Search NASA⌕ Search

SEARCH · Search NASA

Results for “SULFIDE CORROSION”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 127 records · Page 7

Succession in the petroleum reservoir microbiome through an oil field production lifecycle

Subsurface petroleum reservoirs are an important component of the deep biosphere where indigenous microorganisms live under extreme conditions and in isolation from the Earth's surface for millions of years. However, unlike the bulk of the deep biosphere, the petroleum reservoir deep biosphere is subject to extreme anthropogenic perturbation, with the introduction of new electron acceptors, donors and exogenous microbes during oil exploration and production. Despite the fundamental and practical significance of this perturbation, there has never been a systematic evaluation of the ecological changes that occur over the production lifetime of an active offshore petroleum production system. Analysis of the entire Halfdan oil field in the North Sea (32 producing wells in production for 1-15 years) using quantitative PCR, multigenic sequencing, comparative metagenomic and genomic bins reconstruction revealed systematic shifts in microbial community composition and metabolic potential, as well as changing ecological strategies in response to anthropogenic perturbation of the oil field ecosystem, related to length of time in production. The microbial communities were initially dominated by slow growing anaerobes such as members of the Thermotogales and Clostridiales adapted to living on hydrocarbons and complex refractory organic matter. However, as seawater and nitrate injection (used for secondary oil production) delivered oxidants, the microbial community composition progressively changed to fast growing opportunists such as members of the Deferribacteres, Delta-, Epsilon- and Gammaproteobacteria, with energetically more favorable metabolism (for example, nitrate reduction, H2S, sulfide and sulfur oxidation). This perturbation has profound consequences for understanding the microbial ecology of the system and is of considerable practical importance as it promotes detrimental processes such as reservoir souring and metal corrosion. These findings provide a new conceptual framework for understanding the petroleum reservoir biosphere and have consequences for developing strategies to manage microbiological problems in the oil industry.

02 PETROLEUM↗

Sulfur Loading and Speciation Control the Hydrophobicity, Electron Transfer, Reactivity, and Selectivity of Sulfidized Nanoscale Zerovalent Iron

Sulfidized nanoscale zerovalent iron (SNZVI) is a promising material for groundwater remediation. However, the relationships between sulfur content and speciation and the properties of SNZVI materials are unknown, preventing rational design. Here, the effects of sulfur on the crystalline structure, hydrophobicity, sulfur speciation, corrosion potential, and electron transfer resistance are determined. Sulfur incorporation extended the nano-Fe 0 BCC lattice parameter, reduced the Fe local vacancies, and lowered the resistance to electron transfer. Impacts of the main sulfur species (FeS and FeS 2 ) on hydrophobicity (water contact angles) are consistent with density functional theory calculations for these FeS x phases. These properties well explain the reactivity and selectivity of SNZVI during the reductive dechlorination of trichloroethylene (TCE), a hydrophobic groundwater contaminant. Controlling the amount and speciation of sulfur in the SNZVI made it highly reactive (up to 0.41 L m -2 d -1 ) and selective for TCE degradation over water (up to 240 moles TCE per mole H 2 O), with an electron efficiency of up to 70%, and these values are 54-fold, 98-fold, and 160-fold higher than for NZVI, respectively. These findings can guide the rational design of robust SNZVI with properties tailored for specific application scenarios.

