Search NASA⌕ Search

SEARCH · Search NASA

Results for “lamellar”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 127 records · Page 7

Hydrogen-Aided Microstructural Engineering of Additively Manufactured Ti–6Al–4V

Electron beam melting (EBM) additive manufacturing of Ti–6Al–4V subjects the material to complex thermal cycles, resulting in a columnar morphology of the prior β grains (PBGs). While the columnar PBGs of EBM-processed Ti–6Al–4V can be transformed to an equiaxed morphology through a super-transus (i.e., above the β -transus temperature) heat treatment, this also leads to the formation of a coarse lamellar two-phase microstructure. Such a microstructure is prone to strain localization and premature fracture. In this study, we present a thermohydrogen post-process treatment that achieves equiaxed PBG morphology in EBM-processed Ti–6Al–4V without sacrificing mechanical properties. Our results show that a three-step thermohydrogen post-process treatment can transform the columnar PBG morphology to an equiaxed morphology with fine microstructure, and strength and ductility levels comparable to those of the most optimum as-fabricated samples. This three-step thermohydrogen post-process treatment involves hydrogenation and phase transformation treatment in a hydrogen atmosphere, and subsequent dehydrogenation treatment in vacuum. Notably, all these treatments are carried out at temperatures well below the β -transus temperature of hydrogen-free Ti–6Al–4V.

36 MATERIALS SCIENCE↗

In situ and ex situ studies of anomalous eutectic formation in undercooled Ni–Sn alloys

Anomalous eutectic formation in undercooled Ni-Sn alloys was investigated by in situ X-ray diffraction and ex situ remelting and annealing experiments. Dynamic recrystallization and partial remelting of primary solids followed by repeated nucleation and growth of eutectic grains in the mushy zone were revealed by time-resolved X-ray diffraction. Ex situ experiments demonstrated that partial remelting of near-equilibrium solidified alloys of eutectic or near-eutectic composition can convert regular lamellar eutectic into anomalous eutectic, whereas high-temperature annealing of splat-quenched alloys of similar composition can convert eutectic or two-phase dendrites into anomalous eutectic. It is concluded that compared to ripening in solid-states, partial remelting of eutectic or two-phase dendrites in a mushy zone provides a more realistic mechanism for anomalous eutectic formation in undercooled solidification of Ni-Sn eutectic alloys. (C) 2020 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.

Crystal growth↗

Kinetics and evolution of solid-state metal dealloying in thin films with multimodal analysis

Thin-film solid-state metal dealloying (thin-film SSMD) is an emerging technique that uses self-organization to design nanostructured thin films. The resulting 3D bicontinuous nanostructures are promising for a wide range of applications, such as catalysis and energy storage. In this work, we prepared thin films by SSMD using Ti-Cu as the parent alloy and Mg as the solvent. Using a multimodal approach, we combined synchrotron X-ray spectroscopy, diffraction, and high-resolution electron-based spectroscopy and imaging to study their morphological, structural, and chemical evolution. The processing-structure relationship was analyzed as a function of parent alloy composition and dealloying temperature and time. Morphological transitions from globular, to lamellar, to bicontinuous structures, in conjunction with a ligament size evolution, were identified as functions of the parent alloy composition. The dealloying rate increased with increasing concentration of interdiffusing elements (dissolving component) in the parent alloy. The parting limit, a dealloying compositional threshold, was systematically analyzed and determined to be 30%–40%. The order of crystalline phase formation is CuMg 2 , Cu 2 Mg, and Ti; the Ti phase first shows self-reorganization during dealloying, separate from the crystallization process. The coarsening in thin-film SSMD was identified and not entirely self-similar; in addition to the increase of ligament size over time, the formation of larger globular ligaments were also observed. This work furthers our fundamental understanding of thin-film SSMD and nanostructured thin-film design, where the thermodynamic and kinetic effects differ from the bulk counterparts. The fact that dealloying and diffusion outpaces the crystallization and new phase formation also offers opportunities to utilize thin-film SSMD in certain alloy systems in which deleterious intermetallic phases need to be suppressed, that may not be possible in the bulk geometry.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Effects of chemical segregation on ductility-anisotropy in high strength Fe-Mn-Al-C lightweight austenitic steels

