Search NASA⌕ Search

SEARCH · Search NASA

Results for “pouch cell”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 127 records · Page 7

Phloroglucinol–2,6‐Diaminoanthraquinone as a Durable Redox Mediator for Enhancing Conversion Reaction Kinetics in Lithium‐Sulfur Batteries

Abstract Lithium‐sulfur batteries, despite being a promising solution for next‐generation secondary batteries, require substantial efforts to overcome the challenges of sluggish sulfur redox kinetics, polysulfides shuttling, and Li metal instability before achieving practical viability. Conventional strategies that utilize metal catalysts or soluble redox mediators (RMs) are limited by either impractical producing processes or unsatisfactory service life. Herein, an electrochemically active organic material, phloroglucinol – 2,6‐diaminoanthraquinone (PG‐DAAQ) is synthesized through a green and facile polymerization process to better resolve these issues. Serving as an RM at the cathode, PG‐DAAQ exhibits enduring redox activity within the sulfur operating potential window, leading to enhanced redox kinetics and sulfur utilization. Remarkably, even without any metal elements, PG‐DAAQ exhibits an excellent affinity to polysulfides, thereby suppressing the shuttling and facilitating the formation of a more favorable solid‐electrolyte interface to stabilize Li deposition at the anode. As a result, Li‐S cells employing PG‐DAAQ show significantly enhanced cycling and rate performances than the control cells. Even with a low electrolyte‐to‐sulfur ratio of 6, pouch cells with PG‐DAAQ deliver a reversible discharge capacity of 821 mA h g −1 after 100 cycles at a C/10 rate.

Lai, Tianxing↗

Making Plasticized Polymer Electrolytes Stable Against Sodium Metal for High‐Energy Solid‐State Sodium Batteries

Abstract Solid polymer electrolytes based on plastic crystals are promising for solid‐state sodium metal (Na 0 ) batteries, yet their practicality has been hindered by the notorious Na 0 ‐electrolyte interface instability issue, the underlying cause of which remains poorly understood. Here, by leveraging a model plasticized polymer electrolyte based on conventional succinonitrile plastic crystals, we uncover its failure origin in Na 0 batteries is associated with the formation of a thick and non‐uniform solid electrolyte interphase (SEI) and whiskery Na 0 nucleation/growth. Furthermore, we design a new additive‐embedded plasticized polymer electrolyte to manipulate the Na 0 deposition and SEI formulation. For the first time, we demonstrate that introducing fluoroethylene carbonate (FEC) additive into the succinonitrile‐plasticized polymer electrolyte can effectively protect Na 0 against interfacial corrosion by facilitating the growth of dome‐like Na 0 with thin, amorphous, and fluorine‐rich SEIs, thus enabling significantly improved performances of Na//Na symmetric cells (1,800 h at 0.5 mA cm −2 ) and Na//Na 3 V 2 (PO 4 ) 3 full cells (93.0 % capacity retention after 1,200 cycles at 1 C rate in coin cells and 93.1 % capacity retention after 250 cycles at C/3 in pouch cells at room temperature). Our work provides valuable insights into the interfacial failure of plasticized polymer electrolytes and offers a promising solution to resolving the interfacial instability issue.

Zou, Peichao↗

Making Plasticized Polymer Electrolytes Stable Against Sodium Metal for High‐Energy Solid‐State Sodium Batteries

Solid polymer electrolytes based on plastic crystals are promising for solid-state sodium metal (Na 0 ) batteries, yet their practicality has been hindered by the notorious Na 0 -electrolyte interface instability issue, the underlying cause of which remains poorly understood. Here, in this study, by leveraging a model plasticized polymer electrolyte based on conventional succinonitrile plastic crystals, we uncover its failure origin in Na 0 batteries is associated with the formation of a thick and non-uniform solid electrolyte interphase (SEI) and whiskery Na 0 nucleation/growth. Furthermore, we design a new additive-embedded plasticized polymer electrolyte to manipulate the Na 0 deposition and SEI formulation. For the first time, we demonstrate that introducing fluoroethylene carbonate (FEC) additive into the succinonitrile-plasticized polymer electrolyte can effectively protect Na 0 against interfacial corrosion by facilitating the growth of dome-like Na 0 with thin, amorphous, and fluorine-rich SEIs, thus enabling significantly improved performances of Na//Na symmetric cells (1,800 h at 0.5 mA cm −2 ) and Na//Na 3 V 2 (PO 4 ) 3 full cells (93.0 % capacity retention after 1,200 cycles at 1 C rate in coin cells and 93.1 % capacity retention after 250 cycles at C/3 in pouch cells at room temperature). Our work provides valuable insights into the interfacial failure of plasticized polymer electrolytes and offers a promising solution to resolving the interfacial instability issue.

