Suppressing Cation Migration in Triple-Cation Lead Halide Perovskites

Ion migration represents an intrinsic instability of metal halide perovskite solar cells. In this work, we show that triple-cation FA x MA y Cs 1–x–y PbI 3 [FA + = (NH 2 ) 2 CH + , MA + = CH 3 NH 3 + ] active layers with mixed orthorhombic, post-perovskite (δ ortho -CsPbI 3 ), and cubic perovskite (α) phases (i.e., α/δ-phase FA x MA y Cs 1–x–y PbI 3 ) exhibit improved cation stability against applied bias relative to pure α-phase perovskites (i.e., FA 0.85 Cs 0.15 PbI 3 and FA 0.76 MA 0.15 Cs 0.09 PbI 3 ). Infrared photothermal heterodyne imaging and time-of-flight secondary ion mass spectrometry are used to visualize exclusive α-phase perovskite lateral device A + cation accumulation (depletion) at perovskite negative (positive) electrode interfaces. The resulting compositional heterogeneities lead to degradation. Operational stability testing of solar cells reveals similar degradation behavior; α/δ-phase FA x MA y Cs 1–x–y PbI 3 lateral devices/solar cells, by contrast, show improved stabilities. Enhanced α/δ-FA x MA y Cs 1–x–y PbI 3 stability is rationalized by δortho-phase inclusions, acting as barriers through which A + cations do not easily migrate. This study thus provides new insights into cation migration in FA x MAyCs 1–x–y PbI 3 perovskites and suggests a materials design strategy toward suppressing cation instabilities in hybrid perovskites.

14 SOLAR ENERGY↗

A Silicon-Based Heterojunction Integrated with a Molecular Excited State in a Water-Splitting Tandem Cell

Semiconductor-based photocathodes with high light-absorption capability are of interest in the production of solar fuels, but many of them are limited by low efficiencies due to rapid interfacial back electron transfer. We demonstrate here that a nanowire-structured p-type Si (p-Si) electrode, surface-modified with a perylene-diimide derivative (PDI’), can undergo photo-reduction of a surface-bound, water reduction catalyst towards efficient H2 evolution under a low applied bias. At the electrode interface, the PDI’ layer converts green light into high-energy holes at its excited state for extraction of photogenerated electrons at the photoexcited p-Si. The photogenerated electrons at the reduced PDI’ are subsequently transferred to a surface-bound, molecular H2-evolution catalyst. Involvement of the photoexcited PDI’ enables effective redox separation between the electrons at the reduced catalyst and the holes at the valence band of p-Si. The heterojunction photocathode was used in a tandem cell by coupling with a dye-sensitized photoanode for solar-driven water splitting into H2 and O2.

water-splitting↗

Micron-gap spacers with ultrahigh thermal resistance and mechanical robustness for direct energy conversion

Abstract In thermionic energy converters, the absolute efficiency can be increased up to 40% if space-charge losses are eliminated by using a sub-10-µm gap between the electrodes. One practical way to achieve such small gaps over large device areas is to use a stiff and thermally insulating spacer between the two electrodes. We report on the design, fabrication and characterization of thin-film alumina-based spacers that provided robust 3–8 μm gaps between planar substrates and had effective thermal conductivities less than those of aerogels. The spacers were fabricated on silicon molds and, after release, could be manually transferred onto any substrate. In large-scale compression testing, they sustained compressive stresses of 0.4–4 MPa without fracture. Experimentally, the thermal conductance was 10–30 mWcm −2 K −1 and, surprisingly, independent of film thickness (100–800 nm) and spacer height. To explain this independence, we developed a model that includes the pressure-dependent conductance of locally distributed asperities and sparse contact points throughout the spacer structure, indicating that only 0.1–0.5% of the spacer-electrode interface was conducting heat. Our spacers show remarkable functionality over multiple length scales, providing insulating micrometer gaps over centimeter areas using nanoscale films. These innovations can be applied to other technologies requiring high thermal resistance in small spaces, such as thermophotovoltaic converters, insulation for spacecraft and cryogenic devices.

