Search NASA⌕ Search

SEARCH · Search NASA

Results for “ZIRCONIUM ALLOY”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 127 records · Page 7

VZr_BCC_SolidSolution_128atoms_VASP6

We performed density functional theory (DFT) calculations for body-centered-cubic (BCC) structures with 128 lattices sites of solid solution binary alloys vanadium-zirconium (V-Zr). The electronic structures of alloys have been calculated using Vienna Ab initio Simulation Package (VASP). Within this package the DFT approach is used to reduce many-body Schrodinger equation to set of single particle Kohn-Sham (KS) equations. The generalized electronic exchange-correlation functional is described by generalized gradient approximation with the Perdew-Burke-Ernzerhof parametrization. The electron-ion interactions is described by pseudopotentials developed within the plane-wave basis projector augmented-wave (PAW) approach \cite{PAW}. These pseudopotentials are available at the VASP portal (http://cms.mpi.univie.ac.at/vasp/). Our calculations have been run with the pseudopotentials treating s and p semi-core states as valence in case for the elements V and Zr. The electronic densities and potentials are expanded over plane-waves with energy cutoff of 350 eV. 2x2x2 k-mesh and normal precision were used. The alloys were modeled by supercell containing 128 randomly distributed atoms. At initial step the atoms occupy perfect bcc lattice cites. This initial structure was optimized until energy changes less than 1e-6 eV, while forces acting on atoms don't exceed 1e-2 eV/angstrom. The electron-ion interaction is described by PAW pseudopotentials. The calculations have been collected by sampling chemical compositions across the entire compositional range. The chemical compositions have been sampled by progressively changing the number of atoms per constituent by 4. For each chemical composition of binaries and ternaries, the first-principle calculations have been run for 100 randomized arrangements of the constituents on the BCC lattice sites. We collected data for a total of 3,100 randomized atomic structures over 31 chemical compositions.

36 MATERIALS SCIENCE↗

Enhanced Mechanical Properties and Wear Resistance of FeCrAl Alloys at ~ 300°C and Higher Temperatures

Abstract Worldwide, light water reactors (LWRs) have been using zirconium (Zr)-based alloys for the cladding of the uranium dioxide fuel for more than 6 decades. Zr alloys oxidize rapidly in the presence of water and steam at temperatures > 450°C; therefore, they do not respond well to scenarios of loss of coolant accidents. There is a global effort by nuclear materials technologists to find more robust or stronger cladding materials for LWRs. One option is to use an iron-chromium-aluminum (FeCrAl) alloy since they have excellent resistance to high temperature oxidation and superior mechanical properties at LWR operation temperatures. Results show that (1) FeCrAl alloys have better mechanical properties than Zr alloy and are orders of magnitude more resistant to creep at temperatures higher than LWR normal operation conditions. (2) FeCrAl alloys have better resistance to fretting wear than Zr alloys at the normal operation conditions of LWRs.

Materials Science↗

Investigation of breakaway corrosion observed during oxide growth in pure and low alloying element content Zr exposed in water at 360°C

The addition of small concentrations of alloying elements to pure zirconium can prevent nuclear fuel cladding material from undergoing unstable oxide growth in aqueous environments at light water reactor operating temperatures. The role of alloying elements in stabilizing the oxide growth is examined in this paper, to better understand the oxide growth stabilization mechanism. To this end, a set of initial, short-duration corrosion experiments were performed, followed by oxide layer characterization. Specifically, ten model Zr alloys were selected to test the effect of small alloying additions on the alloy corrosion rate and corrosion breakaway. Additionally, these alloys were corrosion tested in pure water in an autoclave at 360°C for up to 70 days. The alloys included crystal bar Zr, sponge Zr, and model alloys with small concentrations of Sn, Fe, and Cr. After testing, the alloys were characterized using scanning electron microscopy (SEM) and synchrotron µ-X-ray fluorescence (µXRF) to study how the structure of the oxide and alloying element distribution related to unstable oxide growth. Initial results in the 360°C water environment showed breakaway oxidation may be caused by unstable oxide growth due to heterogeneous distribution of the alloying elements. Heterogeneous distribution of alloying elements was correlated to the occurrence of unstable oxide growth (either nodule-like, grain boundary penetration, or differential grain-to-grain growth). It is possible that this heterogeneity, made possible by low alloying element content, can cause breakaway corrosion, but further study is warranted.

