Fuel cell systems for First Lunar Outpost-reactant storage option

The office of Space, DOE, appointed a Lunar Surface Power Working Group to review candidate systems for the First Lunar Outpost habitat. The working group met for a total of five days in the fall of 1992 and concluded that the candidate involving a photovoltaic unit, a fuel cell, a regenerator to recycle the reactants, and storage of oxygen and hydrogen gases was the most attractive for this application. Most of the volume (97 percent) and weight (63 percent) are taken up by the reactants and their storage tanks. Therefore, in my work for the Group, and in this report, I have concentrated on finding ways to reduce these volumes and weights. Three options were considered: (1) the baseline case considered in the preliminary system design, that of separate high pressure (200 bar) storage tanks; (2) the use of two of the descent storage propellant tanks wrapped with graphite fibers to increase the pressure capability; and (3) the use of cryogenic storage of reactants in the propellant tanks. The first option results in high storage tank mass and volume. The second option saves 90 percent of the volume by making use of the propellant tanks, but it has little if any weight advantages; the weight saved by not providing extra tanks for reactant storage is nearly entirely added back by the weight of the additional material (graphite fibers) to strengthen the propellant tanks. Use of the descent storage propellant tanks for storage of the fuel cell reactants as cryogenic liquids requires a gas liquefaction system. The weight of this system is expected to be less than that of the storage tanks but it would require development and testing to prove its reliability. The solar array would have to be 40 percent larger and the heat projection range would be 170 percent larger than for storage of reactants as high pressure gases. For a high power system (greater than 20 kW) the larger energy storage requirement would probably favor the cryogenic storage option.

Nelson, P. A.↗

LBNF 1.2 MW TARGET: CONCEPTUAL DESIGN & FABRICATION

Fermilab’s Long-Baseline Neutrino Facility (LBNF) will utilize a modified design based on the NuMI low energy target that is reconfigured to accommodate beam operation at 1.2 MW. Achieving this power with a graphite target material and ancillary systems originally rated for 400 kW requires several design changes and R&D efforts related to material bonding and electrical isolation. Target cooling, structural design, and fabrication techniques must address higher stresses and heat loads that will be present during 1.2 MW operation, as the assembly will be subject to cyclic loads and thermal expansion. Mitigations must be balanced against compromises in neutrino yield. Beam monitoring and subsystem instrumentation will be updated and added to ensure confidence in target positioning and monitoring. Remote connection to the target hall support structure must provide for the eventual upgrade to a 2.4 MW target design, without producing excessive radioactive waste or unreasonable exposure to technicians during reconfiguration. Current designs and assembly layouts will be presented, in addition to current findings on processes and possibilities for prototype and final assembly fabrication.

43 PARTICLE ACCELERATORS↗

LBNF 1.2 MW Target: Conceptual Design & Fabrication

Fermilab’s Long-Baseline Neutrino Facility (LBNF) will utilize a modified design based on the NuMI low energy target that is reconfigured to accommodate beam operation at 1.2 MW. Achieving this power with a graphite target material and ancillary systems originally rated for 400 kW requires several design changes and R&D efforts related to material bonding and electrical isolation. Target cooling, structural design, and fabrication techniques must address higher stresses and heat loads that will be present during 1.2 MW operation, as the assembly will be subject to cyclic loads and thermal expansion. Mitigations must be balanced against compromises in neutrino yield. Beam monitoring and subsystem instrumentation will be updated and added to ensure confidence in target positioning and monitoring. Remote connection to the target hall support structure must provide for the eventual upgrade to a 2.4 MW target design, without producing excessive radioactive waste or unreasonable exposure to technicians during reconfiguration. Current designs and assembly layouts will be presented, in addition to current findings on processes and possibilities for prototype and final assembly fabrication.

43 PARTICLE ACCELERATORS↗

LAMMR: A new generation satellite microwave radiometer - Its concepts and capabilities

Definition studies and baseline design are summarized for the proposed, and now discontinued, LAMMR. The instrument is an offset parabolic reflector with Cassegrain feeds. The three-meter aperture reflector, to be constructed using graphite-epoxy technology, rotates continuously at 0.833 rps. The scan drive subsystem includes momentum compensation for the rotating mass which includes the reflector, the support arm and Cassegrain subreflector, feed horns and radiometer. Two total power radiometers are recommended for each frequency, one each for horizontal and vertical polarizations. The selection plan, definition study specifications, LAMMR performance specifications, and predicted accuracies and resolutions after processing are shown.