Ductile Fe-Mn-Al-C lightweight steels offer great potential as high specific strength materials for weight critical applications. In the present work, very high yield (~1 GPa) and ultimate tensile strength levels (~1.5 GPa) were obtained along the rolling and transverse directions of Fe-30Mn-8.5Al-0.9Si-0.9C-0.5Mo (wt.%), with high tensile elongation to failure of ~35%. This excellent mechanical behavior was attributed to the nanoscale, ordered κ-carbide precipitates formed during aging after rolling. However, tensile ductility was not isotropic through all directions of the rolled plate. In particular, the ductility was consistently lower than 5% true strain along the normal direction. Upon detailed microstructural investigations, micro-scale lamellar chemical micro-segregation bands were detected, which caused the observed anisotropic embrittlement along certain plate directions. These bands resulted in low failure strains along the normal direction since it is oriented perpendicular to these chemical segregation bands, resulting in a failure type reminiscent of delamination-induced cleavage fracture. Chemical segregation causes an inhomogeneous κ-carbide precipitate distribution upon aging, producing more pronounced mechanical anisotropy after peak-aging as compared to the solution heat treated samples. Surprisingly, deformation twinning was observed after tensile deformation of solution-heat treated specimens via electron-backscatter diffraction experiments, which is anomalous for a high stacking faulty energy (SFE) material. Further, it was proposed that chemical micro-segregation promotes locally different SFE regions, leading to deformation twinning in this nominally high SFE material. Overall, this work demonstrates the effects of chemical segregation on mechanical properties and microstructural evolution in a high performance, lightweight Fe-Mn-Al-C steel.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Transmission electron microscopy of the rapid solidification microstructure evolution and solidification interface velocity determination in hypereutectic Al-20at.%Cu after laser melting

The evolution of rapid solidification (RS) microstructure and solidification interface velocity has been studied experimentally by in-situ transmission electron microscopy and postmortem characterization for hypereutectic Al-20at.%Cu (37 wt.%Cu) after laser melting. Four morphologically distinct regions formed via growth modes changing from θ-Al 2 Cu phase dendrites to eutectic cell growth, possibly α-Al dendrite growth (α-cell), banded growth, and α-Al plane front growth. Tendency for faceting and low capacity for solute trapping limited the θ-phase dendrite growth to solidification interface velocity v < 0.07 m/s. Consequently, formation of pro-eutectic micro-constituent was suppressed, and RS microstructure formation was dominated by eutectic, α-cell, and banded morphology grains for the Al-20at.%Cu alloy. Eutectic growth operated for interface velocity of 0.1 m/s ≤ v < 0.3 m/s, with a transition from regular lamellar, 2-λ and 1-λ mode to a dense irregular morphology dominated by α-phase at v = 0.3 m/s. Interface temperature calculations indicated feasibility of α-cell growth mode for 0.3 m/s ≤ v < 0.7 m/s. Banded growth occurred for 0.7 m/s ≤ v < 1.3 m/s. Plane front α-phase growth was evident for interface velocities v ≥ 1.3 m/s. Previous work on rapid solidification microstructure development in hypereutectic Al-Cu alloys reported a regime of α-cell growth subsequently to eutectic and prior to transition to banded growth for Al-19at.%Cu (36 wt.%Cu), while for Al-22at.%Cu (40 wt.%Cu) eutectic growth transitioned directly to α-plane front growth without emergence of a banded regime. Finally, based on the current study the disappearance of the banded growth regime occurs for a composition larger than 20at.%Cu.

