Search NASA⌕ Search

SEARCH · Search NASA

Results for “WELDING, GAS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 127 records · Page 7

Characterization of microstructure and texture across dissimilar super duplex/austenitic stainless steel weldment joint by austenitic filler metal

The evolution of microstructure and texture across an as-welded dissimilar UNS S32750 super duplex/UNS S30403 austenitic stainless steel joint welded by UNS S30986 (AWS A5.9 ER309LMo) austenitic stainless steel filler metal using gas tungsten arc welding process was evaluated by optical micrography and EBSD techniques. Due to their fabrication through rolling process, both parent metals had texture components resulted from deformation and recrystallization. The weld metal showed the highest amount of residual strain and had large austenite grain colonies of similar orientations with little amounts of skeletal ferrite, both oriented preferentially in the < 001 > direction with cub-on-cube orientation relationship. While the super duplex stainless steel's heat affected zone contained higher ferrite than its parent metal, an excessive grain growth was observed at the austenitic stainless steel's counterpart. At both heat affected zones, austenite underwent some recrystallization and formed twin boundaries which led to an increase in the fraction of high angle boundaries as compared with the respective base metals. These regions showed the least amount of residual strain and highest amount of recrystallized austenite grains. Due to the static recrystallization, the fraction of low degree of fit (Σ) coincident site lattice boundaries, especially Σ3 boundaries, was increased in the austenitic stainless steel heat affected zone, while the formation of subgrains in the ferrite phase increased the content of < 5° low angle boundaries at that of the super duplex stainless steel. - Graphical abstract: Display Omitted - Highlights: • Extensive grain growth in the HAZ of austenitic stainless steel was observed. • Intensification of < 100 > orientated grains was observed adjacent to both fusion lines. • Annealing twins with Σ3 CSL boundaries were formed in the austenite of both HAZ. • Cub-on-cube OR was observed between austenite and ferrite in the weld metal. • Weld metal had the lowest texture intensity and ratio of low angle and CSL boundaries.

36 MATERIALS SCIENCE↗

Multi-Pass Hybrid Laser Arc Welding of Alloy 740H

The presentation reviews the progress made toward reducing the joining time of an advanced nickel-based alloy, Alloy 740H by a factor of two using a novel two step fusion welding approach. In the first step, a high powered laser is used to rapidly join thick weld groove lands (~10-12 mm thick) during a single pass. Hybrid laser arc welding (HLAW) is then used to fill the remaining weld groove and complete the joint. This sequential process also utilizes laser wobble in both steps to reduce welding defects and refine the weld microstructure to obtain improved properties compared to conventional gas tungsten or gas metal arc welds, GTAW and GMAW, respectively. The creep behavior of laser-only thick weld groove land welds and HLAW welds were found to be the same or slightly improved compared to conventional GMAW or GTAW welds in this alloy. Creep tests have been started to verify the long-term creep behavior (~10,000 hrs) of these welds. Modeling results on deep penetration laser welding are presented and the initial simulations of laser welding with laser wobble are shown. The next phase of the project will combine the two processes to make complete welds - deep penetration laser welds of thick weld groove lands followed by rapid filling of the remaining weld groove by HLAW - in thick plates (32 mm thick) Alloy 740H plate and entails development of narrow weld groove welding to further decrease the joining time of this alloy.

36 MATERIALS SCIENCE↗

Microstructure of a safe-end dissimilar metal weld joint (SA508-52-316L) prepared by narrow-gap GTAW

The microstructure, residual strain and interfacial chemical composition distribution of a safe-end dissimilar metal weld joint (DMWJ, SA508-52-316L) prepared by narrow-gap gas-tungsten arc welding (NG-GTAW) were studied by optical microscope (OM) and scanning electron microscope equipped with an energy dispersive X-ray microanalysis (SEM/EDX) and an electron back scattering diffraction (EBSD) system. Complex microstructure and chemical composition distribution are found, especially at the SA508-52 interface and the 52-316L interface. In brief, a complicated microstructure transition exists within the SA508 heat affected zone (HAZ); the residual strain, the fraction of high angle random grain boundaries and low angle boundaries decrease with increasing the distance from the fusion boundary in 316L HAZ; neither typical type II boundary nor obvious carbon-depleted zone is found near the SA508-52 interface; dramatic and complicated changes of the contents of the main elements, Fe, Cr and Ni, are observed at the distinct interfaces, especially at the SA508-52 interface. No carbon concentration is found at the SA508-52 interface. - Highlights: •Residual strain and GBCD change as a function of the distance from FB in 316L HAZ. •Neither type II boundary nor obvious carbon-depleted zone is found in SA508 HAZ. •No carbon concentration is found at the SA508-52 interface. •The middle part of the DMWJ has the highest residual strain.

