At least 127 records · Page 7

Structural differences between single crystal and polycrystalline UBe 13

Here, we report on observations of structural and chemical differences between samples of UBe 13 that were synthesised using two different methods. Unexplained discrepancies in properties between samples with differing synthesis had previously been found in this heavy fermion superconductor. A polycrystalline UBe 13 sample was made by arc-melting the constituents. Single crystals were grown using an aluminium flux and had a consistently slightly larger lattice parameter than the polycrystals, which merited further study. Neutron diffraction data were collected at the Lujan Center at LANSCE on the HIPPO diffractometer. Aluminium was detected by inductively coupled plasma mass spectrometry (ICP-MS) in the flux-grown single crystal (0.803 wt%), and small amounts (~0.2 wt%) of thorium were detected in the UBe 13 polycrystalline sample. In order to probe the implications of the presence of Al, calculations by spin-polarised DFT-GGA+U show that the incorporation of Al onto the 96i site (the lowest symmetry site in the structure) is energetically more favourable than on other sites. In general, the trends calculated by DFT for bond lengths and lattice parameter increases are consistent with bond lengths experimentally observed by neutron diffraction, but specific percentage changes with aluminium incorporation may be obscured by the unexpected thorium in the polycrystalline sample. The aggregate of our initial observations suggests that incorporation of aluminium from the flux into single crystal UBe 13 is significant.

36 MATERIALS SCIENCE↗

Investigation of magnetic and electrical transport properties of YMB 4 (M = Cr, Fe, and Co) compounds

We have studied the structural, magnetic, and electrical transport properties of the YMB 4 series of compounds (M= Cr, Fe, and Co). These materials exhibit high stability and possess notable refractory and thermoelectric properties. Furthermore, recent theoretical predictions suggest that some of these compounds may display quantum magnetism and dimer formation among the magnetic ions. We have synthesized almost single phase YMB 4 compounds in the orthorhombic crystal structure (space group Pbam) using arc-melting and annealing. The Rietveld analysis of the room-temperature X-ray diffraction patterns reveals a clear change in the lattice parameter c, which correlates with the atomic radii of Cr, Fe, and Co. The temperature variation of resistivity measured between 2 K and 300 K reveals a metallic electron transport in all three YMB 4 compounds. However, no abrupt change in resistivity due to structural or magnetic phase transitions is observed. Additionally, a weak positive magnetoresistance of 1%–2% has been measured at 2.5 K, the contribution from the metallic impurity cannot be ruled out. The carrier concentration, on the order of 10 21 cm −3 , has been determined using conventional Hall measurements. The thermomagnetic curves recorded between 2 K and 350 K reveal the non-magnetic behavior of all these compounds. However, a small magnetic moment from paramagnetic/ferromagnetic impurity phases is detected at low temperatures. Above room temperature, no magnetic transition associated with the breaking of a dimer is observed.

borides↗

Effects of Al content and annealing on the phases formation, lattice parameters, and magnetization of A l x F e 2 B 2 ( x = 1.0 , 1.1 , 1.2 ) alloys

AlFe 2 B 2 is a ferromagnet with the Curie temperature around 300 K and has the potential to be an outstanding rare-earth free candidate for magnetocaloric applications. However, samples prepared from the melt contain additional phases which affect the functional response of the AlFe 2 B 2 phase. Here, we report on the effects of Al content in samples with the initial (nominal) composition of Al x Fe 2 B 2 where x=1.0, 1.1, and 1.2 prepared by arc-melting followed by suction casting and annealing. The as-cast Al x Fe 2 B 2 alloys contain AlFe 2 B 2 as well as additional phases including the primary solidifying FeB and Al 13 Fe 4 compounds which are ferromagnetic and paramagnetic, respectively, at 300 K. The presence of these phases makes it difficult to extract the intrinsic magnetic properties of AlFe 2 B 2 phase. Annealing of Al x Fe 2 B 2 alloys at 1040°C for 3 days allows for reaction of the FeB with Al 13 Fe 4 to form the AlFe 2 B 2 phase, significantly reduces the amount of additional phases, and results in nearly pure AlFe 2 B2 phase as confirmed with XRD, magnetization, scanning electron microscopy, and electronic transport. The values of the magnetization, effective magnetic moment per Fe atom, specific heat capacity, electrical resistivity and Seebeck coefficient for the AlFe 2 B 2 compound have been established.

