Search NASA⌕ Search

SEARCH · Search NASA

Results for “WELDING, ARC”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 127 records · Page 7

Welding investigation of a wrought FeMnAl steel for armor application

A new wrought FeMnAl steel contains high Mn content and high Al content. This steel has high strength. When it is compared to conventional steels with the similar strength, its density is lower. FeMnAl steels can be used in armor vehicle manufacturing, in which welding is a common practice to join the steel plates together. The welding of FeMnAl steels has not been sufficiently studied before. Here, this work studied the weldability and weld microstructure of an FeMnAl steel and provided useful data for the welding practice of FeMnAl steels. The influences of weld filler metals and shielding gases were studied, using single-pass bead-on-plate gas metal arc welding (GMAW) and gas tungsten arc welding (GTAW) two processes. The optimal filler metals and shielding gases have been determined to achieve the better weldability. Autogenous GTAW and electron beam welding were also conducted. Cracks were found in the HAZ in the GMAW welds and electron beam welds. Fewer or no cracks were found in the HAZ of GTAW welds. SEM, SEM/EDX, TEM, TEM/EDX, and EBSD were used to analyze the grain boundaries in the HAZ and the cracks. The grain boundaries of FeMnAl base metal are mostly high angle grain boundaries (HAGBs), which attract impurity and solute atoms and cause intergranular cracking. The proposed cracking mechanisms are liquation cracking and ductility-dip cracking. It was found that GTAW provides much better weldability for the FeMnAl steel than GMAW and EBW.

FeMnAl steel↗

Controlling Arc Length in Plasma Welding

Circuit maintains arc length on irregularly shaped workpieces. Length of plasma arc continuously adjusted by control circuit to maintain commanded value. After pilot arc is established, contactor closed and transfers arc to workpiece. Control circuit then half-wave rectifies ac arc voltage to produce dc control signal proportional to arc length. Circuit added to plasma arc welding machines with few wiring changes. Welds made with circuit cleaner and require less rework than welds made without it. Beads smooth and free of inclusions.

Iceland, W. F.↗

Ocular hazards of light

The eye is protected against bright light by the natural aversion response to viewing bright light sources. The aversion response normally protects the eye against injury from viewing bright light sources such as the sun, arc lamps and welding arcs, since this aversion limits the duration of exposure to a fraction of a second (about 0.25 s). The principal retinal hazard resulting from viewing bright light sources is photoretinitis, e.g., solar retinitis with an accompanying scotoma which results from staring at the sun. Solar retinitis was once referred to as 'eclipse blindness' and associated 'retinal burn'. Only in recent years has it become clear that photoretinitis results from a photochemical injury mechanism following exposure of the retina to shorter wavelengths in the visible spectrum, i.e., violet and blue light. Prior to conclusive animal experiments at that time, it was thought to be a thermal injury mechanism. However, it has been shown conclusively that an intense exposure to short-wavelength light (hereafter referred to as 'blue light') can cause retinal injury. The product of the dose-rate and the exposure duration always must result in the same exposure dose (in joules-per-square centimeter at the retina) to produce a threshold injury. Blue-light retinal injury (photoretinitis) can result from viewing either an extremely bright light for a short time, or a less bright light for longer exposure periods. This characteristic of photochemical injury mechanisms is termed reciprocity and helps to distinguish these effects from thermal burns, where heat conduction requires a very intense exposure within seconds to cause a retinal coagulation otherwise, surrounding tissue conducts the heat away from the retinal image. Injury thresholds for acute injury in experimental animals for both corneal and retinal effects have been corroborated for the human eye from accident data. Occupational safety limits for exposure to UVR and bright light are based upon this knowledge. As with any photochemical injury mechanism must consider the action spectrum, which describes the relative effectiveness of different wavelengths in causing a photobiological effect. The action spectrum for photochemical retinal injury peaks at approximately 440 nm.

