Toxicity of the pyrolysis products of spacecraft materials

A number of spacecraft construction materials are evaluated for the toxic effects of their thermodegradation products on rats. Pyrolysis toxicity testing of pyrolysate fumes establish carbon monoxide, carbon dioxide and hydrogen cyanide as the most common intoxicating agents. Generally, COHb levels of animals expiring in the test chamber suggest higher concentrations of CO are produced with larger samples of most materials.

Lawrence, W. H.↗

The distribution in lunar soil of hydrogen released by pyrolysis

The hydrogen contents of various Apollo 15 rocks and Apollo 15 and 16 soil particle types and sieve fractions have been determined by the pyrolysis method. The Apollo 15 crystalline rocks analyzed release very little hydrogen (approximately 6 micromoles H/g sample). The mineral, glass, and light-colored breccia fragments in the soils contain approximately 5, 30, and 10 micromoles H/g sample, respectively. The dark breccias and glassy agglutinates examined have much higher hydrogen contents (60 and 110 micromoles H/g sample). For soil particle diameters less than 105 microns, hydrogen content increases linearly with particle surface area per particle mass. The calculated grain surface average concentrations of hydrogen in the Apollo 15 and 16 soils fall short of experimentally determined saturation values by a factor of 20. The volume-correlated component of hydrogen in a soil increases with the maturity of the soil.

Desmarais, D. J.↗

The response of smoke detectors to pyrolysis and combustion products from aircraft interior materials

The following projects were completed as part of the effort to develop and test economically feasible fire-resistant materials for interior furnishings of aircraft as well as detectors of incipient fires in passenger and cargo compartments: (1) determination of the sensitivity of various contemporary gas and smoke detectors to pyrolysis and combustion products from materials commonly used in aircraft interiors and from materials that may be used in the future, (2) assessment of the environmental limitations to detector sensitivity and reliability. The tests were conducted on three groups of materials by exposure to the following three sources of exposure: radiant and Meeker burner flame, heated coil, and radiant source only. The first test series used radiant heat and flame exposures on easily obtainable test materials. Next, four materials were selected from the first group and exposed to an incandescent coil to provide the conditions for smoldering combustion. Finally, radiant heat exposures were used on advanced materials that are not readily available.

Mckee, R. G.↗

Effect of species on relative toxicity of pyrolysis products

One of the principal factors in animal toxicity studies is the choice of animal species. A limited study of the relative toxicity of the pyrolysis products from cotton and wool indicated that values of concentrations and doses required to produce death in 50% of the test animals obtained with Swiss albino mice were approximately one-half the values obtained with Sprague-Dawley rats. The toxicity of cotton relative to that of wool was the same using Swiss albino mice or Sprague-Dawley rats. Rankings of relative toxicity appear to be more sensitive to differences in apparatus and procedure than to interspecies differences.

Hilado, C. J.↗

A study of the toxicology of pyrolysis gases from synthetic polymers

An apparatus and procedure for evaluating the toxicity of pyrolysis gases from synthetic polymers are described. In each test, four Swiss albino mice are exposed in a 5-liter chamber to the gases from materials pyrolyzed at 700 C. The apparatus is simple in design, easy to clean, inexpensive and gives reproducible results. Data on several fluorine-containing and polyamide polymers are presented.

Young, W.↗

A model for the pyrolysis of unfilled and filled polymers and comparisons with NBS smoke-density chamber data

This paper considers a model for the pyrolysis of polymers for use in mass loss and smoke density predictions in a fire situation. It is based on the fundamental postulate that the overall rate-limiting reactions are in the relatively low temperature condensed phase; the rate limiting step is the polymer degradation to a vaporizable state. The state of the polymer (chain length) at the surface is specified by the vapor pressure equilibrium criterion. For the case of polymers with inert fillers, like alumina trihydrate, the further assumption is made that the linear regression rate of the material is identical to the unfilled material's at the same surface temperature. The fraction of polymer mass loss converted to smoke is inferred from the literature. The smoke density in the NBS-smoke density chamber is predicted for a polyester and the same polyester with two different loads of alumina trihydrate filler. Diffusional effects in the smoke spreading are considered in an elementary manner. The comparisons with experimental data are encouraging. The overall fire characteristics are predicted using only the fundamental physicochemical property values of ingredients.

