Search NASA⌕ Search

SEARCH · Search NASA

Results for “Solid electrolyte interphase”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 127 records · Page 7

Multi-modal characterization methods of solid-electrolyte interphase in silicon-graphite composite electrodes

Composite silicon-graphite (Si-Gr) anodes can improve battery energy density, due to Si's high gravimetric capacity, while mitigating mechanical degradation of the anode and solid-electrolyte interphase (SEI) caused by Si volumetric expansion. Optimizing these anodes is challenging, in part due to difficulty characterizing the SEI structure and composition. In this work, we present multi-modal characterization of the SEI on composite Si-Gr anodes to relate SEI chemical composition and structure to functional properties. Discrepancies in elemental concentrations from X-ray photoelectron spectroscopy, Auger electron spectroscopy, and energy-dispersive X-ray spectroscopy (EDS) are attributed to varying information depth and lateral resolution of the individual probes. However, by combining quantitative composition information with spatially resolved element mapping from scanning transmission electron microscopy, EDS, and electron energy loss spectroscopy, a holistic picture of the SEI emerges. We observe the bilayer SEI structure and a direct correlation between elemental Li and F, suggesting that most Li in the SEI exists as lithium fluoride (LiF). Further, LiF concentration is directly proportional to the maximum SEI resistivity, as determined by scanning spreading resistance microscopy. Lastly, there is an inverse relationship between lithium carbonate and LiF concentration in the SEI, providing insight into the detailed chemistry of SEI formation and evolution.

25 ENERGY STORAGE↗

Phosphorus Enrichment as a New Composition in the Solid Electrolyte Interphase of High-Voltage Cathodes and Its Effects on Battery Cycling

Immersion of a solid into liquid often leads to the modification of both the structure and chemistry of surface of the solid, which subsequently affects the chemical and physical properties of the system. For the case of the rechargeable lithium ion battery, such a surface modification is termed as solid electrolyte interphase (SEI) layer, which has been perceived to play critical role for the stable operation of the batteries. However, the structure and chemical composition of SEI layer and its spatial distribution and dependence on the battery operating condition remain unclear. By using aberration corrected scanning transmission electron microscopy coupled with ultra-high sensitive energy dispersive x-ray spectroscopy, we probed the structure and chemistry of SEI layer on several high voltage cathodes. We show that layer-structured cathodes, when cycled at a high cut off voltage, can form a P-rich SEI layer on their surface, which is a direct evidence of Li-salt (LiPF6) decomposition. Our systematical investigations indicate such cathode/Li-salt side reaction shows strong dependence on structure of the cathode materials, operating voltage and temperature, indicating the feasibility of SEI engineering. These findings provide us valuable insights into the complex interface between the high-voltage cathode and the electrolyte.

Environmental Molecular Sciences Laboratory↗

Heterogeneous Solid Electrolyte Interphase Interactions Dictate Interface Instability in Sodium Metal Electrodes

Sodium (Na) metal batteries have attracted recent attention due to their low cost and high abundance of Na. However, the advancement of Na metal batteries is impeded due to key challenges such as dendrite growth, solid electrolyte interphase (SEI) fracture, and low Coulombic efficiency. This study examines the coupled electro‐chemo‐mechanical interactions governing the electrodeposition stability and morphological evolution at the Na/electrolyte interface. The SEI heterogeneities influence transport and reaction kinetics leading to the formation of current and stress hotspots during Na plating. Further, it is demonstrated that the heterogeneity‐induced Na metal evolution and its influence on the stress distribution critically affect the mechanical overpotential, contributing to a faster SEI failure. The analysis reveals three distinct failure mechanisms—mechanical, transport, and kinetic—that govern the onset of instabilities at the interface. Finally, a comprehensive comparative study of SEI failure in Na and lithium (Li) metal anodes illustrates that the electrochemical and mechanical characteristics of the SEI are crucial in tailoring the anode morphology and interface stability. This work delineates mechanistic stability regimes cognizant of the SEI attributes and underlying failure modes and offers important guidelines for the design of artificial SEI layers for stable Na metal electrodes.