42 ENGINEERING↗

Insight into induced charges at metal surfaces and biointerfaces using a polarizable Lennard–Jones potential

Metallic nanostructures have become popular for applications in therapeutics, catalysts, imaging, and gene delivery. Molecular dynamics simulations are gaining influence to predict nanostructure assembly and performance; however, instantaneous polarization effects due to induced charges in the free electron gas are not routinely included. Here we present a simple, compatible, and accurate polarizable potential for gold that consists of a Lennard–Jones potential and a harmonically coupled core-shell charge pair for every metal atom. The model reproduces the classical image potential of adsorbed ions as well as surface, bulk, and aqueous interfacial properties in excellent agreement with experiment. Induced charges affect the adsorption of ions onto gold surfaces in the gas phase at a strength similar to chemical bonds while ions and charged peptides in solution are influenced at a strength similar to intermolecular bonds. The proposed model can be applied to complex gold interfaces, electrode processes, and extended to other metals.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

An ultrathin ionomer interphase for high efficiency lithium anode in carbonate based electrolyte

High coulombic efficiency and dendrite suppression in carbonate electrolytes remain challenges to the development of high-energy lithium ion batteries containing lithium metal anodes. Here we demonstrate an ultrathin (≤100 nm) lithium-ion ionomer membrane consisting of lithium-exchanged sulfonated polyether ether ketone embedded with polyhedral oligosilsesquioxane as a coating layer on copper or lithium for achieving efficient and stable lithium plating-stripping cycles in a carbonate-based electrolyte. Operando analyses and theoretical simulation reveal the remarkable ability of the ionomer coating to enable electric field homogenization over a considerably large lithium-plating surface. The membrane coating, serving as an artificial solid-electrolyte interphase filter in minimizing parasitic reactions at the electrolyte-electrode interface, enables dendrite-free lithium plating on copper with outstanding coulombic efficiencies at room and elevated (50 °C) temperatures. The membrane coated copper demonstrates itself as a promising current collector for manufacturing high-quality pre-plated lithium thin-film anode.

25 ENERGY STORAGE↗

High-entropy electrolytes for practical lithium metal batteries

Electrolyte engineering is crucial for improving battery performance, particularly for lithium metal batteries. Recent advances in electrolytes have greatly improved cyclability by enhancing electrochemical stability at the electrode interfaces, but concurrently achieving high ionic conductivity has remained challenging. Here we report an electrolyte design strategy for enhanced lithium metal batteries by increasing the molecular diversity in electrolytes, which essentially leads to high entropy electrolytes (HEEs). We find that in weakly solvating electrolytes, the entropy effect reduces ion clustering while preserving the characteristic anion-rich solvation structures, which is characterized by synchrotron-based X-ray scattering and molecular dynamics simulations. Electrolytes with smaller- sized clusters exhibit a 2-fold improvement in ionic conductivity compared to conventional weakly- solvating electrolytes, enabling stable cycling at high current densities up to 2C (6.2 mA cm -2 ) in anode- free LiNi 0.6 Mn 0.2 Co 0.2 (NMC622)||Cu pouch cells. In conclusion, the efficacy of the design strategy is verified by performance improvements in three disparate weakly solvating electrolyte systems.

25 ENERGY STORAGE↗

The critical role of configurational flexibility in facilitating reversible reactive metal deposition from borohydride solutions

Development of calcium metal batteries has been historically frustrated by a lack of electrolytes capable of supporting reversible calcium electrodeposition. In this paper, we report the study of an electrolyte consisting of Ca(BH 4 ) 2 in tetrahydrofuran (THF) to gain important insight into the role of the liquid solvation environment in facilitating the reversible electrodeposition of this highly reactive, divalent metal. Through interrogation of the Ca 2+ solvation environment and comparison with Mg 2+ analogs, we show that an ability to reversibly electrodeposit metal at reasonable rates is strongly regulated by dication charge density and polarizability. Our results indicate that the greater polarizability of Ca 2+ over Mg 2+ confers greater configurational flexibility, enabling ionic cluster formation via neutral multimer intermediates. Increased concentration of the proposed electroactive species, CaBH 4 + , enables rapid and stable delivery of Ca 2+ to the electrode interface. Finally, this work helps set the stage for future progress in the development of electrolytes for calcium and other divalent metal batteries.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Understanding the switching mechanism of interfacial phase change memory