36 MATERIALS SCIENCE↗

Influence of Nb alloying on Nb recrystallization and the upper critical field of Nb 3 ⁢Sn

Nb 3 Sn conductors are important candidates for high-field magnets for particle accelerators, and they continue to be widely used for many laboratory and NMR magnets. However, the critical current density, J c , of present Nb 3 Sn conductors declines swiftly above 12-15 T. State-of-the-art Ta- and Ti-doped strands exhibit upper critical field, H c2 , values of ~ 24-26.5 T (4.2 K) and do not reach the FCC target J c , which serves as the present stretch target for Nb 3 Sn development. As recently demonstrated, to meet this goal requires enhanced vortex pinning but an independent and supplementary approach is to significantly enhance H c2 . In this study, we have arc-melted multiple Nb alloys with added Hf, Zr, Ta and Ti and drawn them successfully into monofilament wires to investigate the possibilities of H c2 enhancement through alloying. H c2 (T) was measured for all samples in fields up to 16 T and some up to 31 T. We have found that all alloys show good agreement with the standard Werthamer, Helfand, and Hohenberg (WHH) fitting procedure without the need to adjust the paramagnetic limitation parameter (α) and spin-orbit scattering parameter (λ so ). The evaluation of dH c2 /dT near T c , which is proportional to the electronic specific heat coefficient γ and the normal state resistivity ρn, allows a better understanding of the induced disorder introduced by alloying in the A15 phase. So far, we have observed that Hf alloying of pure Nb can enhance H c2 (0) by 3-4 T to ~28 T, while adding just 1 at. %Hf or Zr into a Nb4Ta base alloy can raise H c2 (0) to ~31 T. Very importantly we find that Hf and Zr raise the alloy recrystallization temperature above the usual A15 reaction temperature range of 650°C – 750°C, thus ensuring denser A15 phase nucleation in the Nb alloy grain boundaries, possibly leading to a more homogeneous A15 phase Sn content and refined A15 grain size. Furthermore, the potential for further advancements in Nb 3 Sn properties is explored in relation to the recrystallization of the Nb alloy and the factors controlling the upper critical field.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Magnetic and Structural Properties of Rapidly Quenched Tetragonal Mn3-xGa Nanostructures

Nanostructured Mn3-x Ga ribbons with x = 0, 0.4, 0.9 and 1.1 were prepared using arc-melting, melt-spinning and annealing. As-spun samples crystallized into hexagonal D0(19) and cubic L2(1) Heusler crystal structures based on the concentration of Mn in Mn3-xGa. Upon vacuum-annealing the samples at 450 degrees C for about 50 hours, both the hexagonal and cubic structures transformed into a tetragonal D0(22) structure. High-temperature x-ray diffraction and high-temperature magnetometry showed that the samples with low Mn content (Mn-1.9 Ga and Mn-2.1 Ga) retain their tetragonal structure up to 850 K but the samples with high Mn concentrations (Mn-2.6 Ga and Mn-3.0 Ga) undergo a structural phase transition from tetragonal to hexagonal phases around 800 K. The magnetic properties of Mn3-x Ga ribbons were very sensitive to Mn concentration, where the magnetization and anisotropy energy increased and the coercivity decreased as x increased from 0 to 1.1. Although the Curie temperatures of Mn-2.6 Ga and Mn-3.0 Ga samples could not be determined because of the structural phase transition, the Curie temperature decreased with increasing x in Mn3-x Ga. The maximum magnetization of 57 emu/g (300 emu/cm(3)) and the coercivity of 6.5 kOe were measured in the Mn-1.9 Ga and Mn-3.0 Ga ribbons, respectively.

