Search NASA⌕ Search

SEARCH · Search NASA

Results for “YIELD STRENGTH”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 127 records · Page 7

Tailoring Carbide Dispersed Steels: A Path to Increased Strength and Hydrogen Tolerance

The use of transition metal carbides is reported for use as a hydrogen trapping mechanism for ferritic and austenitic steel materials. The program combined computational modeling and simulations to guide experiments towards candidate metal carbide traps, both for interfacial and interior trapping. It was found that interfacial trapping is less effective than interior trapping, with the group IVB transition metal carbides being the most effect internal traps with a loss of carbon. The sub-stoichiometric rocksalt structure accommodate the hydrogen atoms in its octahedral interstices. Using percolation theory, carbon loss of approximately 25% or more was sufficient to ensure an interconnected network of vacancies for such trapping from the surface to the internal sites within the carbide. Using this as a guide, the program developed a means to provide a uniform dispersion of ZrC nanoparticles with either Fe or 304L micron-scale powders which was then consolidated by direct current sintering. Electrolytic hydrogen diffusivity studies confirmed the reduction of hydrogen diffusion in the matrix with increasing ZrC content, which was a linear response over the sample range studied (0.01 to 1.0 wt.%). The consolidated material was micro-tensile tested in either a non-hydrogen or hydrogen charge condition and compared to a control with no carbides. Additions up to 0.05 wt.% ZrC increased the yield strength with no loss in ductility in either the non-hydrogen or hydrogen tested condition. ZrC concentrations above this amount further increased the yield strength at the expense of ductility. While these samples had a lower absolute ductility value prior to failure, the relative change in ductility between the non-hydrogen and hydrogen charge states was less for the carbides than that of the control. Metal-rich ZrC nanoparticles were fabricated through a conformal coating process yielding ZrC0.66 particles that were then incorporated into a metal matrix. Notch fatigue testing in a hydrogen environment was conducted where the number of cycles to failure was found to be less in the control than that of the carbide addition. However, the spread in experimental data and the number of samples tested limits a conclusive outcome based on defects noticed in the gauge section of all the powder processed samples. The collective outcomes of this report provide further insight into the mechanisms by which carbides act as hydrogen traps; a means to process such carbides through powder metallurgy; and their associated mechanical performance in either a non-hydrogen or hydrogen-charged condition.

08 HYDROGEN↗

The effects of high-temperature brazing and thermal cycling on the mechanical properties of Hastelloy X

Data are presented on the effects of brazing alloy, brazing operation, thermal cycling, and combinations of these on the yield strength, elongation, tensile strength, and fatigue life of thin gage Hastelloy X. These data show that brazing at 1461 K (2170 F) with a Ni-Pd-Au alloy and subsequent exposure to 200 service thermal cycles between 533 and 1144 K (500 and 1600 F) result in reduction of as much as 39 percent in yield strength, 33 percent in elongation, 14 percent in tensile strength, and 26 percent in fatigue limit of Hastelloy X, as compared to as-received materials. These property losses are primarily caused by the brazing operation rather than the subsequent service thermal cycles.

Dicus, D. L.↗

Transient Chemo‐Mechanical Model of Lithium Plating Impacted by External Pressure

Abstract Lithium anodes show great promise in commercial applications, but are hindered by lithium plating and dendrite growth which cause safety concerns during long‐term cell operation. Stack pressure is experimentally observed to improve cell lifetime; however, the relationship between stress and lithium deposition has remained difficult to elucidate. In this work, a transient, 3D, finite‐element model of the evolution of a lithium anode due to stripping and plating is developed. The evolution of a microscale protrusion on the anode surface is tracked over one charge‐discharge cycle with respect to stack pressure and lithium yield strength. Lithium plastic deformation, nonconformal anode‐separator contact, and separator porosity effects are accounted for. Over the course of several hours of stripping/plating, the anode surface evolves to a similar morphology under pressure regardless of the initial conditions due to lithium plastic deformation and hardening. The rate of this evolution highly depends on the applied pressure and assumed lithium yield strength.

