SEARCH · Search NASA
Results for “STEELS, STAINLESS - WELDING”
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Compatibility Assessment of Advanced Stainless Steels in Sodium
Type 316L stainless steel capsules containing commercially pure sodium and miniature tensile specimens of HT-UPS (austenitic, 14Cr-16Ni), NF-616 (ferritic/martensitic, 9Cr-2W-0.5Mo), or 316L (austenitic, 17Cr-10Ni-2Mo) stainless steel were exposed at 600 or 700 C for 100 and 400 h as a screening test for compatibility. Using weight change, tensile testing, and metallographic analysis, HT-UPS and 316L were found to be largely immune to changes resulting from sodium exposure, but NF-616 was found susceptible to substantial decarburization at 700 C. Subsequently, two thermal convection loops (TCLs) constructed of 316L and loaded with commercially pure sodium and miniature tensile specimens of HT-UPS and 316L were operated for 2000 h each one between 500 and 650 C, the other between 565 and 725 C at a flow rate of about 1.5 cm/s. Changes in specimen appearance, weight, and tensile properties were observed to be very minor in all cases, and there was no metallographic evidence of microstructure changes, composition gradients, or mass transfer resulting from prolonged exposure in a TCL. Thus, it appears that HT-UPS and 316L stainless steels are similarly compatible with commercially pure sodium under these exposure conditions.
Explosive fragmentation of additively manufactured stainless steel
Properties of fragmentation from an explosively driven 316L stainless steel spherical shell section fabricated by a laser powder bed additive manufacturing process with minimal surface finishing are investigated. This shell is driven by an insensitive high explosive, resulting in high strain rate deformation (>8 × 10 3 s –1 ) and failure of the stainless steel. Photonic Doppler velocimetry measures the expansion rate; dynamic radiography and high-speed imaging capture the fracture behavior of the stainless steel. The fracture response of the additively manufactured stainless steel shell is compared to published experimental results on additively manufactured 316L stainless steel and conventionally manufactured wrought 316L and 304 stainless steel shell fragmentation. Despite preferred crack orientation, suggesting the influence of surface grooves on fracture time, fragment size is identical to that measured in a similar experiment on wrought 304 stainless steel. Further analysis indicates that the 316L additively manufactured stainless steel shell exhibits comparable spall strength and fragmentation toughness to conventionally manufactured stainless steel yet lower failure strain due to surface stress concentrations.
Tritium Effects on Mechanical Properties of Austenitic Stainless Steels
Why Austenitic Stainless Steel for Tritium Service? • High strength and ductility for structural components and pressure boundaries • Austenitic SS is highly resistant to hydrogen isotope embrittlement • Not immune though
High Mn austenitic stainless steel
An austenitic stainless steel alloy includes, in weight percent: >4 to 15 Mn; 8 to 15 Ni; 14 to 16 Cr; 2.4 to 3 Al; 0.4 to 1 total of at least one of Nb and Ta; 0.05 to 0.2 C; 0.01 to 0.02 B; no more than 0.3 of combined Ti+V; up to 3 Mo; up to 3 Co; up to 1W; up to 3 Cu; up to 1 Si; up to 0.05 P; up to 1 total of at least one of Y, La, Ce, Hf, and Zr; less than 0.05 N; and base Fe, wherein the weight percent Fe is greater than the weight percent Ni, and wherein the alloy forms an external continuous scale including alumina, nanometer scale sized particles distributed throughout the microstructure, the particles including at least one of NbC and TaC, and a stable essentially single phase FCC austenitic matrix microstructure that is essentially delta-ferrite-free and essentially BCC-phase-free.
