At least 127 records · Page 7

Stable catalyst layers for hydrogen permeable composite membranes

The present invention provides a hydrogen separation membrane based on nanoporous, composite metal carbide or metal sulfide coated membranes capable of high flux and permselectivity for hydrogen without platinum group metals. The present invention is capable of being operated over a broad temperature range, including at elevated temperatures, while maintaining hydrogen selectivity.

Way, J. Douglas↗

Conductive polymer layers to limit transfer of fuel reactants to catalysts of fuel cells to reduce reactant crossover

An apparatus of an aspect includes a fuel cell catalyst layer. The fuel cell catalyst layer is operable to catalyze a reaction involving a fuel reactant. A fuel cell gas diffusion layer is coupled with the fuel cell catalyst layer. The fuel cell gas diffusion layer includes a porous electrically conductive material. The porous electrically conductive material is operable to allow the fuel reactant to transfer through the fuel cell gas diffusion layer to reach the fuel cell catalyst layer. The porous electrically conductive material is also operable to conduct electrons associated with the reaction through the fuel cell gas diffusion layer. An electrically conductive polymer material is coupled with the fuel cell gas diffusion layer. The electrically conductive polymer material is operable to limit transfer of the fuel reactant to the fuel cell catalyst layer.

36 MATERIALS SCIENCE↗

Methods of fabrication of graphene nanoribbons

Methods of fabricating graphene nanoribbons include depositing a catalyst layer on a substrate. A masking layer is deposited on the catalyst layer. The masking layer and the catalyst layer are etched to form a structure on the substrate, the structure comprising a portion of the catalyst layer and a portion of the masking layer disposed on the catalyst layer, with sidewalls of the catalyst layer being exposed. A graphene layer is formed on a sidewall of the catalyst layer with a carbon-containing gas.

36 MATERIALS SCIENCE↗

Iridium-Doped Nanosized Zn–Al Layered Double Hydroxides as Efficient Water Oxidation Catalysts

Layered double hydroxides (LDHs) are an ideal platform to host catalytic metal centers for water oxidation (WO) owing to the high accessibility of water to the interlayer region, which makes all centers potentially reachable and activated. In this paper, we report the syntheses of three iridium-doped zinc–aluminum LDHs (Ir-LDHs) nanomaterials (1–3, with about 80 nm of planar size and a thickness of 8 nm as derived by field emission scanning electron microscopy and powder X-ray diffraction studies, respectively), carried out in the confined aqueous environment of reverse micelles, through a very simple and versatile procedure. These materials exhibit excellent catalytic performances in WO driven by NaIO 4 at neutral pH and 25 °C, with an iridium content as low as 0.5 mol % (~0.8 wt %), leading to quantitative oxygen yields (based on utilized NaIO 4 , turnover number up to ~10,000). Nanomaterials 1–3 display the highest ever reported turnover frequency values (up to 402 min –1 ) for any heterogeneous and heterogenized catalyst, comparable only to those of the most efficient molecular iridium catalysts, tested under similar reaction conditions. The boost in activity can be traced to the increased surface area and pore volume (>5 times and 1 order of magnitude, respectively, higher than those of micrometric materials of size 0.3–1 μm) estimated for the nanosized particles, which guarantee higher noble metal accessibility. X-ray absorption spectroscopy (XAS) studies suggest that 1–3 nanomaterials, as-prepared and after catalysis, contain a mixture of isolated, single octahedral Ir(III) sites, with no evidence of Ir–Ir scattering from second-nearest neighbors, excluding the presence of IrO 2 nanoparticles. The combination of the results obtained from XAS, elemental analysis, and ionic chromatography strongly suggests that iridium is embedded in the brucite-like structure of LDHs, having four hydroxyls and two chlorides as first neighbors. These results demonstrate that nanometric LDHs can be successfully exploited to engineer efficient WOCs, minimizing the amount of iridium used, consistent with the principle of the noble-metal atom economy.