Walton, W. T.↗

Liquid ammonia chemical lithiation: an approach for high energy and high voltage Si-graphite | Li 1+ x Ni 0.5 Mn 1.5 O 4 Li-ion batteries

Chemical lithiation using lithium metal dissolved in liquid ammonia is introduced for the first time as a viable, potentially scalable method to over-lithiate cathode materials, in this case, the 5V spinel Li 1+ x Ni 0.5 Mn 1.5 O 4 . In this formula the value of x represents the amount of extra lithium inserted into the spinel. Such over-lithiated cathodes can subsequently be used to pre-lithiate high-energy anodes in a lithium-ion battery configuration during the first charge step. Lithiated 5V spinel Li 1+ x Ni 0.5 Mn 1.5 O 4 cathode materials prepared by this technique show higher first delithiation capacities, confirming the chemically inserted lithium is electrochemically active. Full cells with a Si-graphite anode and the Li 1+ x Ni 0.5 Mn 1.5 O 4 (x=0.62) cathode show a 23 % higher reversible capacity in the first cycle than LiNi 0.5 Mn 1.5 O 4 baseline cells, and improved capacity retention. The extra, chemically inserted lithium therefore sacrificially compensates for the loss of lithium at the anode allowing higher utilization of the cathode capacity in following cycles.

25 ENERGY STORAGE↗

Methodologies for Design, Characterization and Testing of Electrolytes that Enable Extreme Fast Charging of Lithium-ion Cells

Selection, testing and validation of electrolyte candidates for Li-ion cells are discussed, based on a 10-minute target for extreme fast charge (XFC). A combination of modeling and laboratory measurements create a timely and synergistic approach to identifying candidate electrolyte formulations. Multi-solvent systems provide a balanced set of properties, wherein lower molecular-weight solvents offer reduced viscosity, increased species diffusivity, and mitigation of concentration polarization at high charge rates. Carefully selected formulations can exhibit peak conductivity and usable conductivity range of two to three times that of the baseline EC-EMC (3:7, wt.) + LiPF 6 . Candidates are also chosen based on stability and longevity within the cell environment. Lab testing coincides with property predictions from the Advanced Electrolyte Model (AEM) and a macro-scale cell model. Furthermore, cell testing utilized coin and pouch cells having NMC532 or NMC811 cathodes with graphite electrodes. Results indicate combinations of low-molecular weight solvents are key for fast-charge electrolytes as they extend the useful conductivity range to both low and higher salt concentrations, and possess higher self-diffusivities compared to conventional solvents. This reduces impacts from concentration polarization. The choice of electrolyte also influences the tendency for lithium metal deposition at the anode, as showcased by experimental and modeling results herein.

25 ENERGY STORAGE↗

Investigation of Glutaric Anhydride as an Electrolyte Additive for Graphite/LiNi 0.5 Mn 0.3 Co 0.2 O 2 Full Cells

The effects of glutaric anhydride (GA) as an electrolyte additive for graphite/LiNi0.5Mn0.3Co0.2O2 full cells operating between 3.0-4.4 V were investigated. Linear scan voltammetry (LSV) revealed that GA preferentially oxidized prior to the carbonate-based electrolyte while Li/graphite half cells revealed that GA can suppress electrolyte decomposition on the graphite electrode giving rise to the bifunctional nature of this additive. The addition of both 0.5 and 1.0 wt% of GA into the carbonate-based electrolyte resulted in superior cycling performance compared to the baseline electrolyte as demonstrated by the slight increase in initial capacities and significant increases in capacity retention over 117 cycles at C/3. Electrochemical impedance spectroscopy (EIS) showed that while the overall impedance of the GA containing cells was higher than the cells with the baseline electrolyte the change in impedance between post-formation and post-cycling was smallest for the cells containing GA. Additionally, X-ray photoelectron spectroscopy (XPS) analysis confirmed that GA decomposed on the cathode surface leading to an increase in oxygen-containing species, a decrease in LiF species and a simultaneous increase in LixPOyFz species. (C) 2016 The Electrochemical Society. All rights reserved.

additive↗

Analytical and experimental investigation of rubbing interaction in labyrinth seals for a liquid hydrogen fuel pump

Cracking of the titanium knife edges on the labyrinth seals of the liquid hydrogen fuel pump in the Space Shuttle main engine is considered. Finite element analysis of the thermal response of the knife edge in sliding contact with the wear ring surface shows that interfacial temperatures can be quite high and they are significantly influenced by the thermal conductivity of the surfaces in rubbing contact. Thermal shock experiments on a test specimen similar to the knife edge geometry demonstrate that cracking of the titanium alloy is possible in a situation involving repeated thermal cycles over a wide temperature range, as might be realized during a rub in the liquid hydrogen fuel pump. High-speed rub interaction tests were conducted using a representative knife edge and seal geometry over a broad range of interaction rates and alternate materials were experimentally evaluated. Plasma-sprayed aluminum-graphite was found to be significantly better than presently used aluminum alloy seals from the standpoint of rub performance. Ion nitriding the titanium alloy knife-edges also improved rub performance compared to the untreated baseline.