25 ENERGY STORAGE↗

Effect of Thermal Exposure on the Tensile Properties of Aluminum Alloys for Elevated Temperature Service

Tensile properties were evaluated for four aluminum alloys that are candidates for airframe applications on high speed transport aircraft. These alloys included the Al-Cu-Mg-Ag alloys C415 and C416 and the Al-Cu-Li-Mg-Ag alloys RX818 and ML377. The Al-Cu-Mg alloys CM001, which was used on the Concorde SST, and 1143, which was modified from the alloy used on the TU144 Russian supersonic aircraft, were tested for comparison. The alloys were subjected to thermal exposure at 200 F, 225 F and 275 F for times up to 30,000 hours. Tensile tests were performed on thermally-exposed and as-received material at -65 F, room temperature, 200 F, 225 F and 275 F. All four candidate alloys showed significant tensile property improvements over CM001 and 1143. Room temperature yield strengths of the candidate alloys were at least 20% greater than for CM001 and 1143, for both the as-received and thermally-exposed conditions. The strength levels of alloy RX818 were the highest of all materials investigated, and were 5-10% higher than for ML377, C415 and C416 for the as-received condition and after 5,000 hours thermal exposure. RX818 was removed from this study after 5,000 hours exposure due to poor fracture toughness performance observed in a parallel study. After 30,000 hours exposure at 200 F and 225 F, the alloys C415, C416 and ML377 showed minor decreases in yield strength, tensile strength and elongation when compared to the as-received properties. Reductions in tensile strength from the as-received values were up to 25% for alloys C415, C416 and ML377 after 15,000 hours exposure at 275 F.

Edahl, Robert A., Jr.↗

Fracture temperature and flaw growth in nitronic 40 at cryogenic temperatures

The fracture resistance and fatigue response of Armco Nitronic 40 austenitic stainless steel were evaluated under cryogenic conditions. Tensile, fracture toughness and fatigue crack growth properties were measured at -275 F. The tensile yield strength was approximately 120 ksi and the fracture toughness was estimated to be 350 ksi-in /2 on the basis of fracture toughness measurements. Testing was conducted to evaluate the behavior of a simulated section of the wing of the Pathfinder 1 model subject to a load and temperature history typical of that for testing in the National Transonic Facility. The wing section model incorporated a proposed brazing technique for pressure-transducer attachment. The simulated wing section performed satisfactorily at stress levels of nearly 60 percent of the material yield strength. The brazing technique proved to be an effective method of transducer attachment under conditions of high stress levels and large temperature excursions.

Domack, M. S.↗

Impact cratering in viscous targets - Laboratory experiments

To determine the effects of target yield strength and viscosity on the formation and morphology of Martian multilobed, slosh and rampart-type impact craters, 75 experiments in which target properties and impact energies were varied were carried out for high-speed motion picture observation in keeping with the following sequence: (1) projectile initial impact; (2) crater excavation and rise of ejecta plume; (3) formation of a transient central mound which generates a surge of material upon collapse that can partly override the plume deposit; and (4) oscillation of the central mound with progressively smaller surges of material leaving the crater. A dimensional analysis of the experimental results indicates that the dimensions of the central mound are proportional to (1) the energy of the impacting projectile and (2) to the inverse of both the yield strength and viscosity of the target material, and it is determined that extrapolation of these results to large Martian craters requires an effective surface layer viscosity of less than 10 to the 10th poise. These results may also be applicable to impacts on outer planet satellites composed of ice-silicate mixtures.