36 MATERIALS SCIENCE↗

Light-Driven Water Oxidation Using Polyelectrolyte Layer-by-Layer Chromophore–Catalyst Assemblies

Layer-by-Layer (LbL) polyelectrolyte self-assembly occurs by the alternate exposure of a substrate to solutions of oppositely charged polyelectrolytes or polyions. Here, we report the application of LbL to construct chromophore–catalyst assemblies consisting of a cationic polystyrene-based Ru polychromophore (PS-Ru) and a [Ru(tpy)(2-pyridyl-N-methylbenzimidazole) (OH 2 )] 2+ water oxidation catalyst (RuC), codeposited with poly(acrylic acid) (PAA) as an inert polyanion. These assemblies are deposited onto planar indium tin oxide (ITO, Sn:In 2 O 3 ) substrates for electrochemical characterization and onto mesoporous substrates consisting of a SnO 2 /TiO 2 core/shell structure atop fluorine doped tin oxide (FTO) for application to light-driven water oxidation in a dye-sensitized photoelectrosynthesis cell. Cyclic voltammetry and ultraviolet–visible absorption spectroscopy reveal that multilayer deposition progressively increases the film thickness on ITO glass substrates. Under an applied bias, photocurrent measurements of the (PAA/PS-Ru) 5 /(PAA/RuC) 5 LbL films formed on FTO//SnO 2 /TiO 2 mesoporous core–shell electrodes demonstrate a clear anodic photocurrent response. Prolonged photoelectrolysis experiments, with the use of a dual working electrode collector–generator cell, reveal production of O 2 from the illuminated photoanode with a Faradaic efficiency of 22%. Finally, this is the first report to demonstrate the use of polyelectrolyte LbL to construct chromophore–catalyst assemblies for water oxidation.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Few layer graphene synthesis on transition metal ferrite catalysts

Development of cheap, green and up scalable production methods for graphene is one of the most challenging problems in its manufacture on an industrial scale. We report here a large scale substrate-free fluidized bed catalytic chemical vapour deposition (FB-CCVD) process for few layer graphene (FLG) powder production that uses a crystalline oxide catalyst of the general formula A(x)B(3-x)O(4), wherein the FLG layer thickness and domain sizes can be varied. A and B can be chosen from a list of transition elements including Co, Fe, Ni, Mn, Cu and Zn. The best results in terms of activity and selectivity are obtained for the CoxFe3-xO4 system. We also investigated the reaction mechanism using in situ EXAFS and Raman spectroscopy, and electron tomography. Since FB-CCVD processes are already used for industrial scale production of carbon nanotubes, this process should enable the large scale production of free standing FLG in the near future.

Bacsa, Revathi R.↗

Apparatus and Process for Controlled Nanomanufacturing Using Catalyst Retaining Structures

An apparatus and method for the controlled fabrication of nanostructures using catalyst retaining structures is disclosed. The apparatus includes one or more modified force microscopes having a nanotube attached to the tip portion of the microscopes. An electric current is passed from the nanotube to a catalyst layer of a substrate, thereby causing a localized chemical reaction to occur in a resist layer adjacent the catalyst layer. The region of the resist layer where the chemical reaction occurred is etched, thereby exposing a catalyst particle or particles in the catalyst layer surrounded by a wall of unetched resist material. Subsequent chemical vapor deposition causes growth of a nanostructure to occur upward through the wall of unetched resist material having controlled characteristics of height and diameter and, for parallel systems, number density.

Nguyen, Cattien↗

Low cost fuel cell diffusion layer configured for optimized anode water management

A fuel cell comprises a cathode gas diffusion layer, a cathode catalyst layer, an anode gas diffusion layer, an anode catalyst layer and an electrolyte. The diffusion resistance of the anode gas diffusion layer when operated with anode fuel is higher than the diffusion resistance of the cathode gas diffusion layer. The anode gas diffusion layer may comprise filler particles having in-plane platelet geometries and be made of lower cost materials and manufacturing processes than currently available commercial carbon fiber substrates. The diffusion resistance difference between the anode gas diffusion layer and the cathode gas diffusion layer may allow for passive water balance control.

