Search NASA⌕ Search

SEARCH · Search NASA

Results for “ZIRCONIUM”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 127 records · Page 7

Methods to increase solid solution zirconium in aluminum alloys

A method of making an aluminum alloy containing zirconium includes heating a first composition comprising aluminum to a first temperature of greater than or equal to about 580° C. to less than or equal to about 800° C. The method further includes adding a second composition including a copper-zirconium compound to the first composition to form a third composition. The copper-zirconium compound of the second composition has a molar composition of greater than or equal to about 41% zirconium to less than or equal to about 67% zirconium and a balance of copper. The method also includes solidifying the third composition at a cooling rate of greater than or equal to about 0.1° C./second to less than or equal to about 100° C./second to a second temperature less than or equal to a solidus temperature and decomposing the copper-zirconium compound at a third temperature of less than or equal to about 715° C.

36 MATERIALS SCIENCE↗

Preliminary irradiation effect on corrosion resistance of zirconium alloys - 2016-0067

In order to improve the composition and structure of zirconium alloys, it is important to know how changes in their structure-phase state under irradiation affect various properties, including corrosion. In this work, autoclave corrosion tests were carried out on fuel cladding samples made of zirconium-niobium and zirconium-niobium-tin-iron alloy systems. All samples were preliminarily irradiated in a BOR-60 nuclear reactor at a fluence of 2 X10{sup 26} m{sup -2} (E>0.1 MeV). The autoclave tests of irradiated and unirradiated samples were performed at 350 deg. C for 240 days in distilled water containing 10 ppm lithium and 1,600 ppm boron. The irradiation of all alloys resulted in a significant change in their initial structure-phase state. The content of niobium in b-niobium-phase precipitates was reduced from 80 % to - 90 % to 50 % to - 60 %. Iron atoms from the Laves-phase particles were diffused into a matrix, and their lattice transformed from hexagonal close-packed to body-centered cubic. An average size of the transformed second-phase precipitates in the irradiated alloys increased relatively to an average size of the initial precipitates. Elongated radiation-induced precipitates (RIPs) with an average length up to 7 nm were formed in all alloys under irradiation. In comparison with the unirradiated state, irradiation reduced the corrosion of zirconium-niobium alloys, and this effect became more apparent with increased niobium content in the alloy. For zirconium-niobium-tin-iron alloys, irradiation led to more severe corrosion, mostly because of increasing tin content. Niobium content increased up to 2.37 %, and iron content decreased up to 0.18 % in the alloys, contributing to higher corrosion resistance. An interconnection between the niobium/(tin + iron) alloying parameter, quantity of nanometric precipitates formed therein under irradiation, and their corrosion performance has been suggested. (authors)

36 MATERIALS SCIENCE↗

Composition and microstructure of zirconium and hafnium germanates obtained by different chemical routes

The phase composition and morphology of zirconium and hafnium germanates synthesized by ceramic and co-precipitation routes were studied. The products were characterized using high-temperature X-ray diffraction analysis (XRD), Raman spectroscopy, scanning electron microscopy (SEM) and thermal (TG/DTA) analysis. To investigate the phase composition and stoichiometry of compounds the unit cell parameters were refined by full-profile Rietveld XRD analysis. The morphology of products and its evolution during high-temperature treatment was examined by SEM analysis. It was stated that there is the strong dependence of the phase composition and morphology of products on the preparation route. The ceramic route requires a multi-stage high-temperature treatment to obtain zirconium and hafnium germanates of 95% purity or more. Also, there are strong diffusion limitations to obtain hafnium germanate Hf{sub 3}GeO{sub 8} by ceramic route. On the contrary, the co-precipitation route leads to the formation of nanocrystalline single phase germanates of stoichiometric composition at a relatively low temperatures (less than 1000 °C). The results of quantitative XRD analysis showed the hafnium germanates are stoichiometric compounds in contrast to zirconium germanates that form a set of solid solutions. This distinction may be related to the difference in the ion radii of Zr and Hf. - Graphical abstract: The phase composition and morphology of zirconium and hafnium germanates synthesized by ceramic and co-precipitation routes were studied. It was stated that there is the strong dependence of the phase composition and morphology of products on the preparation route. Display Omitted - Highlights: • Zr and Hf germanates were synthesized by ceramic and co-precipitation routes. • The morphology of products depends on the synthesis parameters. • Zirconium germanates forms a set of solid solutions. • Hafnium germanates are stoichiometric compounds.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Crystal-structure refinement of zirconium-rich eudialyte and its place among calcium-poor eudialyte-group minerals

