Search NASA⌕ Search

SEARCH · Search NASA

Results for “crystalline silicon”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 127 records · Page 7

Evaluating Materials Design Parameters of Hole-Selective Contacts for Silicon Heterojunction Solar Cells

Silicon heterojunction (SHJ) solar cell efficiencies are limited by parasitic absorption from the hydrogenated amorphous silicon (a-Si:H) front contact, but this may be mitigated by selecting an alternative carrier selective contact material with a wider band gap. When choosing such a material as the hole-selective contact (“p-layer”), the alignment of the material's valence band edge energy (E VB ) with that of crystalline silicon (c-Si) is an important criterion, but several other material parameters can also influence the band bending at the contact interface. Here, we simulate an (n)c-Si/(i)a-Si:H/p-layer interface to explore the influence of six materials parameters in a variable p-layer on the SHJ performance. We find a strong influence on the fill factor (FF) from thickness, doping, and E VB , and on V OC from the interfacial defect density; notably, optimal E VB is ~ 0.1 eV higher than the valence band edge energy of a-Si:H. Multiparameter sensitivity analyses demonstrate how performance is simultaneously influenced by E VB and doping; thus, both parameters should be optimized alongside one another. To assess the influence of these parameters experimentally, we grow p-type NiO x as a test-case p-layer, which shows that FFs decrease with the oxygen content likely from the increased misalignment of E VB . Although modest efficiencies are achieved experimentally (>7%), what is important is that our model simulates performance trends. With these results, we apply a materials discovery pipeline to suggest new materials (e.g., ZnTe and BeTe) to try as p-layers in the SHJ. This combination of simulations, experiments, and materials discovery informs a better understanding of contact selection in SHJ cells.

14 SOLAR ENERGY↗

Hydrogen Transport from Dielectrics to poly-Si/SiOx Passivating Contacts Measured by Mass Spectrometry and Vibrational Spectroscopy

We demonstrate the relationship between Si solar cell passivation and hydrogen content of various passivating films, including hydrogenated amorphous silicon (a-Si:H), aluminum oxide (Al2O3), silicon nitride (SiNx) and combinations thereof. Through isotopic studies using quadrupole mass spectrometry (QMS), Fourier transform infrared spectroscopy (FTIR), and Raman spectroscopy, we determine how hydrogen content and stability within each type of film relates to final passivation quality of solar cell test structures. Si solar cells using polycrystalline silicon on silicon oxide (poly-Si/SiOx) passivating contacts are at the forefront of Si solar cell research and emerging as top performers within industrial production. Performance of passivating contact Si solar cells is largely determined by a parameter known as the open-circuit voltage Voc, which directly relates to material quality within the bulk of the device and at surfaces. High Voc is achieved when defects within the bulk crystalline silicon (c-Si) and at interfaces are passivated, preventing them from acting as charge carrier recombination centers. One of the most important means of passivating defects within Si solar cells is via hydrogenation, injecting the cells with large amounts of H to satisfy dangling bonds in the bulk and at interfaces. Hydrogen is especially important in deactivating a prevalent defect in industrial p-type devices which leads to decreased device performance over long-term exposure to light, called light-induced degradation (LID). Some of the most common materials used to supply H to devices are a-Si:H, Al2O3, and SiNx, which can contain very large amounts of H. Upon annealing at elevated temperatures, the hydrogen becomes mobile enough to find and disable defect sites. However, too much hydrogen can also be problematic, sometimes leading to an effect called light and elevated temperature induced degradation (LeTID). It has been shown that these films passivate the interfaces of poly-Si passivating contacts differently, leading to differing performance. Though Al2O3 is a well-defined dielectric material, SiNx can have many different values of x depending on precursor gases and deposition conditions. We observe different FTIR and Raman spectra from different SiNx over a range of x values films to determine the bonding environments within them and further correlate the relative concentrations of Si, N, and H to the stability of H within SiNx and the passivation performance of each film. Because deuterium is chemically identical to hydrogen within these systems, but gives different signals in FTIR and Raman spectroscopy as well as in QMS, isotopic substitution can be used as an excellent tool to probe the H within films. In addition to measuring the H and D bonding within films using FTIR and Raman spectroscopy, we will use such isotopic experiments to observe H and D movement out of these hydrogenating films at elevated temperatures using QMS to determine the stability of H bonding within such systems. With these films characterized based on elemental composition, we will relate such measurements to passivation quality of these films and combinations thereof on poly-Si/SiOx contact structures using quasi-steady state photoconductance decay measurements to obtain implied open-circuit voltage (iVoc) and saturation current density J0 values. Such investigations into the performance of different passivating films and film stacks will lead to greater understanding of dielectrics in semiconductor devices, further improvements in passivated contact design, and eventually, greater proliferation of renewable solar energy worldwide.