42 ENGINEERING↗

Innovative Method for Reliable Measurement of PEM Water Electrolyzer Component Resistances

Understanding the sheet resistance of porous electrodes is essential for improving the performance of polymer electrolyte membrane (PEM) water electrolyzers and related technologies. Despite its importance, existing methods often fail to provide reliable and comprehensive data, especially for porous materials with complex morphologies and non‐uniform thicknesses. This study introduces a robust and straightforward method for determining the sheet resistance of porous electrodes using a novel probe concept based on industrial printed circuit board (PCB) technology. This probe measures resistance across ten distances, ranging from 250 µm to 2500 µm, enabling local mapping of resistance. The study focuses on the sheet resistance of key components in PEM water electrolyzers, including the gas diffusion layer (GDL), porous transport layer (PTL), and catalyst layers deposited on a membrane. Additionally, an image‐processing‐based method is presented to obtain the thickness distribution of the studied catalyst layers, facilitating a detailed analysis of the electrical in‐plane resistivity with thickness variations. Overall, this methodology has the potential to expedite material integration and bridge the gap between electrode engineering and single‐cell testing, thereby advancing the development of PEM water electrolyzers.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effect of Commercial Gas Diffusion Layers on Catalyst Durability of Polymer Electrolyte Fuel Cells in Varied Cathode Gas Environment

Gas diffusion layers (GDLs) play a crucial role in heat transfer and water management of cathode catalyst layers in polymer electrolyte fuel cells (PEFCs). Thermal and water gradients can accelerate electrocatalyst degradation and therefore the selection of GDLs can have a major influence on PEFC durability. Currently, the role of GDLs in electrocatalyst degradation is poorly studied. Here, we perform electrocatalyst accelerated stress test studies on membrane electrode assemblies (MEAs) prepared using three most commonly used GDLs. The effect of GDLs on electrocatalyst degradation is evaluated in both nitrogen (non-reactive) and air (reactive) gas environments at 100% relative humidity. In situ electrochemical characterization and extensive physical characterization is performed to understand the subtle differences in electrocatalyst degradation and correlated to the use of different GDLs. Overall, no difference is observed in the electrocatalyst degradation due to GDLs based on polarization curves at the end of life. But interestingly, MEA with a cracked microporous layer (MPL) in the GDL exhibited a higher electrocatalyst loading loss, which resulted in a lower and more heterogeneous increase in the average electrocatalyst nanoparticle size.

25 ENERGY STORAGE↗

Suppressing CO formation in low-temperature methanol steam reforming via Ce-modified CuZnGa layered oxide catalysts

Cu-based layered double hydroxides (LDHs) are widely recognized as effective catalysts for low-temperature methanol steam reforming, yet achieving high hydrogen productivity together with near-complete suppression of CO formation remains challenging. Here, we report the synthesis and evaluation of a series of CuZnGa LDH-derived catalysts and Ce-modified analogues prepared via an aqueous miscible organic method, which enables high metal dispersion and precise structural control. The optimized CuZnGa catalyst exhibits a hydrogen production rate of 16.9 µmol H 2 ·g cat −1 ·s −1 at 180 °C with an H 2 /CO ratio exceeding 3500, outperforming many state-of-the-art low-temperature systems. Importantly, the incorporation of small amounts of Ce further suppresses CO formation while maintaining high hydrogen productivity. Combined spectroscopic characterization and density functional theory calculations reveal that Ce is incorporated into the LDH lattice by substituting Ga 3+ sites up to a critical threshold, beyond which highly dispersed CeO x species are formed. These species provide mobile lattice oxygen that participates in a Mars-van Krevelen-type pathway, selectively oxidizing CO and suppressing the reverse water-gas shift reaction. This study establishes a clear relationship between Ce speciation, oxygen mobility, and catalytic selectivity in LDH-derived systems. The resulting catalysts demonstrate the potential of interface-engineered Cu-based materials for efficient low-temperature hydrogen production with minimal CO contamination.

09 BIOMASS FUELS↗

Interfacial engineering via laser ablation for high-performing PEM water electrolysis

A rationalized interfacial design strategy was applied to tailor the porous transport layer (PTL)-catalyst layer (CL) contact and the PTL bulk-phase architecture. Particularly, at the PTL-CL interface, our results reveal that laser ablated sintered titanium power-based PTLs improve electrolyzer performance at both the H2NEW Consortium baseline catalyst loading of 0.4 mgIr cm -2 as well as at the ultra-low catalyst loading of 0.055 mgIr cm -2 . Under ultra-low catalyst loadings, the laser ablated PTL demonstrates maximum reduction of 230 mV compared to the commercial PTL at 4 A cm -2 , and reduces by 68 mV at 3.2 A cm -2 under H2NEW baseline loading. Laser ablation alters the titanium phase at the interface, so it forms more uniform structure like a microporous layer or a backing layer, leading to an increase in the surface area in contact with the catalyst layer while preventing the membrane from deforming into the PTL. Moreover, we reveal that bulk-phase architecture modification of the PTL by ablating patterned pores at the flow field-PTL interface improves mass transport without sacrificing contact at the CL-PTL interface. Overall, laser ablation of the PTL is an effective method to customize interfacial design to enhance proton exchange membrane electrolyzer performance.

