A lithium-sulfur battery with a solution-mediated pathway operating under lean electrolyte conditions

Lithium-sulfur (Li-S) battery is one of the most promising candidates for the next generation energy storage systems. However, several barriers, including polysulfide shuttle effect, the slow solid-solid surface reaction pathway in the lower discharge plateau, and corrosion of Li anode still limit its practical applications, especially under the lean electrolyte condition required for high energy density applications. Here, we propose a solution-mediated sulfur reduction pathway to improve the capacity and reversibility of the sulfur cathode and suppress dendrite growth on the Li metal anode simultaneously. With this method, a high coulombic efficiency (99%) and stable cycle life over 100 cycles were achieved under application-relevant conditions (S loading: 6.2 mg cm-2; electrolyte to sulfur ratio: 3 mLE gs-1; sulfur weigh ratio: 72 wt%). This result is enabled by a specially designed Li2S4-rich electrolyte, in which Li2S is formed through a chemical disproportionation reaction instead of electrochemical routes. A diglyme solvent was used to obtain electrolytes with the optimum range of Li2S4 concentration. Operando X-ray absorption spectroscopy confirms the solution pathway in a practical Li-S cell. This solution pathway not only introduces a new electrolyte regime for practical Li-S batteries, but also provides a new perspective for bypassing the inefficient surface pathway for other electrochemical processes.

Wang, Hui↗

Mitigating Hydrogen-Induced Degradation of Iridium Anodes in Proton Exchange Membrane Water Electrolyzers

One promising method for reducing precious metal usage in proton exchange membrane water electrolysis is lowering iridium (Ir) loading at the anode. However, low-loading Ir catalysts often suffer from poor stability under high current densities. In this study, hydrogen (H2) crossover from the cathode to the anode is identified as a key degradation pathway. Temperature-programmed reduction confirms the reduction of IrO2 at 80 °C in a hydrogen environment, highlighting the vulnerability of IrO2-based catalysts to H2 exposure. To mitigate this effect, palladium (Pd) is introduced as an anode additive, acting as an H2 oxidation catalyst and mitigating IrO2 reduction. This protective role is verified by inductively coupled plasma optical emission spectroscopy and in situ X-ray absorption spectroscopy, showing significantly suppressed Ir dissolution at 80 °C under H2 flow when an O-covered Pd surface is present at oxygen evolution reaction potentials. Results from the current study identify a new strategy in improving activity and durability of catalysts in electrolyzers.

58 GEOSCIENCES↗

Electrochemical-mechanical coupling failure mechanism of composite cathode in all-solid-state batteries

Composite cathode composed of active particles and solid electrolytes (SEs) can considerably enlarge the particle-SE contact areas and achieve high areal loadings in all-solid-state batteries (ASSBs). However, the challenging interfacial instability and particle damage problems remain unsolved. Herein, we establish a 3D electrochemical-mechanical coupled model to investigate the underlying failure mechanism by considering the governing electrochemical and physics processes. Micro-scale heterogeneous primary particles with random crystallographic orientation and size inside the LiNi 1/3 Co 1/3 Mn 1/3 O 2 (NCM111) secondary particle of the model result in the anisotropic Li diffusion and volume variation within the secondary particle, leading to significant nonuniformity of the Li concentration, and GPa-level stress distributions at primary particle boundaries, and finally causing the particle internal cracks. The particle volume shrinkage under the constraint of stiff Li 7 La 3 Zr 2 O 12 (LLZO) SE triggers the interface debonding (gap>50 nm) with increased interfacial impedance to degrade cell capacity. Higher C-rates result in larger residual stress (~100 MPa)/strain/debonding gap at dis-charging end, more likely to deteriorate the cell performance. Increasing the interfacial strength between the particle and SE can suppress the interface debonding but induces high stress (up to 10 GPa). In conclusion, results reveal the underlying mechanism of the electrochemical-mechanical coupling failure mechanism for composite cathode and provide promising guidance on the further improvement of a more robust composite cathode for ASSBs.