25 ENERGY STORAGE↗

In Situ Measurement of the Plane-Strain Modulus of the Solid Electrolyte Interphase on Lithium-Metal Anodes in Ionic Liquid Electrolytes

In this paper, we present an experimental approach for in situ measurement of elastic modulus of the solid electrolyte interphase (SEI), which is formed from reactions between a lithium thin-film [on a polydimethylsiloxane (PDMS) substrate] and a room-temperature ionic liquid (RTIL) electrolyte. The SEI forms under a state of compressive stress, which causes buckling of the sample surface. In situ atomic force microscopy is used to measure the dominant wavelength of the wrinkled surface topography. A mechanics analysis of strain-induced elastic buckling instability of a stiff thin film on a soft substrate is used to determine the plane strain modulus of the SEI from the measured wavelength. The measurements are performed for three RTIL electrolytes: 1-butyl 1-methylpiperidinium bis(trifluoromethylsulfonyl)imide (P 14 TFSI) without any lithium salt, 1.0 M lithium bis(trifluoromethylsulfonyl)imide (Li TFSI) in P 14 TFSI, and 1.0 M lithium bis(fluorosulfonyl)imide (Li FSI) in P 14 TFSI to investigate the influence of lithium salts on the plane strain modulus of the SEI. The measurements yield plane-strain moduli of approximately 1.3 GPa for no-salt P 14 TFSI and approximately 1.6 GPa for 1.0 M Li TFSI in P 14 TFSI and 1.0 M Li FSI in P 14 TFSI. Finally, the experimental technique presented here eliminates some of the uncertainties associated with traditional SEI mechanical characterization approaches and offers a platform to engineer an SEI with desired mechanical properties by approaches that include altering the electrolyte composition.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Three-dimensional electronic resistivity mapping of solid electrolyte interphase on Si anode materials

Silicon is a promising candidate for the lithium ion battery (LIB) anode because of the order-of-magnitude improvement in capacity over current state-of-the-art graphite anodes. In systems featuring both C and Si anodes, electronic resistivity of the solid-electrolyte interphase (SEI) layer is a critical factor for preventing continuous electrolyte-decomposition reactions at the electrode/electrolyte interface. However, the in-situ measurement of SEI electronic resistance has been complicated by ion transport and electronic contributions from other parts of the battery circuit. Ex-situ measurements of SEI resistivity at microscopic scales are also lacking. We report on a nanometer-resolution three-dimensional technique that enables ex-situ mapping of electronic resistivity of SEI formed on a model single-crystalline wafer Si anode. Our novel experimental approach uses scanning spreading-resistance microscopy resistance imaging and mechanical depth profiling. In addition to resistance mapping, this method also provides an alternative technique for locating buried interfaces, where mechanical or electronic properties differ sufficiently between layers. Further validation of this method was obtained by resistance mapping of a reference sample with a designed a-Si:H layer stack of different doping concentrations. The results show relatively uniform lateral resistivity distribution of the SEIs but steep decreases in resistivity in the vertical direction. Resistivity vs. depth profiles are highly dependent on cycling conditions, but they generally show a resistivity decrease from the most superficial levels of SEI and a thickness increase with continued cycling prior to SEI stabilization. The most prominent resistivity increase was observed on SEI formed in Gen2 electrolyte (EC:EMC [3:7 by wt.] + 1.2 M LiPF6) with 10 wt% fluoroethylene carbonate additive; this result may partially explain the significant improvements of sustained electrochemical cycling and coulombic efficiency observed with this electrolyte additive. Our approach provides a novel and unparalleled three-dimensional approach in characterizing electronic resistivity, which contributes significantly to understanding SEI formation and the intrinsic properties critical to battery performance.

25 ENERGY STORAGE↗

Identification of Solid-Electrolyte Interphase Species by Joint Characterization of Li-Ion Battery Chemistry by Mass Spectrometry and Electrochemical Reaction Networks

The formation and stability of the solid-electrolyte interphase (SEI) play central roles in determining the long-term performance and safety of modern electrochemical energy storage systems. Despite decades of research, the SEI’s heterogeneous, dynamic, and multiphase nature has defied comprehensive molecular-level characterization, creating a critical knowledge gap that limits rational battery design. In this work, we introduce a computational−experimental framework that integrates high-throughput quantum chemistry calculations, data-driven electrochemical reaction networks (eCRNs), stochastic algorithms, and laser desorption/ionization Fourier transform ion cyclotron resonance mass spectrometry (LDI-FTICR-MS) to unravel SEI formation in carbonatebased electrolytes without imposing predefined mechanisms. We constructed the most comprehensive eCRN to date, spanning over 10,000 species and 209 million reactions. Through stochastic network analysis, we successfully recovered 27 species that were previously reported in the literature and predicted 28 novel SEI species nearly doubling our scientific knowledge in this area. Each new species was rigorously confirmed through advanced mass spectral analysis of its distinct molecular and isotopic signatures. We kinetically refined the formation pathways for a select set of both previously reported and novel SEI products, revealing kinetically feasible elementary reaction mechanisms with activation barriers below 1 eV. This computational−experimental approach deepens our molecular-level understanding of SEI chemistry by resolving which species form and through which decomposition mechanisms they emerge. Such knowledge provides the foundation necessary to connect electrolyte composition to the resulting SEI components, a critical step toward a more informed electrolyte development in next-generation lithium-based batteries.