Al2O3↗

Electro-optic transduction in silicon via gigahertz-frequency nanomechanics

Interfacing electronics with optical fiber networks is key to the long-distance transfer of classical and quantum information. Piezo-optomechanical transducers enable such interfaces by using gigahertz-frequency acoustic vibrations as mediators for converting microwave photons to optical photons via the combination of optomechanical and piezoelectric interactions. However, despite successful demonstrations, efficient quantum transduction remains out of reach due to the challenges associated with hybrid material integration and increased loss from piezoelectric materials when operating in the quantum regime. Here, we demonstrate an alternative approach in which we actuate 5-GHz phonons in a conventional silicon-on-insulator platform. In our experiment, microwave photons resonantly drive a phononic crystal oscillator via the electrostatic force realized in a charge-biased narrow-gap capacitor. The mechanical vibrations are subsequently transferred via a phonon waveguide to an optomechanical cavity, where they transform into optical photons in the sideband of a pump laser field. Operating at room temperature and atmospheric pressure, we measure a microwave-to-optical photon conversion efficiency of 1.72±0.14×10 −7 in a 3.3 MHz bandwidth. Our results mark a stepping stone towards quantum transduction with integrated devices made from crystalline silicon, which promise efficient high-bandwidth operation and integration with superconducting qubits. Additionally, the lack of need for piezoelectricity or other intrinsic nonlinearities makes our approach applicable to a wide range of materials for potential applications beyond quantum technologies.

42 ENGINEERING↗

Study of the Staebler-Wronski degradation effect in a-Si:H based p-i-n solar cell

Conversion of solar energy into electricity using environmentally safe and clean photovoltaic methods to supplement the ever increasing energy needs has been a cherished goal of many scientists and engineers around the world. Photovoltaic solar cells on the other hand, have been the power source for satellites ever since their introduction in the early sixties. For widespread terrestrial applications, however, the cost of photovoltaic systems must be reduced considerably. Much progress has been made in the recent past towards developing economically viable terrestrial systems, and the future looks highly promising. Thin film solar cells offer cost reductions mainly from their low processing cost, low material cost, and choice of low cost substrates. These are also very attractive for space applications because of their high power densities (power produced per kilogram of solar cell pay load) and high radiation resistance. Amorphous silicon based solar cells are amongst the top candidates for economically viable terrestrial and space based power generation. Despite very low federal funding during the eighties, amorphous silicon solar cell efficiencies have continually been improved - from a low 3 percent to over 13 percent now. Further improvements have been made by the use of multi-junction tandem solar cells. Efficiencies close to 15 percent have been achieved in several labs. In order to be competitive with fossil fuel generated electricity, it is believed that module efficiency of 15 percent or cell efficiency of 20 percent is required. Thus, further improvements in cell performance is imperative. One major problem that was discovered almost 15 years ago in amorphous silicon devices is the well known Staebler-Wronski Effect. Efficiency of amorphous silicon solar cells was found to degrade upon exposure to sunlight. Until now their is no consensus among the scientists on the mechanism for this degradation. Efficiency may degrade anywhere from 10 percent to almost 50 percent within the first few months of operation. In order to improve solar cell efficiencies, it is clear that the cause or causes of such degradation must be found and the processing conditions altered to minimize the loss in efficiency. This project was initiated in 1987 to investigate a possible link between metallic impurities, in particular, Ag, and this degradation. Such a link was established by one of the NASA scientists for the light induced degradation of n+/p crystalline silicon solar cells.