The repeated refinement of the crystal structure of zirconium-rich eudialyte based on the X-ray diffraction data set collected earlier revealed new structural features. The trigonal unit-cell parameters are a = 14.222(3) A, c = 30.165(5) A, V = 5283.9 A{sup 3}. The refinement resulted in the reduction of the R factor from 0.045 (2347F > 4{sigma}(F)) to 0.035 (3124F > 3{sigma}(F)). It was found that the ordering of Ca and Fe in six-membered rings leads to the lowering of the symmetry to R3. An excess amount of zirconium (more than three atoms per symmetrically independent unit) is located in the M2 microregion in square and five-vertex polyhedral positions. However, this amount is insufficient to be dominant, and the deficiency of zirconium is compensated for by sodium atoms. Based on the new data, zirconium-rich eudialyte can be assigned to the oneillite subtype, being a zirconium-rich and aluminum variety of raslakite.

36 MATERIALS SCIENCE↗

Understanding irradiation growth through atomistic simulations: Defect diffusion and clustering in α-zirconium and the influence of alloying elements - 2016-0093

Irradiation-induced structural changes of α-zirconium alloys and in particular the effect of iron were investigated by molecular dynamics simulations using embedded atom potentials derived from first-principles calculations. The simulations revealed that at temperatures between 500 and 600 K self-interstitial atoms (SIAs) diffuse rapidly in a cooperative movement, preferably parallel to basal planes (a directions; ), forming nano-clusters with an extension in and . Vacancies diffuse more slowly than SIAs and remain isolated for a longer period of time. Nano-clusters associated with SIAs cause a pronounced overall expansion in a directions, as well as local strains. Under compressive strain in the c direction, vacancy diffusivity increases in the c direction. In contrast, the diffusivity of SIAs increases in the c direction under a tensile strain in the c direction. SIA nano-clusters are highly mobile within basal planes. Vacancy clusters grow by merging, leading to a contraction in the a direction, compensating for the expansion caused by SIA nano-clusters and possibly contributing to the plateau in growth after the initial rapid expansion. At the onset of breakaway growth, possibly due to stress buildup, the vacancy nano-clusters can condense into c loops, thereby diminishing the compensation effect. The alloying elements iron, nickel, chromium, and niobium liberated from secondary phase particles under irradiation or already in solution are attracted to vacancies and SIAs and are found inside vacancy and SIA loops. The interaction of alloying elements with defect clusters is discussed, with a particular focus on iron. Iron has been found to promote cluster formation in zirconium, and the structures of zirconium-iron clusters have been analyzed. Tin is repelled by SIA clusters and only weakly attracted by vacancies. Niobium impedes the diffusion of SIAs (and therefore may increase annihilation rates with nearby vacancies) and does not destabilize vacancy or SIA clusters. Ab initio calculations of the dimensional and elastic coefficients of the intermetallic phases occurring in secondary phase particles, such as Zr{sub 2}Fe and Zr{sub 3}Fe, are presented, allowing an assessment of local strains in a zirconium matrix. Thus, novel results from extended molecular dynamics simulations provide new insights and contribute to a deeper understanding of the complex mechanisms causing irradiation-induced dimensional changes and the breakaway growth of zirconium alloys. (authors)