36 MATERIALS SCIENCE↗

Welding Heat Input Influence on UNS S82441 Lean Duplex Stainless Steel Corrosion Resistance Assessed by Scanning Vibrating Electrode Technique (SVET)

The precipitation of the intermetallic phases can impair mechanical and corrosion properties. In the case of lean duplex stainless steels, they present solidification mode as primary ferrite, with austenite precipitation in the solid state, during cooling. This means the heat-affected zone balanced microstructure can be changed during the welding by the cooling rate, which is associated to the welding heat input, the thickness of the plate and the physical properties of the material. This work intends to present the influence of welding heat input on the corrosion resistance of UNS S82441 lean duplex stainless steel. The gas metal arc welding process was used to make the weld beads, using ER2209 as filler metal, which characterizes a dissimilar welded joint. The corrosion resistance of these specimens was analyzed through scanning vibrating electrode technique. It was observed that welding heat input variation distinctly influences corrosion in different zones of the weld beads over the specimen exposure time. The weld bead under intermediate welding heat input showed the highest corrosion rate and the one under the highest welding heat input, the lowest corrosion rate intensity.

36 MATERIALS SCIENCE↗

Microstructure-Property Correlations in Fiber Laser Welded Nb-Ti Microalloyed C-Mn Steel

Mechanical Performance of traditional gas-shielded arc welded joints of 700 MPa grade microalloyed C-Mn steel cannot meet service requirements. Laser welding, with its characteristic high energy density, is known to improve the welding performance of experimental steels. In the present study, Nb-Ti microalloyed steel with a thickness of 4.5 mm was welded using a 4 kW fiber laser. The microstructure, precipitation, and mechanical properties of the welded joints were studied. The hardness and tensile strength of the welded joints were higher than those of the base metal (BM). The microstructure of the fusion zone (FZ) and coarse grain heat affected zone (CGHAZ) was lath martensite (LM), while the microstructure of the fine grain HAZ and mixed grain HAZ consisted of ferrite and martensite/austenite islands. Although LM was observed in both the FZ and CGHAZ, the hardness and calculated tensile strength of the FZ were lower than those of the CGHAZ, due to a reduction in solid solution strengthening by element loss and the dissolution of high-hardness precipitates in FZ. Most precipitates such as [(Nb,Ti)C and (Nb,Ti)(C,N)] that were present in the BM were dissolved, which led to an increase in C and N in solid solution in the FZ. Thus, the elastic modulus of the FZ was higher than that of the BM. Similarly, the elastic modulus of the CGHAZ was higher than that of the BM due to the segregation of C and N atoms during the welding process. The toughness of the FZ was superior to that of the BM, and the toughness of the HAZ approached 91% of that of the BM. The change in toughness primarily depended on the microstructural refinement, the increase in the fraction of grains with high misorientation, the residual austenite in the FZ and CGHAZ, and the dissolution of coarse precipitates.

36 MATERIALS SCIENCE↗

Evolution of carbide precipitates in Hastelloy N joints during welding and post weld heat treatment

Highlights: • The formation and spheroidization of the eutectic-like carbides are found in the Hastelloy N alloy during welding and PWHT. • All precipitates in the joints before and after the PWHT are identified as a M{sub 6}C type carbide with different morphology. • The diffusion of main element of Mo leads to the decrease of lattice parameter of the carbide during the welding and PWHT. - Abstract: The effects of welding and post weld heat treatment (PWHT) on the morphology, composition and lattice parameter of the precipitates in the welding joints of Hastelloy N alloy have been investigated. Joint samples were prepared using a gas tungsten arc welding process with ERNiMo-2 fillers, and then solid-solution treated at 1100 °C for 20 min. After welding, eutectic M{sub 6}C carbides can be observed in the heat affected zones (HAZ) and weld zones (WZ). These eutectic M{sub 6}C carbides become spheroidized during the following PWHT. The concentration of Si decreases during the transformation from the primary ones to eutectic ones, and then increases during the spheroidizing process. The total concentration of Si + Cr in M{sub 6}C carbides remains stable during welding and PWHT. At the same time, the heat leads to the outward diffusion of Mo from the M{sub 6}C carbides, which results in a decrease of the lattice parameter.