25 ENERGY STORAGE↗

High protonic resistance of hydrocarbon-based cathodes in PEM fuel cells under low humidity conditions: Origin, implication, and mitigation

Hydrocarbon-based electrodes for proton-exchange membrane fuel cells face challenges in closing the performance gap with electrodes based on perfluorosulfonic acid ionomers, particularly under low humidity conditions. Alongside increased oxygen transport resistance and higher kinetic-induced overpotentials, the protonic resistance of these fluorine-free electrodes is the primary hurdle to improved performance. This study systematically investigates the origin and impact of the cathode protonic resistance on fuel cell performance, utilizing sulfonated phenylated polyphenylenes as hydrocarbon ionomers. Electrochemical characterization at low relative humidity (≤50 %) reveal a high protonic resistance arising from both lower conductivity of the hydrocarbon thin film compared to the bulk membrane and increased cathode tortuosity at a gas transport-optimized ionomer to carbon (I/C) ratio of 0.2. The poor protonic resistance at low relative humidities leads to a non-homogeneous current distribution across the thickness of the cathode electrode, resulting in lower catalyst utilization. To address this issue, reducing the thickness of the cathode CL while maintaining a constant Pt loading (i.e., increasing the Pt on carbon ratio) significantly reduces protonic resistance. This improvement compensates for the kinetic disadvantages of highly loaded carbon particles and results in a considerable performance increase by 40 % at 0.75 V under low relative humidities.

25 ENERGY STORAGE↗

Rapid Load Transition for Integrated Solid Oxide Fuel Cell - Gas Turbine (SOFC-GT) Energy Systems: A Demonstration of the Potential for Grid Response

Rapid load transition is an essential requirement for integrated energy systems to maintain grid resilience as more renewable resources are added to the grid. Integrated solid oxide fuel cell - gas turbine (SOFC-GT) systems can provide high efficiency and low carbon emissions over a broad range of turndown. These hybrids also have the potential to enable rapid grid response. The challenge has been to demonstrate effective control strategies to manage load transitions. In the present study, a load transition of ~50% was achieved in 10 s using a novel but simple strategy. Power demand on the SOFC and the GT were ramped down concurrently. During this transition, the SOFC anode fuel was manipulated to maintain SOFC fuel utilization while the cathode inlet air flow and temperature were also manipulated to thermally protect the SOFC. This study was conducted using the Hybrid Performance (Hyper) facility at the National Energy Technology Laboratory (NETL) in a co-simulation environment with the Idaho National Laboratory (INL)'s grid-simulation. The load ramping strategy was tested using a hardware-based cyber-physical simulation methodology. The results demonstrate a high-fidelity representation of SOFC-GT hybrid dynamics and validation of the control strategy. Thermal and electrochemical transients indicated that the SOFC was well protected during rapid load turndown without violating operability constraints. This demonstration revealed the non-linear nature of tightly coupled SOFC-GT system components, especially the non-linear response of SOFC cathode air flow and inlet temperature controls. These results highlight the needs and challenges in developing adaptive automatic controls for autonomous rapid load transitions. This work demonstrates that SOFC-GT hybrids are a viable option to provide the fast-ramping characteristics essential to accommodate high levels of variable renewable power while maintaining grid resilience, reliability, and environmental performance. The results also demonstrate the utility of co-simulation in advancing the tightly-coupled integrated energy systems needed to meet goals for zero-carbon power generation.