Sliney, David H.↗

Gas Shielding Technology for Welding and Brazing

Welding is a common method that allows two metallic materials to be joined together with high structural integrity. When joints need to be leak-tight, light-weight, or free of contaminant-trapping seams or surface asperities, welding tends to be specified. There are many welding techniques, each with its own advantages and disadvantages. Some of these techniques include Forge Welding, Gas Tungsten Arc Welding, Friction Stir Welding, and Laser Beam Welding to name a few. Whichever technique is used, the objective is a structural joint that meets the requirements of a particular component or assembly. A key practice in producing quality welds is the use of shielding gas. This article discusses various weld techniques, quality of the welds, and importance of shielding gas in each of those techniques. Metallic bonds, or joints, are produced when metals are put into intimate contact. In the solid-state "blacksmith welding" process, now called Forge Welding (FOW), the site to be joined is pounded into intimate contact. The surfaces to be joined usually need to be heated to make it easier to deform the metal. The surfaces are sprinkled with a flux to melt surface oxides and given a concave shape so that surface contamination can be squeezed out of the joint as the surfaces are pounded together; otherwise the surface contamination would be trapped in the joint and would weaken the weld. In solid-state welding processes surface oxides or other contamination are typically squeezed out of the joint in "flash."

Nunes, Arthur J.↗

Manufacturing High-Quality Carbon Nanotubes at Lower Cost

A modified electric-arc welding process has been developed for manufacturing high-quality batches of carbon nanotubes at relatively low cost. Unlike in some other processes for making carbon nanotubes, metal catalysts are not used and, consequently, it is not necessary to perform extensive cleaning and purification. Also, unlike some other processes, this process is carried out at atmospheric pressure under a hood instead of in a closed, pressurized chamber; as a result, the present process can be implemented more easily. Although the present welding-based process includes an electric arc, it differs from a prior electric-arc nanotube-production process. The welding equipment used in this process includes an AC/DC welding power source with an integral helium-gas delivery system and circulating water for cooling an assembly that holds one of the welding electrodes (in this case, the anode). The cathode is a hollow carbon (optionally, graphite) rod having an outside diameter of 2 in. (approximately equal to 5.1 cm) and an inside diameter of 5/8 in. (approximately equal to 1.6 cm). The cathode is partly immersed in a water bath, such that it protrudes about 2 in. (about 5.1 cm) above the surface of the water. The bottom end of the cathode is held underwater by a clamp, to which is connected the grounding cable of the welding power source. The anode is a carbon rod 1/8 in. (approximately equal to 0.3 cm) in diameter. The assembly that holds the anode includes a thumbknob- driven mechanism for controlling the height of the anode. A small hood is placed over the anode to direct a flow of helium downward from the anode to the cathode during the welding process. A bell-shaped exhaust hood collects the helium and other gases from the process. During the process, as the anode is consumed, the height of the anode is adjusted to maintain an anode-to-cathode gap of 1 mm. The arc-welding process is continued until the upper end of the anode has been lowered to a specified height above the surface of the water bath. The process causes carbon nanotubes to form in the lowest 2.5 cm of the anode. It also causes a deposit reminiscent of a sandcastle to form on the cathode. The nanotube-containing material is harvested. The cathode and anode can then be cleaned (or the anode is replaced, if necessary) and the process repeated to produce more nanotubes. Tests have shown that the process results in approximately equal to 50-percent yield of carbon nanotubes (mostly of the single-wall type) of various sizes. Whereas the unit cost of purified single-wall carbon nanotubes produced by other process is about $1,000/g in the year 2000, it has been estimated that for the present process, the corresponding cost would be about $10/g.

Benavides, Jeanette M.↗

Electron Beam Welding of Pure Tungsten Hex Cans for Nuclear Thermal Propulsion Engines

