Search NASA⌕ Search

SEARCH · Search NASA

Results for “Nickel alloy”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 127 records · Page 7

Advanced Ultra-Supercritical Component Test (ComTest) Project for 760*C Steam Conditions

ComTest is a $27M Department of Energy-funded project. Phase I, which began in November 2015, served to identify the technology gaps, as well as the scope and cost of required testing. Phase II, which was awarded in December 2018, includes an advanced manufacturing effort to complete U.S. based supply chain development for full commercial scale (800-850 MWe) AUSC components made of nickel-based alloys, components operating at up to 760°C. Completion of Phase II scheduled for September 30, 2021. Strategic Objectives of U.S. AUSC Project include: Power Plant Efficiency Improvements –Develop cost-effective, reliable technologies to improve the efficiency of new and existing high-temperature advanced generation power plants. Close gaps to achieve readiness for commercial scale demonstration of Advanced Ultra-Supercritical (AUSC) technology. Fabricate full-scale versions of key nickel-based alloy components. Validate capabilities of US supply chain for cost certainty. Support cross-cutting high-temperature generation technologies. Obtain ASME Code approval for new materials, components and processes. Increase power plant steam temperatures for higher cycle efficiency (Note: Average efficiency of US coal-fired fleet = 33% HHV; A-USC plant efficiency over 47% HHV at 1,400°F (760°C) steam temperature).

fireside corrosion↗

Solvent Influence on the Magnetization and Phase of Fe-Ni Alloy Nanoparticles Generated by Laser Ablation in Liquids

The synthesis of bimetallic iron-nickel nanoparticles with control over the synthesized phases, particle size, surface chemistry, and oxidation level remains a challenge that limits the application of these nanoparticles. Pulsed laser ablation in liquid allows the properties tuning of the generated nanoparticles by changing the ablation solvent. Organic solvents such as acetone can minimize nanoparticle oxidation. Yet, economical laboratory and technical grade solvents that allow cost-effective production of FeNi nanoparticles contain water impurities, which are a potential source of oxidation. Here, we investigated the influence of water impurities in acetone on the properties of FeNi nanoparticles generated by pulsed laser ablation in liquids. To remove water impurities and produce “dried acetone”, cost-effective and reusable molecular sieves (3 Å) are employed. The results show that the Fe50Ni50 nanoparticles’ properties are influenced by the water content of the solvent. The metastable HCP FeNi phase is found in NPs prepared in acetone, while only the FCC phase is observed in NPs formed in water. Mössbauer spectroscopy revealed that the FeNi nanoparticles oxidation in dried acetone is reduced by 8% compared to acetone. The high-field magnetization of Fe50Ni50 nanoparticles in water is the highest, 68 Am2/kg, followed by the nanoparticles obtained after ablation in acetone without water impurities, 59 Am2/kg, and acetone, 52 Am2/kg. The core-shell structures formed in these three liquids are also distinctive, demonstrating that a core-shell structure with an outer oxide layer is formed in water, while carbon external layers are obtained in acetone without water impurity. The results confirm that the size, structure, phase, and oxidation of FeNi nanoparticles produced by pulsed laser ablation in liquids can be modified by changing the solvent or just reducing the water impurities in the organic solvent.

36 MATERIALS SCIENCE↗

The dynamic evolution of swelling in nickel concentrated solid solution alloys through in situ property monitoring

Defects and microstructural features spanning the atomic level to the microscale play deterministic roles in the expressed properties of materials. Yet studies of material evolution in response to environmental stimuli most often correlate resulting performance with one dominant microstructural feature only. In this work, the dynamic evolution of swelling in a series of Ni-based concentrated solid solution alloys under high-temperature irradiation exposure is observed using continuous, in situ measurements of thermoelastic properties in bulk specimens. Unlike traditional evaluation techniques which account only for volumetric porosity identified using electron microscopy, direct property evaluation provides an integrated response across all defect length scales. In particular, the evolution in elastic properties during swelling is found to depend significantly on the entire size spectrum of defects, from the nano- to meso-scales, some of which are not resolvable in imaging. Observed changes in thermal transport properties depend sensitively on the partitioning of electronic and lattice thermal conductivity. This emerging class of in situ experiments, which directly measure integrated performance in relevant conditions, provides unique insight into material dynamics otherwise unavailable using traditional methods.