DIRECT ENERGY CONVERSION,POWER TRANSMISSION AND DI↗

Extreme fast charge aging: Effect of electrode loading and NMC composition on inhomogeneous degradation in graphite bulk and electrode/electrolyte interface

Empowering extreme fast charging (XFC) requires a comprehensive understanding of its application with advanced anode and cathode materials in lithium-ion batteries. No report exists for the full extent of limitations for the anode with crosstalk effect from paired cathode as well as Li plating due to electrode loading under XFC. In this study, a combination of cell testing and multiple length characterization is used to investigate XFC aging mechanism in cells with a low loading of 1.5 mAh cm -2 and high loading of 2.5 mAh cm -2 for graphite (Gr)/Ni-rich LiNi x Mn y Co 1-x-y O 2 (NMCs). Operando XRD mappings show 1.5 mAh cm -2 loadings result in higher strain in graphite for all three cathode types. Among the three NMC cathodes, the graphite from NMC532 and NMC811 cells show comparable strain. Scanning electron microscopy (SEM) images show distinct differences between 6-C-charged anodes in two loadings. Significantly increased electrode thickness can be seen due to more damage in the graphite bulk and accumulation of the electrolyte decomposition products in electrode pores. X-ray photoelectron spectroscopy (XPS) reveals both cathode chemistry and Li plating influence the non-uniform SEI composition on graphite surface. We report higher Ni content in NMC811 promotes the higher levels of salt decomposition on the SEI and formation of higher mass of electrolyte aging products.

25 ENERGY STORAGE↗

Carbon-Binder Weight Loading Optimization for Improved Lithium-Ion Battery Rate Capability

Battery performance is strongly correlated with electrode microstructure and weight loading of the electrode components. Among them are the carbon-black and binder additives that enhance effective conductivity and provide mechanical integrity. However, these both reduce effective ionic transport in the electrolyte phase and reduce energy density. Therefore, an optimal additive loading is required to maximize performance, especially for fast charging where ionic transport is essential. Such optimization analysis is however challenging due to the nanoscale imaging limitations that prevent characterizing this additive phase and thus quantifying its impact on performance. Herein, an additive-phase generation algorithm has been developed to remedy this limitation and identify percolation threshold used to define a minimal additive loading. Improved ionic transport coefficients from reducing additive loading has been then quantified through homogenization calculation, macroscale model fitting, and experimental symmetric cell measurement, with good agreement between the methods. Rate capability test demonstrates capacity improvement at fast charge at the beginning of life, from 37% to 55%, respectively for high and low additive loading during 6C CC charging, in agreement with macroscale model, and attributed to a combination of lower cathode impedance, reduced electrode tortuosity and cathode thickness.

25 ENERGY STORAGE↗

Carbon-Binder Optimization for Lithium-Ion Battery Extreme Fast Charge

Battery performance is strongly correlated with electrode microstructure and weight loading of the electrode components. Among them are the carbon-black and binder additives that enhance effective conductivity and provide mechanical integrity. However, these both reduce effective ionic transport in the electrolyte phase and reduce energy density. Therefore, an optimal additive loading is required to maximize performance, especially for fast charging where ionic transport is essential. Such optimization analysis is however challenging due to the nanoscale imaging limitations that prevent characterizing this additive phase and thus quantifying its impact on performance. Herein, an additive-phase generation algorithm has been developed to remedy this limitation and identify percolation threshold used to define a minimal additive loading. Improved ionic transport coefficients from reducing additive loading has been then quantified through homogenization calculation, macroscale model fitting, and experimental symmetric cell measurement, with good agreement between the methods. Rate capability test demonstrates capacity improvement at fast charge at the beginning of life, from 37% to 55%, respectively for high and low additive loading during 6C CC charging, in agreement with macroscale model, and attributed to a combination of lower cathode impedance, reduced electrode tortuosity and cathode thickness.

carbon-binder additives↗

The Impact of Anomalous Resistivity in Vacuum Contaminant Plasmas on the Electrothermal Instability