36 MATERIALS SCIENCE↗

Corrosion of Zinc Cold Spray Coatings in a Wet Sweet and Sour Gas Environment

Internal corrosion is a problem for steel pipelines transporting natural gas or CO 2 containing water and partial pressures of H 2 S higher than 0.3 kPa (0.05 psi). This work aims to mitigate internal corrosion in steel pipelines transporting natural gas containing H 2 S using cold spray coatings. Two types of the cold spray binary metallic coatings (zinc chromium [ZnCr]. zinc niobium [ZnNb]) were studied using electrochemical techniques: potentiodynamic polarization, linear polarization resistance, and electrochemical impedance spectroscopy. The corrosion resistance of cold spray coatings (ZnCr, ZnNb) was evaluated in an environment containing 4 bar CO 2 pressure, simulating the partial pressures found in gas transmission lines over a solution of 3.5 wt% NaCl heated to 40°C. A concentration of 0.003 M Na 2 S 2 O 3 ·5H 2 O, corresponding to H 2 S partial pressures around 0.079 bar (1.146 psi), was used to simulate sour conditions. Postcorrosion surface characterization was performed using a scanning electron microscope (SEM) equipped with an energy-dispersive x-ray spectroscope (EDS) and x-ray diffraction analysis. The data showed that the presence of 0.003 M Na 2 S 2 O 3 ·5H 2 O shifted the corrosion potential to more anodic values and decreased the corrosion current density. Both coatings showed similar behavior after 1 h of exposure in the CO 2 /H 2 S environment, indicating that similar electrochemical reactions were occurring on ZnNb and ZnCr. SEM images and EDS surface analyses for specimens showed a significant change in the surface chemical composition of carbon steel coated with ZnNb and ZnCr after 24 h of immersion. In the presence of thiosulfate (under sour conditions), the formation of corrosion product layers (ZnCO 3 and ZnS) on top of ZnNb and ZnCr coatings increased their corrosion resistance, which helped to reduce their corrosion by a factor of 2. Under a sweet environment, the corrosion rates for steel coated with cold spray coatings after 14 d of exposure are lower than that for galvanized steel by a factor of 5 due to the ZnCO 3 layer formed on top of the coatings. The ZnCO 3 layer formed on the steel surface acts as a physical barrier against corrosion by blocking the diffusion of corrosive species to the surface. No localized attack was observed. ZnCr Cold spray coating with defect showed promising corrosion protection against CO 2 corrosion (sweet corrosion) after 14 d of exposure to a CO 2 environment. Here, the scratch on the coating simulated damage created in service, and it was deep enough to expose the substrate material (steel). The formation of zinc oxide (ZnO) and zinc carbonate (ZnCO 3 ) on the scratch confirmed the cathodic protection of the steel by ZnCr and ZnNb coatings.

36 MATERIALS SCIENCE↗

Thermal stability of anisotropic bonded magnets prepared by additive manufacturing

Abstract In this research, anisotropic NdFeB + SmFeN hybrid and NdFeB bonded magnets are additively printed in a polyphenylene sulfide (PPS) polymer binder. Printed NdFeB + SmFeN PPS bonded magnets displayed excellent magnetic properties ( B r [remanence] = 6.9 kG [0.69 T], H cj [coercivity] = 8.3 kOe [660 kA/m], and BH max [energy product] = 9.9 MGOe [79 kJ/m 3 ]) with superior corrosion resistance and thermal stability. The anisotropic NdFeB bonded magnet shows a high coercivity of 14.6 kOe (1162 kA/m) with a BH max of 8.7 MGOe (69 kJ/m 3 ). The coercivity and remanence temperature coefficients for NdFeB + SmFeN hybrid bonded magnets are −0.10%/K and −0.46%/K, and for NdFeB bonded magnets are −0.14%/K and −0.53%/K in the range of 300–400 K, indicating that the hybrid bonded magnets are thermally stable. The average flux aging loss for hybrid magnets was also determined to be very stable over 2000 h at 448 K (175°C) in air with 2.04% compared to that of NdFeB magnets with 3.62%.

thermal stability↗

Structural, Thermal, and Mechanical Characterization of a Thermally Conductive Polymer Composite for Heat Exchanger Applications

Polymer composites are being considered for numerous thermal applications because of their inherent benefits, such as light weight, corrosion resistance, and reduced cost. In this work, the microstructural, thermal, and mechanical properties of a 3D printed polymer composite with high thermal conductivity are examined using multiple characterization techniques. Infrared spectroscopy and X-ray diffraction reveal that the composite contains a polyphenylene sulfide matrix with graphitic fillers, which is responsible for the high thermal conductivity. Furthermore, differential scanning calorimetry determines that the glass transition and melting point of the composite are 87.6 °C and 285.6 °C, respectively. Thermogravimetric analysis reveals that the composite is thermally stable up to ~400 °C. Creep tests are performed at different isotherms to evaluate the long-term performance of the composite. The creep result indicates that the composite can maintain mechanical integrity when used below its glass transition temperature. Nanoindentation tests reveal that modulus and hardness of the composite is not significantly influenced by heating or creep conditions. These findings indicate that the composite is potentially suitable for heat exchanger applications.

