Search NASA⌕ Search

SEARCH · Search NASA

Results for “aging”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 127 records · Page 7

Minimized aging of isocyanurate-based rigid cellular foams for buildings through tailored barrier facers and optimized formulation

The thermal resistivity (h·ft 2 ·°F/Btu/in.) of closed-cell rigid foam insulation materials significantly decreases over time. Diffusion-tight facers are designed to significantly enhance initial thermal resistivity and long-term thermal performance by preventing gas diffusion into the foam cells and inhibiting the escape of low thermal conductivity blowing agents. In addition to the gas diffusion property of the facer film, adhesion between the foam and the facer is crucial for achieving diffusion-tight bonding. Here, this study addresses the challenge of thermal aging by investigating how facer film properties and foam formulation influence the durability of thermal performance. A systematic evaluation was conducted to understand the effects of polymeric barrier films, surface treatments, facer coverage, and foam matrix rigidity on thermal resistivity over time. Key findings reveal that diffusion-tight facers, particularly those with metallized layers and compatible heat seal layers, significantly reduce gas exchange and improve foam-facer adhesion. The optimized system, incorporating barrier facers and a tailored polyisocyanurate foam formulation, achieved initial and aged thermal resistivity values after 200 days of approximately 8.3 and 7.4 h ft 2 ·°F/Btu/in., respectively representing only a 10 % reduction compared to a 17 % reduction observed in control samples without facers. Notably, polyurethane spray foams with facers exhibited only a 4 % reduction in thermal resistivity, compared to a 23 % decrease in control samples, demonstrating nearly six times better retention of thermal performance. This innovative facer technology presents a promising solution for reducing energy costs and represents a significant advancement in optimizing energy management for building envelopes in future technologies. This technology can also be adapted for other applications that necessitate the preservation of long-term thermal performance.

Wanasinghe, Shiwanka Vidarshi [Oak Ridge National ↗

Mitigating Calendar Aging in Si-NMC Batteries with Advanced Dual-Salt Glyme Electrolytes

In addressing the critical challenge of calendar aging in silicon (Si)-based lithium-ion batteries, this study introduces a groundbreaking strategy utilizing glyme-type dual-salt electrolytes (lithium bis(trifluoromethanesulfonyl)imide [LiTFSI] and lithium difluoro(oxalato)borate [LiDFOB]). These electrolytes are demonstrated to significantly mitigate parasitic reactions and capacity loss in Si-NMC (lithium nickel manganese cobalt oxide) full cells, especially when compared with traditional carbonate-based electrolytes. Further, our exhaustive mechanistic analysis reveals that such electrolytes not only preserve the integrity of the Si anode but also improve the cathode/electrolyte interphases (CEI) through the formation of a conformal coating on the high-voltage cathode surface. This dual-salt approach, enhanced by the addition of a phosphate additive, effectively decelerates calendar aging, marking a substantial advance in the quest for durable and reliable Si-based energy storage technologies. The findings underscore the vital role of electrolyte composition in extending the calendar life of Si batteries, offering an alternative avenue toward maximizing the performance and longevity of next-generation Li-Si batteries.

36 MATERIALS SCIENCE↗

Bio-Oil Impact on Water Diffusion and Durability of Bitumen: Influence of Aging and Salinity

Bio-oils derived from inexpensive biomass offer environmentally friendly options for modifying bitumen for improved durability or rejuvenating aged material, although their impact on bitumen moisture resistance can be mixed. A better understanding of water diffusion into bitumen and its interactions with bio-oil compounds would aid the development of effective bio-oils. In this study, the effect of water exposure on bio-oil-modified bitumen blends was examined by de-wetting contact angle measurements and differential FTIR spectroscopy. The bio-oils improved the anti-stripping behavior of the bitumen but also increased water absorption which could weaken cohesive strength. Short-term thermal aging increased water diffusion for all bitumen blends including the control, probably due to the presence of more oxidized compounds. Negative peaks of alkanes and polar groups in the differential FTIR data suggest the co-diffusion of surfactant molecules towards the bitumen-water interface. Basic pH increased de-wetting of some bitumen blends from silica, possibly by attacking the silica surface itself. The presence of salt in solution altered the bitumen surface composition through the formation of salt complexes with bitumen or bio-oil compounds. In particular, the formation of calcium-carboxylate complexes appeared to greatly improve anti-stripping effects of bio-oils. Water diffusion into most of the bitumen blends was insensitive to pH or salt concentration except for a few notable outliers. Identifying the compounds responsible for increasing or decreasing water diffusion in these outlier cases would be valuable developing future bio-oil formations that avoid or promote those compounds.