Huh, Y↗

High-Performance MnBi Alloy Prepared Using Profiled Heat Treatment

The profiled heat treatment (PHT) method has been used to synthesize MnBi alloys with high-purity low-temperature phase (LTP). In the PHT method, the arc-melted MnBi alloy was remelted then slowly cooled by a pseudo-equilibrium solidification process to promote the formation of LTP phase. The PHT-treated MnBi alloys had an LTP phase up to 94 wt.% and a magnetization of 73 emu/g under a field of 9 T. Scanning electron microscopy showed that there exist some micrometer-sized Mn-rich inclusions in the LTP matrix of the PHT MnBi alloy. The PHT MnBi alloys were crushed into powders with an average size of ~3 μm by low-energy ball milling. These MnBi powders were aligned in an 18 kOe field and warm compacted into a bulk magnet at 300 °C for 30 min. The magnet had a density of 8.2 g/cm3 and magnetic properties of Ms = 6.7 kG, Mr = 5.3 kGs, i Hc = 5 kOe, and (BH)max = 6.1 MGOe

MnBi↗

Microstructure and Hard Magnetic Properties of Sm 1-x Zr x (Fe,Co) 11.3-y Ti 0.7 By Ingots and Thick Melt-Spun Ribbons

Permanent magnets made from Sm(Fe,Co) 12 -based compounds are being actively pursued through nanostructuring and powder metallurgy. This study was aimed at the development of hard magnetic properties in bulk as-cast alloys and in melt-spun alloys for very low wheel speeds. Slower solidification rates and alloying with Zr promote the tetragonal ThMn 12 -type crystal structure, whereas higher solidification rates and alloying with B replace the ThMn 12 structure type with the TbCu 7 structure type. When introduced simultaneously, Zr and B dramatically reduce the alloy solidification rates required for both the refinement of the 1:12 crystallites and their replacement with the 1:7 phase. In bulk arc-melted alloys, this allowed for a microstructure of separated 1:12 crystallites 1–3 μm in size, although, because of the ferromagnetic nature of a minority phase, the coercivity of these fine-grained alloys reached only 0.73 kOe. A moderately accelerated solidification further refined the 1:12 crystallites and increased the coercivity; a Sm 0.7 Zr 0.4 (Fe,Co) 10.8 Ti 0.7 B 0.5 alloy exhibited a coercivity of 1.5 kOe and a maximum energy product of 3.4 MGOe when it was melt-spun into a 0.26-mm-thick ribbon. A more rapid solidification suppressed the 1:12 phase and after annealing at 800–850 °C, the alloys modified with Zr and B developed reasonably high coercivity and maximum energy product even when melt-spun at a wheel speed of 6 m/s. For the above-mentioned alloy, these values were 4.1 kOe and 7.8 MGOe, respectively. Further, a similarly processed very-Sm-lean Sm 0.5 Zr 0.6 (Fe,Co) 10.6 Ti 0.7 B 0.7 alloy exhibited a remanence of 8.8 kG and an energy product of 7.4 MGOe.

36 MATERIALS SCIENCE↗

Assessment of Directionally Solidified Eutectic Sm–Fe(Co)–Ti Alloys as Permanent Magnet Materials

Sm–Fe–Ti and Sm–Fe0.8Co0.2–Ti alloys were prepared via arc-melting and directionally solidified on a water-cooled copper hearth. The as-solidified alloys featured cells of the Sm(Fe,Co,Ti)12–Ti(Fe,Co) 2+δ –(α-Fe) lamellar eutectic. The lamellae of Sm(Fe,Co,Ti)12 phase with a crystal structure of the ThMn12 type were less than 0.2 μm thick, and had their [001] easy-magnetization directions oriented along the temperature gradient of the solidification. The eutectic microstructure led to an increased coercivity, especially in the Co-added alloys. Below 250 °C, this coercivity was found not to vary much with temperature with a temperature coefficient of -0.18 %/°C. However, the modest absolute values, reaching only 0.7 kOe, are insufficient for utilization of the directionally solidified alloys as anisotropic permanent magnets.

36 MATERIALS SCIENCE↗

Applications of analytical electron microscopy to guide the design of boron carbide

Compositional analysis of boron carbide on nanometer length scales to examine or interpret atomic mechanisms, for example, solid-state amorphization or grain-boundary segregation, is challenging. This work reviews advancements in high-resolution microanalysis to characterize multiple generations of boron carbide. First, ζ-factor microanalysis will be introduced as a powerful (scanning) transmission electron microscopy ((S)TEM) analytical framework to accurately characterize boron carbide. Three case studies involving the application of ζ-factor microanalysis will then be presented: (1) accurate stoichiometry determination of B-doped boron carbide using ζ-factor microanalysis and electron energy loss spectroscopy, (2) normalized quantification of silicon grain-boundary segregation in Si-doped boron carbide, and (3) calibration of a scanning electron microscope X-ray energy-dispersive spectroscopy (XEDS) system to measure compositional homogeneity differences of B/Si-doped arc-melted boron carbides in the as-melted and annealed conditions. Overall, the improvement and application of advanced analytical tools have helped better understand processing–microstructure–property relationships and successfully manufacture high-performance ceramics.

