Correlation of optical properties and temperature-induced irreversible phase transitions in europium-doped yttrium carbonate nanoparticles
Nanophase europium-doped yttrium carbonate precursors are subjected to heat treatments, ranging from 300 Degree-Sign C to 1100 Degree-Sign C for dwell times of 5 min, 30 min, and 180 min. XRD, TEM, FT-IR, fluorescence, fluorescence excitation, and fluorescence lifetime measurements are used to characterize the materials. Upon heating, the material transitions through several amorphous stages until it reaches the crystalline cubic Y{sub 2}O{sub 3} phase. DSC measurements show an exothermic transition at 665.7 Degree-Sign C, indicating the formation of crystalline Y{sub 2}O{sub 3}. The grain size development is fitted by the relaxation equation and yields an activation energy of 50.3 kJ/mol. The amorphous phases are characterized by inhomogenously broadened optical spectra. Heating up to 700 Degree-Sign C leads to an increased fluorescence lifetime (from about 1 ms to 2.4 ms). As the material is heated to higher temperatures and completes the formation of the crystalline cubic Y{sub 2}O{sub 3} phase, the optical spectra become narrower and the fluorescence lifetime decreases to about 1.2 ms. - Graphical abstract: Fluorescence lifetimes of Eu-doped Y{sub 2}O{sub 3} precursors heated for 5, 30, and 180 min to various temperatures. Highlights: Black-Right-Pointing-Pointer Irreversible phase transitions in nanoparticles are of interest for thermometry. Black-Right-Pointing-Pointer Eu-doped nanophase yttrium carbonate precursors were heat-treated. Black-Right-Pointing-Pointer The material undergoes decomposition and crystallization. Black-Right-Pointing-Pointer Morphological and optical properties are measured. Black-Right-Pointing-Pointer Optical properties can be used to deduce the temperature.