Hung, Albert M.↗

Stratification of fluoride uptake among enamel crystals with age elucidated by atom probe tomography

Dental enamel is subjected to a lifetime of de- and re-mineralization cycles in the oral environment, the cumulative effects of which cause embrittlement with age. However, the understanding of atomic scale mechanisms of dental enamel aging is still at its infancy, particularly regarding where compositional differences occur in the hydroxyapatite nanocrystals and what underlying mechanisms might be responsible. Here, we use atom probe tomography to compare enamel from a young (22 years old) and a senior (56 years old) adult donor tooth. Findings reveal that the concentration of fluorine is elevated in the shells of senior nanocrystals relative to young, with less significant differences between the cores or intergranular phases. It is proposed that the embrittlement of enamel is driven, at least in part, by the infusion of fluorine into the nanocrystals and that the principal mechanism is de- and re-mineralization cycles that preferentially erode and rebuild the nanocrystals shells.

36 MATERIALS SCIENCE↗

Effects of catholyte aging on high-nickel NMC cathodes in sulfide all-solid-state batteries

Sulfide solid-state electrolytes (SSEs) in all-solid-state batteries (SSBs) are recognized for their high ionic conductivity and inherent safety. The LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) cathode offers a high thermodynamic potential of approximately 3.8 V vs. Li/Li + and a theoretical specific capacity of 200 mA h g −1 . However, the practical utilization of NMC811 in sulfide SSBs faces significant interfacial challenges. The oxidation instability of sulfide solid electrolytes against NMC811 and the formation of the cathode electrolyte interphase (CEI) during cycling lead to degradation and reduced cell performance. Volumetric changes in NMC during lithiation and de-lithiation can also cause detachment from sulfide electrolytes or internal particle cracking. Despite extensive galvanostatic cycling studies to address the issues, the calendar life of sulfide SSBs remains poorly understood. Here, we systematically studied the effects of four different catholytes on the calendar aging of LiNbO 3 (LNO)-coated NMC811, including Li 6 PS 5 Cl (LPSCl), Li 3 InCl 6 –Li 6 PS 5 Cl (LIC–LPSCl), Li 3 YCl 6 –Li 6 PS 5 Cl (LYC–LPSCl), and Li 10 GeP 2 S 12 (LGPS). Our results indicate that LPSCl provides optimal capacity retention when stored at high state-of-charge (SOC) at room temperature, but the LIC–LPSCl cathode shows significant capacity degradation and chemical incompatibility. We also established an effective electrochemical calendar aging testing protocol to simulate daily usage, enabling quick inference of the calendar life of SSBs. In conclusion, this new testing approach accelerates materials selection strategies for high-nickel NMC composite cathodes in sulfide SSBs.

25 ENERGY STORAGE↗

Strategies for Developing High-Volume Fly Ash Concrete with High Early-Age Strength for Precast Applications

Partial replacement of portland cement with supplementary cementitious materials (SCMs), such as fly ash, is an effective strategy for improving durability and reducing the CO 2 footprint of concrete. However, using high-volume fly ash (HVFA) binders in precast and prestressed concrete is currently limited; largely due to reduced early-age strength development that impedes rapid production and prestressing of precast concrete. To investigate and address this challenge, HVFA mortars with a minimum of 40% fly ash by mass of cementitious materials were developed and tested in this study. Two fresh fly ashes (an ASTM C618 Class F and a Class C) and a landfilled fly ash (Class F) were included. Various strategies for improving the early strength were evaluated, including gypsum optimization, chemical accelerators, steam curing, use of CSA cements, and adding other reactive SCMs like silica fume, calcined clay, and slag cement. Steam curing and the use of CSA cement at high dosages (40% of total binder) were found to be the most successful strategies across all three fly ashes. Additionally, significant improvements were observed with gypsum optimization (for Class C fly ash) and the use of accelerators (for Class F fly ashes), and these strategies are likely to be more feasible considering later-age strength and economic viability. Interestingly, HVFA mixtures made with the landfilled fly ash used in this study were able to achieve high early strengths with water-to-cementitious materials ratio adjustment alone. As a result, these HVFA mixtures were also found to be less responsive to accelerators when compared to the fresh Class F fly ash, highlighting an important distinction between the materials despite the similarity in chemical composition.