Phase Change Memory (PCM) is a top candidate for next generation data storage, but it typically suffers from high switching (RESET) current density (20–30 MA/cm 2 ). Interfacial Phase Change Memory (IPCM) is a type of PCM using multilayers of Sb 2 Te 3 /GeTe, with up to 100× lower reported RESET current compared to the standard Ge 2 Sb 2 Te 5 -based PCM. Several hypotheses involving fundamentally new switching mechanisms have been proposed to explain the low switching current densities, but consensus is lacking. Here, we investigate IPCM switching by analyzing its thermal, electrical, and fabrication dependencies. First, we measure the effective thermal conductivity (~0.4 W m -1 K -1 ) and thermal boundary resistance (~3.4 m 2 K GW -1 ) of Sb 2 Te 3 /GeTe multilayers. Simulations show that IPCM thermal properties account only for an ~13% reduction of current vs standard PCM and cannot explain previously reported results. Interestingly, electrical measurements reveal that our IPCM RESET indeed occurs by a melt-quench process, similar to PCM. Finally, we find that high deposition temperature causes defects including surface roughness and voids within the multilayer films. Thus, the substantial RESET current reduction of IPCM appears to be caused by voids within the multilayers, which migrate to the bottom electrode interface by thermophoresis, reducing the effective contact area. These results shed light on the IPCM switching mechanism, indicating that an improved control of layer deposition is necessary to obtain reliable switching.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Investigation of SiO x anode fading mechanism with limited capacity cycling

Silicon suboxide (SiO x ) is one of the promising anode materials for the next-generation lithium-ion batteries. However, SiO x has a severe capacity fading problem during cycling. It is thus desired to investigate the detailed fading mechanisms of SiO x anode materials. In this study, limited capacity cycling was employed to examine the electrochemical behaviors of the SiO x anode, and the lithiation/delithiation cycling was limited within a range of 10% theoretical capacity. This strategy minimizes the volume variation of SiO x materials upon charging/discharging, which helps to reveal their decay factors other than volume fluctuation. It is demonstrated that the instability of the SiO x surface during cycling was likely a parallel factor of active material fading, which seems to cause unfavored electrode interface rearrangements with lowered electric conductivity.

electric vehicles↗

In-Situ Photostability Analysis of Perovskite Solar Cells by Time-Evolving Photoluminescence Imaging

In this work we investigate reversible metastabilities and irreversible degradation due to light soaking of triple-cation mixed-halide perovskite p-i-n solar cells. We use spatially resolved luminescence imaging to document the spatial inhomogeneities that exist even in high-performance devices with median efficiencies >20%. We monitor light-soaking degradation in-situ using time-evolving photoluminescence images, electro-luminescence images, and transient photovoltage. Post-stress measurements of external quantum efficiency and Kelvin- probe force microscopy suggest that long-term degradation primarily affects electrode interfaces rather than the absorber layer.

electroluminescence↗

Fast-Charging Li 4 Ti 5 O 12 Anode Driven by Light

Lithium-ion batteries with fast charging capabilities are crucial for widespread adoption of electric vehicles, as they will increase acceptance of the technology and reduce range anxiety for drivers. To achieve this, advanced fast charging technologies and alternative methods to enhance the slow electrochemical processes are desperately required. This study applied light-emitting diode (LED) photo-assisted fast charging to Li 4 Ti 5 O 12 (LTO), a large bandgap cubic spinel material, to enhance charging speed through electronic-structure coupling. UV LED-generated light irradiation on to the electrode interface boosted the ion diffusion and lithium cation addition by a factor of 1.3 during electrochemical lithiation, resulting in a 30% decrease in charging time under ambient conditions. Red LED light was not effective in accelerating the reaction as it does not provide sufficient energy. The first-principles calculations support the concept that UV illumination generates charges by overcoming the material’s bandgap and effectively reducing it through the introduction of additional titanium defect states.