36 MATERIALS SCIENCE↗

Isothermal oxidation of zirconium using steam

Oxidation of zirconium and its alloys under any atmosphere is generally characterised by a protective and non-protective stage. During the protective stage, the kinetics of oxidation are quasi-parabolic, while the oxide scale formed on the surface of the metal is black, compact, and protective in nature. For the non-protective stage, the oxidation rate becomes linear, while the protective oxide film turns into a deteriorated white scale. Breakaway is known as the transition point from protective to non-protective stage. The actual mechanism leading to breakaway of zirconium is still a matter of controversy, however some of the most common factors affecting breakaway are the following: - Impurities on the metal (Carbon, Oxygen, Nitrogen); - Oxidizing atmosphere (Presence of H{sub 2}O (g) or N{sub 2} (g)); - Sample preparation (Chemically etched or polished); - Temperature (LWR, LOCA). This research investigates the effect of temperature on 'breakaway' when zirconium is oxidized isothermally in steam for 60 min at 800 and 900 deg. C using thermogravimetric and optical microscopic imaging techniques. 1. Steam isothermal oxidations were performed on zirconium at 800 and 900 deg. C using a Thermogravimetric Analyzer (TGA). 2. Log-log plots of mass gain vs time were obtained from thermogravimetric results to calculate the reaction orders (n) and reaction rate constants (K) during oxidation. 3. Results of the kinetics of reaction were correlated with optical microscopic images form Light Microscope (LM) and Scanning Electron Microscope (SEM). Breakaway depends very strongly on temperature. At 800 deg. C, the weight gain followed a cubic-parabolic behaviour with evidence of a protective oxide film. On the other hand, oxidation at 900 deg. C showed signs of breakaway since the oxide film was cracked and oxidation rate was almost linear throughout the reaction.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Analysis of the Surface Morphology and Chemical Composition of Zr-Nb3Sn Alloys with Different Zr Concentrations

In the field of superconducting science, Nb has been the material of choice for Radio Frequency (RF) Cavities for years. However, in recent years Nb3Sn has shown to be a promising alternative to Nb. Its combination of a significantly high superconducting transition temperature and a much higher value of upper critical magnetic field (Hc2), has been the reason the alloy has been so widely studied. This project aims to develop materials to further improve the high magnetic field performance of Nb3Sn by improving its upper critical magnetic field and critical current density (Jc). One way to improve the Jc and the Hc2 is to create more grain boundaries in the Nb3Sn alloy allowing them to trap more magnetic flux lines in the materials. To do this the grains must be made smaller which will naturally cause the formation of more grain boundaries. A common way to create smaller grains is by doping an impurity in the alloy. In this study, Nb3Sn was doped with Zr to form Zr-Nb3Sn alloys. This project investigates the surface properties and chemical composition of Zr-Nb3Sn alloys with varying zirconium concentrations (~0.5% and ~24% Zr). Using Scanning Electron Microscopy (SEM), Energy Dispersive Spectroscopy (EDS), and X-ray Photoemission Spectroscopy (XPS), allowed for the characterization of the differences in surface morphology and elemental composition between samples. SEM images were quantified using ImageJ giving insight into grain distribution. The results indicate that increased Zr concentration creates smaller grains in the Zr-Nb3Sn alloy. Furthermore, the ~ 24% Zr grew nanoscale particles on the surface that are possible oxides. XPS data revealed that as Zr concentration increased, the total Nb oxides (NbOx) thickness decreased. Conversely, as Zr concentration increased, the surface Sn oxides (SnOx) also increased slightly. Quantification via ImageJ of SEM data showed that the ~ 0.5% Zr sample had a grain size of ~ 5300 nm2. These results show that Zr inclusion leads to smaller grain formations, which is promising in the world of superconducting RF cavities for high magnetic field applications.