36 MATERIALS SCIENCE↗

White Paper Summary of 2nd ASTM International Workshop on Hydrides in Zirconium Alloy Cladding

This white paper recommends that ASTM International develop standards to address the potential impact of hydrides on the long term performance of irradiated zirconium alloys. The need for such standards was apparent during the 2nd ASTM International Workshop on Hydrides in Zirconium Alloy Cladding and Assembly Components, sponsored by ASTM International Committee C26.13 and held on June 10-12, 2014, in Jackson, Wyoming. The potentially adverse impacts of hydrogen and hydrides on the long term performance of irradiated zirconium-alloy cladding on used fuel were shown to depend on multiple factors such as alloy chemistry and processing, irradiation and post irradiation history, residual and applied stresses and stress states, and the service environment. These factors determine the hydrogen content and hydride morphology in the alloy, which, in turn, influence the response of the alloy to the thermo-mechanical conditions imposed (and anticipated) during storage, transport and disposal of used nuclear fuel. Workshop presentations and discussions showed that although hydrogen/hydride induced degradation of zirconium alloys may be of concern, the potential for occurrence and the extent of anticipated degradation vary throughout the nuclear industry because of the variations in hydrogen content, hydride morphology, alloy chemistry and irradiation conditions. The tools and techniques used to characterize hydrides and hydride morphologies and their impacts on material performance also vary. Such variations make site-to-site comparisons of test results and observations difficult. There is no consensus that a single material or system characteristic (e.g., reactor type, burnup, hydrogen content, end-of life stress, alloy type, drying temperature, etc.) is an effective predictor of material response during long term storage or of performance after long term storage. Multi-variable correlations made for one alloy may not represent the behavior of another alloy exposed to identical conditions and the material responses to thermo-mechanical exposures will be different depending on the materials and systems used. The discussions at the workshop showed several gaps in the standardization of processes and techniques necessary to assess the long term performance of irradiated zirconium alloy cladding during dry storage and transport. The development of, and adherence to, standards to help bridge these gaps will strengthen the technical basis for long term storage and post-storage operations, provide consistency across the nuclear industry, maximize the value of most observations, and enhance the understanding of behavioral differences among alloys. The need for, and potential benefits of, developing the recommended standards are illustrated in the various sections of this report.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Chemical Vapor Deposition of Zirconium Compounds: A Review

Coatings of zirconium compounds are used in a wide variety of fields, yet an understanding and descriptions of deposition mechanisms are scant in the public literature. The mechanisms of deposition for metallic zirconium, ZrC, ZrN, ZrO 2 , ZrB 2 , and zirconium silicides are discussed based on the direct vapor deposition research of those compounds where possible or compared to complementary titanium systems when direct research is lacking. Both inorganic and organometallic deposition systems are discussed. As a class of compounds, an understanding of the vapor deposition mechanisms can be significantly improved by investigations on metallic zirconium deposition by zirconium halides and hydrogen and by in situ analysis techniques such as Fourier-transform infrared (FTIR) spectroscopy or x-ray photoelectron spectroscopy (XPS).

organometallic↗

Purification of Zirconium Tetrachloride (ZrCl{sub 4}) from UNF Cladding - A Progress Report

Zirconium-based cladding materials that surround used nuclear fuel (UNF) rods represent a significant fraction of the total amount of high level waste that must be disposed of in long term geological repositories. The decontamination and/or recovery and reuse of these materials would significantly reduce the amount of high level waste associated with light water nuclear energy reactors and could provide a new source of hafnium free zirconium for the fabrication of new nuclear components. A step in a strategy to recycle zirconium from used cladding materials is the direct, high yield chlorination reaction that produces zirconium tetrachloride (ZrCl{sub 4}). The ZrCl{sub 4} so obtained is contaminated with other metal chloride species (FeCl{sub 3}, NbCl{sub 5}, NbOCl{sub 3}, SnCl{sub 4}, CsCl, SbCl{sub 5}, etc.) that originate from the alloying metals present initially as well as contaminants from oxide layers on the cladding, trace fission products, fuel residues, activation byproducts, and tritium. The suggested strategy to remove the metal chloride impurities is based on sublimation at atmospheric pressure combined with chemical treatments influencing volatility of the impurities.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Alternate Methods for Cleaning Zirconium Plate