36 MATERIALS SCIENCE↗

Development and performance of INCONEL® alloy 740H® seam-welded piping

INCONEL® alloy 740H® is an age-hardenable nickel-based alloy approved for pressure vessels and piping within ASME Section I, VIII, and B31.1. Currently, the code applies a weld strength reduction factor (WSRF) of 0.7 to the allowable stresses for longitudinal seam welds in the time dependent creep regime. In this work, a full-scale seam weld was successfully produced using typical industrial practices. The component was solution heat-treated and aged after fabrication to improve the performance of the weldment. Tensile, bend, impact, and low-cycle fatigue tests showed the component met all the specification requirements and elevated temperature properties were within base metal expectations with failures predominately in the weld metal. Long-term creep tests, including large samples more representative of the entire weldment, were fabricated and tested to times in excess of 10,000 h at multiple temperatures. Analysis of the creep data supports a WSRF of 0.9 for the solution annealed + aged weldments in contrast to the WSRF of 0.7 currently applied to welded + aged weldments. Metallurgical analysis shows that the solution annealing causes recrystallization of the weld metal and reduces the chemical compositional and microstructural gradients in the weldments resulting in acceptable short-term performance. In long-term creep, evidence for coarsened zones in the weldments due to discontinuous coarsening reactions were identified as the mechanism leading to accelerated creep damage formation in the weld metal and sample failure.

14 SOLAR ENERGY↗

Rapid Alloy Selection and Additive Manufacturing of Nickel Based Superalloys

In this work the rapid alloy selection and subsequent processability via additive manufacturing of nickelbased superalloys was investigated. Rapid alloy selection protocols developed within the project produced two viable nickel-based superalloys. This phase I CRADA demonstrates a viable route for selecting new nickel-based superalloys for additive manufacturing.

36 MATERIALS SCIENCE↗

Design and Development of Low Weight, Titanium Aluminide Airfoils for High Performance Industrial Gas Turbines meeting 65% Combined Cycle Efficiency (Final Report)

This project funded under DOE-FOA-0001816 was performed with the intent of evaluating the potential of utilizing a low density, high specific strength Titanium Aluminide (TiAl) alloy in a large annulus last stage gas turbine blade with the intent of improving combined cycle gas turbine efficiency toward a goal of reaching 65% efficiency. The project consisted of identifying a potentially suitable TiAl material for manufacture of such a large blade by investment casting. This included estimation of design properties for the selected alloy, trade studies using a baseline design created for a nickel based alloy cast in the TiAl alloy to evaluate potential design changes required for the use of this material and optimization of a prototype design for the same baseline application using the selected TiAl alloy. Several rounds of optimization were completed with the intent of meeting the baseline design targets with a resulting design that showed at least equivalent performance in terms of creep, LCF/TMF, HCF and aerodynamic damping potential. While it was found that significant reductions in blade loading on the disk were possible, the design resulting from the optimization met most lifing targets at the baseline size, but showed a reduction in margins in some areas in comparison to the Ni-based baseline design. Additionally, it was found that the low strain tolerance of the TiAl alloy for temperatures at and below the operational temperature of the attachment resulted in marginal, although still acceptable, creep rupture performance of the design. Due to results indicating the reduced potential for increasing turbine annulus compared to expectations a Phase II award was not proposed and it is not recommended to pursue additional design optimization efforts until further material advances with TiAl materials are achieved.

03 NATURAL GAS↗

Dislocation loop evolution and radiation hardening in nickel-based concentrated solid solution alloys

Effects of chemical composition, ion irradiation dose and temperature on unfaulting of irradiation induced Frank dislocation loops to perfect loops in two nickel based single-phase solid solution alloys, Ni–20Fe and NiFe–20Cr, have been studied. The fraction of Frank loops decreases with irradiation dose from 7.2 to 38.4 dpa at 500°C, but with more Frank loops remaining in the ternary alloy. However, perfect loops and dislocation networks become the dominant features of defects at 580°C in both alloys. The results indicate a thermally assisted loop unfaulting process that may be hindered by more sluggish defect motion in the alloy with more chemical components. Nano-indentation with both continuous stiffness method and single indentation method are used to measure radiation hardening. Loop unfaulting in both alloys irradiated at 580°C reduced radiation hardening while significant hardening is observed after irradiation at 500°C. The quasi-static single indentation method exhibits lower hardness results compared to continuous stiffness method, because dislocations induced from the cyclic loading in the latter method get relaxed and stabilized, resulting in higher resistance to the indenter.