25 ENERGY STORAGE↗

Artificial Solid Electrolyte Interphase to Address the Electrochemical Degradation of Silicon Electrodes

Electrochemical degradation on Si anodes prevents them from being successfully used in lithium-ion full cells. Unlike the case of graphite anodes, natural solid electrolyte interphase (SEI) films generated from carbonate electrolyte do not self-passivate on Si and causes continuous electrolyte decomposition. In this work we aim at solving the issue of electrochemical degradation by fabricating artificial SEI films using a solid electrolyte material, lithium phosphor oxynitride (Lipon), that conducts Li ions and blocks electrons. For Si anodes coated with Lipon of 50 nm or thicker, significant effect is observed in suppressing the electrolyte decomposition, while Lipon of thinner than 40 nm has little effect. Ionic and electronic conductivity measurement reveals that the artificial SEI is effective when it is a pure ionic conductor, and the electrolyte decomposition is not suppressed when the artificial SEI is a mixed electronic-ionic conductor. The critical thickness for this transition in conducting behavior is found to be 40~50 nm. This work provides guidance for designing artificial SEI for high capacity lithium-ion battery electrodes using solid electrolyte materials.

anodes↗

Lithium metal stripping beneath the solid electrolyte interphase

Lithium stripping is a crucial process coupled with lithium deposition during the cycling of Li metal batteries. Lithium deposition has been widely studied, whereas stripping as a subsurface process has rarely been investigated. Here we reveal the fundamental mechanism of stripping on lithium by visualizing the interface between stripped lithium and the solid electrolyte interphase (SEI). We observed nanovoids formed between lithium and the SEI layer after stripping, which are attributed to the accumulation of lithium metal vacancies. High-rate dissolution of lithium causes vigorous growth and subsequent aggregation of voids, followed by the collapse of the SEI layer, i.e., pitting. We systematically measured the lithium polarization behavior during stripping and find that the lithium cation diffusion through the SEI layer is the rate-determining step. Nonuniform sites on typical lithium surfaces, such as grain boundaries and slip lines, greatly accelerated the local dissolution of lithium. As a result, the deeper understanding of this buried interface stripping process provides beneficial clues for future lithium anode and electrolyte design.

25 ENERGY STORAGE↗

Predicting Calendar Aging in Lithium Metal Secondary Batteries: The Impacts of Solid Electrolyte Interphase Composition and Stability

Calendar aging of lithium metal batteries, in which cells’ components degrade internally due to chemical reactions while no current is being applied, is a relatively unstudied field. In this work, a model to predict calendar aging of lithium metal cells is developed using two sets of readily obtainable data: solid electrolyte interphase (SEI) layer composition (measured via X-ray photoelectron spectroscopy) and SEI stability (measured as a degradation rate using a simple constant current–constant voltage charging protocol). Electrolyte properties such as volume and salt concentration are varied in order to determine their effect on SEI stability and composition, with subsequent impacts to calendar aging. Lower salt concentrations produce a solvent-based, more soluble SEI, while the highest concentration produces a salt-based, less soluble SEI. Higher electrolyte volumes promote dissolution of the SEI and thus decrease its stability. The model predicts that lithium metal would be the limiting factor in calendar aging, depleting long before the electrolyte does. Furthermore, the relative composition of the electrolyte during aging is modeled and found to eventually converge to the same value independent of initial salt concentration.

25 ENERGY STORAGE↗

Boosting Superior Lithium Storage Performance of Alloy-Based Anode Materials via Ultraconformal Sb Coating–Derived Favorable Solid-Electrolyte Interphase

Alloy materials such as Si and Ge are attractive as high-capacity anodes for rechargeable batteries, but such anodes undergo severe capacity degradation during discharge-charge processes. Compared to the over-emphasized efforts on the electrode structure design to mitigate the volume changes, understanding and engineering of the solid-electrolyte interphase (SEI) are significantly lacking. This work demonstrates that modifying the surface of alloy-based anode materials by building an ultraconformal layer of Sb can significantly enhance their structural and interfacial stability during cycling. Combined experimental and theoretical studies consistently reveal that the ultraconformal Sb layer is dynamically converted to Li 3 Sb during cycling, which can selectively adsorb and catalytically decompose electrolyte additives to form a robust, thin, and dense LiF-dominated SEI, and simultaneously restrain the decomposition of electrolyte solvents. Hence, the Sb-coated porous Ge electrode delivers much higher initial Coulombic efficiency of 85% and higher reversible capacity of 1046 mAh g -1 after 200 cycles at 500 mA g -1 , compared to only 72% and 170 mAh g -1 for bare porous Ge. The present finding has indicated that tailoring surface structures of electrode materials is an appealing approach to construct a robust SEI and achieve long-term cycling stability for alloy-based anode materials.