This manuscript presents an assessment of the electrothermal instability (ETI) in the presence of anomalous resistivity (AR) in vacuum contaminant plasmas (VCP) when applied to a magnetized liner inertial fusion (MagLIF)-like load.Pulsed-power driven dielectrically coated metallic liners, like in MagLIF, experience the current-driven electrothermal instability which occurs when a material’s resistivity changes with temperature and is subject to ohmic heating. Large scale pulsed-power facilities that use magnetically insulated transmission lines (MITL) have been shown to generate low-density plasma which enters the target chamber and coalesces around the load. The low-density high-temperature vacuum contaminant plasmas (VCP) can parasitically divert current from the load through causing a short in the anode-cathode gap inside the target chamber. Resistive magnetohydrodynamic (MHD) simulations of these VCP experience unphysical runaway ohmic heating due to under predicting the resistivity by using a purely collisional resistivity model.AR provides a physics-based way to address this runaway heating through increasing the resistivity in a proportional way with the drift speed. In this work, 1D simulations probe the effect that AR in VCP has on the magnetic diffusion rate, and 2D simulations show how this effect manifests in the nonlinear striation form of the ETI for a MagLIF-like load. Beryllium and aluminum dielectrically coated liners are used for the 1D and 2D simulations in this work. The1D simulations show that a VCP causes a delay in the current delivery to the load by upwards of 8 ns at 60 ns into atypical current pulse for an 1 × 10 7 A scale pulsed-power accelerator. The 2D simulations show the delay observed in the 1D simulations is reduced substantially (4 ns) by 2D turbulence that disrupts the VCP layer early in time. Here, the 2Dsimulated ETI growth varies across AR models, more so for the beryllium liner than the aluminum liner because the beryllium liner shows an enhanced rate of penetration for the magnetic diffusion wave in comparison to the aluminum liner. The 2D simulations show the bulk dielectric thickness varies across AR models with the Davidson AR model beingthe largest and the Buneman AR model being the smallest, and in connection with the thickness the Rayleigh-Taylor bubble-spike distances varies correspondingly.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

High-performance and cost-effective membrane electrode assemblies for advanced proton exchange membrane water electrolyzers: Long-term durability assessment

In this work, improved activity and durability performance of a two-cell (86 cm 2 ) proton exchange membrane water electrolyzer (PEMWE) stack is reported for the first time. Both membrane electrode assemblies (MEAs) contain one order of magnitude lower platinum group metal (PGM) loadings compared to the state-of-the-art PEMWEs and incorporate novel Pt recombination layers. The high-performance and cost-effective MEAs are fabricated by the unique reactive spray deposition technology (RSDT). This advanced methodology allows for one-step fabrication of MEAs and ensures precise control and distribution of the catalyst composition and loading. The RSDT-fabricated MEAs contain only 0.2 and 0.3 mg PGM cm –2 loading in the cathode and anode electrodes, respectively, and demonstrate excellent activity and durability for over 3000 h of operation at industrially-relevant operating conditions without showing significant loss in performance. This novel work shows that a significant cost reduction for PEMWEs is achieved while maintaining excellent durability, high catalysts activities, and low hydrogen cross-over.

Proton exchange membrane water electrolyzer↗

Achieving high rate performance in hybrid pristine-recycled cathodes using model-informed electrode designs

Direct recycling lithium-ion battery cathodes, a process that retains the engineered oxide structures from end-of-life materials, presents a cost-effective and energy-efficient alternative to other battery recycling methods. However, while direct-recycled cathodes have demonstrated performance comparable to that of pristine materials at low cycling rates, their high-rate performance remains uncertain. Morphology changes in cathode particles, a main mode of degradation, directly impact rate performance by limiting surface kinetics and solid-phase diffusion. If direct recycling processes do not sufficiently restore pristine-like morphologies, the recycled materials may retain structural defects that hinder high-rate performance. The present work uses a physics-based pseudo-2D model to simulate hybrid electrodes with pristine and artificially “aged/recycled” NMC materials to investigate potential impacts of incorporating performance-limited aged cathode materials into cells. The study highlights how differences in transport and kinetic properties can influence rate capabilities in mixed electrodes — particularly in high-loading cells in high-demand applications. However, model results also reveal a possible mitigation strategy via dual-layer electrode architectures with lower-performing materials positioned near the current collector. Simulations of 4.0 mAh cm −2 cells cycled at 4C using a dual-layer architecture provided approximately 5%–30% more capacity in constant-current protocols compared to homogeneously blended electrode architectures with the same loadings and mixed-material compositions. These findings highlight the importance of strategic electrode design in minimizing potential performance losses and facilitating the integration of recycled materials into high-performance batteries, advancing sustainable and cost-effective battery manufacturing.