36 MATERIALS SCIENCE↗

Superconductivity in the intermetallic compound Zr 5 Al 4

Polycrystalline Zr 5 Al 4 was synthesized using the arc-melting method. Powder X-ray diffraction confirms the previously reported crystal structure of the Ti 5 Ga 4 -type ( P 6 3 / mcm ) with lattice parameters: a = 8.4312(6) Å, and c = 5.7752(8) Å. Electrical resistivity and low-temperature magnetic susceptibility measurements indicate that Zr 5 Al 4 exhibits superconducting behavior below 2K. The normalized heat capacity jump at T c = 1.82 K, Δ C/γT c = 1.50, confirms the bulk superconductivity. The Sommerfeld coefficient γ = 28.5 mJ mol -1 K -2 and the Debye temperature Θ D = 320 K were obtained by fitting the low-temperature heat capacity data. The electron-phonon coupling strength λ el-ph = 0.49 and estimated upper critical field μ 0 H c2 (0) = 1.09 T (dirty limit) suggest that Zr 5 Al 4 is a weakly coupled type-II superconductor. Finally, first-principles calculations show the presence of a van Hove singularity near the Fermi energy.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Uranium Silicide/Nitride Pellet Fabrication Demonstration: Report on Powder Characteristics (Final CRADA Report)

This report details experimental procedures and results of work at the Idaho National Lab to fabricate U 3 Si 2 and UN ceramic powders from their basic elements. The reaction procedure centers on arc melting using a cold, copper hearth. The reacted "buttons" are then ground into powder, and the powder is characterized. The preliminary experiments utilized feeding pieces of metallic U and Si (in the proper ratio) into the arc-melting furnace for melting into "buttons." This melting was repeated several times with the intent of homogenizing the reaction to produce phase pure U 3 Si 2 powder. However, sintering of the pressed-powder at over 1400C showed partial melting and slumping of the pellets. Characterization of the powder using x-ray diffraction (XRD) indicated the crystalline portion of the powder was U 3 Si 2 . However, further investigations indicated a significant portion (12.4%) of the powder was amorphous Si that was transformed into crystalline Si after a period of annealing. Therefore, a greatly improved method of powder fabrication was developed using mixing fine powders of U and Si together, pressing into a pellet, followed by arc melting and grinding into U 3 Si 2 powder. This method was highly successful in producing high phase purity (>98.5% U 3 Si 2 ) powder. One feature of this method is that the fine U powder is made by a hydride/de-hydride cycle. The equipment available at INL only allows for fabrication of relatively small batches, and the method (using INL equipment) is somewhat labor intensive. The powder was used to successfully press and sinter U 3 Si 2 pellets ("Final Report on Pellet Fabrication," INL/LTD-13-29465). A limited attempt was made to fabricate high purity UN powder using the fine U powder made at INL (hydride/de-hydride method) and heating it under flowing nitrogen gas. X-ray diffraction was used to characterize the resulting powder, and a Rietveld refinement was performed on the data. The refinement showed a result of 70.0% UN and 30.0% U 2 N 3 . It is thought that the UN content can be easily increased

Source record↗

Letter Report Documenting Progress of Second Generation ATF FeCrAl Alloy Fabrication