25 ENERGY STORAGE↗

Electrochemically Responsive Self-Formed Li-ion Conductors for High Performance Li Metal Anodes

The project will develop and optimize organo-Li x S y , organo-Li x P y S z , and organo-Li x S y /organo-Li x P y S z composite materials as protective layers for Li metal anodes in Li-S batteries. The core focus will be on synthesis methods and precursors for new organic/inorganic hybrid Li-ion conductors, protective layer composition, and protective layer fabrication methods. This will be accompanied by property measurement and characterization (conductivity, mechanical properties, etc.) for the protective layer on Li metal, as well as detailed diagnostics and cell testing. At the conclusion of the project, twelve ~300 mAh pouch cells will be delivered which use the optimal protection layer.

25 ENERGY STORAGE↗

Correlating capacity fade with film resistance loss in fast charging of lithium-ion battery

Fast charging of lithium-ion (Li-ion) batteries makes it susceptible to lithium plating. Here, we report the correlation between capacity loss and cell impedance changes in the battery due to lithium electrodeposition. Li-ion pouch cells with nickel-manganese-cobalt cathode and graphite anode were charged at rates varying from 0.5C to 6C. The cell voltage evolution immediately after charging was monitored to identify the C-rates that result in lithium plating. Electrochemical impedance spectroscopy (EIS) was used to monitor the cell impedance evolution. The impedance of battery cells at C-rates lower than 1C and no lithium plating showed minimal changes from their baseline values in the period immediately after charging. However, the impedance of battery cells undergoing lithium plating and C-rates higher than 3C showed a substantial reduction immediately after charging, with recovery back to baseline values after 30 min of relaxation. These observations suggest that lithium plating causes damage to the solid electrolyte interface (SEI) layer on the anode particles during the charging period, followed by the reformation of the SEI during the relaxation period. The measured capacity loss has a linear correlation with observed impedance change. The linear relationship suggests that impedance monitoring may be used for prognostication of the state-of-health of Li-ion batteries.

25 ENERGY STORAGE↗

Asymmetric ether solvents for high-rate lithium metal batteries

Recent electrolyte solvent design based on weakening lithium-ion solvation have shown promise in enhancing cycling performance of Li-metal batteries. However, they often face slow redox kinetics and poor cycling reversibility at high rate. Here we report using asymmetric solvent molecules substantially accelerates Li redox kinetics. Asymmetric ethers (1-ethoxy-2-methoxyethane, 1-methoxy-2-propoxyethane) showed higher exchange current densities and enhanced high-rate Li 0 plating/stripping reversibility compared to symmetric ethers. Adjusting fluorination levels further improved oxidative stability and Li 0 reversibility. The asymmetric 1-(2,2,2-trifluoro)-ethoxy-2-methoxyethane, with 2 M lithium bis(fluorosulfonyl)imide, exhibited high exchange current density, oxidative stability, compact solid–electrolyte interphase (~10 nm). This electrolyte exhibited superior performance among state-of-the-art electrolytes, enabling over 220 cycles in high-rate Li (50 μm)||LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811, 4.9 mAh cm −2 ) cells and for the first time over 600 cycles in anode-free Cu | |Ni95 pouch cells (200 mAh) under electric vertical take-off and landing cycling protocols. Our findings on asymmetric molecular design strategy points to a new pathway towards achieving fast redox kinetics for high-power Li-metal batteries.

batteries↗

Superionic conducting vacancy-rich β-Li 3 N electrolyte for stable cycling of all-solid-state lithium metal batteries