25 ENERGY STORAGE↗

Anion Exchange Membrane Water Electrolysis Using a Catalyst-Coated Membrane Cathode

A catalyst-coated membrane (CCM) approach to electrode fabrication for high pH water electrolysis offers enhanced interfacial contact between the catalyst layer and the membrane surface in comparison to the catalyst-coated substrate (CCS) electrode configuration. The CCM facilitates enhanced ionic and water transport between the cathode and the anion exchange membrane (AEM). This advantage is particularly significant with AEM water electrolysis (compared to proton exchange membrane water electrolysis) because the cathode typically operates under dry conditions and relies solely on diffusive water transport across the AEM from the liquid-fed anode. This study presents a direct performance comparison between CCS and CCM cathode configurations using identical hydrogen evolution reaction (HER) catalysts and other components. The use of a pseudo-reference electrode integrated into the membrane electrode assembly enabled detailed analysis of the CCM cathode polarization behavior. Surface characterization provided insight into the degradation mechanisms associated with the CCM configuration. Optimization of the cathode ionomer cross-link density improved both the cathode polarization performance and the electrolysis device durability. Further optimization of the HER catalyst loading in the CCM cathode resulted in additional gains in the electrolysis efficiency. Collectively, these findings offer valuable guidance for the design and fabrication of high-performance, durable AEM electrolysis CCMs.

Water electrolysis↗

Operando Investigation on the Role of Densification and Chemo-Mechanics on Solid-State Cathodes

All solid-state batteries are desirable for a range of energy storage applications which require high energy density. Achieving a high energy density in a solid-state battery requires the operation of an energy dense anode with a composite solid-state cathode. Pores and/or voids within a solid state cathode are ion-blocking and thus control over the concentration and distribution of pores in the initial electrode and cycled electrode is desirable. This study provides an understanding of the interplay between electrode microstructure and mechanics on active material utilization in solid state cathodes composed of NCM 811 and Li 6 PS 5 Cl. Decreasing the solid electrolyte particle size leads to greater active material-electrolyte contact and less total deformation when exposed to an external load. Composite cathodes with greater compliance can potentially decrease strain between the active material and solid electrolyte, decrease delamination events and result in higher overall active material utilization and high capacity retention.

25 ENERGY STORAGE↗

Upcycling Polyethylene Waste into Hybrid Graphitic Porous Carbon Materials Used in High‐Performance Zinc‐Ion Hybrid Capacitors

Polyethylene (PE) waste is a challenge to upcycle into useful materials because this plastic tends to decompose into volatile compounds when heated at relatively low temperatures. In this work, mixtures of PE wastes into a hybrid graphitic porous carbon (HGPC) by a thermal oxidation pretreatment step, with assistance of an inert solid additive (KCl), to functionalize, crosslink, and stabilize the PE waste followed by carbonization and catalytic graphitization steps with a potassium carbonate catalyst, are upcycled. The PE waste‐derived HGPC (PW‐HGPC) has a hybrid structure composed of graphene‐like carbon nanosheets grown on the surface of carbon particles, high porosity with specific surface area, up to 1,763 m 2 g −1 , and good graphitic degree with average Raman I 2D / I G ratios of 0.53. When used as cathode material for zinc‐ion hybrid capacitors, this PW‐HGPC exhibits an excellent specific capacity, up to 126.7 mAh g −1 , at high mass loading of 10 mg cm −2 . Moreover, PW‐HGPC exhibits remarkable cycling stability with capacity retention of >94% after 10 000 cycles. Additionally, the KCl is recycled and reused over five times. This method provides a new solution for upcycling PE wastes into high value‐added carbon materials, not only for zinc‐ion hybrid capacitors but also for other electrochemical energy storage device applications.

hybrid graphitic porous carbon↗

Mitigation of rapid capacity decay in silicon-LiNi 0.6 Mn 0.2 Co 0.2 O 2 full batteries