Greeley, R.↗

Structure-Property Relationships of Bismaleimides

The purpose of this research was to control and systematically vary the network topology of bismaleimides through cure temperature and chemistry (addition of various coreactants) and subsequently attempt to determine structure-mechanical property relationships. Characterization of the bismaleimide structures by dielectric, rheological, and thermal analyses, and density measurements was subsequently correlated with mechanical properties such as modulus, yield strength, fracture energy, and stress relaxation. The model material used in this investigation was 4,4'-BismaleiMidodIphenyl methane (BMI). BMI was coreacted with either 4,4'-Methylene Dianiline (MDA), o,o'-diallyl bisphenol A (DABA) from Ciba Geigy, or Diamino Diphenyl Sulfone (DDS). Three cure paths were employed: a low- temperature cure of 140 C where chain extension should predominate, a high-temperature cure of 220 C where both chain extension and crosslinking should occur simultaneously, and a low-temperature (140 C) cure followed immediately by a high-temperature (220 C) cure where the chain extension reaction or amine addition precedes BMI homopolymerization or crosslinking. Samples of cured and postcured PMR-15 were also tested to determine the effects of postcuring on the mechanical properties. The low-temperature cure condition of BMI/MDA exhibited the highest modulus values for a given mole fraction of BMI with the modulus decreasing with decreasing concentration of BMI. The higher elastic modulus is the result of steric hindrance by unreacted BMI molecules in the glassy state. The moduli values for the high- and low/high-temperature cure conditions of BMI/MDA decreased as the amount of diamine increased. All the moduli values mimic the yield strength and density trends. For the high-temperature cure condition, the room- temperature modulus remained constant with decreasing mole fraction of BMT for the BMI/DABA and BMI/DDS systems. Postcuring PMR-15 increases the modulus over that of the cured material even though density values of cured and postcured PMR were essentially the same. Preliminary results of a continuous and intermittent stress relaxation experiment for BMI:MDA in a 2:1 molar ratio indicate that crosslinking is occurring when the sample is in the undeformed state. Computer simulation of properties such as density, glass transition temperature, and modulus for the low- temperature cure conditions of BMI/MDA and BMI/DABA were completed. The computer modeling was used to help further understand and confirm the structure characterization results. The simulations correctly predicted the trends of these properties versus mole fraction BMI and were extended to other BMI/diamine systems.

Tenteris-Noebe, Anita D.↗

Titanium/beryllium laminates - Fabrication, mechanical properties, and potential aerospace applications

The paper describes an investigation to assess the fabricability, mechanical properties, and possible aerospace applications of adhesively-bonded titanium/beryllium Tiber laminates. The results of the investigation indicate that structural laminates can be made which have: a modulus of elasticity comparable to steel, fracture strength comparable to the yield strength of titanium, density comparable to aluminum, impact resistance comparable to titanium, and little or no notch sensitivity. These laminates can have stiffness and weight advantages over other materials, including advanced fiber composites, in some aerospace applications where buckling resistance, vibration frequencies, and weight considerations control the design.

Chamis, C. C.↗

Effect of a prior stretch on the aging response of an Al-Cu-Li-Ag-Mg-Zr alloy

Recently, a family of Al-Cu-Li alloys containing minor amounts of Ag, Mg, and Zr and having desirable combinations of strength and toughness were developed. The Weldalite (trademark) alloys exhibit a unique characteristic in that with or without a prior stretch, they obtain significant strength-ductility combinations upon natural and artificial aging. The ultra-high strength (approximately 690 MPa yield strength) in the peak-aged tempers (T6 and T8) were primarily attributed to the extremely fine T(sub 1) (Al2CuLi) or T(sub 1)-type precipitates that occur in these alloys during artificial aging, whereas the significant natural aging response observed is attributed to strengthening from delta prime (Al3Li) and GP zones. In recent work, the aging behavior of an Al-Cu-Li-Ag-Mg alloy without a prior stretch was followed microstructurally from the T4 to the T6 condition. Commercial extrusions, rolled plates, and sheets of Al-Cu-Li alloys are typically subjected to a stretching operation before artificial aging to straighten the extrusions and, more importantly, introduce dislocations to simulate precipitation of strengthening phases such as T(sub 1) by providing relatively low-energy nucleation sites. The goals of this study are to examine the microstructure that evolves during aging of an alloy that was stretch after solution treatment and to compare the observations with those for the unstretched alloy.