25 ENERGY STORAGE↗

Impact of the LiPF6 Concentration on the Interfacial Charge Transfer and Fast-charging Capabilities of Lithium-Ion Batteries

Fast-charging lithium-ion batteries (LIB) demand optimized electrolyte formulations to balance ionic conductivity, viscosity, and interfacial charge transfer kinetics. This study examines how LiPF 6 concentration shapes solvation structure, desolvation energy, charge transfer activation energy, and solid electrolyte interphase (SEI) properties, which are critical for fast-charging performance. Using Raman spectroscopy, electrochemical cycling, X-ray photoelectron spectroscopy, and atomistic modeling, we analyze how varying LiPF 6 concentrations impact interfacial and bulk transport properties. Our findings show that increasing LiPF 6 concentration alters lithium solvation structures, reduces desolvation energy, and accelerates charge transfer at the electrode interface. Higher concentrations lower the activation energy for charge transfer and suppress excessive SEI growth, improving interfacial kinetics. However, concentrations above a certain threshold increase viscosity and reduce ionic conductivity, limiting transport efficiency. These results offer insights into electrolyte solvation and interfacial charge transfer mechanisms, providing guidelines for designing next-generation fast-charging LIB electrolytes with enhanced efficiency, stability, and longevity.

Son, Seoung-Bum [Argonne National Laboratory (ANL)↗

Solvent–Diluent Engineering of Normal-Concentration Organosulfur Electrolytes for High-Voltage Lithium-Ion Batteries

Enabling high‑voltage batteries depends critically on rational electrolyte design. Conventional carbonate electrolytes with LiPF 6 suffer from insufficient oxidative stability, motivating the use of lithium bis(fluorosulfonyl)imide (LiFSI) for its superior high‑temperature and high‑voltage performance. However, LiFSI is relatively costly, and its electrolytes often require high concentrations to suppress aluminum current collector corrosion in cathode architectures and to adequately passivate electrode interfaces. Here, a low‑concentration LiFSI electrolyte is realized by combining a high‑voltage organosulfur solvent, ethyl methyl sulfone (EMS), with a non‑solvating fluorinated diluent, fluorobenzene (FB). Extended cycling of LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) full cells to 4.5 V reveals substantial long‑term performance advantages over conventional carbonate electrolytes. Comparison with a popular cyclic sulfone, tetramethylene sulfone (TMS), shows that ring‑containing structures such as TMS strongly influence passivation behavior, ultimately limiting performance and narrowing the viable operating window. Overall, EMS is identified as a uniquely stable solvent for LiFSI‑based electrolytes operating at moderately high voltages.

Dato, Michael A. [Argonne National Laboratory (ANL↗

Operando Spectromicroscopy of Sulfur Species in Lithium-Sulfur Batteries

Here, a novel cross-sectional battery cell was developed to characterize lithium-sulfur batteries using X-ray spectromicroscopy. Chemically sensitive X-ray maps were collected operando at energies relevant to the expected sulfur species and were used to correlate changes in sulfur species with electrochemistry. Significant changes in the sulfur/carbon composite electrode were observed from cycle to cycle including rearrangement of the elemental sulfur matrix and PEO10LiTFSI binder. Polysulfide concentration and area of spatial diffusion increased with cycling, indicating that some polysulfide dissolution is irreversible, leading to polysulfide shuttle. Fitting of the maps using standard sulfur and polysulfide XANES spectra indicated that upon subsequent discharge/charge cycles, the initial sulfur concentration was not fully recovered; polysulfides and lithium sulfide remained at the cathodes with higher order polysulfides as the primary species in the region of interest. Quantification of the polysulfide concentration across the electrolyte and electrode interfaces shows that the polysulfide concentration before the first discharge and after the third charge is constant within the electrolyte, but while cycling, a significant increase in polysulfides and a gradient toward the lithium metal anode forms. Finally, this chemically and spatially sensitive characterization and analysis provides a foundation for further operando spectromicroscopy of lithium-sulfur batteries.