Nuclear thermal propulsion (NTP) is an in-space propulsion method currently being developed at the NASA Marshall Space Flight Center (MSFC). NTP systems are a high specific impulse (750–1,100 s), high thrust (15,000–250,000 lbf ) method of propulsion which have the potential to allow for faster transit times when optimizing for high ΔV. In the nuclear rocket engine, the heat from the nuclear fission reaction is transferred to a low molecular mass propellant (such as hydrogen). Hot propellant is expanded through a nozzle to generate thrust. Development of ceramic metal (cermet) fuel systems for NTP applications is currently ongoing at MSFC. In cermet fuel systems, ceramic fissile fuel particles such as uranium nitride or uranium dioxide are dispersed within a net-shaped, high-density structural matrix. The composite material is cladded by a protective metal structure to make up an NTP fuel element. Cladding materials must be able to withstand the demanding operating conditions required of the engine as well as retain a hermetic seal to allow for retention of fuel element structural integrity, prevent hydrogen attack or migration of the ceramic fuel, and limit release of fission products during operation. For NTP applications, tungsten is a prime material for both the metal matrix and cladding in cermet fuel systems because of its high melting point, high temperature strength, and compatibility with hot hydrogen. If a weld in tungsten with the capability of holding a hermetic seal is achievable, tungsten becomes a strong candidate for NTP applications. This Technical Memorandum focuses on determining the weldability of pure tungsten using electron beam welding (EBW). Tungsten appears well suited for NTP applications, but it has a high ductile to brittle transition temperature (DBTT) dependent upon chemical composition, structure/stress distribution, and mechanical conditions. Therefore, it is highly subject to brittle fracture. Because of its high susceptibility to brittle fracture, it is very difficult to weld. EBW was chosen for joining pure tungsten because of its low heat input compared to gas tungsten arc welding. Reduced heat input can be directly correlated with an increase in ductility of a tungsten weld. EBW is a high energy density welding process in which a stream of electrons penetrates a weld joint in a deep, narrow spike in contrast to a broad gas tungsten arc weld pool. The investigation initially focused on EBW of tungsten plates of both 0.01 in and 0.03 in thickness to determine if EBW could weld pure tungsten without the presence of visual defects—particularly cracking—in the welds. Variation in the weld procedure and post-weld heat treatment (PWHT) was used to improve the surface appearance of flat EBWs on a pure tungsten sheet. The investigation moved on to weld 0.05-in-thick hexagonal tungsten cans with a weld joint thickness of 0.025 in. The goal for welding the pure tungsten hex cans was to avoid any visual surface defects and generate a weld capable of a hermetic seal. This proved difficult. Cold welds commonly exhibited porosity that leaked air. Hot welds exhibited cracks, typically observed immediately after welding. Later welds were preheated to increase ductility and decrease the likelihood of through-thickness cracking. PWHT was used to arrest microcrack growth both in the flat weld samples and hexagonal weld samples.

Courtright, Z. S.↗

Opposed arcs permit deep weld penetration with only one pass

Arc welding technique uses opposed electrodes on either side of the workpiece, operated in right angles, out-of-phase, pulsating direct current. complete penetration has been obtained with this technique in metals ranging from 0.062 to 1.0 inch thickness.

Budds, L. E.↗

Plasma-Arc Torch For Welding Ducts In Place

Plasma-arc-welding torch redesigned, more suitable for applications in which moved in circular or other orbits about stationary cylindrical workpieces. Preserves elements of original design critical to performance and endurance, but modifies other elements to decrease overall size of torch. Electrode collet and collet nut installed and removed through hole in top; makes installation and removal easier.

Gangl, Kenneth J.↗

Pulsed-Current Welding Of Nickel-Based Alloy

Joints as strong (or stronger than) joints made with constant current. Report based on study of pulsed-current versus constant-current gas/tungsten arc welding of butt joints between panels of nickel-based alloy 718. In pulsed-current welding, arc current alternated between high and low value. Enables greater control of freezing and depth of penetration of weld puddle at given heat input. Thicker sections joined. Readily incorporated into automated welding system, with resultant greater uniformity and reproducibility of welds than attained in manual welding.

Gamwell, W. R.↗

Vacuum Deposition From A Welding Torch

Process derived from arc welding produces films of high quality. Modified gas/tungsten-arc welding process developed for use in outer space. Welding apparatus in process includes hollow tungsten electrode through which inert gas flows so arc struck between electrode and workpiece in vacuum of space. Offers advantages of fast deposition, possibility of applying directional impetus to flow of materials, very low pressure at surface being coated, and inert environment.