42 ENGINEERING↗

Analysis of differential scanning calorimetry data for aged plutonium

Differential scanning calorimetry data for samples of a 52 year old plutonium alloy with 3.3 at. % Ga that were heated beyond the melting point is analyzed using transition state theory to find activation energies for the δ to ε and ε to liquid phase transitions. A Bayesian statistical method involving a Gaussian process model is used to find mean values and confidence intervals for the activation energies. The activation energy for the δ to ε phase transition increases by 3.3 ± 3.8% per decade, relative to the case when all age related plutonium lattice point defects have been removed through annealing. The corresponding increase in activation energy for the ε to liquid transition is shown to be 7.1 ± 1.8% per decade. It is postulated that the change in activation energy with age for both phase transitions is caused, in part, by the accumulation of the same type of lattice point defects associated with the observed increase in elastic bulk modulus over time.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Aging heat treatment design for Haynes 282 made by wire-feed additive manufacturing using high-throughput experiments and interpretable machine learning

Wire-feed additive manufacturing (WFAM) produces superalloys with complex thermal cycles and unique microstructures, often requiring optimized heat treatments. To address this challenge, we present a hybrid approach that combines high-throughput experiments, precipitation simulation, and machine learning to design effective aging conditions for the WFAM Haynes 282 superalloy. Our results demonstrate that the γ’ radius is the critical microstructural feature for strengthening Haynes 282 during post-heat treatment compared with the matrix composition and γ’ volume fraction. New aging conditions at 770°C for 50 hours and 730°C for 200 hours were discovered based on the machine learning model and were applied to enhance yield strength, bringing it on par with the wrought counterpart. This approach has significant implications for future AM alloy production, enabling more efficient and effective heat treatment design to achieve desired properties.

CALPHAD↗

Primeval very low-mass stars and brown dwarfs – VIII. The first age benchmark L subdwarf, a wide companion to a halo white dwarf

ABSTRACT We report the discovery of five white dwarf + ultracool dwarf systems identified as common proper motion wide binaries in the Gaia Catalogue of Nearby Stars. The discoveries include a white dwarf + L subdwarf binary, VVV 1256−62AB, a gravitationally bound system located 75.6$^{+1.9}_{-1.8}$ pc away with a projected separation of 1375$^{+35}_{-33}$ au. The primary is a cool DC white dwarf with a hydrogen dominated atmosphere, and has a total age of $10.5^{+3.3}_{-2.1}$ Gyr, based on white dwarf model fitting. The secondary is an L subdwarf with a metallicity of [M/H] = $-0.72^{+0.08}_{-0.10}$ (i.e. [Fe/H] = $-0.81\pm 0.10$) and $T_{\rm eff}$ = 2298$^{+45}_{-43}$ K based on atmospheric model fitting of its optical to near infrared spectrum, and likely has a mass just above the stellar/substellar boundary. The subsolar metallicity of the L subdwarf and the system’s total space velocity of 406 km s−1 indicates membership in the Galactic halo, and it has a flat eccentric Galactic orbit passing within 1 kpc of the centre of the Milky Way every $\sim$0.4 Gyr and extending to 15–31 kpc at apogal. VVV 1256−62B is the first L subdwarf to have a well-constrained age, making it an ideal benchmark of metal-poor ultracool dwarf atmospheres and evolution.

Zhang, Z. H. (ORCID:000000033047607X)↗

Diagnosis of PV Cell Antireflective Coating Degradation Resulting From Hot-Humid High-Voltage Potential Aging