Development of the 2 nd generation ATF FeCrAl alloy has been initiated, and a candidate alloy was selected for trial tube fabrication through hot-extrusion and gun-drilling processes. Four alloys based on Fe-13Cr-4.5Al-0.15Y in weight percent were newly cast with minor alloying additions of Mo, Si, Nb, and C to promote solid-solution and second-phase precipitate strengthening. The alloy compositions were selected with guidance from computational thermodynamic tools. The lab-scale heats of ~ 600g were arc-melted and drop-cast, homogenized, hot-forged and -rolled, and then annealed producing plate shape samples. An alloy with Mo and Nb additions (C35MN) processed at 800°C exhibits very fine sub-grain structure with the sub-grain size of 1-3μm which exhibited more than 25% better yield and tensile strengths together with decent ductility compared to the other FeCrAl alloys at room temperature. It was found that the Nb addition was key to improving thermal stability of the fine sub-grain structure. Optimally, grains of less than 30 microns are desired, with grains up to and order of magnitude in desired produced through Nb addition. Scale-up effort of the C35MN alloy was made in collaboration with a commercial cast company who has a capability of vacuum induction melting. A 39lb columnar ingot with ~81mm diameter and ~305mm height (with hot-top) was commercially cast, homogenized, hot-extruded, and annealed providing 10mm-diameter bar-shape samples with the fine sub-grain structure. This commercial heat proved consistent with materials produced at ORNL at the lab-scale. Tubes and end caps were machined from the bar sample and provided to another work package for the ATF-1 irradiation campaign in the milestone M3FT-14OR0202251.

2nd generation ATF FeCrAl alloy↗

Accelerated development of Zr-containing new generation ferritic steels for advanced nuclear reactors

The mission of the Nuclear Energy Enabling Technologies (NEET) program is to develop crosscutting technologies for nuclear energy applications. Advanced structural materials with superior performance at elevated temperatures are always desired for nuclear reactors, which can improve reactor economics, safety margins, and design flexibility. They benefit not only new reactors, including advanced light water reactors (LWRs) and fast reactors such as the sodium-cooled fast reactor (SFR) that is primarily designed for management of high-level wastes, but also life extension of the existing fleet when component exchange is needed. Developing and utilizing the modern materials science tools (experimental, theoretical, and computational tools) is an important path to more efficient alloy development and process optimization. The ultimate goal of this project is, with the aid of computational modeling tools, to accelerate the development of Zr-bearing ferritic alloys that can be fabricated using conventional steelmaking methods. The new alloys are expected to have superior high-temperature creep performance and excellent radiation resistance as compared to Grade 91. The designed alloys were fabricated using arc-melting and drop-casting, followed by hot rolling and conventional heat treatments. Comprehensive experimental studies have been conducted on the developed alloys to evaluate their hardness, tensile properties, creep resistance, Charpy impact toughness, and aging resistance, as well as resistance to proton and heavy ion (Fe 2+ ) irradiation.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Casting and Characterization of U-50Zr

Uranium alloyed with 50 wt% zirconium (U-50Zr) is a proposed light water reactor (LWR) nuclear fuel by Lightbridge Corporation (LTBR). The proposed method for making the U-50Zr alloy is to arc-melt master alloys and then remelt in a vacuum induction melter (VIM) to consolidate the material and cast into an intermediate shape. After casting, the material will eventually need to be formed into a desired fuel shape. The work discussed in this report resulted from a joint effort between Ltbr and Pacific Northwest National Laboratory (PNN) to investigate a 500g – 1kg scale casting process to produce the U-50Zr alloy in the desired δ-UZr 2 phase and characterize the impurities and microstructure that result from the casting process. Master alloys were fabricated in an arc melter, then five castings were carried out in a VIM with multiple inert coating and crucible materials to find an appropriate combination. Both ZrO 2 and graphite crucibles were used and different combinations of Y 2 O 3 , CaZrO 3 , and TiC to identify which would contain the molten metal with the least reaction. On each casting, the C, O, N, H impurities were analyzed as well as the phase by x-ray diffraction and microstructure. Of the five castings, two resulted in majority of δ-UZr 2 phase-pure material and had impurity levels within acceptable ranges. The two most successful castings utilized a graphite crucible with a TiC undercoating and a Y 2 O 3 overcoat. The O and N levels were below 1000 ppm and the C content was variable but did not result in measurable carbide formation. The highest success casting resulted in an average of 282 ppm C, 567 ppm O, 217 ppm N and 79 ppm H. This casting's crucible and inert coating material was repeated with slightly different casting parameters and resulted in higher C numbers but similar phase identification. The differences between each casting are discussed and recommendations are made for future experiments to better decide on a casting process to go forward with.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

UN Synthesis, Fabrication, and Characterization and UC Oxidation Study in support of Advanced LEU Fuel Concepts