36 MATERIALS SCIENCE↗

Chemical and Microstructural Changes in Metallic and Ceramic Materials Exposed to Venusian Surface Conditions

The chemical and microstructural behavior of steels (304, 310, 316, and 1018), nickel-based alloys (beta-NiAl, G30, and 625), gold, coatings (4YSZ, SilcoNert(TradeMark) 1040 (SilcoTek Co.), Dursan(TradeMark) (SilcoTek Co.), and porcelain), and bulk ceramics (alpha-Al2O3, fused quartz, beta-SiC, and alpha-Si3N4) were probed after exposure to supercritical fluid with temperature, pressure, and composition mimicking the Venus lower atmosphere. Exposures were carried out in the Glenn Extreme Environments Rig (GEER) chamber with the Venusian gas mixture (96.5% CO2, 3.5% N2, 30 ppm H2O, 150 ppm SO2, 28 ppm CO, 15 ppm OCS, 3 ppm H2S, 0.5 ppm HCl, and 5 ppb HF) at 92 bar (1330 psi) and 467 C (873 F) for durations of 10 and 42 days. An additional 21-day exposure was done to stainless steel uncoated and coated with SilcoNert(TradeMark) and Dursan(TradeMark). Samples were characterized before and after the experiment by gravimetric analysis, X-ray diffraction, X-ray photoelectron and Auger electron spectroscopies, and cross section electron microscopy analysis. All steels exposed for 10 and 42 days formed double-layered scales consisting mainly of metal (Cr, Fe, Ni) oxides and sulfides showing different chemistry, microstructure, and crystalline phases. The alloys G30 and 625 formed double-layered scales consisting mainly of nickel sulfides. After 10 days, the beta-NiAl exhibited no detectable scale, suggesting only a very thin film was formed. The 304 and 316 stainless steels coated with 4YSZ that were exposed for 10 and 42 days exhibited no significant oxidation. Steel 1018 coated with 4YSZ exhibited a corrosion scale of iron and/or chromium oxide formed at the base of the alloy. The 304 steel coated with porcelain did not exhibit corrosion, although the coating exhibited recession. SilcoNert(TradeMark) exposed for 10 and 42 days exhibited recession, although no oxidation was found to occur at the base of the alloy. Stainless steel 316 coated with Dursan(TradeMark)  exhibited corrosion at the base of the alloy. All ceramics tested showed no clear evidence of reaction. The weight-gain-per-area performance of the materials exposed in the GEER for 10 and 42 days are reported from the lowest to the highest weight gain per area as follows: gold did not exhibit any weight change; nickel-based alloys: beta- NiAl < G30 < 625; steels: 304 < 310 < 316 < 1018; ceramics: considering the experimental uncertainties, no weight change was observed for all ceramics of this work (alpha-Al2O3, Si3N4, SiC, and amorphous SiO2).

Costa, Gustavo C. C.↗

Recent advances in hydrotreating of pyrolysis bio-oil and its oxygen-containing model compounds

There is considerable world-wide interest in discovering renewable sources of energy that can substitute for fossil fuels. Lignocellulosic biomass, which is the most abundant and inexpensive renewable feedstock on the planet, has a great potential for sustainable production of fuels, chemicals, and carbon-based materials. Fast pyrolysis integrated with hydrotreating is one of the simplest, most cost-effective and most efficient processes to convert lignocellulosic biomass to liquid hydrocarbon fuels for transportation, which has attracted significant attention in recent decades. However, effective hydrotreating of pyrolysis bio-oil presents a daunting challenge to the commercialization of biomass conversion via pyrolysis-hydrotreating. Specifically, development of active, selective, and stable hydrotreating catalysts is the bottleneck due to the poor quality of pyrolysis bio-oil feedstock (high oxygen content, molecular complexity, coking propensity, and corrosiveness). Significant research has been conducted to address the practical issues and provide the fundamental understanding of the hydrotreating/hydrodeoxygenation (HDO) of bio-oils and their oxygen-containing model compounds, including phenolics, furans, and carboxylic acids. A wide range of catalysts have been studied, including conventional Mo-based sulfide catalysts and noble metal catalysts, with the latter being the primary focus of the recent research because of their excellent catalytic performances and no requirement of environmentally unfriendly sulfur. The reaction mechanisms of HDO of model compounds on noble metal catalysts as well as their efficacy for hydrotreating or stabilization of bio-oil have been recently reported. This review provides a survey of the relevant literatures of recent 10 years about the advances in the understanding of the HDO chemistry of bio-oils and their model compounds mainly on noble metal catalysts.

biomass, lignocellulose, pyrolysis bio-oil, hydrod↗

The development of a potassium-sulfide glass fiber cell and studies on impurities in alkali metal-sulfur cells

Potassium sulfur rechargeable cells, having as the electrolyte the thin walls of hollow glass fibers made from permeable glass, were developed. The cells had short lives, probably due to the construction materials and impurities in the potassium. The effect of the impurities in the analogous NA-S system was studied. Calcium, potassium, and NaOH/oxide impurities caused increased resistance or corrosion of the glass fibers. For long lived cell operation, the Na must contain less than 1 ppm Ca and less than a few ppm of hydroxide/oxide. Up to 150 ppm K can be tolerated. After purification of the Na anolyte, cell lifetimes in excess of 1000 deep charge-discharge cycles or over 8 months on continuous cycling at 10-30 percent depth of discharge were obtained.