Dolan, F. X.↗

Fracture behavior of hybrid composite laminates

The tensile fracture behavior of 15 center-notched hybrid laminates was studied. Three basic laminate groups were tested: (1) a baseline group with graphite/epoxy plies, (2) a group with the same stacking sequence but where the zero-deg plies were one or two plies of S-glass or Kevlar, and (3) a group with graphite plies but where the zero-deg plies were sandwiched between layers of perforated Mylar. Specimens were loaded linearly with time; load, far field strain, and crack opening displacement (COD) were monitored. The loading was stopped periodically and the notched region was radiographed to reveal the extent and type of damage (failure progression). Results of the tests showed that the hybrid laminates had higher fracture toughnesses than comparable all-graphite laminates. The higher fracture toughness was due primarily to the larger damage region at the ends of the slit; delamination and splitting lowered the stress concentration in the primary load-carrying plies. A linear elastic fracture analysis, which ignored delamination and splitting, underestimated the fracture toughness. For almost all of the laminates, the tests showed that the fracture toughness increased with crack length. The size of the damage region at the ends of the slit and COD measurements also increased with crack length.

Kennedy, J. M.↗

Evaluation of Cathode Materials with Lithium-Metal Anodes: Baseline Performance and Protocol Standardization of Coin Cells

The collaborative evaluation of electrode materials across multiple research entities requires standardized electrochemical testing protocols to produce reliable, one-to-one comparisons between different systems of interest. Similar to the work done by Long et al. on protocol standardization for coin-cell testing with graphite anodes [J. Electrochem. Soc., 163, A2999, (2016)], here we introduce two standardized testing protocols designed to quickly evaluate important electrochemical properties of cathode materials using lithium-metal anodes. The two protocols measure kinetic and thermodynamic capacity losses, rate- and voltage-dependent cycling capacities, instabilities at high voltage and high cycling rate, and overpotentials at various states of charge. We then apply these protocols to four commercially available cathode materials to establish benchmark performance metrics that can be used to screen and evaluate new cathode materials.

25 ENERGY STORAGE↗

Structural Response of Compression-Loaded, Tow-Placed, Variable Stiffness Panels

Results of an analytical and experimental study to characterize the structural response of two compression-loaded variable stiffness composite panels are presented and discussed. These variable stiffness panels are advanced composite structures, in which tows are laid down along precise curvilinear paths within each ply and the fiber orientation angle varies continuously throughout each ply. The panels are manufactured from AS4/977-3 graphite-epoxy pre-preg material using an advanced tow placement system. Both variable stiffness panels have the same layup, but one panel has overlapping tow bands and the other panel has a constant-thickness laminate. A baseline cross-ply panel is also analyzed and tested for comparative purposes. Tests performed on the variable stiffness panels show a linear prebuckling load-deflection response, followed by a nonlinear response to failure at loads between 4 and 53 percent greater than the baseline panel failure load. The structural response of the variable stiffness panels is also evaluated using finite element analyses. Nonlinear analyses of the variable stiffness panels are performed which include mechanical and thermal prestresses. Results from analyses that include thermal prestress conditions correlate well with measured variable stiffness panel results. The predicted response of the baseline panel also correlates well with measured results.

Wu, K. Chauncey↗

An experimental investigation of rubbing interaction in labyrinth seals at cryogenic temperature

An experimental program was carried out to address issues related to the observed cracking of the titanium knife edges on the labyrinth seals of the high pressure fuel pump (HPFP) in the Space Shuttle main engine (SSME). Thermal shock experiments were carried out using a jet specimen with geometry similar to the knife edge geometry. These tests demonstrate that cracking of the titanium alloy is possible in a situation involving repeated thermal cycles over a wide temperature range, as might be realized during a rub in the liquid hydrogen fuel pump. High speed rub interaction tests were conducted using a representative knife edge and seal geometry over a broad range of interaction rates. Alternative materials were also experimentally evaluated. These tests provide information which can be used to design improved labyrinth seals for the HPFP of the SSME. In particular, plasma-sprayed aluminum-graphite was found to be significantly better than aluminum alloy seals used at present from the standpoint of rub performance. Ion nitriding of the titanium alloy knife edges was also found to improve rub performance compared with the untreated baseline knife edge material.