High Nb, Ta, and Al creep- and oxidation-resistant austenitic stainless steel
An austenitic stainless steel HTUPS alloy includes, in weight percent: 15 to 30 Ni; 10 to 15 Cr; 2 to 5 Al; 0.6 to 5 total of at least one of Nb and Ta; no more than 0.3 of combined Ti+V; up to 3 Mo; up to 3 Co; up to 1 W; up to 0.5 Cu; up to 4 Mn; up to 1 Si; 0.05 to 0.15 C; up to 0.15 B; up to 0.05 P; up to 1 total of at least one of Y, La, Ce, Hf, and Zr; less than 0.05 N; and base Fe, wherein the weight percent Fe is greater than the weight percent Ni wherein said alloy forms an external continuous scale comprising alumina, nanometer scale sized particles distributed throughout the microstructure, said particles comprising at least one composition selected from the group consisting of NbC and TaC, and a stable essentially single phase fcc austenitic matrix microstructure, said austenitic matrix being essentially delta-ferrite-free and essentially BCC-phase-free.
Gas Atomization of Stainless Steel - Slow Motion
Stainless steel liquid atomized by supersonic argon gas into a spray of droplets at ~1800ºC. Atomization of metal requires high pressure gas and specialized chambers for cooling and collecting the powders without contamination. The critical step for morphological control is the impingement of the gas on the melt stream. The video is a black and white high speed video of a liquid metal stream being atomized by high pressure gas. This material was atomized at the Ames Laboratory's Materials Preparation Center http://www.mpc.ameslab.gov
Oxidation resistant high creep strength austenitic stainless steel
An austenitic stainless steel displaying high temperature oxidation and creep resistance has a composition that includes in weight percent 15 to 21 Ni, 10 to 15 Cr, 2 to 3.5 Al, 0.1 to 1 Nb, and 0.05 to 0.15 C, and that is free of or has very low levels of N, Ti and V. The alloy forms an external continuous alumina protective scale to provide a high oxidation resistance at temperatures of 700 to 800.degree. C. and forms NbC nanocarbides and a stable essentially single phase fcc austenitic matrix microstructure to give high strength and high creep resistance at these temperatures.
Nano-composite stainless steel
A composite stainless steel composition is composed essentially of, in terms of wt. % ranges: 25 to 28 Cr; 11 to 13 Ni; 7 to 8 W; 3.5 to 4 Mo; 3 to 3.5 B; 2 to 2.5 Mn; 1 to 1.5 Si; 0.3 to 1.7 C; up to 2 O; balance Fe. The composition has an austenitic matrix phase and a particulate, crystalline dispersed phase.
Effects of Heat Treatment on Phase Transformation and Corrosion Resistance of Boride Layer on Austenitic Stainless Steel AISI 304
The austenitic stainless steel AISI 304 was thermochemically surface treated using a powder-packed boronizing process at a temperature of 950 °C for about 4 hours. Double-phase boride layer (FeB and Fe{sub 2}B) was detected and then investigated for the corrosion resistance compared with the untreated one. Heat treatment was performed at a temperature range of 800 to 900 °C for 2 hours on the boronized austenitic stainless steel AISI 304 to diminish the double-phase boride layer. Afterward, corrosion tests were performed to clarify the effects of heat treatment as well as phase transformation on the corrosion resistance of the boronized austenitic stainless steel AISI 304. The results of this study showed that the formation of single-phase Fe{sub 2}B layer offers the best corrosion resistance.
Surface Processes Control the Fate of Reactive Oxidants Generated by Electrochemical Activation of Hydrogen Peroxide on Stainless-Steel Electrodes
Low-cost stainless-steel electrodes can activate hydrogen peroxide (H 2 O 2 ) by converting it into a hydroxyl radical ( • OH) and other reactive oxidants. At an applied potential of +0.020 V, the stainless-steel electrode produced • OH with a yield that was over an order of magnitude higher than that reported for other systems that employ iron oxides as catalysts under circumneutral pH conditions. Decreasing the applied potential at pH 8 and 9 enhanced the rate of H 2 O 2 loss by shifting the process to a reaction mechanism that resulted in the formation of an Fe(IV) species. Significant metal leaching was only observed under acidic pH conditions (i.e., at pH <6), with the release of dissolved Fe and Cr occurring as the thickness of the passivation layer decreased. Despite the relatively high yield of • OH production under circumneutral pH conditions, most of the oxidants were scavenged by the electrode surface when contaminant concentrations comparable to those expected in drinking water sources were tested. The stainless-steel electrode efficiently removed trace organic contaminants from an authentic surface water sample without contaminating the water with Fe and Cr. With further development, stainless-steel electrodes could provide a cost-effective alternative to other H 2 O 2 activation processes, such as those by ultraviolet light.