36 MATERIALS SCIENCE↗

Factors Influencing Propensity for Stress Relaxation Cracking in Inconel® Alloy 740H® and Practical Guidance for Applications

Inconel® alloy 740H® (UNS N07740) was the first age-hardenable nickel-based alloy approved by the ASME Boiler & Pressure Vessel Code for use in pressure-boundary applications. In recent years, advanced energy systems such as supercritical CO2 power cycles have utilized alloy 740H in large demonstration projects driven by the requirement for higher fluid temperatures and pressures. Stress relaxation cracking (SRxC) following post-weld heat-treatment (PWHT), also known as strain age cracking (SAC), has been identified in a limited number of weldments during these industrial builds resulting in focused research to further clarify factors influencing this cracking tendency. This paper will summarize some of the findings from shop and field fabrication leading to successful welds and characteristics of observed SRxC. Laboratory experiments supported by microstructural characterization will be presented to highlight the importance of variables such as strain, material starting condition, and PWHT temperatures. Finally, the results will be summarized within the context of practical guidance for industry to successfully weld the material in boiler, heat exchanger, and piping applications.

14 SOLAR ENERGY↗

Thermal Stability of Nanocrystalline Gradient Inconel 718 Alloy

Gradient structures containing nanograins in the surface layer have been introduced into Inconel 718 (IN718) nickel-based alloy using the surface mechanical grinding treatment technique. The thermal stability of the gradient IN718 alloy was investigated. Annealing studies reveal that nanograins with a grain size smaller than 40 nm exhibited significantly better thermal stability than those with larger grain size. Transmission electron microscopy analyses reveal that the enhanced thermal stability was attributed to the formation of grain boundaries with low energy configurations. This study provides new insight on strategies to improve the thermal stability of nanocrystalline metals.

36 MATERIALS SCIENCE↗

Multi-Pass Hybrid Laser Arc Welding of Alloy 740H

The presentation reviews the progress made toward reducing the joining time of an advanced nickel-based alloy, Alloy 740H by a factor of two using a novel two step fusion welding approach. In the first step, a high powered laser is used to rapidly join thick weld groove lands (~10-12 mm thick) during a single pass. Hybrid laser arc welding (HLAW) is then used to fill the remaining weld groove and complete the joint. This sequential process also utilizes laser wobble in both steps to reduce welding defects and refine the weld microstructure to obtain improved properties compared to conventional gas tungsten or gas metal arc welds, GTAW and GMAW, respectively. The creep behavior of laser-only thick weld groove land welds and HLAW welds were found to be the same or slightly improved compared to conventional GMAW or GTAW welds in this alloy. Creep tests have been started to verify the long-term creep behavior (~10,000 hrs) of these welds. Modeling results on deep penetration laser welding are presented and the initial simulations of laser welding with laser wobble are shown. The next phase of the project will combine the two processes to make complete welds - deep penetration laser welds of thick weld groove lands followed by rapid filling of the remaining weld groove by HLAW - in thick plates (32 mm thick) Alloy 740H plate and entails development of narrow weld groove welding to further decrease the joining time of this alloy.

36 MATERIALS SCIENCE↗

Preliminary Report on Compositional Specification for Printed 316SS

The Advanced Materials and Manufacturing Technologies Program is focused on accelerating the development and deployment of advanced materials and components fabricated via additive manufacturing (AM). A key challenge for the widespread adoption of AM is the variability in material properties, which can originate from powder feedstock, process parameters, geometry, and the machine. AM powder feedstock compositions are based on those developed for conventional manufacturing. However, the smaller melt pools combined with multiple melt cycles over the course of a build can have substantial effects on the local phase selection resulting from minor batch-to-batch feedstock variability. Therefore, this report focuses on coupling CALPHAD calculations with data mining and visualization to aid the development of compositional specifications for stainless steel 316, an important alloy for nuclear applications and suitable for AM. This work reports that δ-ferrite formation has a stronger dependence on the amount of nickel in the alloy despite nickel being an austenite stabilizer. These findings show the need for exercising a tighter control on the amount of nickel in the alloy compared with the amount of chromium, which is a ferrite stabilizer.

36 MATERIALS SCIENCE↗

Evaluation of high-temperature properties of binary, eutectic Ni-X alloys (X = B, Ca, Ce, La, Y, Zr)