25 ENERGY STORAGE↗

Microscopic Observation of Solid Electrolyte Interphase Bilayer Inversion on Silicon Oxide

Silicon has been investigated in recent years as an alloying anode material to enhance gravimetric energy density in lithium-ion batteries. Although recent developments have suggested that silicon oxides exhibit improved cycling stability over pure Si, the origin of the improved cycling performance is still poorly understood. The initial solid electrolyte interphase (SEI) formation mechanisms on Si wafers with both native oxide and chemically etched thermal oxide coatings are investigated structurally, chemically, and morphologically in the nanoscale. After one electrochemical cycle, microscopy reveals that SEI formed on native SiO x features the typical SEI bilayer structure with a carbon-rich outer SEI layer and an inorganic-rich inner SEI layer. In contrast, the SEI formed on chemically etched thermal oxide shows an inversion in the structure. This work observes distinct initial SEI formation mechanisms on the HF-etched SiO 2 surface, which may be partially responsible for improved cycle life observed in SiO x -based anode materials.

25 ENERGY STORAGE↗

Tuning Solid Electrolyte Interphase Formation before Plating Onset in Anode-Free Sodium Batteries

Sodium (Na) batteries are of growing interest due to the higher earth abundance of sodium than lithium, as well as their promising theoretical energy density when metallic Na anodes are used. However, Na plating and stripping are heavily influenced by the physicochemical properties of the solid electrolyte interphase (SEI), which is directly influenced by the solvent and salt used for the electrolyte. While most studies focus on the SEI that forms on the surface of Na metal after plating, we expand this analysis by identifying a nanoscale “pre-plating” SEI that forms on the current collector (CC) prior to the onset of Na plating. Here, we systematically investigate an array of Na salt and glyme solvents in the electrolyte and determine the associated impacts on pre-plating SEI formation on aluminum CCs. By combining analytical electrochemistry approaches with a multimodal suite of spectroscopy techniques (X-ray, infrared, and Raman), supported by density functional theory calculations, we reveal a direct correlation between the Na + coordination environment and pre-plating SEI composition. We find that longer-chain glymes produce larger proportions of organic alkoxide products in the interphase, consistent with increased Na + −glyme interactions, while the fraction of salt-derived inorganic products (e.g., NaF) correlates with Na + −anion coordination. These insights highlight the critical influence of electrolyte composition particularly solvent identity and Na + coordination on the initial SEI formation in anode-free Na batteries.

anode-free batteries↗

Concentration dependent properties and plastic deformation facilitate instability of the solid-electrolyte interphase in Li-ion batteries

Lithium-ion batteries (LIBs) often suffer from capacity fading and poor cyclic performance due to mechanical degradation of the solid-electrolyte interphase (SEI). Here we perform numerical simulations and theoretical analysis to elucidate the role of plasticity in wrinkling and ratcheting behaviors of an SEI/electrode system. A coupled diffusion and finite deformation framework is formulated and numerically implemented as a user-element subroutine (UEL) to describe transient lithium diffusion and accompanying elastic–viscoplastic deformation of the electrode. It is found that concentration dependent properties and plastic deformation facilitate wrinkling in such a system. A wrinkled morphology may further lead to ratcheting and related failure under cycling. A phase diagram of four types of cyclic behaviorsis identified in terms of the charging rate and time. Our analysis suggests several potential strategies to avoid wrinkling and ratcheting instabilities, such as charging/discharging the electrode at a sufficiently slow rate, and/or introducing a thick artificial SEI with a pre-tension.

25 ENERGY STORAGE↗

Direct determination of solid-electrolyte interphase thickness and composition as a function of state of charge on a silicon anode

Using neutron reflectometry we have determined the thickness and chemistry of the solid-electrolyte interphase (SEI) layer grown on a silicon anode as a function of state of charge and during cycling. We show the chemistry of this SEI layer becomes more LiF like with increasing lithiation and more Li-C-O-F like with delithiation. More importantly the SEI layer thickness appears to increase (about 250 ) as the electrode becomes less lithiated and thins to 180 with increasing Li content (Li 3.7 Si). We attribute this breathing to the continual consumption of electrolyte with cycling.