Tsang, F. Y.↗

Environmental Impact Analysis on the Hydraulic Fracture Test Site (HFTS)

Objective The Hydraulic Fracture Test Site (HFTS) provided a platform to test new extraction and production techniques and technologies to understand fracture geometry and increase the efficiency of shale hydrocarbon production. Eleven test wells were drilled in the Upper and Middle Wolfcamp formations, hydraulically fractured, and produced. Air quality, groundwater quality, and produced water chemistry and microbiology were monitored through the duration of the field experiment and one year into production. Methods BTEX, methane, VOCs, SOx, NOx, and PM 10 were measured 1,000 ft up-wind and 1,000 ft down-wind of the HFTS experiment before operations began, during hydraulic fracturing, flowback, and several months into production to evaluate operational impact on local air quality. The underlying Edward-Trinity Plateau aquifer was monitored using 5 groundwater wells within 2 miles of the HFTS pad; BTEX, methane, petroleum hydrocarbons, and a comprehensive suite of anions and metals were analyzed from samples taken before operations began, during hydraulic fracturing, flowback, and one year after production. Water produced from 3 of the 11 HFTS wells was analyzed for chemical and microbiological properties 1.5 years into production. Observations There was no significant impact to air quality from HFTS operations, although elevated BTEX concentrations were measured 1,000 ft. away from the well-pads during the flowback period. We detected no migration of hydrocarbon or fracture fluid chemical migration into the Edward-Trinity Plateau aquifer. Source waters used for hydraulic fracturing contained naturally occurring high concentrations (~500ppm) of sulfate. Rapid microbially induced corrosion was detected in several wells, leading to biocide dosing. Microbiological populations were significantly altered by biocide treatment, but still continued to increase in population size six months after application. Significance After hydraulic fracturing, detailed chemical and microbiological analysis provides evidence for microbiologicallymediated sub-surface transformations of supplied sulfate and organic carbon into sulfides. This report discusses air quality, water quality, and produced water analytical results for the HFTS experiment and further implications for the unconventional oil and gas industry.

Eisenlord, Sarah↗

Antimony(III) Sulfide Thin Films as a Photoanode Material in Photocatalytic Water Splitting

Here, we introduce exploratory investigations on the performance of thermally evaporated Sb 2 S 3 thin film photoanodes for solar-assisted water splitting applications. With a bandgap of 1.72 eV, a 250 nm thick Sb 2 S 3 photoanode showed a saturation photocurrent density of ~600 µA cm -2 measured at 1.0 V vs. reversible hydrogen electrode (RHE) in 0.1 M Na 2 SO 4 under 1-sun illumination, with an onset potential of ~0.25 V vs. RHE. However, subsequent photodegradation studies revealed that the material dissolves relatively quickly with the application of both illumination and bias. Nonetheless, Sb 2 S 3 does have the advantage of having a relatively low optimal fabrication temperature of 300 °C and thus may have utility as a top cell absorber of a tandem device where the bottom cell is temperature sensitive, if protected from corrosion. Thus, we characterized relevant aspects of the material in an attempt to explain the large difference between the theoretical maximum and measured current density. From our characterization it is believed that the photocatalytic efficiency of this material can be improved by modifying the surface to reduce optical reflection and addressing inherent issues such as high electrical resistivity and surface defects.

36 MATERIALS SCIENCE↗

Low temperature hot corrosion

The reaction of Co-Cr, Ni-Cr, Co-Cr-Al, and Ni-Cr-Al alloys with Na2SO4 in the presence of SO3 at temperatures between 700 and 750 C leads to the formation of liquid CoSO4-Na2SO4 or NiSO4-Na2SO4 deposits on the alloy surface. The formation of Cr2O3 and/or Al2O3 below this deposit results in a locally low P(O2) and a higher P(S2) and P(SO2). It is noted that these conditions can prevent protective oxide formation either by sulfide formation in the alloy, which localizes the Cr and/or Al in discrete particles, or by acid fluxing involving a reaction between Al2O3 or Cr2O3 and SO2 to form a salt-soluble species and subsequent reprecipitation as porous oxides in regions of higher P(O2). These processes may occur simultaneously, although a given alloy generally exhibits features of predominantly one type. Here, the Ni-Cr and Ni-Cr-Al alloys, and to some extent the Co-Cr alloys, exhibit features indicative of the sulfidation mechanism, whereas the morphology for the Co-Cr-Al alloy is more consistent with a predominant acid fluxing mechanism.