36 MATERIALS SCIENCE↗

Paleotribological models using preserved fossil tissue properties reveal functional significance of Eurasian mammoth dental evolution

Eurasian mammoths (Mammuthus) underwent substantial modifications in molar morphology as later-diverging species evolved progressively thinner enamel and increased enamel crest complexity. These features have been hypothesized to reduce whole-tooth wear and extend dental longevity as increasingly graze-dominated diets evolved within the lineage. This hypothesis has yet to be directly tested. Here, in this study, we developed an in-silico wear model using experimentally derived wear rates from fossil and extant proboscidean dental tissues. The models revealed that shifts in tissue topology do not affect whole-tooth wear rate, as inverse trends in lamellar frequency and enamel thickness preserve a consistent surface enamel area fraction; the determining factor of wear. Rather, topological shifts produce a wear-emergent secondary occlusal surface with greater numbers of triturating crests that create a regular, low-relief, file-like shearing pavement. These changes in occlusal architecture likely directly impacted the mastication capacity of Mammuthus dentitions, facilitating their dietary expansion to incorporate fibrous, lower-nutrient graze.

Dental wear↗

Microstructure and strengthening of Al-6Ce-3Ni-0.7Fe (wt%) alloy manufactured by laser powder-bed fusion

In this study, an Al-6Ce-3Ni-0.7Fe (wt%) alloy was fabricated via laser powder-bed fusion and its microstructure, thermal stability, tensile properties, and creep properties are investigated for two rapid-solidification rates with different eutectic spacings. For both faster- and slower-cooled states, the as-fabricated alloy mostly shows elongated grains with very fine eutectic networks (~40 nm lamellar width) comprising a high-volume fraction (~18 %) of intermetallic phases. Faster-cooled samples, however, display a less continuous eutectic network with finer spacing (~100 nm), leading to higher Orowan strengthening and therefore superior microhardness and yield stress up to ~350 °C. Upon aging (300 - 450 °C), micron-size Al 9 (Ni,Fe) 2 needle-like precipitates form within grains, and the Al 11 Ce 3 eutectic network spheroidizes, while retaining a submicron width and spacing, resulting in 33–37 % drop in microhardness after 144 h aging at 400 °C. Limited tensile ductility (~6 %) and creep ductility (~1-2 %) are measured for both faster- and slower-cooled alloys due to an inhomogeneous microstructure, where cavitation preferentially initiates at melt-pool boundaries, precipitate-free zones, and/or denuded zones, eventually leading to local fracture. Denuded zones, induced by stress, form due to diffusional flow with stress-dependent orientations, and are identified as microstructurally weak regions leading to strain localization. The present alloy does not show a significant difference in 300 °C creep resistance between: (i) tensile and compressive loading, (ii) faster- and slower-cooled samples, and (iii) continuous and spheroidized eutectics. Creep resistance at 300 °C is comparable to that of a Ce-richer Al-10.5Ce-3.1Ni-1.2Mn (wt%) alloy, despite the formation of denuded zones and needle-like Al 9 (Ni,Fe) 2 precipitates.

36 MATERIALS SCIENCE↗

Aerogel-derived nickel-iron oxide catalysts for oxygen evolution reaction in alkaline media

Anion exchange membrane water electrolyzers (AEMWEs) can generate hydrogen with a pure water feed using noble metal-free catalysts. Here, the development of highly active and stable catalysts for oxygen evolution reaction (OER) is required for improving performance of AEMWEs systems. Ni-Fe (oxy)hydroxides show high OER catalytic activity in alkaline media, but typically have low surface area. In this work, we investigate a series of Ni-Fe oxides with high surface area and disordered morphology, obtained using an aerogel synthesis method. We evaluate the impact of different synthesis variables on the OER activity and demonstrate that heat treatment at high temperatures generates more ordered structure, resulting in a decrease in OER activity. Advanced characterization reveals that maintaining highly disordered and porous structure of the aerogel is essential to achieving high OER activity, as it enables the formation of highly OER-active lamellar structures of the catalyst.