Dolan, F. X.↗

Co-Extrusion (CoEx) for Cost Reduction of Advanced High-Energy-and-Power Battery Electrode Manufacturing

Co-Extrusion (CoEx) is a deposition technology developed at PARC that uses engineered fluidic channels to cause multiple streams of dissimilar fluids to impart shape to one another. Here, we describe the use of CoEx to produce structured cathode electrode films to improve electrochemical performance of thick electrode films. CoEx enables us to create structured electrode films that have periodic regions of enhanced ionic conductivity, enabling higher utilization of thicker cathode films at high discharge rates. While increasing electrode thickness is a known method for increasing energy density of battery electrodes, this increase in energy density typically also results in reduced power density. This project, a collaboration between the Palo Alto Research Center, Oak Ridge National Laboratories, and Ford Motor Company, seeks to first validate the benefits of CoEx at the coin cell level, before performing the necessary R&D effort to scale production up to large (10+ Ah) pouch cells that will show increased energy density without a reduction in power density. We used conventional battery materials (commercially available NMC, PVDF, carbon black, and graphite) to produce structured electrodes via CoEx and compared them to thick and thin conventionally produced (unstructured) battery electrodes. CoEx electrodes show improved high rate performance compared to unstructured electrodes, resulting in higher energy density pouch cells compared to the baseline electrode of 7 and 11% in volumetric and gravimetric energy density, respectively. These electrodes also showed substantially improved electrochemical performance at high discharge rates compared to thick conventional electrodes.

25 ENERGY STORAGE↗

Extensive cost reduction studies: Composite empennage component - L-1011 commercial airliner

A series of cover skin laminate studies was conducted. The baseline laminate design is composed of 34 plies with doublers interwoven. This is costly to produce, since the broad goods tape dispersing machine must stop frequently while the doubler plies are inserted by hand during the layup sequence. The use of graphite cloth was investigated for the cover skin. Attention is also given to low resin content prepreg, the selection of optimum tape width, an increase in gap/overlap tolerances, the use of large reusable vacuum bags with mechanical edge seals for production, an integrated laminating center machine, automated hat stiffener processing, a secondary bond assembly process, and a single-stage cure process.

Van Hamersveld, J.↗

Tritium Control and Capture in Salt-Cooled Fission and Fusion Reactors: Status, Challenges, and Path Forward

Three advanced nuclear power systems use liquid salt coolants that generate tritium and thus face the common challenges of containing and capturing tritium to prevent its release to the environment. The fluoride salt–cooled high-temperature reactor (FHR) uses clean fluoride salt coolants and the same graphite-matrix coated-particle fuel as high-temperature gas-cooled reactors. Molten salt reactors (MSRs) dissolve the fuel in a fluoride or chloride salt with release of fission product tritium into the salt. In most FHR and MSR systems, the baseline salts contain lithium where isotopically separated 7 Li is proposed to minimize tritium production from neutron interactions with the salt. The Chinese Academy of Sciences plans to start operation of a 2-MW(thermal) molten salt test reactor by 2020. For high-magnetic-field fusion machines, the use of lithium enriched in 6 Li is proposed to maximize tritium generation—the fuel for a fusion machine. Advances in superconductors that enable higher power densities may require the use of molten lithium salts for fusion blankets and as coolants. Recent technical advances in these three reactor classes have resulted in increased government and private interest and the beginning of a coordinated effort to address the tritium control challenges in 700°C liquid salt systems. In this paper, we describe characteristics of salt-cooled fission and fusion machines, the basis for growing interest in these technologies, tritium generation in molten salts, the environment for tritium capture, models for high-temperature tritium transport in salt systems, alternative strategies for tritium control, and ongoing experimental work. Several methods to control tritium appear viable. Finally, limited experimental data are the primary constraint for designing efficient cost-effective methods of tritium control.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Layered oxide, graphite and silicon-graphite electrodes for Lithium-ion cells: Effect of electrolyte composition and cycling windows

