capacity degradation during cycling. Sn also forms a Li 22 Sn 5 compound with the equivalent stoichiometric Li capacity but with enhanced ductility. Nano-sized Si and Sn have demonstrated distinctive nanoscale properties, facilitating the retention of higher capacities, particularly when coated with carbon, which improves mechanical stability. To date, the methods of synthesizing coated Si, Sn, or Si-Sn alloyed nanoparticles are complicated, costly, and not readily scalable to meet the demands of cost-effective manufacturing. Spark plasma erosion in a hydrocarbon dielectric has been explored as a one-step process to produce Sn-Si alloy nanoparticles coated with a thin carbon film, offering a scalable and cost-effective processing route. The resulting Sn-Si particles exhibited a bi-modal size distribution at ~5 nm and ~500 nm and were carbon-coated, as intended, from the hydrocarbon dielectric breakdown. The spark-eroded nanoparticles were thoroughly characterized using TEM/EDS, XPS, AES, SSNMR, and TGA, and their improved electrochemical performance was assessed through half-cell experiments.

25 ENERGY STORAGE↗

Africa Battery Energy Storage Systems (BESS) Capacity Building Li-Ion Battery Degradation and Performance [Slides]

This presentation is intended for power system engineers, operators, and planners who work on isolated power systems that have (or may soon have) high levels of power generation coming from wind turbines, solar farms, and battery energy storage, which are collectively referred to as inverter-based resources. It describes the basics of lithium-ion battery energy storage systems and lithium-ion battery degradation. Battery degradation at the cell-level is explained, and then the structure and degradation of battery energy storage systems is also explained. This is intended to help power system engineers, operators, and planners to understand and effectively utilize battery energy storage systems.

24 POWER TRANSMISSION AND DISTRIBUTION↗

Experimental Aging and Lifetime Prediction in Grid Applications for Large-Format Commercial Li-Ion Batteries

Due to the growth of electric vehicle and stationary energy storage markets, the production and use of lithium-ion batteries has grown exponentially in recent years. For many of these applications, large-format lithium-ion batteries are being utilized, as large cells have less inactive material relative to their energy capacity and require fewer electrical connections to assemble into packs. And especially for stationary energy storage systems, where energy delivered is the only revenue source, the economics of these battery systems is highly dependent on cell lifetime. However, testing of large-format lithium-ion batteries is time consuming and requires high current channels and large testing chambers, making information on the performance of commercial, large-format lithium-ion batteries hard to come by. Here, accelerated aging test data from four commercial large-format lithium-ion batteries is reported. These batteries span both NMC-Gr and LFP-Gr cell chemistries, pouch and prismatic formats, and a range of cell designs with varying power capabilities. Accelerated aging test results are analyzed to examine both cell performance, in terms of efficiency and thermal response under load, as well as cell lifetime. Cell thermal response is characterized by measuring temperature during cycle aging, which is used to calculated a normalized thermal resistance value that may help estimate both cell cooling needs or to help extrapolate aging test results to different thermal environments. Cell lifetime is evaluated qualitatively, considering simply the average calendar and cycle life across a range of conditions, as well as quantitatively, using statistical modeling and machine-learning methods to identify predictive aging models from the accelerated aging data. These predictive aging models are then used to investigate cell sensitivities to stressors, such as cycling temperature, voltage window, and C-rate, as well as to predict cell lifetime in various stationary storage applications. Results from this work show that cell lifetime and sensitivity to aging conditions varies substantially across commercial cells, necessitating testing for specific cell formats to make quantitative lifetime predictions. That being said, all commercial cells tested here are predicted to reach at least 10-year lifetimes for stationary storage applications. Based on the aging test results and modeling, some cells are expected to be relatively insensitive to temperature and use-case, making them suited for simple use cases with little or no thermal management and simple controls, while the lifetime of other cells could be extended to 20+ years if operated with thermal management and degradation-aware controls.

battery↗