36 MATERIALS SCIENCE↗

Osteocytic oxygen sensing: Distinct impacts of VHL and HIF-2alpha on bone integrity

Skeletal fracture resistance emerges from multiple components of bone structure like microarchitecture, matrix mineralization, and organization. These characteristics are engendered via mechanisms like the hypoxia-inducible factors (HIF) pathway, involving two paralogs, HIF-1α and HIF-2α. Under normoxia, HIF-α is targeted for degradation via von-Hippel Lindau (VHL); hypoxia enables HIF-α stabilization and induction of target genes. We previously showed that osteocytic Vhl deletion or expression of degradation-resistant HIF-2α cDR female mice each produced high bone mass, whereas degradation-resistant osteocytic HIF-1α produced no overt phenotype. We report within that Vhl cKO increased bone strength, while HIF-2α cDR displayed markedly reduced bone strength below Cre-negative controls. This suggests that VHL and HIF-2α drive distinct responses that promote disparate effects on bone strength. Both Vhl deletion or HIF-2α accumulation generated two discrete bone morphologies: an outer lamellar cortex and a woven, poorly mineralized endocortex that imparted dramatically different functional outcomes. Our studies reveal novel influence of osteocytic HIF-2α signaling on collagen matrix organization, mineralization, and bone strength.

60 APPLIED LIFE SCIENCES↗

Effect of ethoxylation and lauryl alcohol on the self-assembly of sodium laurylsulfate: Significant structural and rheological transformation

Fatty alcohols are added to the surfactant solutions to modify foaming and lubrication properties, while the degree of ethoxylation is increased to improve mildness to the skin. However, it is envisioned that both parameters are capable of manipulating rheological and morphological properties. Therefore, an efficient control over the carbon chain length, amount of fatty alcohol and degree of ethoxylation could modify the surfactant self-assembly in an unprecedented way. The present work is focused on understanding the structural transformation, intermolecular interactions and rheological properties of the colloidal systems containing various amounts of lauryl alcohol (LA), and surfactant with varying degrees of ethoxylation. Additionally, combined small-angle neutron scattering (SANS), nuclear magnetic resonance (NMR) spectroscopy, rheological and morphological studies were performed to elucidate these properties. The results reveal that an increase in LA content increases the system viscosity ultimately forming a gel, and drives the assembly pattern of the surfactant from ellipsoidal micellar to lamellar via a vesicular and vesicular/lamellar mixed intermediates. Conversely, higher degrees of ethoxylation delay the onset of morphological transformation and gel formation. The interplay between hydrophobic and polar interactions coupled with hydrogen bonding interactions drive the overall rheological and morphological transformations. Therefore, fine-tuning residual chemicals can offer a novel tool for optimization of the product formulation.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Protective role of silicon in the high-temperature oxidation of titanium

We investigated the oxidation of pure titanium and Ti-0.8 at.% Si at 800 ° C in Ar-O 2 and O 2 to clarify how dilute silicon additions enhance the oxidation resistance of titanium. The effect of silicon stemmed from differences in oxide growth rather than oxygen dissolution in the metal. Initially, silicon reduced outward oxide growth and completely eliminated inward growth, which we attributed to the continuous Ti 5 Si 3 layer formed at the oxide-metal interface. Furthermore, after breakdown of the Ti 5 Si 3 layer, the oxide — containing silicon — became lamellar but remained more compact and possibly slower growing than the oxide on pure titanium.

36 MATERIALS SCIENCE↗

Role of nitrogen in the high-temperature oxidation of titanium alloys

Here, we characterized the oxidation of pure Ti, Ti-0.8Si, and Ti-2Nb at 800 °C in N 2 -20% O 2 and in sequential isotopically labeled N 2 -20% O 2 atmospheres to clarify how nitrogen influences the high-temperature oxidation mechanisms of titanium alloys. The alloys always exhibited a nitride layer beneath a compact oxide scale with localized nitrogen concentrations in the underlying metal. Nitrogen is found to limit the oxygen concentrations in the metal. The synergy between alloying and nitrogen helps maintain compact oxide scales, preventing the formation of the lamellar scales observed during oxidation in nitrogen-free atmosphere and the oxidation of pure Ti regardless of the atmosphere.