Kumar, K. S.↗

Microstructural Evolution and Mechanical Properties of LP-DED NASA HR-1 – A Hydrogen Resistant AM Superalloy for Space Propulsion Applications

The National Aeronautics and Space Administration (NASA) has actively pursued metal additive manufacturing (AM) technologies for spaceflight applications since the late 2000s. AM offers transformative advantages in cost, schedule, part consolidation, and design flexibility. Among the various AM techniques, laser powder directed energy deposition (LP-DED) is particularly well suited for fabricating complex geometries with fine feature resolution. In propulsion systems that utilize high-pressure gaseous hydrogen—such as liquid hydrogen rocket engines—hydrogen environment embrittlement (HEE) presents a serious threat to material performance 1,2 . Mechanical property degradation under these conditions can compromise component reliability, especially under cyclic loading. To address this challenge, NASA developed NASA HR-1 (Hydrogen Resistant-1) as a solution for liquid rocket engine components operating in hydrogen-rich environments, using the LP-DED technique 3-9 . A key component in a liquid rocket engine is the exhaust nozzle, which is typically regeneratively cooled (regen) due to the high heat flux. NASA HR-1 was specifically developed for regen nozzle applications using hydrogen as a propellant, providing resistance to HEE, a critical issue for many materials. The AM version of NASA HR-1 was also formulated to achieve high ultimate tensile strength, along with high yield strength and ductility in this environment 5,6 . Low-cycle fatigue (LCF) is another important consideration in nozzle design, as components are expected to endure multiple starts and missions. Additionally, the LP-DED version of the alloy exhibits improved thermal conductivity compared to its wrought counterpart, which benefits nozzle cooling. Overall, NASA HR-1 offers an excellent balance of high strength, HEE resistance, LCF performance, thermal conductivity, and ductility to meet the demanding requirements of channel-cooled nozzles and other components used with hydrogen and other propellants. The LP-DED–processed NASA HR-1 requires several post-processing heat treatment steps to achieve the material properties desirable for its intended application 6 . These steps include stress relief, homogenization, solution annealing, and aging for precipitation hardening. The stress relief treatment mitigates residual stresses accumulated during the LP-DED process and minimizes the potential for distortion. Homogenization, a common step for AM materials, reduces elemental segregation and promotes recrystallization to develop a more equiaxed grain structure. The subsequent solution annealing treatment heats the part to a solid solution temperature to dissolve the undesirable η-phase that forms during cooling from homogenization, followed by rapid cooling to retain an η-phase–free microstructure. Finally, aging promotes precipitation of the strengthening γ′ phase in the alloy. The integration of compositional design and optimized thermal processing enables high-quality LP-DED NASA HR-1 components with excellent microstructural and mechanical stability. Improved chemical and microstructure homogeneity enhances ductility and fatigue resistance—both critical for safe and reliable operation in high-pressure hydrogen environments. NASA has successfully fabricated and hot-fire tested multiple subscale and full-scale channel wall nozzles using LP-DED NASA HR-1 5,6, 9-14 . These efforts included process refinements to support thin-wall construction and various channel geometries. Throughout development, several key observations emerged. After homogenization, the as-built columnar grain structure transforms into a fully equiaxed microstructure. However, subsequent treatments—such as solution annealing and aging—result in changes that are more difficult to track. The grain structure remains largely unchanged, and the γ′ precipitates, typically 5–10 nm in diameter, are beyond the resolution of scanning electron microscopy (SEM). While transmission electron microscopy (TEM) can resolve these fine precipitates, TEM sample preparation is time-consuming and difficult for LP-DED material. As an alternative, differential scanning calorimetry (DSC) offers a useful, qualitative approach to monitor precipitate evolution throughout different stages of heat treatment. The overall goal is to improve the understanding of how heat treatment affects the microstructure and mechanical performance of LP-DED NASA HR-1. This paper presents heat treatment design considerations, microstructural characterization, mechanical testing – including tensile and LCF testing in both air and hydrogen environments.