25 ENERGY STORAGE↗

Revealing the aging process of solid electrolyte interphase on SiOx anode

Abstract As one of the most promising alternatives to graphite negative electrodes, silicon oxide (SiO x ) has been hindered by its fast capacity fading. Solid electrolyte interphase (SEI) aging on silicon SiO x has been recognized as the most critical yet least understood facet. Herein, leveraging 3D focused ion beam-scanning electron microscopy (FIB-SEM) tomographic imaging, we reveal an exceptionally characteristic SEI microstructure with an incompact inner region and a dense outer region, which overturns the prevailing belief that SEIs are homogeneous structure and reveals the SEI evolution process. Through combining nanoprobe and electron energy loss spectroscopy (EELS), it is also discovered that the electronic conductivity of thick SEI relies on the percolation network within composed of conductive agents (e.g., carbon black particles), which are embedded into the SEI upon its growth. Therefore, the free growth of SEI will gradually attenuate this electron percolation network, thereby causing capacity decay of SiO x . Based on these findings, a proof-of-concept strategy is adopted to mechanically restrict the SEI growth via applying a confining layer on top of the electrode. Through shedding light on the fundamental understanding of SEI aging for SiO x anodes, this work could potentially inspire viable improving strategies in the future.

25 ENERGY STORAGE↗

Solid electrolyte interphase (SEI) application on anode of fluoride ion/shuttle batteries

The present disclosure is directed to fluoride (F) ion batteries and F shuttle batteries comprising an anode with a solid electrolyte interphase (SEI) layer, a cathode comprising a core shell structure, and a liquid fluoride battery electrolyte. According to some aspects, the components therein enable discharge and recharge at room-temperature.

Xu, Qingmin↗

An Inorganic‐Rich Solid Electrolyte Interphase for Advanced Lithium‐Metal Batteries in Carbonate Electrolytes

Abstract In carbonate electrolytes, the organic–inorganic solid electrolyte interphase (SEI) formed on the Li‐metal anode surface is strongly bonded to Li and experiences the same volume change as Li, thus it undergoes continuous cracking/reformation during plating/stripping cycles. Here, an inorganic‐rich SEI is designed on a Li‐metal surface to reduce its bonding energy with Li metal by dissolving 4 m concentrated LiNO 3 in dimethyl sulfoxide (DMSO) as an additive for a fluoroethylene‐carbonate (FEC)‐based electrolyte. Due to the aggregate structure of NO 3 − ions and their participation in the primary Li + solvation sheath, abundant Li 2 O, Li 3 N, and LiN x O y grains are formed in the resulting SEI, in addition to the uniform LiF distribution from the reduction of PF 6 − ions. The weak bonding of the SEI (high interface energy) to Li can effectively promote Li diffusion along the SEI/Li interface and prevent Li dendrite penetration into the SEI. As a result, our designed carbonate electrolyte enables a Li anode to achieve a high Li plating/stripping Coulombic efficiency of 99.55 % (1 mA cm −2 , 1.0 mAh cm −2 ) and the electrolyte also enables a Li||LiNi 0.8 Co 0.1 Mn 0.1 O 2 (NMC811) full cell (2.5 mAh cm −2 ) to retain 75 % of its initial capacity after 200 cycles with an outstanding CE of 99.83 %.

Liu, Sufu↗

The Role of Oxygen in Lithiation and Solid Electrolyte Interphase Formation Processes in Silicon-Based Anodes

Silicon oxides (SiO x ) have been considered as promising alternatives to pure Si in high energy anodes in lithium-ion batteries (LIBs) due to their improved cycling stability. However, their fundamental lithiation mechanism has not yet been systematically investigated, and potential collateral downsides remain unclear. In this work, we report on the role of oxygen in lithiation/delithiation and solid electrolyte interphase (SEI) formation processes in SiO x thin film model electrodes with different oxygen contents. Here, we show that the SiO x anodes with higher oxygen content experience smaller volume change and form a thinner and more stable SEI, both of which are beneficial for cycling stability. However, these SiO x anodes also show an irreversible lithiation at around 0.7 V attributed to the reduction of Si oxides, leading to lower first cycle coulombic efficiency that is undesirable for practical applications. Overall, these results offer a balanced perspective on the advantages and disadvantages that oxygen brings to Si-based anodes in LIBs.

25 ENERGY STORAGE↗