The advancement of all-solid-state lithium metal batteries requires breakthroughs in solid-state electrolytes (SSEs) for the suppression of lithium dendrite growth at high current densities and high capacities (>3 mAh cm -2 ) and innovation of SSEs in terms of crystal structure, ionic conductivity and rigidness. Here we report a superionic conducting, highly lithium-compatible and air-stable vacancy-rich β-Li 3 N SSE. This vacancy-rich β-Li 3 N SSE shows a high ionic conductivity of 2.14 × 10 -3 S cm -1 at 25 °C and surpasses almost all the reported nitride-based SSEs. A Li- and N-vacancy-mediated fast lithium-ion migration mechanism is unravelled regarding vacancy-triggered reduced activation energy and increased mobile lithium-ion population. All-solid-state lithium symmetric cells using vacancy-rich β-Li 3 N achieve breakthroughs in high critical current densities up to 45 mA cm -2 and high capacities up to 7.5 mAh cm -2 , and ultra-stable lithium stripping and plating processes over 2,000 cycles. The high lithium compatibility mechanism of vacancy-rich β-Li 3 N is unveiled as intrinsic stability to lithium metal. In addition, β-Li 3 N possesses excellent air stability through the formation of protection surfaces. All-solid-state lithium metal batteries using the vacancy-rich β-Li 3 N as SSE interlayers and lithium cobalt oxide (LCO) and Ni-rich LiNi 0.83 Co 0.11 Mn 0.06 O 2 (NCM83) cathodes exhibit excellent battery performance. Extremely stable cycling performance is demonstrated with high capacity retentions of 82.05% with 95.2 mAh g -1 over 5,000 cycles at 1.0 C for LCO and 92.5% with 153.6 mAh g -1 over 3,500 cycles at 1.0 C for NCM83. Utilizing the vacancy-rich β-Li 3 N SSE and NCM83 cathodes, the all-solid-state lithium metal batteries successfully accomplished mild rapid charge and discharge rates up to 5.0 C, retaining 60.47% of the capacity. Notably, these batteries exhibited a high areal capacity, registering approximately 5.0 mAh cm -2 for the compact pellet-type cells and around 2.2 mAh cm -2 for the all-solid-state lithium metal pouch cells.

25 ENERGY STORAGE↗

Exploring the Promise of Multifunctional “Zintl-Phase-Forming” Electrolytes for Si-Based Full Cells

Li-M-Si ternary Zintl phases have gained attention recently due to their high structural stability, which can improve the cycling stability compared to a bulk Si electrode. Adding multivalent cation salts (such as Mg 2+ and Ca 2+ ) in the electrolyte was proven to be a simple way to form Li-M-Si ternary phases in situ in Si-based Li-ion cells. To explore the promise of Zintl-phaseforming electrolytes, we systematically investigated their application in pouch cells via electrochemical and multiscale postmortem analysis. The introduction of multivalent cations, such as Mg 2+ , during charging can form Li x M y Si ternary phases. They can stabilize Si anions and reduce side reactions with electrolyte, improving the bulk stability. More importantly, Mg 2+ and Ca 2+ incorporate into interfacial side reactions and generate inorganic-rich solid- electrolyte interphase, thus enhancing the interfacial stability. Therefore, the full cells with Zintl-phase-forming electrolytes achieve higher capacity retentions at the C/3 rate after 100 cycles, compared to a baseline electrolyte. Additionally, strategies for mitigating the electrode-level fractures of Si were evaluated to make the best use of Zintl-phase-forming electrolytes. In conclusion, this work highlights the significance of synergistic impact of multifunctional additives to stabilize both bulk and interface chemistry in high-energy Si anode materials for Li-ion batteries.

25 ENERGY STORAGE↗

New High-Energy & Safe Battery Technology with Extreme Fast Charging Capability for Automotive Applications (Final Technical Report)

Being able to refill a cars gas tank when low on fuel is incredibly convenient and is a lacking feature for battery elective vehicles. New High-Energy & Safe Battery Technology with Extreme Fast Charging Capability for Automotive Applications was a research project designed to help correct this lacking feature by developing automotive sized Li-ion battery cells and demonstrating their ability to charge in under 10-minutes. To address the technical challenges Microvast, a cell manufacturer, was joined by Argonne National Labs, battery technology innovator, and BMW, a renown OEM, worked together to define and validate materials and cells for this project. By projects end, Microvast had successfully built and demonstrated a 240 Wh/kg, 35 Ah pouch cell that was capable of over 800 10-minute charge, full discharge cycles. From the outset of the project the plan was to use large amp-hour cells (ie automotive relevant sizes) to ensure the project findings and outcomes were most relevant for electric vehicle applications. The manufacture of cells was done using test manufacturing lines at Microvast and BMW that closely resemble the procedures of a Li-ion battery cell factory.