Corrosion of the antireflective coating on a photovoltaic cell ("ARc corrosion") has previously been observed in studies using hot-humid test conditions with external high-voltage (HV) bias. This study primarily focuses on known vulnerable legacy aluminum back surface field cells in mini-modules (MiMos) put through comparative stepped stress tests. Each cell type had MiMos at +1500 V, -1500 V, or unbiased ("Voc") potential, which were sequentially subjected to test conditions of 60 degrees C/60% relative humidity (RH) for 96 h, as in International Electrotechnical Commission Technical Specification 62804-1; 70 degrees C/70% RH for 200 h; and 85 degrees C/85% RH for 200 h. Characterizations at each step included visual camera and electroluminescence (EL) imaging, colorimetry, and current-voltage curve tracing. Final characterizations included: Suns-Voc, spatial mapping of external quantum efficiency, high-resolution photoluminescence, EL, and dark lock-in thermography imaging. Forensics were performed on extracted cores, including scanning electron microscopy (SEM) with energy-dispersive X-ray spectroscopy (EDS), X-ray photoelectron spectroscopy, and scanning Auger microscopy (SAM). Forensics were also conducted on MiMos from previous studies that underwent stepped HV aging and separate outdoor aged full-sized modules. ARc corrosion was specifically seen for the glass/encapsulant/cell side of the +1500 V (HV+) stressed MiMos and modules. Appearance, color, and reflectance were the most distinguishing characteristics relative to glass corrosion, gridline corrosion and delamination, and other concurrent degradation modes. SEM/EDS and SAM identified the conversion of silicon nitride to hydrated silica, hydrous silica, or hydrated amorphous silica, which preferentially occurred at the edges and tips of the pyramidal textured cell surface.

14 SOLAR ENERGY↗

Are Capacity and Energy Loss Equivalent Metrics for Battery Aging Reporting?

Battery aging in research publications and manufacturer specification sheets for individual cells is commonly reported as capacity (Ah) versus cycle number. However, the key measured quantity in battery-powered devices is energy (Wh), which is derived from integrating capacity with voltage. In this work, we compare the rate of capacity and energy loss across a wide range of Li-ion single-cell cycling studies with different positive electrode chemistries, charge–discharge rates, and temperatures. We find that the relative rate of discharge energy loss varies with cycling conditions. For many cells cycled under moderate conditions, the rate of discharge energy fade is only slightly faster than the rate of discharge capacity fade. However, some cells demonstrated up to a 15% decline in cycle count when 80% energy retention rather than 80% capacity retention was used as the end-of-life metric. These results highlight the importance of reporting cell aging based on energy fade to avoid overestimating battery lifetime in full systems.

batteries↗

Effects cascade debris and helium bubbles on the strength of aged plutonium

The radioactive decay of aging Pu is dominated by α-decay. This persistent α-decay produces crystalline defects in the form of dislocation loops and helium bubbles that evolve with time. Comparable defects are produced in other metallic alloys when subject to neutron irradiation, and these defects are known to modify the plastic deformation of irradiated materials. Models have been developed for these irradiated materials and validated against experimental confirmations of yield strength and the concomitant microstructural evolution. In this paper, we deploy those previously developed models and apply their mechanics to plutonium aging.

Chemical elements↗

Model Scripts for "Old-Aged Groundwater Contributes to Mountain Hillslope Hydrologic Dynamics"

The partitioning of water inputs between deep and shallow groundwater flow paths is a fundamental processes, yet is challenging to observe. Numerical models provide a valuable tool to further develop insights on these groundwater mixing processes. This repository contains scripts to run the ParFlow-CLM and EcoSLIM integrated hydrologic models along the Pumphouse Hillslope in the East River Watershed and associated python scripts to process model outputs. Files includes input decks for the associated models, python scripts, and text and css files to support the model runs and processing. The 2-D hillslope model simulates from 2000 to 2021 using transient forcing conditions from the publicly available NLDAS-2 dataset. We develop an ensemble of models with variable hydrogeologic and soil parameters. Model outputs from the ensemble of runs are compared to to water level observations at the PLM1 and PLM6 wells published at (https://data.ess-dive.lbl.gov/view/doi:10.15485/1866836) and groundwater mean ages published at (https://data.ess-dive.lbl.gov/datasets/doi:10.15485/1960042. The model results are used to evaluate hillslope water mass-balance transience and mixing dynamics between groundwater flow paths with young (<10 year) and old (>10 year) ages.

54 ENVIRONMENTAL SCIENCES↗

AmeriFlux FLUXNET-1F US-Me5 Metolius-first young aged pine

This is the AmeriFlux Management Project (AMP) created FLUXNET-1F version of the carbon flux data for the site US-Me5 Metolius-first young aged pine. This is the FLUXNET version of the carbon flux data for the site US-Me5 Metolius-first young aged pine produced by applying the standard ONEFlux (1F) software. Site Description - Previously old-growth ponderosa pine, clearcut in 1978 and allowed to regenerate naturally. Law et al (2001) Global Change Biology 7, 755-777; Law et al (2001) Agricultural and Forest Meteorology 110, 27-43; Anthoni et al (2002) Agricultural and Forest Meteorology 111, 203-222; Irvine & Law (2002) Global Change biology 8,1183-1194, Irivne et al (2004) Tree Physiology 24,753-763.