Effects of Thiocyanate on Anodic Dissolution of Iron, Chromium, Nickel and Type 304 Stainless Steel: I. Electrochemical Measurements and Surface Morphology
Recently published work investigated themechanism of the catalytic effect of thiocyanate on the active dissolution of ferritic stainless steel (Type 430 stainless steel). This work has been extended to Type 304 stainless steel. Potentiostatic and impedance measurements were performed on pure iron, pure chromium, pure nickel and Type 304 stainless steel in 1 M sulfate solutions at pH = 2.5 and pH= 0. As proposed for Type 430 stainless steel, the catalytic effect of thiocyanate on anodic dissolution of Type 304 stainless steel also appears to be primarily caused by the increased dissolution rate of chromium, counteracting the formation of the Cr-O-Cr passivating network at ledges. Nickel does contribute to the corrosion resistance of Type 304 stainless steel in the presence of thiocyanate, but its beneficial effect appears to be secondary to that of chromium.
In-situ Characterization of Cast Stainless Steel Microstructures
Cast austenitic stainless steel (CASS) that was commonly used in U.S. nuclear power plants is a coarse-grained, elastically anisotropic material. The engineering properties of CASS made it a material of choice for selected designs of nuclear power reactor systems. However, the fabrication processes result in a variety of coarse-grain microstructures that are difficult to inspect ultrasonically, largely due to detrimental effects of wave interactions with the microstructure. To address the inspection needs, new approaches that are robust to these phenomena are being sought. However, overcoming the deleterious effects of the coarse-grained microstructure on the interrogating ultrasonic beam will require knowledge of the microstructure and the corresponding acoustic properties of the material, for potential optimization of inspection parameters to enhance the probability of detecting flaws. The goal of improving the reliability and effectiveness of ultrasonic inspection of CASS specimens can therefore potentially be achieved by first characterizing the microstructure of the component. The characterization of CASS microstructure must be done in-situ, to enable dynamic selection and optimization of the ultrasonic inspection technique. This paper discusses the application of ultrasonic measurement methods for classifying the microstructure of CASS components, when making measurements from the outside surface of the pipe or component. Results to date demonstrate the potential of ultrasonic and electromagnetic measurements to classify the material type of CASS for two consistent microstructures-equiaxed-grain material and columnar-grain material.
Crystallography of intergranular corrosion in sensitized austenitic stainless steel
Highlights: • Intergranular corrosion (IGC) in stainless steel was crystallographically discussed. • Grain boundaries (GBs) were classified based on the coincidence site lattice (CSL). • Influence of the Σ value on their IGC susceptibility had a wide range scatter. • IGC susceptibility was characterized by the Σ value and unit cell area of CSL GBs. - Abstract: This study deals with the susceptibility to intergranular corrosion (IGC) in type 304 austenitic stainless steel from a crystallographic viewpoint. An IGC test was conducted using oxalic acid and sensitized stainless steel, whose crystal orientation was analyzed by electron backscattered diffraction (EBSD). GBs were classified according to the misorientation of adjacent grains, and subclassified using the Σ value based on the coincidence site lattice (CSL) model. The width of corroded groove was measured for each GB category, and the effect of GB category on the susceptibility to IGC was examined. Then, the area of the unit cell of CSL boundaries was used to characterize the susceptibility to IGC of CSL boundaries. It was found that no IGC occurred in low-angle GBs with a misorientation of 15°, the width of corroded groove at each Σ boundary exhibited large scatter. The relationship between the width and unit cell area was characterized by a sigmoid curve, and the susceptibility to IGC was well described by the unit cell area.