We investigated the high-temperature behavior of binary eutectic nickel-base alloys with low-solubility elements, towards developing alloys with new combinations of structural and functional (e.g. thermal or corrosion) properties. Based on thermodynamic screening, we cast binary near-eutectic Ni-B, Ni-Ca, Ni-Ce, Ni-La, Ni-Y, and Ni-Zr alloys and characterized their microstructure and high-temperature properties. All alloys (except Ni-Ca) contain a fine eutectic microstructure, containing submicron alternating lamellae of γ-Ni and continuous intermetallic phases. The eutectic microstructure did not significantly coarsen at 700°C (except for Ni-B), but measurably coarsened in all alloys at 900°C, most quickly in Ni-B, followed by Ni-Ce, Ni-La, Ni-Y, and Ni-Zr. Coarsening in these alloys occurs by fault migration; diffusion within the intermetallic, and its interfacial energy, likely influence coarsening kinetics. At room-temperature, all alloys possess negligible ductility due to the continuous, brittle intermetallic. At 700 and 900°C, the Ni-Zr alloy showed the best combination of strength and ductility. Oxidation experiments at 900°C on Ni-Zr and Ni-Ce revealed heavy internal oxidation of the continuous intermetallic phase. Overall, the Ni-Zr alloy showed good high-temperature coarsening resistance and strength, though ductility and oxidation resistance require improvement for use in structural applications. Possible routes for improving alloy properties via additive manufacturing are discussed.

Ekaputra, Clement [ORNL] (ORCID:0000000307166479)↗

Electric field enhanced diffusion welding of alloy 617: Microstructural characteristics and mechanical properties

This study investigated the microstructural characteristics and mechanical behavior of diffusion welded nickel-based Alloy 617 obtained by electric field-assisted sintering (EFAS) using various parameters. The interfacial microstructure exhibited different characteristics including good grain boundary (GB) migration across the interface in the samples diffusion-welded at 1100 °C and a flat interface in the samples joined at 1000 °C and 1050 °C. The interface consisted of fine Al 2 O 3 oxides, while precipitation of interfacial M 23 C 6 carbides was not observed. Grain boundaries migrated across the Al 2 O 3 oxides, leaving these oxides within the grains. Graded grain size was observed, with grain coarsening being more significant near the sample surface due to the temperature gradient induced by EFAS. Tensile testing revealed that the specimens fractured in the matrix away from the interface, indicting strong diffusion-welded joints. Further, the peak tensile strength of 807 MPa was obtained in the samples welded at 1000 °C due to minimal grain growth. The materials obtained at 1100 °C exhibited reduced tensile strength but improved ductility. Strain maps revealed by digital image correlation showed alternating high and low strain segments in the samples produced at 1000 °C and 1050 °C, indicating that the flat interfaces with no GB migration were less ductile compared to the matrix. A greater strain uniformity was observed along the bond interfaces with improved GB migration. The hardness reduced near the sample surfaces due to enlarged grains induced by temperature gradient. This study demonstrates that GB migration and enhanced mechanical strength can be achieved in diffusion-welded Alloy 617.

36 MATERIALS SCIENCE↗

A percolation theory for designing corrosion-resistant alloys

Iron-chromium and nickel-chromium binary alloys containing sufficient quantities of chromium serve as the prototypical corrosion-resistant metals owing to the presence of a nanometre-thick protective passive oxide film. Should this film be compromised by a scratch or abrasive wear, it reforms with little accompanying metal dissolution, a key criterion for good passive behaviour. This is a principal reason that stainless steels and other chromium-containing alloys are used in critical applications ranging from biomedical implants to nuclear reactor components. Unravelling the compositional dependence of this electrochemical behaviour is a long-standing unanswered question in corrosion science. Herein, we develop a percolation theory of alloy passivation based on two-dimensional to three-dimensional crossover effects that accounts for selective dissolution and the quantity of metal dissolved during the initial stage of passive film formation. We validate this theory both experimentally and by kinetic Monte Carlo simulation. Our results reveal a path forward for the design of corrosion-resistant metallic alloys.

36 MATERIALS SCIENCE↗

Distribution of Tritium in the Near Surface of Candidate Structural Materials for Fusion Reactors. Type 304L Stainless Steel, Inconel, Hastelloy, Eurofer-97, Oxide Dispersion-Strengthened Alloy 14YWT

Five different candidate structural materials for fusion have undergone pure tritium gas soaking at room temperature and at 310-mbar(a) pressure. The tritium uptake on the surface and in the bulk of the alloys has been analyzed using surface leaching, chemical etching, and thermal desorption. The nickel-based alloys: Inconel-X-750 and Hastelloy-X, absorbed the least amount of total tritium compared with austenitic stainless steel AISI 304L, reduced activation ferritic-martensitic (RAFM) Eurofer-97, and advanced nanoferritic alloy 14YWT. Microstructural analyses using electron backscatter diffraction (EBSD) indicate that the number of grains and mean grain size is not a dominant factor in near surface tritium uptake. The quantity of iron dissolved in the surface oxide appears to be the major factor in encouraging tritium absorption.

O'Callaghan, James↗