08 HYDROGEN↗

Membrane‐electrode assembly design parameters for optimal CO 2 reduction

Commercial-scale generation of carbon-containing chemicals and fuels by means of electrochemical CO 2 reduction (CO 2 R) requires electrolyzers operating at high current densities and product selectivities. Membrane-electrode assemblies (MEAs) have been shown to be suitable for this purpose. In such devices, the cathode catalyst layer controls both the rate of CO 2 R and the distribution of products. In this study, we investigate how the ionomer-to-catalyst ratio (I:Cat), catalyst loading, and catalyst-layer thickness influence the performance of a cathode catalyst layer containing Ag nanoparticles supported on carbon. In this paper, we explore how these parameters affect the cell performance and establish the role of the exchange solution (water vs. CsHCO 3 ) behind the anode catalyst layer in cell performance. We show that a high total current density is best achieved using an I:Cat ratio of 3 at a Ag loading of 0.01–0.1 mg Ag /cm 2 and with a 1.0 M solution of CsHCO 3 circulated behind the anode catalyst layer. For these conditions, the optimal CO partial current density depends on the voltage applied to the MEA. The work also reveals that the performance of the cathode catalyst layer is limited by a combination of the electrochemically active surface area and the degree to which mass transfer of CO 2 to the surface of the Ag nanoparticles and the transport of OH – anions away from it limit the overall catalyst activity. Hydration of the ionomer in the cathode catalyst layer is found not to be an issue when using an exchange solution. The insights gained allowed for a Ag CO 2 R MEA that operates between 200 mA/cm 2 and 1 A/cm 2 with CO faradaic efficiencies of 78–91%, and the findings and understanding gained herein should be applicable to a broad range of CO 2 R MEA-based devices.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

COMPONENT DEVELOPMENT NEEDS FOR THE HYBRID SULFUR ELECTROLYZER

Fiscal year 2008 studies in electrolyzer component development have focused on the characterization of membrane electrode assemblies (MEA) after performance tests in the single cell electrolyzer, evaluation of electrocatalysts and membranes using a small scale electrolyzer and evaluating the contribution of individual cell components to the overall electrochemical performance. Scanning electron microscopic (SEM) studies of samples taken from MEAs testing in the SRNL single cell electrolyzer test station indicates a sulfur-rich layer forms between the cathode catalyst layer and the membrane. Based on a review of operating conditions for each of the MEAs evaluated, we conclude that the formation of the layer results from the reduction of sulfur dioxide as it passes through the MEA and reaches the catalyst layer at the cathode-membrane interface. Formation of the sulfur rich layer results in partial delamination of the cathode catalyst layer leading to diminished performance. Furthermore we believe that operating the electrolyzer at elevated pressure significantly increases the rate of formation due to increased adsorption of hydrogen on the internal catalyst surface. Thus, identification of a membrane that exhibits much lower transport of sulfur dioxide is needed to reduce the quantity of sulfur dioxide that reaches the cathode catalyst and is reduced to produce the sulfur-rich layer. Three candidate membranes are currently being evaluated that have shown promise from preliminary studies, (1) modified Nafion{reg_sign}, (2) polybenzimidazole (PBI), and (3) sulfonated Diels Alder polyphenylene (SDAPP). Testing examined the activity for the sulfur dioxide oxidation of platinum (Pt) and platinum-alloy catalysts in 30 wt% sulfuric acid solution. Linear sweep voltammetry showed an increase in activity when catalysts in which Pt is alloyed with non-noble transition metals such as cobalt and chromium. However when Pt is alloyed with noble metals, such as iridium or ruthenium, the kinetic activity decreases. We recommend further testing to determine if these binary alloys will provide the increased reaction kinetic needed to meet the targets. We also plan to test the performance of these catalyst materials for both proton and sulfur dioxide reduction. The latter may provide another parameter by which we can control the reduction of sulfur dioxide upon transport to the cathode catalyst surface. A small scale electrolyzer (2 cm{sup 2}) has been fabricated and successfully installed as an additional tool to evaluate the effect of different operating conditions on electrolyzer and MEA performance. Currently this electrolyzer is limited to testing at temperatures up to 80 C and at atmospheric pressure. Selected electrochemical performance data from the single cell sulfur dioxide depolarized electrolyzer were analyzed with the aid of an empirical equation which takes into account the overpotential of each of the components. By using the empirical equation, the performance data was broken down into its components and a comparison of the potential losses was made. The results indicated that for the testing conditions of 80 C and 30 wt% sulfuric acid, the major overpotential contribution ({approx}70 % of all losses) arise from the slow reaction rate of oxidation of sulfur dioxide. The results indicate that in order to meet the target of hydrogen production at 0.5 A/cm{sup 2} at 0.6 V and 50 wt% sulfuric acid, identification of a better catalyst for sulfur dioxide oxidation will provide the largest gain in electrolyzer performance.