Uranium nitride and carbide-based fuels are proposed for use in advanced LEU fuel systems. This report details recent development work to study synthesis, sintering and fabrication methods for single phase UN in monolithic geometries. These samples were intended to support a variety of irradiation testing conditions by tailoring enrichment, geometry, and compositional requirements. Two methods were under evaluation for synthesizing uranium nitride powder – carbothermic reduction-nitridation (CTR-N) of UO 2 powder feedstock and hydride-dehydride/nitridation (HDN) of uranium metal feedstock. Pellets were fabricated from powder feedstocks via conventional pressing and sintering methods. As-fabricated feedstocks and pellets were evaluated via X-ray diffraction (XRD) for phase purity and sintered materials were characterized for density. Both the CTR N and the HDN methods were successfully demonstrated as an effective process for fabricating phase pure UN. Additionally, results from machining efforts for UN are detailed. This report also contains information on a study trying to elucidate the oxidation mechanisms of sintered uranium carbide samples fabricated from feedstock synthesized via an arc-melting method.

11 - NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Effect of Cooling Rate on Nano-Eutectic Formation in Laser Surface Remelted and Rare Earth Modified Hypereutectic Al-20Si Alloys

Laser Surface Remelting (LSR) was applied to arc-melted Al-20Si-0.2Sr, Al-20Si-0.2Ce, and Al-20Si hypereutectic alloys to refine microstructures. Experiments revealed that microstructures in the melt pool varied from fully eutectic to a mixture of Al dendrites and inter-dendritic eutectic. We calculated cooling rates using the Eagar-Tsai model and correlated cooling rates with characteristic microstructures, revealing that a cooling rate on the order of 104 K/s could lead to maximized fully eutectic microstructure morphology. Due to rapid solidification, the Si composition in the LSR eutectic was measured at 18.2 wt.%, higher than the equilibrium eutectic composition of 12.6 wt.%Si. Compared to Al-20Si, Ce addition had no significant effect on the volume fraction of the fully eutectic structure but refined Si fibers to approximately 30 nm in diameter. Sr addition did not further refine the diameter of eutectic Si fibers compared to Al-20Si but increased the volume fraction of the fully eutectic microstructure morphology. The refinement ratio (φ) of the Si fiber diameter from the bottom of the melt pool to the surface for the three alloys was similar, at around 28%. The established correlation between the cooling rate and the size and morphology of the microstructure within the melt pool will enable tailoring of the microstructure in laser-processed as well as deposited alloys for high strength and plasticity.

36 MATERIALS SCIENCE↗

In-Situ TEM Ion Irradiation Investigations on U3Si2 at LWR Temperatures

The radiation-induced amorphization of U3Si2 was investigated by in-situ transmission electron microscopy ion irradiation. Both arc-melted and sintered U3Si2 specimens were irradiated at room temperature to confirm the similarity in their responsesto radiation. The sintered specimens were then irradiated at 350◦C and 550◦C to examine their amorphization behavior under light water reactor (LWR) conditions. U3Si2 maintains its crystalline structure under irradiation at LWR temperatures. Oxidation of the material was observed at high irradiation doses.

Miaoa, Yinbin↗

Characterization Report on Fuels for NEAMS Model Validation

ABSTRACT U3Si2 has become a material of interest for its potential as an accident tolerant fuel used in commercial light water reactors. In order to better understand the nature of the 5f-electrons and mechanisms that govern electrical and heat transport in U3Si2, and to accurately model this compound at all relevant temperatures we have performed detailed studies of this material by means of the heat capacity, electrical resistivity, Seebeck and Hall effects, and thermal conductivity. Polycrystalline samples of U3Si2 were prepared by arc-melting stoichiometric amounts of elemental U and Si. All the results obtained, especially small magneto-resistivity, large low-temperature heat capacity, and characteristic dependence of the Seebeck coefficient, point to delocalized nature of 5f-electrons in U3Si2. The thermal conductivity is ~8.5 W/m-K at room temperature and we show that the lattice part of the total thermal conductivity is small, with electrons dominating heat transport above 300 K. This knowledge of the details of the heat transport in U3Si2 will be useful for researchers working on modeling and simulations of this new advanced fuel.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