Law, Bev [Oregon State University]↗

Fluoropolymer Aging Phenomena

This project aims to investigate structural and morphological changes in fluoropolymers induced by both processing and aging phenomena such as heat, time, and irradiation. Fluoropolymers are an important class of thermoplastics that are broadly used in industry as o-rings and seals when chemical resistance and thermal performance are important. They are also often used in thin film geometries as binders in batteries, insulation layers, water barriers, and anti-fouling coatings. For all of these applications, mechanical integrity and aging are important aspects of their use. Changes in the crystalline morphology are known to impact the mechanical properties of the polymer and can lead to failure. The broad goals of this project are to correlate compositional changes, morphological changes, and mechanical changes. report focuses on the morphological changes that are correlated with nuclear magnetic resonance (NMR), calorimetry and mechanical testing. We plan to compare structure and morphology measurements across complementary bulk and surface techniques. We use in situ atomic force microscopy (AFM) to measure domain shape and crystallization kinetics; in situ NMR to measure crystalline composition; and differential scanning calorimetry (DSC) to measure melting temperatures.

36 MATERIALS SCIENCE↗

Methods and Models for the Study of Aging Effects in Palladium Tritide

We have developed methods to expose milligram-scale samples of metals to tritium for studies of aging effects on material properties, primarily intended for metals that reversibly form hydrides. The tritium decays to helium within the solid, leading to profound changes in microstructural features and macroscopic properties. We present our combined experimental and modeling approach, and provide an example of a palladium foil aged 3 months.

36 MATERIALS SCIENCE↗

Diagnosis of PV Cell Antireflective Coating Degradation Resulting from Hot-Humid, High Voltage Potential Aging

Corrosion of the antireflective coating on a photovoltaic cell ("ARc corrosion") has previously been observed in studies using hot-humid test conditions with external high-voltage (HV) bias. This study primarily focuses on known vulnerable, legacy aluminum back surface field (Al-BSF) cells in mini-modules (MiMos) put through comparative stepped stress tests. Each cell type had MiMos at +1500 V, -1500 V, or unbiased ("Voc") potential, which were sequentially subjected to test conditions of 60deg C/60% relative humidity (RH) for 96 h, as in International Electrotechnical Commission (IEC) Technical Specification 62804-1; 70 deg C/70% RH for 200 h; and 85 deg C/85% RH for 200 h. Characterizations at each step included visual camera and electroluminescence (EL) imaging, colorimetry, and current-voltage (I-V) curve tracing. Final characterizations included: Suns-Voc; spatial mapping of external quantum efficiency (EQE); high-resolution photoluminescence (PL), EL, and dark lock-in thermography (DLIT) imaging. Forensics were performed on extracted cores, including scanning electron microscopy (SEM) with energy-dispersive X-ray spectroscopy (EDS), X-ray photoelectron spectroscopy (XPS), and scanning Auger microscopy (SAM). Forensics were also conducted on MiMos from previous studies that underwent stepped HV aging and separate outdoor aged full-sized modules. ARc corrosion was specifically seen for the glass/encapsulant/cell side of the +1500V (HV+) stressed MiMos and modules. Appearance, color, and reflectance were the most distinguishing characteristics relative to glass corrosion, gridline-corrosion and -delamination as well as other concurrent degradation modes. SEM/EDS and SAM identified conversion of silicon nitride to hydrated silica, hydrous silica, or hydrated amorphous silica, which preferentially occurred at the edges and tips of the pyramidal textured cell surface.

14 SOLAR ENERGY↗

Ratio of 1,275 and 186 keV Gamma Ray Count Rates for Age Determination of Material in UF 6 Cylinders

In this work, a method for using ratios of passive gamma ray measurements to determine the time since the filling of UF 6 cylinders was explored. This method uses the 186 keV gamma ray emitted by 235 U and the 1,275 keV gamma ray that results from interactions of alpha particles in fluorine. Studies were made using MCNP models of both 30B cylinders and smaller 5A cylinders. Results indicate that for enrichments at or above that of natural uranium, this approach may provide a method for determining age up to 10 years or identifying whether the age is greater than 10 years, even if the uranium enrichment is unknown. The calculated results show the same behavior as the results of a recent measurement campaign, indicating the possibility of using this method for real-world cylinders.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