Naseem, H. A.↗

Modeling of transport in carrier-selective contacts in silicon heterojunction solar cells

High-performance silicon heterojunction (SHJ) solar cells use carrier-selective contact structures based on hydrogentated amorphous Si (a-Si:H) to maximize collection of photogenerated carriers. The high open circuit voltages observed experimentally in SHJ cells require that the carrier-selective contacts provide selectivity and passivation. However, a microscopic understanding of the dynamics of carrier transport through the a-Si layer is currently lacking. In this paper, we explicitly simulate the transport of holes across the a-Si:H(i) layer using a novel kinetic Monte Carlo approach. The hole-selective contact structure investigated in this paper uses p-type doped a-Si:H(p) and intrinsic a-Si:H(i) on an n-type crystalline silicon wafer, where the selectivity is provided by the a-Si:H(p) and the passivation is provided by the a-Si:H(i). However, in addition to the passivation provided by the a-Si:H(i), this layer also creates a potential barrier to the collection of photogenerated holes. There have been experimental studies in the literature that have suggested that multi-phonon processes are the main transport mechanism that assists in the transport of holes across the intrinsic a-Si:H barrier. Simulations presented here show that multi-phonon injection of holes into the a-Si:H(i) layer is the rate limiting step for transport across the a-Si:H(i) layer. Our results indicate that multi-phonon transport is strongly dependent on the electric field at the a-Si:H(i)/c-Si heterointerface as well. Transport simulations presented in this paper are consistent with experimental findings that multi-phonon processes limit transport across the a-Si:H(i) layer and are responsible for photocurrent suppression at the a-Si:H(i)/c-Si heterointerface when these processes are slower than the associated incident hole flux due to photo-excitation.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Effect of Iron Contamination and Polysilicon Gettering on the Performance of Polysilicon‐Based Passivating Contact Solar Cells

Over the past decade, silicon solar cells with carrier-selective passivating contacts based on polysilicon capping an ultra-thin silicon oxide (commonly known as TOPCon or POLO) have demonstrated promising efficiency potentials and are regarded as an evolutionary upgrade to the PERC (passivated emitter and rear contact) cells in manufacturing. The polysilicon-based passivating contacts also exhibit excellent gettering effects that relax the wafer and cleanroom requirements to some extent. Here, in this work, we experimentally explore the impact of bulk iron contamination and polysilicon gettering on the passivation quality of the polysilicon/oxide structure and the resulting solar cells performance. Results show that both n- and p-type polysilicon/oxide passivating contacts are not affected by iron gettering, demonstrating robust and stable passivation quality. However, for a very high bulk iron contamination (1 × 10 13 cm −3 ), the accumulated iron in the p-type lightly boron-doped emitter in crystalline silicon would degrade the emitter saturation current density. This can cause a reduction in both open-circuit voltage and short-circuit current. Meanwhile, this very high iron content (1 × 10 13 cm −3 ) can further degrade the fill factor and temperature coefficient of the cells. On the other hand, for an initial iron content of 2 × 10 12 cm −3 , which should be well above the iron level in the current industrial Czochralski silicon wafers, the resulting cells demonstrate similar performance as the control group with no intentional iron contamination. This work brings attention to both the benefits of polysilicon gettering effects as well as the potential degradation due to the accumulation of metal impurities in the p-type emitter region.

14 SOLAR ENERGY↗

Field-Aged Glass/Backsheet and Glass/Glass PV Modules: Encapsulant Degradation Comparison