36 MATERIALS SCIENCE↗

Comparative study of microstructure and properties of low-alloy-steel/nickel-based-alloy interfaces in dissimilar metal weld joints prepared by different GTAW methods

Highlights: • Number of type I and type II boundaries: H-DMWJ > C-DMWJ > W-DMWJ. • Width carbon depleted zones and carbon enriched zones: H-DMWJ > C-DMWJ > W-DMWJ. • Type I and type II boundaries are susceptible to SCC and cracked during mechanical bending. • C-DMWJ has the best performance while H-DMWJ has the worst one. - Abstract: Low-alloy-steel/buttering (or welding) metal interfaces in safe-end dissimilar metal weld joints (DMWJs) at nuclear power plants are weak parts. To optimize the quality of the safe-end DMWJs used for the construction of domestic nuclear power plants and to improve the welding productivity, a series of DMWJs in full-size have been manufactured by using different gas tungsten arc welding (GTAW) methods. The microstructure, chemical composition distribution and local properties across the SA508/52(M) interfaces in these DMWJs are studied. The high heat input and long high temperature duration during hot-wire GTAW process promote the carbon diffusion and grain boundary migration and hence the DMWJ by hot-wire GTAW has the largest amount of type I and type II boundaries and the widest carbon depleted zones and carbon enriched zones, which resulting in the worst performance among the DMWJs in simulated primary water. Type I and type II boundaries are high angle random grain boundaries (RGBs) and Cr-depleted zones are found along type II boundaries resulting in their high susceptibility to SCC. In addition, these boundaries are prone to be cracked during mechanical bending process.

36 MATERIALS SCIENCE↗

High-Speed and High-Quality Field Welding Repair Based on Advanced Non-Destructive Evaluation and Numerical Modeling

Creep strength-enhanced ferritic (CSEF) steels such as Grade 91 (9Cr-1Mo-V) and Grade 92 (Fe-9Cr-2W-0.5Mo) steels are widely used in the fossil-fuel-fired and nuclear power plants. The weld integrity of these steels is crucial for power plants' safe and reliable operations. Due to harsh service conditions, the steel weld can become susceptible to environmental degradation. Field welding repair is used to restore the degraded weld’s performance where a controlled temper-bead welding technique is commonly used to temper the freshly formed martensite during welding. However, knowledge of weld repairability is limited and experimental trial and error optimization to achieve desired microstructure and joint properties is expensive and time-consuming. Many existing computational models, e.g., finite element models, are limited to solving heat conduction equation and ignoring convective heat transfer due to molten metal flow. These models can result in over-prediction of peak temperatures of weld pool and heat-affected zone (HAZ), which in turn can affect the accuracy of tempering prediction. Moreover, these finite element models require an input of the deposit profiles in advance and thus limits the usability of these models. Here, a molten pool-based, multi-pass multi-layer model has been developed based on computational fluid dynamics (CFD) approach with the Volume of Fluid (VOF) method. The model calculates the bead formation, thereby eliminating the need for pre-determined bead profiles required by finite element models. For computational efficiency, a coordinate system attached to the moving heat source is utilized. A subroutine is developed to convert the temperature profiles in the reference frame stationary to the heat source to that stationary to the workpiece. The converted thermal cycles are then imported into a microstructure model to compute the tempering kinetics and resultant hardness using a Johnson-Mehl-Avrami-Kolmogorov (JMAK), and modified Grange-Baughman parameter. The modeling approach is first developed and validated on single- and multi-pass deposition of stainless steel filler metal onto a SA-533 high strength steel substrate. The models are then applied to a multi-pass V-groove repair weld of Grade 91 steel plate as well as directed energy deposition of Grade 92 steel. Non-destructive characterization of microstructures was performed on Grade 91 and 92 steel welds. Two welding processes, cold metal transfer (CMT) and flux-cored arc welding (FCAW), were investigated for the Grade 91 steel weld samples. For the Grade 92 weld samples, three different heat inputs (low, medium, and high) of gas tungsten arc welding (GTAW) were utilized to replicate traditional field welding processes. The non-destructive evaluation (NDE) method used for this research was immersion ultrasonic testing (UT) using a micro-resolution ultrasonic imaging methodology specifically designed to operate in the through-transmission configuration operating at 20 MHz of frequency. The system used a focused ultrasonic beam spot size diameter between 250-300 μm, and a 6 μm laser vibrometer spot size for detection, to produce highly defined images with longitudinal and mode-converted shear waves. From the micro-resolution ultrasonic C-scan images, three microstructural regions, i.e., weld metal (WM), HAZ, and base metal (BM), were clearly identifiable. Various levels of ultrasonic amplitudes distributed over the three regions were correlated with electron beam backscattered diffraction (EBSD) images using grain size, grain boundaries, and dislocation densities. The results showed that areas with relatively higher ultrasonic amplitude levels were associated with smaller grains and higher dislocation densities, while areas with lower amplitude levels were associated with larger grains and lower dislocation densities. In addition, ultrasonic velocity data obtained across the three different weld microstructural regions of Grade 91 test samples were correlated with optical metallographic images and hardness measurements. The results showed distinctive decreases in ultrasonic velocity and hardness over the HAZ region, where weld failures often occur during service.