Kumar, R. N.↗

Chemical Vapor Deposition of Silicon from Silane Pyrolysis

The four basic elements in the chemical vapor deposition (CVD) of silicon from silane are analytically treated from a kinetic standpoint. These elements are mass transport of silane, pyrolysis of silane, nucleation of silicon, and silicon crystal growth. Rate expressions that describe the various steps involved in the chemical vapor deposition of silicon were derived from elementary principles. Applications of the rate expressions for modeling and simulation of the silicon CVD are discussed.

Praturi, A. K.↗

Apparent lethal concentrations of pyrolysis products of some polymeric materials

Thirty-nine samples of polymeric materials were evaluated to determine the apparent lethal concentrations of their pyrolysis products. The materials were compared on the basis of the apparent lethal concentration for 50 percent of the test animals. Relative toxicity rankings based o apparent lethal concentration values can differ significantly depending on whether they are based on weight of sample charged or weight of sample pyrolyzed. The ranking of polyphenylene sulfide is particularly sensitive to this difference.

Hilado, C. J.↗

Effect of temperature and heating rate on apparent lethal concentrations of pyrolysis products

The apparent lethal concentrations for 50 percent of the test animals of the pyrolysis products from twelve polymeric materials were studied as a function of temperature and heating rate. The materials were polyethylene, nylon 6, ABS, polycarbonate, polyether sulfone, polyaryl sulfone, wool fabric, aromatic polyamide fabric, polychloroprene foam, polyvinyl fluoride film, Douglas fir, and red oak. The apparent lethal concentration values of most materials vary significantly with temperature and heating rate. The apparent lethal concentration values, based on weight of sample charged, appears to effectively integrate the thermophysical, thermochemical, and physiological responses from a known quantity of material under specified imposed conditions.

Hilado, C. J.↗

Relative toxicity of pyrolysis products of some materials used in home furnishings

Seventy samples of cushioning and upholstery materials used in home furnishings were evaluated for relative toxicity by means of the USF/NASA toxicity screening test. The materials were variably toxic under pyrolysis conditions, and this test appeared suitable for discriminating among them on the bases of time to incapacitation and time to death. The addition of fire retardants to these materials to comply with flammability regulations either had no significant effect on toxicity, or resulted in a reduction in relative toxicity. The modification of materials to comply with California upholstered furniture flammability regulations appears to have resulted in desirable limitations on toxicity. Fifty percent of the 70 materials tested caused incapacitation earlier than did the materials in compliance, and 30 percent caused death earlier.

Hilado, C. J.↗

Relative toxicity of products of pyrolysis and combustion of polymeric materials using various test conditions

Relative toxicity data for a large number of natural and synthetic polymeric materials are presented which were obtained by 11 pyrolysis and three flaming-combustion test methods. The materials tested include flexible and rigid polyurethane foams, different kinds of fabrics and woods, and a variety of commodity polymers such as polyethylene. Animal exposure chambers of different volumes containing mice, rats, or rabbits were used in the tests, which were performed over the temperature range from ambient to 800 C with and without air flow or recirculation. The test results are found to be sensitive to such variables as exposure mode, temperature, air flow and dilution, material concentration, and animal species, but relative toxicity rankings appear to be similar for many methods and materials. It is concluded that times to incapacitance and to death provide a more suitable basis for relative toxicity rankings than percent mortality alone, that temperature is the most important variable in the tests reported, and that variables such as chamber volume and animal species may not significantly affect the rankings.