The United States High Performance Research Reactor Conversion Program identified the need to transition from highly enriched uranium fuel to lowly enriched uranium fuel for high power research and civil reactors. One of the fuel configurations selected for these reactors was a uranium (U) foil alloyed with 10% molybdenum (Mo). The U-10Mo fuel foil was then covered with a zirconium (Zr) interlayer and pressed into an aluminum cladding. Idaho National Laboratory prescribed a need to remove surface oxidation on the Zr prior to bonding it with U-10Mo fuel foil. To determine the best method of oxidation removal, a variety of polishing methods, including hand polishing with a diamond paste or Scotch-Brite™ pads, mechanically wet-polishing with abrasive belts, and chemical etching with hydrofluoric/nitric acid mixtures, were investigated on pre-polished Zircaloy 702 sheets purchased directly from the manufacturer. No change in surface roughness was detected using any of these methods relative to the as-received material. In fact, scanning electron microscopy detected grit from hand polishing with Amplex Grade 30 waste soluble diamond paste and Scotch-Brite™ pads. Visible staining was found, and fluorine detected via X-ray photoelectron spectroscopy on the flash etching samples. These contaminants were not seen on the as-received material. In addition to the need to remove the oxide layer on the Zr prior to co-rolling, there are concerns that the Neolube debonding agent on the co-rolling can may contaminate the Zr surface after co-rolling. The experimental results found that zirconium in contact with Neolube coated steel plates was easily cleaning with ethanol wiping after heat treated and no carbide inclusions remained on the surface. Overall, all cleaning methods tested did not significantly change the surface roughness of the plates or reduce the oxide layer present on the zirconium. Carbon was found on all the samples, before and after cleaning, except for the flash etch samples which detected fluorine instead. The insignificant changes seen in the cleaned plates relative to the as received plates question the need for cleaning prior to rolling. Further investigation in the requirements for cleaning at this step is recommended. Current methods for cleaning the surface after hot rolling with alcohol appear sufficient. After hot rolling, if Neolube does peel off the can and onto the zirconium coated foil surface, a dry abrasive or diamond paste polish is not recommended due to the chance of abrasive being embedded into the surface. However, the ability of an etchant to lift the lubricant off the zirconium surface indicates that a spot etch method could work to clean specific spots where Neolube is present, if the need arises.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

A simple spectrophotometric method for determination of zirconium or hafnium in selected molybdenum-base alloys

A simple analytical procedure is described for accurately and precisely determining the zirconium or hafnium content of molybdenum-base alloys. The procedure is based on the reaction of the reagent Arsenazo III with zirconium or hafnium in strong hydrochloric acid solution. The colored complexes of zirconium or hafnium are formed in the presence of molybdenum. Titanium or rhenium in the alloy have no adverse effect on the zirconium or hafnium complex at the following levels in the selected aliquot: Mo, 10 mg; Re, 10 mg; Ti, 1 mg. The spectrophotometric measurement of the zirconium or hafnium complex is accomplished without prior separation with a relative standard deviation of 1.3 to 2.7 percent.

Dupraw, W. A.↗

Zirconium fluoride glass - Surface crystals formed by reaction with water

The hydrated surfaces of a zirconium barium fluoride glass, which has potential for application in optical fibers and other optical elements, were observed by scanning electron microscopy. Crystalline zirconium fluoride was identified by analysis of X-ray diffraction patterns of the surface crystals and found to be the main constituent of the surface material. It was also found that hydrated zirconium fluorides form only in highly acidic fluoride solutions. It is possible that the zirconium fluoride crystals form directly on the glass surface as a result of its depletion of other ions. The solubility of zirconium fluoride is suggested to be probably much lower than that of barium fluoride (0.16 g/100 cu cm at 18 C). Dissolution was determined to be the predominant process in the initial stages of the reaction of the glass with water. Penetration of water into the glass has little effect.