Sue, Micah↗

Microstructure study of U–35 wt.% Zr alloy after quick annealing at 650 °C

Uranium-35wt.%zirconium (U-35wt.%Zr) alloy was annealed for 1 hour and 24 hours at 650 ºC and characterized to understand the early stage microstructure evolution. Dendritic microstructure with fine (~300 nm in length) α-U precipitates clustered between dendrite branches were observed in the 1-hour annealed sample. After 24-hour annealing 650 ºC, the α-U precipitates coarsened, and the dendritic microstructure disappeared due to microstructure homogenization. Furthermore, microchemical homogenization observed with Energy-Dispersive X-ray Spectroscopy analysis suggests that α-U precipitates are approaching thermodynamic equilibrium in the 24-hour annealed sample. The findings from this study have potential impacts on the manufacturing and computer modeling of metallic nuclear fuel.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Thermal stability of oxidized ultrathin Li films on TZM for plasma facing components

For improved understanding of the behavior of Li plasma facing components (PFCs) in the presence of oxygen impurities, we report on the thermal stability of ultrathin (up to 1.0 nm) LiO x films on a titanium-zirconium-molybdenum (TZM) alloy substrate over the temperature range of 310–1400 K. LiO x films were prepared by either post-oxidation of Li films or Li films deposited on an oxygen-precovered TZM surface. Thermal stability of these films was studied using a combination of temperature programmed desorption (TPD), X-ray photoelectron spectroscopy (XPS), and low-energy ion scattering (LEIS). For post-oxidized Li films, TPD showed that no Li desorption occurred until temperatures above 620 K, and then Li desorbed from the surface via at least three desorption peaks. The O 1s XPS spectra on the post-oxidized films at 310 K indicate the formation of lithium oxide (Li2O) and peroxide/hydroxide (Li 2 O 2 /LiOH). The peroxide/hydroxide converts to oxide after heating to 680 K with no desorption of Li or O 2 , and then this film decomposes to liberate Li into the gas phase while leaving oxygen at the TZM surface. Heating the LiO x films to 1070 K led to a solid-state reaction with surface Mo atoms of the substrate to form a condensed binary lithium molybdenum oxide (LixMoOy) phase, which upon further heating decomposed to liberate gas phase binary lithium molybdenum oxide species. Li deposition on an oxygen-precovered TZM surface formed a complex, highly stable, oxygen rich, Li-O-Mo interfacial oxide. Li desorption from multilayer Li films on oxygen-precovered TZM surfaces occurred in a metallic Li multilayer peak and three other oxide-derived peaks. These results support the improved thermal stability of oxidized lithium as compared to metallic Li and have implications for Mo impurity transport into the plasma at high temperatures.

36 MATERIALS SCIENCE↗

Development of a Castable High Strength Secondary Aluminum Alloy from Recycled Wrought Aluminum Scrap

A new process for recycling scrap AA7075 aerospace alloys directly into a high strength castable secondary alloy is demonstrated. The process involves enhancing the castability of the utilized primary wrought aluminum scrap feedstock by scrap alloy chemistry optimization and zirconium additions in order to mitigate the inherent hot tearing tendency of 7075 alloys. By utilizing the new process, the hot tearing index of scrap AA7075 was reduced from 26 to 4. Defect-free castings were obtained in pilot-scale castings trials. The developed secondary 7075 alloy also satisfied preset target mechanical properties with strength levels exceeding 250 MPa and elongation levels higher than 3%. The validity of the new approach and its readiness for transition to commercial practice was demonstrated by casting cylinder heads directly from the modified 7075 scrap.