25 ENERGY STORAGE↗

EEL: A MOOSE-based Application for 3D Electro-Chemo-Thermo-Mechanical Modeling of Solid-State Batteries

This report describes a tool for three dimensional, high fidelity, coupled electro-chemo-thermo-mechanical modeling of solid-state batteries. A complete version of the tool is available as open source software at https://github.com/hugary1995/eel.git. The theoretical framework of the tool revolves around an inf-sup statement on a total potential, comprising the Helmholtz free energy, the electrical kinetic potential, the chemical potential, the Fourier potential, the chemical reaction potential, and the external power expenditure. The tool uses the finite element framework of Multiphysics Object-Oriented Simulation Environment (MOOSE) and a variational formulation to solve the boundary value problem for solid-state battery incorporating the full set of multiphysics couplings. The variational formulation also enables a modular software architecture for the tool so additional physics can be easily included by specifying the new contribution to the total potential. The report discusses several method of manufactured solutions that were used to verify the implementation of different physics and the Butler-Volmer reaction kinetics at the electrolyte-electrode interface. Finally, the report discusses results from complete charge/discharge simulations of a quasi-1D and a 3D solid-state battery.

25 ENERGY STORAGE↗

Microstructure-Based Degradation Modeling in Solid Oxide Cells

The presentation is intended for a graduate class in Georgia Southern University taught by Dr. Hayri Sezer on electrochemistry, SOFC and Li ion battery. It summaries NETL's recent works on microstructure-based modeling of degradation in solid oxide cells. It covers the degradation mechanism of Ni coarsening, Ni migration and the build-up of oxygen partial pressure inside the electrolyte. The phase-field models developed for Ni coarsening and migration are reviewed and the results are compared to experiments in literature to examine different diffusion mechanisms (Ni self-diffusion, Ni(OH)2 diffusion in pores and Ni(OH) surface diffusion) and driving forces (Ni(OH)x concentration and Ni-YSZ contact angle change). It also demonstrates the developed model for oxygen partial pressure and shows that the predicted oxygen partial pressure can explain the Ni oxidation in the hydrogen electrode and crack growth on the electrolyte-oxygen electrode interface under certain operating conditions.

nickel coarsening↗

AC impedance analysis of polypyrrole thin films

The AC impedance spectra of thin polypyrrole films were obtained at open circuit potentials from -0.4 to 0.4 V vs SCE. Two limiting cases are discussed for which simplified equivalent circuits are applicable. At very positive potentials, the predominantly nonfaradaic AC impedance of polypyrrole is very similar to that observed previously for finite porous metallic films. Modeling of the data with the appropriate equivalent circuit permits effective pore diameter and pore number densities of the oxidized film to be estimated. At potentials from -0.4 to -0.3 V, the polypyrrole film is essentially nonelectronically conductive and diffusion of polymer oxidized sites with their associated counterions can be assumed to be linear from the film/substrate electrode interface. The equivalent circuit for the polypyrrole film at these potentials is that previously described for metal oxide, lithium intercalation thin films. Using this model, counterion diffusion coefficients are determined for both semi-infinite and finite diffusion domains. In addition, the limiting low frequency resistance and capacitance of the polypyrrole thin fims was determined and compared to that obtained previously for thicker films of the polymer. The origin of the observed potential dependence of these low frequency circuit components is discussed.

Penner, Reginald M.↗

Extraction of oxygen from the Mars atmosphere using glow-discharge and permeation techniques

Oxygen can be extracted from carbon dioxide via thermal dissociation at elevated temperatures. However, temperatures in excess of 1000 K are needed to effect significant levels of dissociation. The experiments reported here have examined the feasibility of using a glow-discharge in low-pressure carbon dioxide to produce increased atomic oxygen yields at lower temperatures (on the order of 800 K). The experiments have shown that when silver membranes are used simultaneously as anodes for the glow discharge and as permeable membranes for oxygen separation, oxygen yields which are comparable to the permeation rates for pure oxygen, can be produced. Since the silver membrane can be employed as the electrode interface between Mars atmosphere and a stabilized-zirconia electrochemical pump, glow-discharge enhancement can be considered as a complementary technology which can be used with the zirconia-based oxygen extraction systems described previously by others. Not only can glow-discharge be used to increase oxygen yields at lowered temperatures, but it can also be considered as a possible way to avoid filtration and compression of Mars atmosphere, since the glow-discharge can be sustained in Mars ambient pressures.

Wu, Dongchuan↗