Ethylene vinyl acetate (EVA) is the predominant encapsulant in crystalline-silicon photovoltaic (PV) modules; however, its degradation is a subject of major concern, which causes significant power loss under field conditions. This article presents a comparison of EVA degradation in field-aged PV modules with glass/backsheet (G/B) and glass/glass (G/G) architectures. Modulelevel characterization included UV fluorescence imaging and I-V measurements. Material analytical techniques, including colorimetry, differential scanning calorimetry, thermogravimetric analysis, Fourier transform infrared spectroscopy, and Raman spectroscopy, were performed to correlate the module performance parameters with EVA material properties. An intense EVA discoloration in G/G modules was observed, which was corroborated by higher module Isc and Pmax degradation rates compared with its counterpart G/B modules. Higher power degradation was accompanied by a significant increase in EVA crosslinking, vinyl acetate content, yellowness index, and presence of functional groups containing unsaturated moieties that are linked to degradation products of photothermal reaction, and a higher decrease in the degree of crystallinity. The absence of a polymeric backsheet in hermetically sealed G/G modules, which restricts photobleaching and enhances the entrapment of volatile acetic acid and other degradation by-products, plays a major role in causing higher EVA degradation in G/G modules. This article concludes that EVA might have been a good choice of an encapsulant for the G/B modules over the decades, but it may prove to be an inappropriate choice for the G/G modules because of potential degassing, corrosion, and/or discoloration issues. Ionomers or polyester-based encapsulants like polyolefins could be best suited for G/G modules as it appears to be a current trend in the industry.

14 SOLAR ENERGY↗

Structural, electronic, and optical-absorption properties of 2D Si thin films

Recent experimental studies highlighted the potential of thin-film crystalline silicon (Si) for high-efficiency solar cells. Using density functional theory, we investigated 2D Si thin films across various orientations, thicknesses, and surface structures to elucidate their structure–property relationships. Through surface-energy calculations and Wulff construction, we determined the crystal habit of Si, which aligns with available experimental observations. Electronic-structure calculations underscored the critical role of valence saturation on surfaces in enabling semiconducting behavior in Si thin films, essential for optical applications. From optical-absorption calculations, we identified the surface index exhibiting the highest absorption coefficients for thin films Si solar cell applications.

36 MATERIALS SCIENCE↗

Characterization of Engineered Pinholes in Dielectric Stacks of High-Performance Poly-Silicon Passivating Contacts

Passivating contact structures are expected to be implemented in > 50 % of industrially manufactured silicon photovoltaics produced over the next decade. One type of passivating contact utilizes a c-Si/dielectric/doped poly-Si layer stack. In cases where the dielectric layer/s are thick enough to impede tunneling of charge carriers, it was shown that disruptions (pinholes) in the dielectric are required to facilitate transport.[1] Pinholes in SiOx layers have typically been formed via high temperature annealing that allows localized breakup of this layer. This approach has drawbacks; 1) high temperature annealing increases cost and 2) pinhole formation is sensitive to both the SiOx thickness and wafer surface morphology making control of density and dimensions difficult. Recently, an alternative method of pinhole formation relying on metal assisted chemical etching (MACE) was shown to allow control over pinhole areal densities.[2] Such control is critical as both the density and dimensions of the pinholes determine saturation current density and contact resistivity. The contacts formed with the MACE process are known as polysilicon on locally etched oxide or PLEO and also result in low saturation current densities and low contact resistivity due to SiOx passivation and engineered pinhole enabled charge carrier transport, respectively. Photovoltaic devices with efficiencies greater than 20 % have recently been produced with these contacts, demonstrating the viability of contacts with engineered pinholes. Experimentally, preferential local collection of excess charge carriers has been observed and definitively connected to thermally induced pinholes in thick SiOx layers within c-Si/SiOx/poly-Si contact structures.[3] Recent work has shown that enhanced local collection of excess carriers can result from enhanced diffusion of dopants through pinholes in SiOx layers.[4] This study was restricted to simulation and characterization of poly-Si with the same dopant type as the c-Si substrates. In this work we focus our analysis on boron doped poly-Si with different stacks of dielectric layers (PLEO and PLENO where the N refers to a SiNy layer on top of the SiOx) on n-type crystalline silicon. This provides insight into how engineered pinholes affect charge collection across the p-n junction. Like previous observations of locally enhanced carrier transport through thermally induced pinholes, the EBIC images in Figure 1 shows that engineered pinholes in PLENO (1a) and PLEO (1b) also exhibit locally enhanced carrier transport at pinhole locations (bright spots in the images). We will also present detailed correlative nanoscale structural and chemical analysis using TEM imaging and EELS analysis with sample preparation guided by EBIC imaging. This allows us to connect the density and dimensions of engineered pinholes with charge carrier transport and measured photovoltaic device parameters. Our findings will accelerate the adoption of PLEO and PLENO contacts in industrially manufactured photovoltaic devices.