Superalloy↗

Low-Cost, High-Performance Combustion Chamber

Ultramet designed and fabricated a lightweight, high-temperature combustion chamber for use with cryogenic LOX/CH4 propellants that can deliver a specific impulse of approx.355 seconds. This increase over the current 320-second baseline of nitrogen tetroxide/monomethylhydrazine (NTO/MMH) will result in a propellant mass decrease of 55 lb for a typical lunar mission. The material system was based on Ultramet's proven oxide-iridium/rhenium architecture, which has been hot-fire tested with stoichiometric oxygen/hydrogen for hours. Instead of rhenium, however, the structural material was a niobium or tantalum alloy that has excellent yield strength at both ambient and elevated temperatures. Phase I demonstrated alloys with yield strength-to-weight ratios more than three times that of rhenium, which will significantly reduce chamber weight. The starting materials were also two orders of magnitude less expensive than rhenium and were less expensive than the C103 niobium alloy commonly used in low-performance engines. Phase II focused on the design, fabrication, and hot-fire testing of a 12-lbf thrust class chamber with LOX/CH4, and a 100-lbf chamber for LOX/CH4. A 5-lbf chamber for NTO/MMH also was designed and fabricated.

Fortini, Arthur J.↗

Microstructure effects on high velocity microparticle impacts of copper

Constitutive models can fail to predict high-rate deformation behavior due to their inability to account for microstructural effects. In part, this is because of a dearth of experimental benchmarking data in the high strain-rate, low pressure regime, since many high-rate experiments also probe a region of strong shockwaves, at which point microstructure effects no longer play a primary role. This work uses laser-induced particle impact testing to quantitatively study high velocity impacts of small, rigid alumina microspheres on flat copper substrates with varying amounts of initial cold work in the weak shock regime, but at very high strain rates up to ~10 7 s –1 . Through paired experiments and numerical simulations, this work shows that the initial microstructure condition can have significant influence on dynamical mechanical properties in this range. Specifically, prior work hardening of the copper substrate leads to increased rebounding of the microparticles (i.e., less plastic dissipation in the impact) as well as smaller craters. Each of these experimental measurables can be converted into a strength measure, i.e., the dynamic yield strength or dynamic hardness, respectively, neither of which is well predicted consistently by existing constitutive laws. The general trend of hardening can be captured by such models by incorporating an existing “pre-strain,” suggesting that future calibration of the materials parameters may yield a good fit over a broader range of conditions. Our results emphasize the importance of reporting the microstructural condition in dynamic studies, as well as the necessity of accounting for these factors when formulating and optimizing constitutive models.

36 MATERIALS SCIENCE↗

Titanium/beryllium laminates: Fabrication, mechanical properties, and potential aerospace applications

The investigation indicated that structural laminates can be made which have: a modulus of elasticity comparable to steel, fracture strength of comparable to the yield strength of titanium, density comparable to aluminum, impact resistance comparable to titanium, and little or no notch sensitivity. These laminates can have stiffness and weight advantages over other materials including advanced fiber composites, in some aerospace applications where buckling resistance, vibration frequencies, and weight considerations control the design.

Chamis, C. C.↗

Preliminary results on the development of vacuum brazed joints for cryogenic wind tunnel aerofoil models

The results of initial experiments show that high-strength void-free bonds can be formed by vacuum brazing of stainless steels using copper and nickel-based filler metals. In Nitronic 40, brazed joints have been formed with strengths in excess of the yield strength of the parent metal, and even at liquid nitrogen temperatures the excellent mechanical properties of the parent metal are only slightly degraded. The poor toughness of 15-5 P.H. stainless steel at cryogenic temperatures is lowered even further by the presence of the brazed bonds investigated. It is highly unlikely that the technique would be used for any critical areas of aerofoil models intended for low-temperature service. Nevertheless, the potential advantages of this simplified method of construction still have attractions for use at ambient temperatures.