Chiang, K. T.↗

Effects of Thiocyanate on Anodic Dissolution of Iron, Chromium, Nickel and Type 304 Stainless Steel. II. Surface Analysis by XPS

As proposed in Part I of this paper, the accelerating effect of thiocyanate on active dissolution of stainless steel in acid sulfate solution occurs by adsorption of sulfur on the steel surface, causing accelerated dissolution of chromium from the steel surface. Surface analysis (X-ray photoelectron spectroscopy) was performed on pure chromium and nickel, a high-purity Fe-20wt% Cr alloy and Type 430 and Type 304 stainless steel to test the proposed mechanism. Surface analysis of the Fe 20wt% Cr alloy and stainless steels (Types 430 and 304) confirmed that chromium enriched on the metal surface during anodic dissolution in thiocyanate-free solution and that the surface enrichment of chromium was smaller in thiocyanate-containing solution. Surface analysis also confirmed the formation of sulfide or adsorbed sulfur on the Fe-20wt% Cr alloy in thiocyanate-containing solution. Surface restructuring of sulfide-covered electrode (Type 304 stainless steel and nickel) was the possible reason why increased anodic current density was observed immediately following interruption of anodic polarization for periods of 5s to 120s.

36 MATERIALS SCIENCE↗

Fracture mechanics and surface chemistry investigations of environment-assisted crack growth

It is pointed out that environment-assisted subcritical crack growth in high-strength steels and other high-strength alloys (particularly in hydrogen and in hydrogenous environments) is an important technological problem of long standing. This problem is directly related to issues of structural integrity, durability, and reliability. The terms 'hydrogen embrittlement' and 'stress corrosion cracking' have been employed to describe the considered phenomenon. This paper provides a summary of contributions made during the past ten years toward the understanding of environmentally assisted crack growth. The processes involved in crack growth are examined, and details regarding crack growth and chemical reactions are discussed, taking into account crack growth in steels exposed to water/water vapor, the effect of hydrogen, reactions involving hydrogen sulfide, and aspects of fracture surface morphology and composition. Attention is also given to the modeling of crack growth response, crack growth in gas mixtures, and the interaction of solute atoms with the crack-tip stress field.

Wei, R. P.↗

FUEL 254: Activation of molecular hydrogen on palladium separation membrane surfaces in the presence of H 2 S

Dense palladium-based membranes are of significant interest for separation of hydrogen from mixed gas streams. In this work, flux measurements, materials characterization, and computational modeling combine to provide a framework for understanding the influence of sulfur on molecular hydrogen's dissociative adsorption on Pd and Pd-alloy surfaces and, thus, a foundation for membrane design improvements. Two modes of sulfur-induced deactivation are observed during membrane flux testing. A corrosive decay mechanism is associated with formation of a thick, low diffusivity, Pd 4 S scale layer on the membrane surface. In this case, both the surface region and top layer of the scale display Pd 4 S stoichiometry; Pd-terminated Pd 4 S low-index faces appear to provide the activity required for hydrogen dissociation. A catalytic poisoning mechanism is not associated with formation of a stable sulfide compound; instead, it may result in formation of a thin, sulfur-rich (relative to Pd 4 S) overlayer that effectively inhibits the dissociation reaction.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Hydrogen Embrittlement