36 MATERIALS SCIENCE↗

Monitoring Weld Pool Surface and Penetration Using Reversed Electrode Images

The three­-dimensional weld pool top surface shape provides important informa­tion about the state of weld penetration during welding. In this study, a method was developed to quantitatively relate weld pool surface height to the reversed electrode image (REI) on the weld pool surface. This new feature was extracted from the weld pool image using a passive vision-­based monitoring system during gas tungsten arc welding (GTAW). Due to the specular reflection of the weld pool top surface, the REI is visible on the weld pool surface during GTAW. The position of the REI was determined with a robust image processing algorithm. Based on the principle of light reflection, the distance between the electrode tip and the REI (DERI) was related to the weld pool surface height. By assuming the weld pool surface was a spherical mirror, a reflection model was established to calculate the surface height (SH) index based on the measurement of the DERI, arc length, and weld pool geometry. The pro­posed method was verified with bead­-on­plate welding experiments. The SH was positively related to the face reinforcement or depression of the weld bead. This method was applied to monitor the penetration state during bead­on­plate autoge­nous welding, particularly when a complete penetration weld was formed.

42 ENGINEERING↗

Modeling of Keyhole-Induced Pore Formation in Laser-Arc Hybrid Welding of Aluminum Alloy with a Horizontal Fillet Joint

A three-dimensional transient model is proposed to investigate the weld pool dynamic behavior in laser + metal inert gas (MIG) hybrid fillet welding of aluminum alloy in the horizontal position, which allows for the joint configuration and coupling of the keyhole, droplet and weld pool as well as the heat and mass exchange between gas and liquid phases and is able to simulate the temperature distribution, fluid flow and formation process of a keyhole-induced pore in hybrid welding with a horizontal fillet joint. The weld porosity is also measured using x-ray nondestructive testing technology. Keyhole behavior and the formation mechanism of keyhole-induced porosity were analyzed. The calculated results are in generally good agreement with the experimental ones. A clockwise vortex always exists at the middle part of the weld pool. The formation and growth of the molten metal bulge on the keyhole wall are responsible for the occurrence of a gas bubble, which has a variation in size and shape and can be split during welding. The keyhole collapses easily at its middle or upper part in horizontal fillet welding, and the capture of the bubble by the upper molten pool boundary enhances the possibility of porosity formation to some degree. The keyhole-induced pore is mainly formed at the regions near the keyhole bottom and the upper fusion line of the weld pool.

36 MATERIALS SCIENCE↗

Assessment of Mechanical Properties for Dissimilar Metal Welds: A Nondestructive Approach

Several engineering components are fabricated by joining similar or dissimilar materials. In the present investigation, welded joints between low alloy steel and austenitic stainless steel were considered. This assembly is one of the critical components in the heat transport system of water-cooled reactors of nuclear power plants. 309L austenitic stainless steel and IN 182 alloys were used for buttering low alloy steel during fabrication of joints. Weld metal was 308L austenitic stainless steel and IN 182, respectively, for the two assemblies. Buttering by 309L SS was performed by gas tungsten arc welding, and the same was done by shield metal arc welding at the time of applying IN 182. Joining of 304L SS and buttered assembly in both the cases was carried out by shield metal arc welding. Evaluation of Vickers micro-hardness was done across the weld centerline for both joints. Microstructure of different regions was examined for the joints. Apart from conventional destructive tests, ultrasonic evaluation of joints was also carried out to ensure weld integrity. In this respect, ultrasonic velocity in longitudinal and shear mode was measured along the transverse direction of the weld. Young’s modulus was determined using ultrasonic tests as well as from the average hardness of different regions. The obtained Young’s modulus by two different techniques revealed satisfactory co-relation. The Young’s modulus obtained from ultrasonic measurements was used to determine the yield strength of different regions across the welds. This technique proved to be useful in identifying the failure prone area across the welded joint.