36 MATERIALS SCIENCE↗

Evaluation of Sb-Nd and Te-Nd phases within the U-Zr fuel matrix and their interactions with HT9 alloy

Antimony (Sb) and tellurium (Te) were investigated as potential additives for U-10Zr (wt.%) metallic fuel to limit the fuel-cladding chemical interaction (FCCI) with HT-9 alloy. Neodymium (Nd) was utilized to simulate the formation of lanthanide-based solid fission products which are known to play a detrimental role in FCCI. Fuel alloys of U-Zr-Sb-Nd and U-Zr-Te-Nd were evaluated in their annealed condition and compared against their as-cast conditions. Isothermal diffusion couple experiments were performed between U-Zr-Nd, U-Zr-Sb-Nd, and U-Zr-Te-Nd against the cladding alloy HT9 to evaluate the effectiveness of the additives to stabilize Nd within the fuel alloys, as well as investigate the interaction regions that form between the different fuel alloys and HT9. Further, SbNd and Sb 3 Nd 4 , and TeNd are found to be the primary neodymium-based phases formed in the U-Zr-Sb-Nd and U-Zr-Te-Nd alloys, respectively. The zirconium-based phase, Zr 2 Sb, is also found to form within the former alloy. All phases were found to remain stable through the diffusion experiments and exhibited no interaction with HT9 constituent elements. Preferential interaction between Nd with additivities Te and Sb compared to constituting elements in HT9 was further verified based on density functional theory (DFT) calculated enthalpy of mixing.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Casting and Characterization of U-50Zr

Uranium alloyed with 50 wt% zirconium (U-50Zr) is a proposed light water reactor (LWR) nuclear fuel by Lightbridge Corporation (LTBR). The proposed method for making the U-50Zr alloy is to arc-melt master alloys and then remelt in a vacuum induction melter (VIM) to consolidate the material and cast into an intermediate shape. After casting, the material will eventually need to be formed into a desired fuel shape. The work discussed in this report resulted from a joint effort between Ltbr and Pacific Northwest National Laboratory (PNN) to investigate a 500g – 1kg scale casting process to produce the U-50Zr alloy in the desired δ-UZr 2 phase and characterize the impurities and microstructure that result from the casting process. Master alloys were fabricated in an arc melter, then five castings were carried out in a VIM with multiple inert coating and crucible materials to find an appropriate combination. Both ZrO 2 and graphite crucibles were used and different combinations of Y 2 O 3 , CaZrO 3 , and TiC to identify which would contain the molten metal with the least reaction. On each casting, the C, O, N, H impurities were analyzed as well as the phase by x-ray diffraction and microstructure. Of the five castings, two resulted in majority of δ-UZr 2 phase-pure material and had impurity levels within acceptable ranges. The two most successful castings utilized a graphite crucible with a TiC undercoating and a Y 2 O 3 overcoat. The O and N levels were below 1000 ppm and the C content was variable but did not result in measurable carbide formation. The highest success casting resulted in an average of 282 ppm C, 567 ppm O, 217 ppm N and 79 ppm H. This casting's crucible and inert coating material was repeated with slightly different casting parameters and resulted in higher C numbers but similar phase identification. The differences between each casting are discussed and recommendations are made for future experiments to better decide on a casting process to go forward with.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Atom Probe characterization of neutron irradiated commercial ZIRLO® and AXIOM X2® alloys

As part of the Mechanistic Understanding of ZIrconium Corrosion (MUZIC) program, this team has been instrumental to obtain EPRI and Westinghouse sponsorships to prepare the neutron irradiated ZIRLO® and X2® from Vogtle nuclear power plant and ship them from Studsvik’s (Sweden) hot cells to Idaho National Laboratory (INL) to be part of the NSUF library. The uniqueness of these sets of neutron irradiated alloys is that they are at the same two extremes of the fuel cycles, allowing us to study the microchemistry evolution as a function of irradiation doses, exposure time and solute content. Advanced commercial Zirconium-Niobium (Zr-Nb) alloys, such as ZIRLO® and AXIOM®, have been developed by Westinghouse to enhance the corrosion resistance of fuel cladding material for longer service time. This study specifically aims at investigating the neutron irradiation induced Nb redistribution in AXIOM® X2® to understand the effect of neutron irradiation induced microchemistry changes and the irradiation enhanced corrosion resistance observed in ZrNb alloys. The detailed sample information on chemical composition and irradiation is given in shown in Table 1a and 1b respectively. To study the neutron IIP/nanoclusters and Nb concentration in the solid solution, atom probe tomography (APT) is the primary tool to obtain reliable chemical information. APT specimens were prepared in shielded focused ion beam (FIB) at the Irradiated Materials Characterization Laboratory (IMCL) at INL followed by APT analysis at CAES facility using LEAP 4000XR

