Search NASA⌕ Search

SEARCH · Search NASA

Results for “NIOBIUM ALLOY”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 127 records · Page 7

Tensile and creep rupture behavior of P/M processed Nb-base alloy, WC-3009

Due to its high strength at temperatures up to 1600 K, fabrication of niobium base alloy WC-3009 (Nb30Hf9W) by traditional methods is difficult. Powder metallurgy (P/M) processing offers an attractive fabrication alternative for this high strength alloy. Spherical powders of WC-3009 produced by electron beam atomizing (EBA) process were successfully consolidated into a one inch diameter rod by vacuum hot pressing and swaging techniques. Tensile strength of the fully dense P/M material at 300-1590 K were similar to the arc-melted material. Creep rupture tests in vacuum indicated that WC-3009 exhibits a class 1 solid solution (glide controlled) creep behavior in the 1480 to 1590 K temperature range and stress range of 14 to 70 MPa. The creep behavior was correlated with temperature and stress using a power law relationship. The calculated stress exponent n, was about 3.2 and the apparent activation energy, Q, was about 270 kJ/mol. The large creep ductility exhibited by WC-3009 was attributed to its high strain rate sensitivity.

Hebsur, Mohan G.↗

Effect of Undercooling in a Low-Gravity Containerless Environment on the Structure and Properties of Alloys

The 30 meter and 100 meter drop tubes at the Marshall Space Flight Center offer a unique opportunity to study solidification in a containerless, microgravity environment. Samples are melted in a furnace at the top of the drop tube and solidify during a 4.5 second free fall in the 100 meter drop tube or a 2.6 second free fall in the 30 meter drop tube. The cooling rate obtained in the drop tubes is lower than cooling rates in atomization and splat-quenching processes. Decoupling the rapid solidification process allows the study of the effects of undercooling and recalescence on alloy morphologies. The research therefore has a three-fold purpose. The first is examination of the limits of undercooling of niobium and niobium-base alloys in the drop tube. The second purpose is the observation of microstructures resulting from the solidification of samples at large undercoolings and moderate cooling rates. The third purpose is the observation of metastable phase formation in highly undercooled samples.

Bayuzick, R. J.↗

Creep Resistance of Disk Alloy CH98 with Tungsten and Niobium Additions

Gas turbine engines for future subsonic transports will likely have higher pressure ratios which will require nickel-base superalloy disks with temperature capability up to 1400 F, an increase of about 200 F over current engines. Several advanced disk alloys are being developed to fill this need. One of these, CH98, is a promising candidate for gas turbine engines and is being studied in NASA's AST Program. Additions of the refractory elements tungsten and niobium have been shown to improve tensile and creep properties while maintaining good high temperature fatigue crack growth resistance. Further improvements in creep and crack growth resistance can be achieved with a coarse grain microstructure. The purpose of the present study is aimed at providing a detailed assessment of 0.2 percent creep rates for coarse grain CH98 with tungsten and niobium additions over a range of temperatures and stresses of interest to disk applications.

Gayda, John↗

Undercooling measurement in a low-gravity containerless environment

A technique is described for measuring the amount of undercooling for samples processed in a low-gravity containerless environment. The time of undercooling is determined by measuring the time of cooling before nucleation and recalescence by two infrared detectors. Once the cooling curve for each drop is calculated, the amount of undercooling can then be found. The technique is demonstrated by measuring the amount of undercooling for drops of pure niobium and select compositions of the niobium-germanium alloy system while free falling in a 32 n evacuated drop tube. The total hemispherical emissivities and specific heats for these materials were measured using a high-temperature containerless calorimeter. An overview of the effect of undercooling on drops of niobium and niobium-germanium is given.

Robinson, M. B.↗

Directionally solidified iron-base eutectic alloys

Pseudobinary eutectic alloys with nominal compositions of Fe-25Ta-22Ni-10Cr and Fe-15.5Nb-14.5Ni-6.0Cr were directionally solidified at 0.5 centimeter per hour. Their microstructure consisted of the fcc, iron solid-solution, matrix phase reinforced by about 41-volume-percent, hcp, faceted Fe2Ta fibers and 41-volume-percent, hcp, Fe2Nb lamellae for the tantalum- and niobium-containing alloys, respectively. The microstructural stability under thermal cycling and the temperature dependence of tensile properties were investigated. These alloys showed low elevated-temperature strength and were not considered suitable for application in aircraft-gas-turbine blades although they may have applicability as vane materials.

Tewari, S. N.↗

Containerless processing of Nb-Ge alloys in a long drop tube

The thirty-two meter drop tube at the Marshall Space Flight Center was used to study the effect of zero gravity containerless processing on the structure and properties of materials. The concept involves the suppression of heterogeneous nucleation of solid in liquid and, therefore, solidification accompanied by large degrees of undercooling. Under these conditions metastable phases can be formed or, at the very least, unique nonequilibrium microstructures (containing equilibrium phases) with unique properties can be produced. The drop tube solidification was applied to niobium base alloys with emphasis on the Nb-Ge binary system in an effort to produce metastable phases with high superconducting transition temperatures in bulk specimens. In the past, only lower Ge alloys (Nb-13 a/o, Nb-18 a/o, and Nb-22 a/o) could be undercooled. Higher Ge alloys (e.g., Nb-25 a/o Ge and Nb-27 a/o Ge) can now be undercooled on a routine basis.

Bayuzick, R. J.↗