EBIC↗

Multi–Resonant Mie Resonator Arrays for Broadband Light Trapping in Ultrathin c–Si Solar Cells

Effective photon management is critical to realize high power conversion efficiencies for thin crystalline silicon (c–Si) solar cells. Standard few–100–µm–thick bulk cells achieve light trapping with macroscopic surface textures covered by thin, continuous antireflection coatings. Such sizeable textures are challenging to implement on ultrathin cells. Here, it is illustrated how nanoscale Mie–resonator–arrays with a bimodal size distribution support multiple resonances that can work in concert to achieve simultaneous antireflection and light–trapping across the broad solar spectrum. The effectiveness of these light–trapping antireflection coatings is experimentally demonstrated on a 2.8 µm–thick c–Si solar cell. The measured short–circuit current and corresponding power conversion efficiency are notably improved, achieving efficiencies as high as 11.2%. Measurements of the saturation current density on completed cells indicate that thermal oxides can effectively limit surface recombination. Finally, the presented design principles are applicable to a wide range of solar cells.

14 SOLAR ENERGY↗

Evaluation of Hybrid Perovskite Prototypes After 10-Month Space Flight on the International Space Station

Metal halide perovskites (MHPs) have emerged as a prominent new photovoltaic material combining a very competitive power conversion efficiency that rivals crystalline silicon with the added benefits of tunable properties for multijunction devices fabricated from solution which can yield high specific power. Perovskites have also demonstrated some of the lowest temperature coefficients and highest defect tolerance, which make them excellent candidates for aerospace applications. However, MHPs must demonstrate durability in space which presents different challenges than terrestrial operating environments. To decisively test the viability of perovskites being used in space, a perovskite thin film is positioned in low earth orbit for 10 months on the International Space Station, which was the first long-duration study of an MHP in space. Postflight high-resolution ultrafast spectroscopic characterization and comparison with control samples reveal that the flight sample exhibits superior photo-stability, no irreversible radiation damage, and a suppressed structural phase transition temperature by nearly 65 K, broadening the photovoltaic operational range. Further, significant photo-annealing of surface defects is shown following prolonged light-soaking postflight. Here these results emphasize that methylammonium lead iodide can be packaged adequately for space missions, affirming that space stressors can be managed as theorized.

14 SOLAR ENERGY↗

Advancing reliability assessments of photovoltaic modules and materials using combined-accelerated stress testing

Previously undiscovered failure modes in photovoltaic (PV) modules continue to emerge in field installations despite passing protocols for design qualification and quality assurance. Failure to detect these modes prior to widespread use could be attributed to the limitations of present-day standard accelerated stress tests (ASTs), which are primarily designed to identify known degradation or failure modes at the time of development by applying simultaneous or sequential stress factors (usually two at most). Here, we introduce an accelerated testing method known as the combined-accelerated stress test (C-AST), which simultaneously combines multiple stress factors of the natural environment. Simultaneous combination of multiple stress factors allows for improved identification of failure modes with better ability to detect modes not known a priori. A demonstration experiment was conducted that reproduced the field-observed cracking of polyamide- (PA-) and polyvinylidene fluoride (PVDF)–based backsheet films, a failure mode that was not detected by current design qualification and quality assurance testing requirements. In this work, a two-phase testing protocol was implemented. The first cycle (“Tropical”) is a predominantly high-humidity and high-temperature test designed to replicate harsh tropical climates. The second cycle (“Multi-season”) was designed to replicate drier and more temperate conditions found in continental or desert climates. Testing was conducted on 2 × 2-cell crystalline-silicon cell miniature modules constructed with both ultraviolet (UV)–transmitting and UV-blocking encapsulants. Cracking failures were observed within a cumulative 120 days of the Tropical condition for one of the PA-based backsheets and after 84 days of Tropical cycle followed by 42 days of the Multi-season cycle for the PVDF-based backsheet, which are both consistent with failures seen in fielded modules. In addition to backsheet cracking, degradation modes were observed including solder/interconnect fatigue, various light-induced degradation modes, backsheet delamination, discoloration, corrosion, and cell cracking. The ability to simultaneously apply multiple stress factors may allow many of the test sequences within the standardized design qualification procedure to be performed using a single test setup.