36 MATERIALS SCIENCE↗

Other Power Reactor Fuels

While oxide fuels have received the bulk of historic interest as power reactor fuels, a range of other uranium compounds and deployment architectures have also been considered and demonstrated to varying degrees. Metal alloys, technical ceramics, and oxycarbide or oxynitride particle fuels are candidates for various power reactor applications. Although in general these families of nuclear fuels have received more limited study than oxides, the benefits of uranium density, favorable thermophysical properties, and other factors have resulted in interest from both the traditional nuclear power industry as well as more recent entrepreneurial efforts. The dominant fuel chemistry issues for these fuel forms differ substantially from those of oxide systems. Synthesis routes, factors that affect fresh fuel properties, and critical aspects of fuel performance are unique to these systems and often dominated by the desired chemical behavior of uranium in each system. This chapter will briefly introduce metallic uranium alloys, specifically uranium-zirconium, non-traditional ceramic fuels such as carbides and nitrides, and oxycarbide/oxynitride particle fuels most familiar as the basis for TRISO fuel designs. A survey of major fuel chemistry issues is provided for each of these families of fuels, with a focus on contemporary challenges and active research avenues.

Nelson, Andrew↗

Fundamental Studies of Tritium Formation and Diffusivity in Pure and Defective Zircaloy-4 Getters

Zirconium (Zr) and its alloys are used as fuel cladding in nuclear reactors. These materials have their low absorption cross-section for thermal neutrons and have good mechanical and thermal properties. In addition, they are used as tritium getters in tritium-producing burnable absorber rods (TPBARs), in the form of nickel-plated Zircaloy-4 tubes. To produce 3 H, the breading blankets such as lithium aluminate are irradiated in pressurized water. 3 H produced in this process is captured by the getter and 3 H reacts chemically with Zr to form metal hydride (ZrTx). The precipitation of metal hydride results in not only the volume increase and hydrogen embrittlement of zircaloy but also changes in getter’s chemical properties. This degrades the getter’s performance. Therefore, understanding the behavior of 3 H (such as diffusion and solubility) in zircaloy is important to understand getter performance.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

First-Principles Studies of Tritium Species Dissociability & Diffusivity Across the Interface of Nickel-Plated Zircaloy-4

Zirconium (Zr) and its alloys (Zircaloy-4) are widely used in nuclear reactors due to their low neutron adsorption cross-section and excellent corrosion resistance. In tritium-producing burnable absorber rods (TPBARs), the metal getter tube located between the cladding and the γ-LiAlO 2 pellets is composed of nickel (Ni)-plated Zircaloy-4, which is used to capture tritium ( 3 H) species (mainly 3 H 2 and 3 H 2 O) generated from γ-LiAlO 2 pellets during irradiation. The 3 H-related products transfer to the surface of metal Ni upon adsorption and dissociation to form new 3 H species and diffuse into the Zircaloy-4 getters to form metal hydrides (Zr 3 H x ). Therefore, exploring 3 H species ( 3 H 2 , 3 H 2 O) dissociation on the surface of Ni and diffusion across the interface of Ni-plated Zircaloy-4 getters can provide a better understanding of 3H species formation and transport from pellets into the getters.

36 MATERIALS SCIENCE↗

Determining the effects of U/Pu ratio on subsolidus phase transitions in U-Pu-Zr metallic fuel alloys