36 MATERIALS SCIENCE↗

Plastic homogeneity in nanoscale heterostructured binary and multicomponent metallic eutectics: An overview

Heterostructured materials comprised of relatively soft/hard disparate phases typically exhibit composite strengthening but lack plastic deformability at ambient temperatures. However, heterostructured systems comprised of nanoscale phases can simultaneously enhance yield strength and strain hardening, thereby promoting uniform distribution of plastic flow. In this review, the atomic-scale deformation mechanisms in model systems of eutectic alloys, Al-Al 2 Cu and Al-Si, refined to nanoscales via laser rapid solidification are discussed, and compared with literature on multi-component (high entropy) eutectics such as Ni-Al-Fe-based with Cr and/or Co additions. The nano-lamellar Al-Al 2 Cu structures exhibit unit defect mechanisms not reported in monolithic Al 2 Cu intermetallic: localized shear on {0 1 1} and shear-induced faults on {1 2 1} planes, constrained by closely-spaced dislocation arrays in Al confined by Al/Al 2 Cu interfaces. The unexpected plasticity mechanisms are enabled by slip continuity in nanoscale Al-Al 2 Cu eutectics associated with the orientation relationship and interface habit planes. In nano-fibrous Al-Si eutectic, tensile ductility at strength approaching 600 MPa is observed resulting from dislocation plasticity in the nano-Al channels and cracking in Si nanofibers. Molecular dynamics simulations show that Al dislocations easily cross-slip (screw) or climb (edge) along Al-Si interfaces, making slip transmission difficult. The propagation of nano-cracks is suppressed by surrounding strain hardening Al, retaining good ductility of the sample, in spite of lack of direct slip transmission. Finally, the critical unit mechanisms of slip transmission and interface-enabled plasticity observed in nanoscale eutectic binary systems can also explain the strength-ductility relationship in multi-component eutectics and homogeneously distributed plastic flow with increasing microstructural heterogeneity.

36 MATERIALS SCIENCE↗

The spore coat is essential for Bacillus subtilis spore resistance to pulsed light, and pulsed light treatment eliminates some spore coat proteins

Microbial surface contamination of equipment or of food contact material is a recurring problem in the food industry. Spore-forming bacteria are far more resistant to a wide variety of treatments than their vegetative forms. Understanding the mechanisms underlying decontamination processes is needed to improve surface decontamination strategies against endospores potentially at the source of foodborne diseases or food-spoilage. Pulsed light (PL) with xenon lamps delivers high-energy short-time pulses of light with wavelengths in the range 200 nm-1100 nm and a high UV-C fraction. Bacillus subtilis spores were exposed to either PL or to continuous UV-C. Gel electrophoresis and western blotting revealed elimination of various proteins of the spore coat, an essential outer structure that protects spores from a wide variety of environmental conditions and inactivation treatments. Proteomic analysis confirmed the elimination of some spore coat proteins after PL treatment. Transmission electron microscopy of PL treated spores revealed a gap between the lamellar inner spore coat and the outer spore coat. Overall, spores of mutant strains with defects in genes coding for spore coat proteins were more sensitive to PL than to continuous UV-C. This study demonstrates that radiations delivered by PL contribute to specific damage to the spore coat, and overall to spore inactivation. Keywords Decontamination, UV, proteins, proteomics, microscopy Journal Pre-proof

59 BASIC BIOLOGICAL SCIENCES↗

Thermal conductivity of 3D-printed block-copolymer-inspired structures

This study primarily focuses on examining the impact that geometric structure has on thermal conductivity of multi-phase constructs in different 3D-printed poly(lactic acid), PLA, samples. The investigated structures are inspired by morphologies formed by diblock copolymers: lamellae, hexagonally packed cylinders, and gyroid. This research also investigates how volume percentage and material combination influence the thermal conductivity of these structures. Further, the samples can be tailored to simulate various thermal management structures observed in practical applications, such as thermal interface materials in electronic devices. Thermal conductivity ratio is controlled using air, the least conductive material at 0.026 W/(m K), PLA at 0.136 W/(m K), and thermal paste at 5.11 W/(m K). Different models were tested against thermal conductivity measurements in order to capture the effect of material type (PLA-Air versus PLA-Thermal Paste), volume percentage, structure, and orientation. Simple, effective medium models were good predictions of thermal conductivity in lamellar structures, but it was necessary to develop models for conduction through cylindrical and gyroid structures. Finally, all results were normalized to find a universal model that is independent of structure and material. This approach provides a simple method to predict how to reduce or enhance transport properties and heat management capabilities of 3D printed objects.