14 SOLAR ENERGY↗

Results from an international interlaboratory study on light‐ and elevated temperature‐induced degradation in solar modules

Abstract This paper reports the results of an international interlaboratory comparison study on light‐ and elevated temperature‐induced degradation (LETID) on crystalline silicon photovoltaic (PV) modules. A large global network of PV module manufacturers and PV testing laboratories collaborated to design a protocol for LETID detection and screen a large and diverse set of prototype modules for LETID. Results across labs indicate the reproducibility of LETID testing is likely within ±1% of maximum power (P MP ). In intentionally engineered LETID‐sensitive modules, mean degradation after the prescribed detection stress is roughly 6% P MP . In other module types the LETID sensitivity is smaller, and in some we observe essentially negligible degradation attributable to LETID. In LETID‐sensitive modules, both open‐circuit voltage (V OC ) and short‐circuit current (I SC ) degrade by a roughly similar magnitude. We observe, as do previous studies, that LETID affects each cell in a module differently. An investigation of the potential mismatch losses caused by nonuniform LETID degradation found that mismatch loss is insignificant compared to the estimated loss of cell I SC , which drives loss of module I SC . Overall, this work has helped inform the creation of a forthcoming standard technical specification for LETID testing of PV modules, IEC TS 63342 ED1, and should aid in the interpretation of results from that and other LETID tests.

14 SOLAR ENERGY↗

Open‐source photovoltaic model pipeline validation against well‐characterized system data

Abstract All freely available plane‐of‐array (POA) transposition models and photovoltaic (PV) temperature and performance models in pvlib‐python and pvpltools‐python were examined against multiyear field data from Albuquerque, New Mexico. The data include different PV systems composed of crystalline silicon modules that vary in cell type, module construction, and materials. These systems have been characterized via IEC 61853‐1 and 61853‐2 testing, and the input data for each model were sourced from these system‐specific test results, rather than considering any generic input data (e.g., manufacturer's specification [spec] sheets or generic Panneau Solaire [PAN] files). Six POA transposition models, 7 temperature models, and 12 performance models are included in this comparative analysis. These freely available models were proven effective across many different types of technologies. The POA transposition models exhibited average normalized mean bias errors (NMBEs) within ±3%. Most PV temperature models underestimated temperature exhibiting mean and median residuals ranging from −6.5°C to 2.7°C; all temperature models saw a reduction in root mean square error when using transient assumptions over steady state. The performance models demonstrated similar behavior with a first and third interquartile NMBEs within ±4.2% and an overall average NMBE within ±2.3%. Although differences among models were observed at different times of the day/year, this study shows that the availability of system‐specific input data is more important than model selection. For example, using spec sheet or generic PAN file data with a complex PV performance model does not guarantee a better accuracy than a simpler PV performance model that uses system‐specific data.

14 SOLAR ENERGY↗

Field‐representative evaluation of PID‐polarization in TOPCon PV modules by accelerated stress testing

Abstract Potential‐induced degradation‐polarization (PID‐p) can reduce module power, but how to project the extent to which PID‐p may occur in field conditions considering the factors of system voltage, condensed moisture, temperature, and illumination has not been clarified. Using tunnel oxide passivated contact (TOPCon) modules, this work demonstrates a method to test full‐size crystalline silicon PV modules for PID‐p to provide field‐representative results. In initial screening tests with positive or negative 1000 V electrical bias applied at 60°C for 96 h using Al foil electrodes on the glass surfaces, the module type exhibited reversible PID‐p only on the front face when the cell circuit was in negative voltage potential. No PID was detected on the rear after testing in either polarity. We then evaluated the PID‐p sensitivity on the front side under different UV irradiances while maintaining the glass surface wet to estimate real‐world susceptibility to PID‐p. The magnitude of the observed behavior was fit using a previously developed charge transfer and depletion by light model. Whereas power loss with −1000 V applied to the cell circuit at 60°C for 96 h in the dark was about 30%, testing the module front under 0.051 W·m −2 nm −1 at 340 nm UVA irradiation using fluorescent tubes, the mean degradation was only 3%. When the modules were tested in the dark for PID‐p with in situ dark current–voltage (I‐V) characterization, the thermal activation energy for degradation was 0.71 eV; for recovery in the dark, it was 0.58 eV. Whereas recovery from the degraded state at 60°C in the dark without voltage bias was 5% absolute in 38 h, rapid recovery of about 5% absolute was observed with 1000 W·s/m 2 exposure at 25°C using a flash tester.