25 ENERGY STORAGE↗

Development of a High-Rate Lithium-Air Battery Using a Gaseous CO 2 Reactant

Li-air batteries are considered a potential alternative to Li-ion batteries for transportation applications due to their high theoretical specific energy. Most works in this area focus on use of O 2 as the reactant. However, newer concepts for using gaseous reactants (such as CO 2 , which has a theoretical specific energy density of 1,876 Wh/kg) provide opportunities for further exploration. The main objective of this project was the development of a novel strategy that enables operation of Li-CO 2 batteries at high-capacity and high-rate, with a long-cycle-life. The team was able to: (1) Synthesize two novel transition metal chalcogenide (TMC) catalysts that work in synergy with ionic liquid-based electrolytes to enhance the efficiency of reactions during discharge and charge processes; (2) Fabricate high-porosity cathode electrodes with 3D printing to increase electrode surface area and gas permeability; (3) Develop a multiscale modeling framework that integrates Density Functional Theory (DFT), Ab-Initio Molecular Dynamics (AIMD), classical Molecular Dynamics (MD), and Finite Element Analysis (FEA) to investigate atomic and cell-level properties of Li-CO 2 batteries; (4) Assemble a stackable Li-CO 2 pouch-cell able to deliver a capacity of >200 mAh. These achievements were realized through an integrated approach based on materials synthesis, testing, characterization, analysis, and computation. This project produced a thorough understanding of key chemical, electronic, and kinetic parameters that govern the operation of Li- CO 2 batteries in realistic conditions. The methodologies employed, and the insight generated, will be valuable beyond advancing the field of Li-CO 2 batteries

25 ENERGY STORAGE↗

Investigating the Effects of Lithium Deposition on the Abuse Response of Lithium-Ion Batteries

Li deposition at the graphitic anode is widely reported in literature as one of the leading causes of capacity fade in lithium-ion batteries (LIBs). Previous literature has linked Li deposition resulting from low-temperature ageing to diminished safety characteristics, however no current research has probed the effects of Li deposition on the abuse response of well-characterized cells. Using overtemperature testing, a relationship between increased concentrations of Li deposition and exacerbated abuse response in 1 Ah pouch cells has been established. A novel Li deposition technique is also investigated, where cells with n:p < 1 (anode-limiting) have been cycled at a high rate to exploit Li + diffusion limitations at the anode. Scanning Electron Microscopy of harvested anodes indicates substantial Li deposition in low n:p cells after 20 cycles, with intricate networks of Li(s) deposits which hinder Li + intercalation/deintercalation. Peak broadening and decreased amplitude of differential capacity plots further validates a loss of lithium inventory to Li + dissolution, and Powder X-ray Diffraction indicates Li + intercalation with staging in anode interstitial sites as the extent of Li deposition increases. A cradle-to-grave approach is leveraged on cell fabrication and testing to eliminate uncertainty involving the effects of cell additives on Li deposition and other degradation mechanisms.

25 ENERGY STORAGE↗

Silicon-Based Anodes for Long-Cycle-Life Lithium-ion Batteries

CVD process has been studied and optimized to achieve 2x scale up of porous Si anode materials with a clean process. The roles of CVD temperature, duration, C 2 H 2 gas pressure, and carrier gas have been optimized. It is found that LHCE (LHCE-1 and LHCE-4) can lead to more than 50% increase in the cycling stability of Si||NMC622 cells. LHCE-4 can also lead to smaller impedance increase and longer calendar life when tested in single layer pouch cells. These results are very helpful in the understanding of the Si based anode and further development of Si based Li ion batteries.

25 ENERGY STORAGE↗

Molecular-level Regulation of PEO-Based Electrolytes with CaF 2 Nanoparticles for Advanced Solid-State Lithium Metal Batteries

The poly(ethylene oxide) (PEO)-based electrolyte has caught much attention for its flexibility, interfacial compatibility, and low cost, but the low ionic conductivity and poor mechanical strength severely hinder its further application in solid-state batteries. Herein, a molecular level regulation through adding CaF 2 nanoparticle fillers is proposed to enhance the electrochemical performance of the PEO-based electrolyte. The strong coordination effects of the Ca cation with a Li salt anion and ether-oxygen increase the dissociated Li ion concentration and accelerate Li ion migration, thus enhancing the ionic conductivity of the electrolyte when combined with their physical disruption in the PEO matrix (0.31 mS cm -1 at 55 °C). Moreover, the spontaneous reaction between Li and CaF 2 generates a LiF-rich solid electrolyte interphase, which promotes homogeneous Li deposition. Consequently, the PEO-CaF 2 electrolyte delivers symmetric cells over 6300 h and maintains full batteries over 1000 cycles with 80% capacity retention. In conclusion, the assembled pouch-cell displays robust performance, further demonstrating its potential practical application.