Silicon (Si)-based materials have been considered as the most promising anode materials for high-energy-density lithium-ion batteries because of their higher storage capacity and similar operating voltage, as compared to the commercial graphite (Gr) anode. But the use of Si anodes including silicon-graphite (Si-Gr) blended anodes often leads to rapid capacity decay in Si-Gr/LiNixMnyCo z O 2 (x+y+z=1) full cells, which has been attributed to surface instability of the Si component. In addition to stabilizing the surface, this work investigates the potential of the Si-Gr blended anodes in a full-cell configuration and its impact on the capacity contribution from active components. Using dQ/dV plots of the full cells, a powerful but simple-to-implement differential potential approach is developed to decouple the capacity contribution and degradation from the graphite and silicon components. Data collected from three-electrode cells confirm the results from the differential potential approach, which suggests a voltage slippage to a higher voltage at the blended anode side. Additionally, the voltage slippage causes a reduced utilization of the Gr component and exacerbates side reactions between the Si-Gr anode and carbonate electrolytes. Furthermore, based on these failure mechanisms, we adopted a mitigation strategy to tune the open circuit voltage of the prelithiated anode while stabilizing the surface. As a result, the full cells with the modified Si-Gr anodes (mass loading, 2.5 mAh/cm 2 ) offer a highly reversible full-cell energy density of 390 Wh/kg (based on the mass of both anode and cathode materials in a full cell) with a cycling CE of 99.9% over 200 cycles.

25 ENERGY STORAGE↗

Operando FTIR investigation of salt dynamics in Li-ion batteries during fast charging

Li-ion batteries, when charged at fast-charging rates ($>$2C), suffer from reduced lifetimes and can undergo catastrophic failure. During high-rate charging, Li-ions are unable to rapidly transport through high-loading electrodes ($>$4 mAh cm −2 ). This results in unequal charge distributions, potentials, and utilization of the active material, which can lead to Li plating. Li-ion concentration polarization, in which Li-ions deplete in the anode and accumulate in the cathode during charging, precedes Li plating. An operando FTIR-ATR graphite/NMC cell developed in this research captured Li-ion concentration polarization in real-time. During fast charging, decreases in Li-ion concentration ($>$95%) were measured at the back of the anode. This is the first verification of complete Li-ion depletion within the anode at high C-rates. The measurements also showed graphite stage transition. A P2D model was developed for comparison to the operando measurements. The measurements agreed with the model in some cases, but disparities existed at high C-rates and loadings. In the experiment, the Li-ion concentration often failed to recover to 1.2 M until several hours after charging, whereas the model Li-ion concentration rapidly recovered. The contrast between the model and experiment results indicates that further investigation is required to improve understanding of Li-ion concentration dynamics during fast charging.

25 - ENERGY STORAGE↗

Pushing Lithium–Sulfur Batteries towards Practical Working Conditions through a Cathode–Electrolyte Synergy

Abstract The commercialization of lithium–sulfur (Li−S) batteries is still hindered by the unsatisfactory cell performance under practical working conditions, which is mainly caused by the sluggish cathode redox kinetics, severe polysulfide shuttling, and poor Li stripping/plating reversibility. Herein, we report an effective strategy by combining Se‐doped S hosted in an ordered macroporous framework with a highly fluorinated ether (HFE)‐based electrolyte to simultaneously address the aforementioned issues in both cathode and anode. A reversible and stable high areal capacity of >5.4 mAh cm −2 with high Coulombic efficiency >99.2 % can be achieved under high areal Se/S loading (5.8 mg cm −2 ), while the underlying mechanism was further revealed through synchrotron X‐ray probes and Time‐of‐Flight Secondary Ion Mass Spectrometry (ToF‐SIMS). The practical application potential was further evaluated at low (0 °C) and high (55 °C) temperatures under high areal Se/S loading (>5.0 mg cm −2 ) and thin Li metal (40 μm).

Zhao, Chen↗