36 MATERIALS SCIENCE↗

Exploring the impact of nucleotide length on lipid nanoparticle structure and properties

Lipid nanoparticles (LNPs) are versatile carriers for nucleic acid (NA) therapeutics, including ASOs, siRNA, mRNA, and poly-IC. While lipid composition is known to influence LNP properties, the impact of NA length on morphology and internal structure is less understood, particularly during the stages of carrier–cargo assembly. Here, we examine NA length and lipid composition immediately after mixing using high-throughput SAXS, dynamic light scattering, and cryogenic electron microscopy. All LNPs form ordered NA/lipid compartments, with longer NAs promoting inverse hexagonal (H II ) phases and larger intercompartment distances. In contrast, short NAs, especially in formulations with SM102 ionizable lipid, favor lamellar phases. SAXS peak deconvolution quantifies ordered versus disordered phases via a Robustness of Ordered Phase factor, which correlates with particle size and encapsulation efficiency. Formulations with MC3 ionizable and DOPE helper lipids exhibit the most stable H II -phase packing, highlighting the role of helper-lipid curvature in compartment stabilization. Variations in NA compartmentalization indicate differences in payload capacity, offering a framework for rational LNP design across diverse nucleic acid cargos.

60 APPLIED LIFE SCIENCES↗

Delayed onset of discontinuous precipitation-based phase transformation in U10Mo alloys doped with Silicon

A uranium-10 wt% molybdenum (U-10Mo) alloy is one of the primary candidates for metallic fuels that would use low-enriched uranium in place of highly enriched uranium, to support nuclear nonproliferation efforts. Optimal performance of a U-based metallic nuclear fuel can be achieved by retaining the high-temperature, body-centered cubic (bcc) allotrope (γ-U) at room temperature, which can be accomplished in the U-10Mo alloy. However, presence of minor alloying elements can influence the final constitution of room-temperature phases in the U10Mo alloy, specifically, formation of α-U phase which results in anisotropic behavior of the fuel in reactor. Further, through a detailed transmission electron microscopy analysis, the present study reports the constituent phases that are present in a U10Mo alloy containing ~0.1 wt% Si after it is subjected to homogenization heat treatment and thermomechanical processing. For comparison, results from an undoped U10Mo alloy are also included. The experimental results reveal that γ-UMo solid solution is the major phase in a hot-rolled, Si-doped U10Mo alloy metallic fuel foil, along with U 2 MoSi 2 C, UC, and U 2 Mo, after isothermal annealing at 460 °C for 10h. In contrast, after the same heat treatment, the undoped U10Mo alloy metallic fuel had formed a noticeable amount of α-U along prior γ-UMo grain boundaries through discontinuous precipitation (DP, area fraction: ~27.9%) with characteristic lamellar morphology, together with γ-UMo, UC, and U 2 Mo. This result indicates that doping with Si could mitigate the DP reaction in U10Mo alloy and prevent formation of undesirable α-U. This work sheds light on optimizing Si-doping–dominated microstructure in U10Mo fuels and facilitates designing and tuning of microstructures of U10Mo alloys for tailoring the final designed performance of the fuel under irradiation.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Impact of microstructure on elastic properties in the alloy Ti-42Al-8.5 Nb

The microstructure of a γ-TiAl alloy containing niobium undergoes continuous transformations during annealing at 550 °C. These take place within the α 2 -phase of lamellar (α 2 +γ) colonies. We have characterized these changes by transmission electron microscopy and made a correlation to the elastic constants determined by resonant ultrasonic spectroscopy during in-situ annealing at the same temperature. Further, the results show a continuous increase of the E-modulus. This can be attributed to elastic strains acting within α 2 lamellae as a result of lattice transformations. After 5000h, a thermodynamic equilibrium was established with equal fractions of α 2 -phase and O-phase that differ only in lattice symmetry and Nb content. Generally, the presence of O-phase should contribute to lower elastic moduli, however in the present case the evolving microstructural characteristics were responsible for the observed increase in the E-modulus.

36 MATERIALS SCIENCE↗