Doremus, R. H.↗

Zirconium-based alloys, nuclear fuel rods and nuclear reactors including such alloys, and related methods

Zirconium-based metal alloy compositions comprise zirconium, a first additive in which the permeability of hydrogen decreases with increasing temperatures at least over a temperature range extending from 350.degree. C. to 750.degree. C., and a second additive having a solubility in zirconium over the temperature range extending from 350.degree. C. to 750.degree. C. At least one of a solubility of the first additive in the second additive over the temperature range extending from 350.degree. C. to 750.degree. C. and a solubility of the second additive in the first additive over the temperature range extending from 350.degree. C. to 750.degree. C. is higher than the solubility of the second additive in zirconium over the temperature range extending from 350.degree. C. to 750.degree. C. Nuclear fuel rods include a cladding material comprising such metal alloy compositions, and nuclear reactors include such fuel rods. Methods are used to fabricate such zirconium-based metal alloy compositions.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

NON-DESTRUCTIVE POST IRRADIATION EXAMINATION OF FIRST CYCLE ACCIDENT TOLERANT AND ADVANCED ZIRCONIUM ALLOY HIGH BURNUP FUEL RODS

Post irradiation examination (PIE) of accident tolerant fuel concepts and high burnup uranium dioxide advanced zirconium alloy clad fuel contribute to near term nuclear industry goals of enhancing light water reactor safety and economics. Westinghouse is developing chromium coated zirconium alloy cladding as an accident tolerant fuel option for current pressurized water reactors. Examination of high burnup fuel further augments the technical foundation for extending the peak rod average burnup limits beyond the current regulatory limit of 62 MWd/kgU. Seven fuel rods were received at the Oak Ridge National Laboratory Irradiated Fuel Examination Facility. This includes three chromium coated zirconium alloy fuel rods and four high burnup advanced zirconium alloy fuel rods. Six of the seven rods were fueled with standard uranium dioxide while one of the chromium coated rods contained Westinghouse’s ADOPT fuel. The overall hot-cell PIE plan and some PIE results have been presented previously. This paper focuses on the additional non-destructive examination and fission gas release. Highlights from visual examination of these rods are presented. The chromium coating showed little to no visual change following irradiation. Observations of the axial burnup trends in the fuel rods are derived from full rod axial gamma-ray scans with additional observations related to local fission product migration. The axial dimensional changes of the seven rods are evaluated. As expected, creep down had not yet occurred in the chromium coated rods, and the maximum diameter strain in the high burnup advanced zirconium alloy cladding was less than 0.5%. Finally, the steady state fission gas release for these rods was measured ranging from 4.1% to 17.6% which matched expectation from literature. These fuel rods now await further destructive examination.

Harp, Jason↗

Synthesis of zirconium oxide nanoparticle by sol-gel technique

Zirconium oxide nanoparticle is synthesized using sol-gel technique. Various mole ratio of ammonia solution and nitric acid relative to zirconium propoxide is added in the reaction to study the effect on the crystallinity and particle size on zirconium oxide particle. Zirconium oxide synthesized with nitric acid have the smallest particle size under FESEM image and show the increasing formation of crystalline tetragonal phase under XRD diffractogram.