The electrochemical performance of cells with a Li 1.03 (Ni 0.5 Co 0.2 Mn 0.3 ) 0.97 O 2 (NCM523) positive electrode and a blended silicon-graphite (Si-Gr) negative electrode are investigated using various electrolyte compositions and voltage cycling windows. Voltage profiles of the blended Si-Gr electrode show a superposition of graphite potential plateaus on a sloped Si profile with a large potential hysteresis. The effect of this hysteresis is seen in the cell impedance versus voltage data, which are distinctly different for the charge and discharge cycles. We confirm that the addition of compounds, such as vinylene carbonate (VC) and fluoroethylene carbonate (FEC) to the baseline 1.2 M LiPF 6 in ethylene carbonate (EC): ethyl methyl carbonate (EMC) (3:7 w/w) electrolyte, improves cell capacity retention with higher retention seen at higher additive contents. We show that reducing the lower cutoff voltage (LCV) of full cells to 2.5 V increases the Si-Gr electrode potential to 1.12 V vs. Li/Li + ; this relatively-high delithiation potential correlates with the lower capacity retention displayed by the cell. Hence, we show that raising the upper cutoff voltage (UCV) can increase cell energy density without significantly altering capacity retention over 100 charge discharge cycles.

25 ENERGY STORAGE↗

Evaluating electrolyte additives for lithium-ion cells: A new Figure of Merit approach

Electrolyte additives are known to improve the performance of lithium-ion cells. In this work we examine the performance of Li 1.03 Ni 0.5 Mn 0.3 Co 0.3 O 2 -graphite (NMC532/Gr) cells containing combinations of lithium bis(oxalate)borate (LiBOB), vinylene carbonate (VC), trivinylcyclotriboroxane (tVCBO), prop-1-ene-1,3-sultone (PES), phenyl boronic acid ethylene glycol ester (PBE), tris(trimethylsilyl) phosphite (TMSPi), triethylphosphite (TEPi), and lithium difluoro(oxalate)borate (LiDFOB) added to our baseline (1.2M LiPF 6 in EC:EMC, 3:7 w/w) electrolyte. In order to rank performance of the various electrolytes, we developed two separate figures of merit (FOM), which are based on the energy retention and power retention of the cells. Using these two metrics in conjunction, we show that only one of the fifteen electrolyte formulations tested significantly outperforms the baseline electrolyte: this electrolyte contains the 0.25 wt% tVCBO + 1 wt% TMSPi additive mix. Little correlation was observed between the FOMs for energy retention and power retention, which indicates that the mechanisms that govern these performance parameters are likely independent of each other. In conclusion, our FOM approach has general applicability and can be used to develop electrolyte and electrode formulations that prolong the life of lithium-ion batteries.

25 ENERGY STORAGE↗

Demonstration of and future perspective on scaling ultrafast-laser-ablation microstructuring of Li-ion battery electrodes to roll-to-roll production and large-format cells

This work demonstrates integration of an ultrafast laser onto a roll-to-roll machine, the laser structuring of a double-sided, 700 m long roll of graphite battery anode and its subsequent manufacture into 27 Ah prismatic cells. The electrode was ablated with a novel hybrid-microstructure composed of both hexagonally arranged pores for enhanced rate performance and channels for fast electrolyte wetting. Subsequently, this anode and a non-ablated baseline anode are paired with an NMC111 cathode for cell building and electrochemical characterization. Compared to the baseline, laser ablated cells demonstrated a reduction in soaking time of at least 60%, an improvement in fast charge capability with >30% more capacity accepted during 6C charging, and an extension of cycle life of >40% during 0.5C cycling. Further, a perspective is provided on scaling ultrafast laser ablation of battery electrodes to industrial throughputs. Additionally, lessons learned from this pilot-scale demonstration are provided in regards to optical architecture, debris removal, and system control. A techno-economic analysis is used to demonstrate that laser ablation can be integrated into existing electrode manufacturing facilities with only ≈$\$$1.3 per kWh increase (≈2%) in manufacturing cost. Preemptive electrode design for laser ablation is discussed as a further method for enhancing performance. Finally, an analysis of available laser systems and beam-scanning architectures is used to determine design requirements to scale process throughput to a state-of-the-art speed of 50 m min −1 . This analysis demonstrates that laser ablating Li-ion battery electrodes has multiple benefits to manufacturing and battery performance, that the technology already exists to achieve high laser-ablation throughputs, and that integrating ultrafast laser ablation to electrode manufacturing will not create a cost or processing bottleneck.

25 ENERGY STORAGE↗