Thermal Aging Degradation of Cast Stainless Steels in LWR Systems
Cast austenitic stainless steels (CASSs) have been extensively used for the large components of light water reactor (LWR) power plants such as primary coolant piping and pump casing. Since a large number of massive CASS components are installed in every modern nuclear power plant, any significant degradation of CASS components will raise serious concerns on the integrity of the entire power plant. Upon the presumption that the replacement cost of such massive components is prohibitive, therefore, thorough scientific understanding and systematic monitoring the thermal aging degradation of CASS components should be essential requirements for assessing the plant safety. In the past few decades many researches have concluded that the formation of Cr-rich α-phase by Spinoidal decomposition of δ-ferrite phase, which is formed in high temperature region during cooling, is the primary mechanism for the thermal embrittlement. Cracking mechanism in the thermally-embrittled duplex stainless steels consists of cleavage initiation at ferrite and crack propagation via separation of ferrite-austenite interphase. It has been known, however, that such thermal aging embrittlement is observed only in accelerated aging conditions and the cast stainless steel grades used in nuclear plants have performed well without experiencing real embrittlement. It has been speculated that long-term thermal aging for ≥ 60 years could lead to further decomposition of designed phases and increase of precipitation. This will result in significantly increased susceptibility to embrittlement or other degradation due to thermal aging-radiation synergistic effect, irradiation-induced degradation, stress-corrosion cracking, and general corrosion. Currently, therefore, the thermal embrittlement of CASS components is one of the most serious concerns for extended operation of nuclear power plants. A scientific research is underway to address the issues related to the thermal aging degradation of CASS components. The research aims to provide knowledge-based conclusive prediction for the integrity of the CASS components of LWR power plants during extended operation up to and beyond 60 years. This presentation intends to provide an introductory overview on the thermal aging phenomena in LWR relevant conditions and discussion on the measurements of mechanical property degradation after accelerated and LWR relevant thermal aging treatments. First, the thermal aging effect on toughness is discussed in terms of the causes of embrittlement and influential parameters. Second, the talk will include a comprehensive discussion on the thermal aging effects in different CASS grades (i.e., CF3, CF3M, CF8, and CF8M), which will focus on the influence of alloying elements such as molybdenum and carbon. Third, approximate analysis on thermal reaction in CASS was carried out using Arrhenius equation to decide the effective temperature range for accelerated aging experiments to simulate 60 and 80 years of services in limited time frame. The results will provide valuable insights in the degree of thermal aging. Fourth, calculation on equilibrium precipitation was performed for model CASS alloys using the CALPHAD program, and the results will be used to describe the precipitation behaviors in association with the degradation in mechanical properties. (authors)
Development of nano-structured duplex and ferritic stainless steels by pulverisette planetary milling followed by pressureless sintering
Nano-structured duplex and ferritic stainless steel powders are prepared by planetary milling of elemental Fe, Cr and Ni powder for 40 h and then consolidated by conventional pressureless sintering. The progress of milling and the continuous refinement of stainless steel powders have been confirmed by means of X-ray diffraction and scanning electron microscopy. Activation energy for the formation of duplex and ferritic stainless steels is calculated by Kissinger method using differential scanning calorimetry and is found to be 159.24 and 90.17 KJ/mol respectively. Both duplex and ferritic stainless steel powders are consolidated at 1000, 1200 and 1400 °C in argon atmosphere to study microstructure, density and hardness. Maximum sintered density of 90% and Vickers microhardness of 550 HV are achieved for duplex stainless steel sintered at 1400 °C for 1 h. Similarly, 92% sintered density and 263 HV microhardness are achieved for ferritic stainless steel sintered at 1400 °C. - Highlights: • Synthesized duplex and ferritic stainless steels by pulverisette planetary milling • Calculated activation energy for the formation of duplex and ferritic stainless steels • Studied the effect of sintering temperature on density, hardness and microstructure • Duplex stainless steel exhibits 90% sintered density and microhardness of 550 HV. • Ferritic stainless steel shows 92% sintered density and 263 HV microhardness.