Wigley, D. A.↗

3D Printed Ceramic Reinforced Polymer Composites Microstructure and Mechanical Properties

In Fused Filament Fabrication (FFF) 3D printing a part is made by extruding material layer by layer. Benefits of FFF are the ability to print complex shapes quickly and at a lower cost compared to other manufacturing methods. In this work, filaments composed of either silicon carbide (SiC) or zirconium silicate ceramic particulates in a polylactic-acid (PLA) matrix were used to print specimens for microstructural analysis and mechanical testing. Pure PLA samples were also printed and tested as a baseline for comparison. A Design of Experiments approach was used to test the interactions between three different parameters and their effect on ultimate strength, Young’s modulus, and yield strength. For compression test specimens, these parameters were infill percentage, number of shells, and print orientation angle. For tensile test specimens, the parameters were layer height, number of shells, and infill orientation angle. Pre- and post-compression test samples were evaluated by scanning electron microscopy for microstructural analysis. Infill percentage had the greatest effect on mechanical properties while number of shells and print orientation angle had minor effects. When changing the layer lines from perpendicular to parallel, relative to the loading direction, SiC-PLA had higher mechanical properties while pure PLA properties had decreased, and zirconium silicate-PLA had mix results.

Fused filament fabrication↗

Experimental Evaluation of Interfacial Bonding Strength Between 304 Stainless Steel Substrate and Electrodeposited Nickel Coating Using Mesoscale Mechanical Testing Methods

Electrodeposition is a commonly used method for depositing a metal layer on a metallic substrate, to provide a decorative finish or for functional purposes including wear and corrosion resistance. The interfacial bonding strength is a critical factor in determining the quality of electrodeposition, as it ensures the adhesion of the deposited layer to the substrate. Despite its importance, there has not previously been a suitable mechanical testing method to quantitatively characterize the bonding strength between the electrodeposited layers and the substrate, due to the high strength of the materials and to restrictions imposed by the geometry (due to the small thickness of the plating layer) to manufacture tensile bars. In this study, we introduce a novel mesoscale mechanical testing method to overcome these limitations. This technique was applied to assess the bonding strength between a 304 stainless steel (SS) substrate and electrodeposited nickel with three different plating formulae (nickel sulfamate, Watts bath, and hard nickel). The thickness of the pure nickel coatings achieved for each of the three electrolyte solutions was approximately 1 mm on each side of the substrate. Mesoscale tensile bars of 1 mm length were manufactured by a femtosecond laser, with the material interface at the center of the gauge section, and then tensile-tested with digital image correlation. Further, the results proved that the electrodeposition technique is able to produce a very high bonding strength that is close to the yield strength of both the substrate material and the electrodeposited nickel layer. Additionally, in the case of the Watts bath formula, the interfacial bonding strength between the SS 304 and electrodeposited nickel can exceed that of the nickel layer. This method is expected to be useful for quantifying the interfacial bonding strength in numerous applications.

36 MATERIALS SCIENCE↗

Deformation and fracture of thin sheet aluminum-lithium alloys: The effect of cryogenic temperatures

The objective is to characterize the fracture behavior and to define the fracture mechanisms for new Al-Li-Cu alloys, with emphasis on the role of indium additions and cryogenic temperatures. Three alloys were investigated in rolled product form: 2090 baseline and 2090 + indium produced by Reynolds Metals, and commercial AA 2090-T81 produced by Alcoa. The experimental 2090 + In alloy exhibited increases in hardness and ultimate strength, but no change in tensile yield strength, compared to the baseline 2090 composition in the unstretched T6 condition. The reason for this behavior is not understood. Based on hardness and preliminary Kahn Tear fracture experiments, a nominally peak-aged condition was employed for detailed fracture studies. Crack initiation and growth fracture toughness were examined as a function of stress state and microstructure using J(delta a) methods applied to precracked compact tension specimens in the LT orientation. To date, J(delta a) experiments have been limited to 23 C. Alcoa 2090-T81 exhibited the highest toughness regardless of stress state. Fracture was accompanied by extensive delamination associated with high angle grain boundaries normal to the fatigue precrack surface and progressed microscopically by a transgranular shear mechanism. In contrast the two peak-aged Reynolds alloys had lower toughness and fracture was intersubgranular without substantial delamination. The influences of cryogenic temperature, microstructure, boundary precipitate structure, and deformation mode in governing the competing fracture mechanisms will be determined in future experiments. Results contribute to the development of predictive micromechanical models for fracture modes in Al-Li alloys, and to fracture resistant materials.

Wagner, John A.↗