08 HYDROGEN↗

Modeling Water Uptake and Pt Utilization in High Surface Area Carbon

Local transport losses limit high-current density performance of fuel-cells, especially at low Pt-loadings. Optimizing catalyst-layer structure and material properties to mitigate these losses is critical for wide-scale fuel-cell commercialization. Carbon supports form the primary porous structure of catalyst layers in which Pt particles are deposited and ionomer films are distributed. Unlike non-porous carbon supports, high surface area carbon support is unique in its relative humidity dependent Pt utilization and performance due to presence of Pt particles in the micropores interior of carbon particles. We model water uptake and Pt utilization in catalyst layers with high-surface-area carbon support. Interactions between functional groups on the carbon pore walls and water play a vital role in controlling water uptake from water vapor by catalyst layers. Ionomer is shown to influence proton access in micropores, even though it may not deposit into the micropores.

08 HYDROGEN↗

Integrated Solar-Driven Device with a Front Surface Semitransparent Catalysts for Unassisted CO 2 Reduction

Monolithic integrated photovoltaic-driven electrochemical (PV-EC) artificial photosynthesis is reported for unassisted CO 2 reduction. The PV-EC structures employ triple junction photoelectrodes with a front mounted semitransparent catalyst layer as a photocathode. The catalyst layer is comprised of an array of microscale triangular metallic prisms that redirect incoming light toward open areas of the photoelectrode to reduce shadow losses. Full wave electromagnetic simulations of the prism array (PA) structure guide optimization of geometries and length scales. An integrated device is constructed with Ag catalyst prisms covering 35% of the surface area. The experimental device has close to 80% of the transmittance with a catalytic surface area equivalent 144% of the glass substrate area. Experimentally this photocathode demonstrates a direct solar-to-CO conversion efficiency of 5.9% with 50 h stability. Selective electrodeposition of Cu catalysts onto the surface of the Ag triangular prisms allows CO2 conversion to higher value products enabling demonstration of a solar-to-C 2+ product efficiency of 3.1%. This design featuring structures that have a semitransparent catalyst layer on a PV-EC cell is a general solution to light loss by shadowing for front surface mounted metal catalysts, and opens a route for the development of artificial photosynthesis based on this scalable design approach.

14 SOLAR ENERGY↗

Carbon corrosion in PEM fuel cells during drive cycle operation

One of the major contributors to degradation involves the electrocatalyst, including the corrosion of the carbons used as catalyst supports, which leads to changes in the catalyst layer structure. We have measured and quantified carbon corrosion during drive cycle operation and as a variation of the upper and lower potential limits used during drive cycle operation. The amount of carbon corrosion is exacerbated by the voltage cycling inherent in the drive cycle compared with constant potential operation. The potential gap between upper and lower potentials appears to be more important than the absolute operating potentials in the normal operating potential regime (0.40V to 0.95V) as changes in the measured carbon corrosion are similar when the upper potential was lower compared to raising the lower potential. Catalyst layer thinning was observed during the simulated drive cycle operation which had an associated decrease in catalyst layer porosity. This catalyst layer thinning is not due solely to carbon corrosion, although carbon corrosion likely plays a role; much of this thinning must be from compaction of the material in the catalyst layer. As a result, the decrease in catalyst layer porosity leads to additional performance losses due to mass transport losses.

30 DIRECT ENERGY CONVERSION↗