Here, ternary alloys consisting primarily of uranium, plutonium, and zirconium (U-Pu-Zr) are among the leading candidate fuel systems considered for fast spectrum nuclear reactors. Despite historical operation data from the testing of U-Pu-Zr rods in the Experimental Breeder Reactor-II, considerable uncertainty about the evolution of phases and microstructure across the ternary composition space exists. Due to sluggish kinetics and other difficulties in handling metal actinide specimens, quantitative measurements of phase-transitions in U-Pu-Zr alloys remain sparse in scientific literature, with most investigators reporting either phase-transition temperatures or phase identification data, but not both from the same specimens. The purpose of this paper is to critically compare experimental and calculated phase transition data and correlate with the microstructure and phase characterization data of as-cast and annealed U-Pu-Zr alloys. Phase transition peaks were measured using differential scanning calorimetry in the subsolidus regions (723-948 K) of three ternary U-Pu-Zr alloys with the same zirconium concentration but various U/Pu ratios. Overlapping peaks were deconvoluted using a Frazier-Suzuki peak fitting algorithm, and the critical peak temperatures and enthalpies were calculated. In general, increasing concentrations of Pu were associated with enhanced thermal stability of the body-centered cubic γ phase upon both heating and cooling. Experimental phase transition temperatures in this study tended to agree well with the predictions of the established ternary phase diagrams and other reported phase transition temperatures in literature. Additionally, the TAF-ID thermodynamic database was used to calculate a U-Pu-40 at.% Zr pseudobinary diagram as well as ternary diagrams from 773 to 973 K. The equilibrium phase transition temperatures tended to be considerably lower than measured peak temperatures upon both heating and cooling. Recommendations for improving the quality of data in future U-Pu-Zr characterization studies are also discussed.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Evaluation of the anisotropic grain boundaries and surfaces of α -U via molecular dynamics

Alloys based on uranium-zirconium are gaining renewed interest as fuels for the Versatile Test Reactor and a number of microreactor designs. Implementing metallic fuel in reactors creates the need for robust descriptive and predictive fuel performance modeling. Here, the current state of metallic fuel performance modeling relies on empirical equations derived from historical experiments, which may be unreliable when applied outside of their temperature, power, and composition phase space. One area where such data is lacking is the irradiation behavior of alpha -U, specifically tearing and porosity formation at the early stages of irradiation. While grain boundaries likely play a key role in this fuel behavior, relatively little is known about grain boundaries in alpha-U. Thus, we evaluate the grain boundary, surface energy, and work of adhesion of alpha -U utilizing molecular dynamics. Symmetric tilt grain boundaries (STGBs) are analyzed with the tilt plane oriented along each major crystallographic axis, for a total of eighty unique grain boundaries. The effect of temperature, tilt plane, and misorientation angle on interfacial energies are analyzed. The interfacial energies typically increase with temperature and there is significant variance as a function of misorientation angle, irrespective of the tilt plane. At 500 K, the average surface energy (1.23 J/m 2 ) is approximately 1.5 times the grain boundary energy (0.79 J/m 2 ), and the work of adhesion is approximately twice the grain boundary energy (1.68 J/m 2 ). Orientations for the likely formation of twins and likely failure planes are identified.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Determination of Thermal Expansion, Defect Formation Energy, and Defect-Induced Strain of α-U Via ab Initio Molecular Dynamics

Uranium (U) is often alloyed with molybdenum (Mo) or zirconium (Zr) in order to stabilize its high-temperature body-centered cubic phase for use in nuclear reactors. However, in all metallic fuel forms, the α phase of U remains in some fraction. This phase decomposition due to temperature or compositional variance can play an outsized role on fuel performance and microstructural evolution. Relatively little is known about fundamental point defect properties in α -U at non-zero temperatures, from either computational or experimental studies. This work performs the first thorough evaluation of the α phase of U via ab initio molecular dynamics (AIMD). A number of thermophysical properties are calculated as a function of temperature, including equilibrium lattice parameters, thermal expansion, and heat capacity. These results indicate a two-region behavior, with the transition at 400 K. The thermal expansion/contraction in the a / b direction occurs rapidly from 100 up to 400 K, after which a more linear and gradual change in the lattice constant takes place. The volumetric expansion matches experiments quantitatively, but the individual lattice constant expansion only matches experiments qualitatively. Point defect formation energies and induced lattice strains are also determined as a function of temperature, providing insight on defect populations and the fundamentals of irradiation growth in α -U. Interstitials induce significantly more strain than vacancies, and the nature of that strain is highly dependent on the individual lattice directions. The direction of point defect-induced lattice strain is contrary to the irradiation growth behavior of α -U. This work shows that isolated point defects cannot be the primary driving force responsible for the significant irradiation-induced growth of α -U observed experimentally.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