14 SOLAR ENERGY↗

Scalable Two–Step Production of High–Efficiency Perovskite Solar Cells and Modules

Perovskite solar cells (PSCs) fabricated in laboratories have already achieved power conversion efficiency (PCE) comparable to market-dominant crystalline silicon solar cells. However, this promising photovoltaic technology suffers from severe loss of PCE during scaling up, limiting its progress toward commercialization. One critical question is to develop scalable, low-cost, high throughput, and well-controlled production methods to deposit high-quality perovskite films. Among various approaches, two-step sequential deposition methods have their unique advantages but have been long overlooked. This review provides an overview of two-step methods for fabricating efficient and stable perovskite solar modules (PSMs). We first discuss the mechanisms of two-step perovskite conversion and advanced engineering approaches to modulate the perovskite formation process. We survey the progress of efficient PSCs prepared by different two-step methods and compare the advantages and disadvantages of each method for scalable production of PSMs. Particularly, we highlight that the vapor-based two-step methods are promising for high-throughput in-line production of PSMs. Finally, we provide insights into the challenges and outlook of the industrialization of two-step processes for producing PSMs.

14 SOLAR ENERGY↗

Spectral Effects on the Energy Harvesting Efficiency of Two- and Four-Terminal Tandem Photovoltaics

In this work, the effect of a varying spectral irradiance and top cell bandgap on the energy harvesting efficiency of two-terminal (2T) and four-terminal (4T) perovskite//silicon tandem solar cells under outdoor operating conditions is investigated. For the comparison, an optoelectronic model employing a 1 year outdoor data set for a 4T mechanical stacked gallium arsenide (GaAs) on crystalline silicon (Si) tandem device is first validated. Then, the verified model is used to simulate perovskite//silicon tandem devices with a varying perovskite top cell bandgap for a location in Golden, Colorado, USA. Here, a spectral binning method to efficiently reduce and improve the visualization of the 1 min-resolved environmental data while maintaining the simulation accuracy is introduced. The findings reveal that, for a device that is current matched under standard testing conditions, the annual spectral deviation reduces the energy harvesting efficiency by only 2% rel . When additional realistic losses for the 4T are taken into account, 2T devices are shown to have an energy-harvesting efficiency that is at parity or higher. Deviations in the top cell bandgap are more than 0.1 eV from current matching result in a reduced energy harvesting efficiency of more than 5% rel for the 2T tandem device.

14 SOLAR ENERGY↗

Measurement of Contact Resistivity In Symmetric Polycrystalline Si/SiO x /Monocrystalline Si Test Structures Using Variable Light Illumination

While different methods exist to determine the contact resistivity in semiconductor devices, these methods are limited to measurement of the majority carrier contacts. The measurement of p‐ or n‐type contacts on n‐ or p‐type crystalline silicon, respectively, is challenging due to the blocking diode formed by the p–n junction. In this article, we address this problem for tunneling oxide passivating contacts used in high‐efficiency Si solar cells. We propose a universal method to extract contact resistivity on symmetric test structures with polycrystalline silicon on SiO x (poly‐Si/SiO x ) passivating contacts under illumination, both for p–n and high–low‐junction passivated contacts. In this method, we demonstrate that the total contact resistance of each cell grid finger to the base wafer is governed by its effective contact area, defined by the transfer length extending from both sides of the finger. Therefore, the grid contact resistance of a poly‐Si contact depends on the ratio of the doped poly‐Si sheet resistance to the tunneling contact resistivity.

14 SOLAR ENERGY↗