36 MATERIALS SCIENCE↗

Characterization of the Chlorination Products of Zirconium Alloys used for Nuclear Fuel Cladding

The United States produces over 2000 metric tons of used nuclear fuel material per year, of which 25% is irradiated fuel cladding, and it is expected to increase for the next 50 years. Previous simulation studies have shown that in the irradiated cladding, the major activation products found are {sup 125}Sb, {sup 60}Co, and {sup 99m}Nb, and the major fission product found is {sup 137}Cs. These radioisotopes make it impossible to treat the cladding as low level waste. A chlorination process has been proposed for zirconium reprocessing as it has been proven more efficient than previous mechanical processes, redox processes, and other chemical methods (e.g. iodination). In the chlorination process, zirconium alloy cladding reacts with Cl{sub 2} at 350- 380 deg. C to produce mainly ZrCl{sub 4}. The zirconium tetrachloride has a relatively low sublimation point (331 deg. C) that allows its separation from other products, and so it can be treated as low level waste for disposal or recycling. However, previous work has observed element impurities (iron, tin, chromium, cesium, antimony, and niobium) in the recovered ZrCl{sub 4}, meaning that additional steps are necessary in a chlorination process previous to the reduction of ZrCl, to metallic Zr. The emphasis of this research summary is on the progress that has been made to isolate and characterize the impurities produced after chlorination of three previously characterized non-irradiated zirconium alloys (Zircaloy-2, Zircaloy-4, and a commercial Zr-Nb alloy) widely used as cladding materials.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Progressing Zirconium-Alloy Corrosion Models Using Synchrotron XANES

The corrosion and hydrogen pickup of in-reactor zirconium-based cladding is currently limiting the maximum fuel burnup in light-water reactors. Since the oxidation rate and hydrogen pickup fraction of zirconium alloys vary significantly as a function of exposure time, burnup, and alloy composition, it is critical to better understand the underlying mechanisms to model and predict corrosion behavior. Following the analysis of ~500 autoclave coupons, a physically based zirconium-alloy corrosion model founded on first principles, named “Coupled Current Charge Compensation (C4)”, has been developed. The model reproduces the differences in oxidation kinetics and hydrogen pickup between different zirconium alloys, such as Zr-Nb and Zircaloy-4. Since oxidized solute elements affect the corrosion process through a space-charge compensation mechanism, synchrotron nano-beam X-ray Absorption Near-Edge Spectroscopy has been performed on multiple oxidized Zr-Nb alloys to determine the oxidation-state profile of niobium in the oxide layer. The results inform the C4 model and the associated hydrogen pickup fraction.

C4 Model↗

Mechanism and Conditions for Continuous Hydride Layer Formation in Zirconium Cladding

Local hydrogenation of zirconium fuel-element cladding, resulting in the formation of continuous hydrides, as a rule occurs when coolant or other hydrogen-containing compound finds its way beneath the fuel-element cladding irradiated in the core of a water moderated and cooled reactor. In this article, the set of processes occurring during hydrogenation of zirconium cladding is analyzed, and estimates are given for the parameters of these processes. The conditions and mechanism of formation of a continuous hydride over the thickness of zirconium cladding are established. It is shown that the duration of the nucleation of the hydride is determined primarily by the time to local destruction of the oxide film on the inner surface of the zirconium cladding of the fuel elements. The shortest possible time for continuous hydride to grow through the thickness of fuel-element cladding is determined.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Separation of zirconium and hafnium from early actinides and rare earth elements with eichrom’s pb resin in HCl

The separation of zirconium and hafnium isotopes from the early actinides and rare earth elements (REE) with Eichrom’s Pb resin has been studied. Batch studies were performed to characterize the behavior of actinium, thorium, zirconium, hafnium, lutetium, and yttrium on Pb resin from HCl solutions (0.001 M to 11 M). The early actinides and REE had no affinity for the resin at any concentration of HCl, but zirconium and hafnium showed a moderate uptake at high concentrations of HCl with a maximum extraction at 11 M HCl. Several column separations were tested, including with only tracer isotopes and with mass. Rapid, simple separations of zirconium from actinium, thorium, protactinium, and the REE with high yields and low elution volumes are presented with applications for tracer isotope production and fission product separations. Furthermore, the resin is less suitable for hafnium separations as hafnium tends to bleed off the resin even at high concentrations of HCl.

38 RADIATION CHEMISTRY, RADIOCHEMISTRY, AND NUCLEA↗