Hydrogen embrittlement (HE) is a process resulting in a decrease in the fracture toughness or ductility of a metal due to the presence of atomic hydrogen. In addition to pure hydrogen gas as a direct source for the absorption of atomic hydrogen, the damaging effect can manifest itself from other hydrogen-containing gas species such as hydrogen sulfide (H2S), hydrogen chloride (HCl), and hydrogen bromide (HBr) environments. It has been known that H2S environment may result in a much more severe condition of embrittlement than pure hydrogen gas (H2) for certain types of alloys at similar conditions of stress and gas pressure. The reduction of fracture loads can occur at levels well below the yield strength of the material. Hydrogen embrittlement is usually manifest in terms of singular sharp cracks, in contrast to the extensive branching observed for stress corrosion cracking. The initial crack openings and the local deformation associated with crack propagation may be so small that they are difficult to detect except in special nondestructive examinations. Cracks due to HE can grow rapidly with little macroscopic evidence of mechanical deformation in materials that are normally quite ductile. This Technical Memorandum presents a comprehensive review of experimental data for the effects of gaseous Hydrogen Environment Embrittlement (HEE) for several types of metallic materials. Common material screening methods are used to rate the hydrogen degradation of mechanical properties that occur while the material is under an applied stress and exposed to gaseous hydrogen as compared to air or helium, under slow strain rates (SSR) testing. Due to the simplicity and accelerated nature of these tests, the results expressed in terms of HEE index are not intended to necessarily represent true hydrogen service environment for long-term exposure, but rather to provide a practical approach for material screening, which is a useful concept to qualitatively evaluate the severity of hydrogen embrittlement. The effects of hydrogen gas on mechanical properties such as tensile strength, ductility, fracture, low and high cycle fatigue, crack growth rate, and creep rupture are analyzed with respect to the general trends established from the HEE index values. It is observed that the severity of HE effects is also influenced by environmental factors such as pressure, temperature, and hydrogen gas purity. The severity of HE effects is also influenced by material factors such as surface finish, heat treatment, and product forms, compositions, grain direction, and crystal orientations.

Jonathan A. Lee↗

Photocatalytic water splitting—The untamed dream: A review of recent advances

Here, photocatalytic water splitting using sunlight is a promising technology capable of providing high energy yield without pollutant byproducts. Herein, we review various aspects of this technology including chemical reactions, physiochemical conditions and photocatalyst types such as metal oxides, sulfides, nitrides, nanocomposites, and doped materials followed by recent advances in computational modeling of photoactive materials. As the best-known catalyst for photocatalytic hydrogen and oxygen evolution, TiO 2 is discussed in a separate section, along with its challenges such as the wide band gap, large overpotential for hydrogen evolution, and rapid recombination of produced electron-hole pairs. Various approaches are addressed to overcome these shortcomings, such as doping with different elements, heterojunction catalysts, noble metal deposition, and surface modification. Development of a photocatalytic corrosion resistant, visible light absorbing, defect-tuned material with small particle size is the key to complete the sunlight to hydrogen cycle efficiently. Computational studies have opened new avenues to understand and predict the electronic density of states and band structure of advanced materials and could pave the way for the rational design of efficient photocatalysts for water splitting. Future directions are focused on developing innovative junction architectures, novel synthesis methods and optimizing the existing active materials to enhance charge transfer, visible light absorption, reducing the gas evolution overpotential and maintaining chemical and physical stability

36 MATERIALS SCIENCE↗

Effect of the amount of Na2SO4 on the high temperature corrosion of Udimet-700

The corrosion of Udimet-700, coated with different doses of Na2SO4, was studied in an isothermal thermogravimetric test in the temperature range 900 to 950 C. The weight gain curve is characterized by five distinct stages: an initial period of linear corrosion; an induction period; a period of accelerated corrosion; a period of decelerating corrosion; and a period of parabolic oxidation. The time required for the failure of the alloy increases with an increase in the amount of Na2SO4, reaches a peak and then decreases with further increase in the amount of Na2SO4. For low and intermediate doses (0.3 to 2.0 mg/sq cm), the catastrophic failure of the material occurs by the formation of Na2MoO4 and interaction of the liquid Na2MoO4 with the alloy. For heavy doses, the degradation of the material is due to the formation of large amounts of sulfides.

Misra, A. K.↗

Application of Atmospheric Pressure Photoionization H/D-exchange Mass Spectrometry for Speciation of Sulfur-containing Compounds

Herein we report the observation of atmospheric pressure in-source hydrogen–deuterium exchange (HDX) of thiol group for the first time. The HDX for thiol group was optimized for positive atmospheric pressure photoionization (APPI) mass spectrometry (MS). The optimized HDX-MS was applied for 31 model compounds (thiols, thiophenes, and sulfides) to demonstrate that exchanged peaks were observed only for thiols. The optimized method has been successfully applied to the isolated fractions of sulfur-rich oil samples. The exchange of one and two thiol hydrogens with deuterium was observed in the thiol fraction; no HDX was observed in the other fractions. Thus, the results presented in this study demonstrate that the HDX-MS method using APPI ionization source can be effective for speciation of sulfur compounds. This method has the potential to be used to access corrosion problems caused by thiol-containing compounds. .

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