36 MATERIALS SCIENCE↗

Welded and Hydrogen Charged Zircaloy-4 and Welded Stainless Steel 347 Property Data and Microstructures for the Target Solution Vessel and Support Lines of SHINE

SHINE Medical Technologies is developing a facility that will produce molybdenum-99 for medical isotope procedures. As part of this facility, a metal tank, called the target solution vessel (TSV), will hold a uranyl sulfite solution. The TSV must withstand neutron irradiation near room temperature and potential corrosion from the aqueous solution. The large cylindrical TSV will be fabricated by welding and will have numerous pipes and connections also attached via welding. The vessel and those pipes will have varying thicknesses so both gas tungsten arc welding (GTAW) and flux-cored arc welding (FCAW) will be necessary to fabricate different sections. The original material under consideration for the TSV was Zircaloy-4 (Zry-4), but it is known to form a hydride which can degrade its mechanical properties. Thus, some investigation here is focused on the effects of hydrogen uptake in the Zry-4. Additionally, the alternative material being considered is AISI 347, a stainless steel. Both materials have little existing data for their neutron irradiation behavior below 100°C, and both have open questions on the weld behavior under neutron irradiation. Testing has focused on characterizing their weld properties with tensile tests and performing neutron irradiation of samples in the High Flux Isotope Reactor (HFIR) at Oak Ridge National Laboratory (ORNL).

07 ISOTOPE AND RADIATION SOURCES↗

Characterization of microstructures and mechanical properties of Inconel 617/310 stainless steel dissimilar welds

The microstructure and mechanical properties of Inconel 617/310 austenitic stainless steel dissimilar welds were investigated in this work. Three types of filler materials, Inconel 617, Inconel 82 and 310 austenitic stainless steels were used to obtain dissimilar joint using the gas tungsten arc welding process. Microstructural observations showed that there was no evidence of any possible cracking in the weldments achieved by the nickel-base filler materials. The welds produced by 617 and 310 filler materials displayed the highest and the lowest ultimate tensile strength and total elongation, respectively. The impact test results indicated that all specimens exhibited ductile fracture. Among the fillers, Inconel 617 exhibited superlative fracture toughness (205 J). The mechanical properties of the Inconel 617 filler material were much better than those of other fillers. - Research Highlights: {yields} A fine dendritic structure was seen for the Inconel 617 weld metal. {yields} A number of cracks were initiated when the 310 SS filler metal was used. {yields} All welded samples showed ductile fracture. {yields} The Inconel 617 filler material presents the optimum mechanical properties.

36 MATERIALS SCIENCE↗

Optimization of a Welding Procedure for Making Critical Aluminum Welds on the LBNF Absorber Core Block

The LBNF Absorber consists of thirteen 6061-T6 aluminum core blocks. The core blocks are water cooled with de-ionized (DI) water which becomes radioactive during beam operations. The cooling water flows through gun-drilled channels in the core blocks. A weld quality optimization was performed to produce National Aeronautical Standard 1514 Class I quality welds on the aluminum core blocks. This was not successful in all cases. An existing Gas Tungsten Arc Welding Procedure Specification was fine tuned to minimize, in most cases, and eliminate detect-able tungsten inclusions in the welds. All the weld coupons, however passed welding inspection as per the piping code: ASME B31.3 Normal Fluid Service. Tungsten electrode diameter, type, and manufacturer were varied. Some of the samples were pre-heated and others were not. It was observed that larger diameter electrodes, 5/32 in., with pre-heated joints resulted in welds with the least number of tungsten inclusions. It is hypothesized that thinner electrodes breakdown easily and get lodged into the weld pool during the welding process. This breakdown is further enhanced by the large temperature differential between the un-preheated sample and the hot electrode.

43 PARTICLE ACCELERATORS↗