Hilado, C. J.↗

Relative toxicity of pyrolysis products of some polyurethane and polychloroprene foams

Results of toxicity screening tests on some polyurethane and polychloroprene flexible foams are presented. The test method involves the exposure of four Swiss albino male mice in a 4.2-liter hemispherical chamber to the pyrolysis effluents from 1 g of sample exposed to temperatures rising from 200 to 800 C at a rate of 40 C/min. Mortality and times to incapacitation and to death are recorded. Comparisons indicate that flexible polyurethane foams without fire retardant are more toxic than the corresponding foams containing fire retardant, and polychloroprene foams are least toxic.

Hilado, C. J.↗

Toxicity of pyrolysis gases from wood

The toxicity of the pyrolysis gases from nine wood samples was investigated. The samples of hardwoods were aspen poplar, beech, yellow birch, and red oak. The samples of softwoods were western red cedar, Douglas fir, western hemlock, eastern white pine, and southern yellow pine. There was no significant difference between the wood samples under rising temperature conditions, which are intended to simulate a developing fire, or under fixed temperature conditions, which are intended to simulate a fully developed fire. This test method is used to determine whether a material is significantly more toxic than wood under the preflashover conditions of a developing fire.

Hilado, C. J.↗

Toxicity of Pyrolysis Gases from Elastomers

The toxicity of the pyrolysis gases from six elastomers was investigated. The elastomers were polyisoprene (natural rubber), styrene-butadiene rubber (SBR), ethylene propylene diene terpolymer (EPDM), acrylonitrile rubber, chlorosulfonated polyethylene rubber, and polychloroprene. The rising temperature and fixed temperature programs produced exactly the same rank order of materials based on time to death. Acryltonitrile rubber exhibited the greatest toxicity under these test conditions; carbon monoxide was not found in sufficient concentrations to be the primary cause of death.

Hilado, Carlos J.↗

Low cost silicon solar array project silicon materials task: Establishment of the feasibility of a process capable of low-cost, high volume production of silane (step 1) and the pyrolysis of silane to semiconductor-grade silicon (step 2)

A quartz fluid bed reactor capable of operating at temperatures of up to 1000 C was designed, constructed, and successfully operated. During a 30 minute experiment, silane was decomposed within the reactor with no pyrolysis occurring on the reactor wall or on the gas injection system. A hammer mill/roller-crusher system appeared to be the most practical method for producing seed material from bulk silicon. No measurable impurities were detected in the silicon powder produced by the free space reactor, using the cathode layer emission spectroscopic technique. Impurity concentration followed by emission spectroscopic examination of the residue indicated a total impurity level of 2 micrograms/gram. A pellet cast from this powder had an electrical resistivity of 35 to 45 ohm-cm and P-type conductivity.

Breneman, W. C.↗

Effect of heating rate on toxicity of pyrolysis gases from some synthetic polymers

The effect of heating rate on the toxicity of the pyrolysis gases from some synthetic polymers was investigate, using a screening test method. The synthetic polymers were polyethylene, polystyrene, polymethyl methacrylate, polycarbonate, ABS, polyaryl sulfone, polyether sulfone, and polyphenylene sulfide. The toxicants from the sulfur-containing polymers appeared to act more rapidly than the toxicants from the other polymers. It is not known whether this effect is due primarily to differences in concentration or in the nature of the toxicants. The carbon monoxide concentrations found do not account for the observed results.

Hilado, C. J.↗

Effect of heating rate on toxicity of pyrolysis gases from some elastomers

The effect of heating rate on the toxicity of the pyrolysis gases from six elastomers was investigated, using a screening test method. The elastomers were polyisoprene (natural rubber), styrene-butadiene rubber (SBR), ethylene propylene diene terpolymer (EPDM), acrylonitrile rubber, chlorosulfonated polyethylene rubber, and polychloroprene. The rising temperature and fixed temperature programs produced exactly the same rank order of materials based on time to death. Acrylonitrile rubber exhibited the greatest toxicity under these test conditions, and carbon monoxide was not found in sufficient concentrations to be the primary cause of death.

Hilado, C. J.↗