Poorman, R. M.↗

Time-Dependent 600 °C Post-Weld Heat Treatment Response of Laser-Wire-Directed Energy Deposited Austenitic Stainless Steel Claddings on Carbon Steel

Austenitic stainless steel overlay claddings are often used to protect nuclear reactor pressure vessels from corrosion. Arc welding processes are traditionally employed, which require a high heat input to bond the dissimilar metals, creating a large heat-affected zone and high residual stress that demands a lengthy stress-relieving post-weld heat treatment, up to 48 hours. High energy beam (e.g., laser, electron beam) directed energy deposition-based overlay cladding processes show promise for fabricating claddings with superior performance compared to arc welded ones because of their localized heat input; however, their necessity and time of post-weld heat treatment are currently unclear. In this research, we investigate the time dependence of a 600 C stress-relieving post-weld heat treatment of austenitic stainless steel clad on low carbon steel by laser-wire-directed energy deposition, comparing the microstructure and mechanical properties of the as-fabricated condition to 2-, 10-, and 48-hour heat treatment times. Diffusion simulations and microscopy show a gradual carburization of the stainless steel cladding and decarburization of the heat-affected zone/base metal. Nanoindentation testing shows up to a 1.8–2.69 embrittlement in the cladding and a 0.33 to 0.69 softening in the heat-affected zone after the 48-hour post-weld heat treatment. Tensile testing of the cladding composites reveals that increasing post-weld heat treatment time raises clad cracking susceptibility due to intergranular carbide formation and shows that laser-wire-directed energy deposition claddings may not require post-weld heat treatment.

Coating↗

Process-Information Display Panel For Welder's Visor

Head-up display (HUD) unit mounted in welder's visor or helmet provides process information in real time. Display enables welder to gain greater awareness of effects of welding while controlling welding process in usual way(s) by use of foot pedal, voice command, and/or manipulation of welding torch. Possible to avoid need for every new welder on job to solve same problems solved by other welders. Graphical display presented to welder, adjacent to normal field of view through visor. Beneficial in supporting and enhancing continued practice of manual arc welding. Valuable in industries that invest millions of technician-hours each year in manual arc welding for variety of products.

Russell, Carolyn↗

Rolling Behavior of Surface Tagged Aluminum 6061 using Photoluminescent Oxides

Physical tagging of nuclear fuel is potentially one way of tracking throughout the fuel lifecycle. The process of tagging can take many forms, but one promising method is to embed a small amount of photoluminescent particles in the surface of a material which are not detectable under normal illumination but are readily visible under excitation by ultraviolet light. The goal of this project was to explore the potential to tag simulated nuclear fuel cladding with small ceramic particles, via laser beam welding or gas tungsten arc welding, and measure the photoluminescent response. Surface tagging using this method has demonstrated viability and detectability throughout this project; work in FY24 focused on the survivability of these tags through subsequent deformation processing similar to what taggants in a fuel manufacturing environment would be subjected to. This work demonstrated that particles are readily visible in the as-welded state (i.e., before subsequent rolling treatment to represent mechanical processing of a fuel material), but visibility is reduced as the deformation is induced. Despite the reduction in photoluminescence, the taggants are still visible after rolling processes are performed, making this surface tagging technique a promising candidate for nuclear fuel cladding tagging. This work demonstrated, though, that targeted optimization work would be necessary to develop a robust taggant depending on the fidelity and luminescent properties required.

36 MATERIALS SCIENCE↗

Gas Metal Arc /GMA/ weld torch proximity control

Adjustable transducer probe, which is attached to a welding torch and maintains a preset touch-to-work distance, accurately follows irregular surfaces, is less sensitive to heat and static interference, and has more positive response because of electro-mechanical control.

Hawkes, E. D.↗

State-of-technology for joining TD-NiCr sheet

At the current state-of-technology there are many joining processes that can be used to make sound welds in TD-NiCr sheet. Some of these that are described in this report are electron beam welding, gas-tungsten arc welding, diffusion welding, resistance spot welding, resistance seam welding, and brazing. The strengths of the welds made by the various processes show considerable variation, especially at elevated temperatures. Most of the fusion welding processes tend to give weak welds at elevated temperatures (with the exception of fusion-type resistance spotwelds). However, solid-state welds have been made with parent metal properties. The process used for a specific application will be dictated by the specific joint requirements. In highly stressed joints at elevated temperatures, one of the solid-state processes, such as DFW, RSW (solid-state or fusion), and RSEW, offer the most promise.

Holko, K. H.↗