Li, Tao [Lanzhou Univ. (China)] (ORCID:00000003196↗

Advanced All-Fluorinated Electrolytes for Extended Cycle Life and Stability of Li||SPAN Batteries

Achieving long-term stability and consistent capacity in lithium (Li) metal batteries with sulfurized polyacrylonitrile (SPAN) cathodes requires precisely engineered electrolytes to optimize interphase formation and redox reversibility. Here, this study presents 1,1-difluoro-2-(2-methoxyethoxy)ethane (DFE)-based localized high-concentration electrolytes (LHCEs), incorporating fluorinated components such as salt, solvating solvent, and diluent for improved electrode stability. Molecular dynamics simulations and surface analyses reveal that the DFE-LHCE with 1,2-bis(1,1,2,2-tetrafluoroethoxy)ethane (BTFEE) diluent produces uniform and robust interphase layers on both cathode and anode, enriched with inorganic species like LiF and Li 2 O. These properties lead to prolonged redox reversibility of the SPAN cathode, suppressed side reactions, and extended cycle life for Li||SPAN cells. Remarkably, DFE-BTFEE-LHCE enables Li||SPAN coin cells with an areal capacity of ∼7 mAh cm -2 for SPAN to retain 81.3% capacity after 200 cycles and pouch cells of 0.12 Ah with 8 mAh cm -2 of SPAN and lean electrolyte to maintain 96.4% capacity over 80 cycles. These findings pave the way for advancing Li||SPAN battery technologies.

25 ENERGY STORAGE↗

Comprehensive Battery Safety Risk Evaluation: Aged Cells versus Fresh Cells Upon Mechanical Abusive Loadings

Abstract Despite their wide applications, lithium‐ion batteries (LIBs) have been struggling with their safety risks arising from different lifetime stages. Here, the NCMA pouch cell is taken as an example, and the safety of both fresh and aged cells from three milestone stages, that is, internal short circuit (ISC) triggering risk, ISC mode, and the subsequent thermal runaway (TR) consequence is investigated. By combining mechanical abusive testing and physics‐based models on commercialized cells with various states‐of‐health (SOH) and states‐of‐charge, it is discovered that the ISC triggering delays with the decay of SOH and soft ISC mode will be triggered more frequently, which is mainly due to the mechanical behaviors of the current collectors. The temperature rises and peak temperature during the subsequent TR also become milder for aged cells due to the reduced capacity and deterministic soft ISC process. Results here provide a mechanistic explanation of the safety risk comparison between the fresh and aged cells, offering cornerstone guidance to the evaluation and design of next‐generation safer LIBs.

25 ENERGY STORAGE↗

Modulating Li + and Polysulfide Solvation with Low-Density Moderately Solvating Electrolytes for Lithium–Sulfur Batteries

Lithium–sulfur (Li–S) batteries show great promise as the next-generation rechargeable batteries, yet they still suffer from polysulfide shuttling and interphasial instability. Electrolyte, as the medium for ion transport and sulfur conversion, plays a crucial role in overcoming these challenges. Here, we introduce a moderately solvating electrolyte (MSE) based on low-density, low-viscosity, and nonfluorinated ether co-solvents that balances polysulfide suppression, Li metal stabilization, and redox kinetics. Through multiple solvent–solvent and solvent-ion interactions, the optimized MSE weakens Li + -solvent pairing while strengthening cation–anion interactions, thereby lowering the desolvation barrier and promoting the formation of a favorable solid–electrolyte interphase (SEI). Meanwhile, MSE limits the polysulfide dissolution but improves the accessibility of active material through better wettability and tailored solvation environment, leading to an altered sulfur deposition mechanism with β – α conversion. This approach enables a stable cycling of high-mass loading Li–S cells (> 3.5 mg cm -2 ) at both room temperature and 45 °C (where shuttling and side reactions are severer), and demonstrates a pouch cell with lean electrolyte content (4.5 µL mg s -1 ). This work highlights a practical route to develop high-performance electrolyte for Li–S cells and provides mechanistic insights into their operation.

25 ENERGY STORAGE↗

Passive Mitigation of Cascading Propagation in Multi-Cell Lithium Ion Batteries

The heat generated during a single cell failure within a high energy battery system can force adjacent cells into thermal runaway, creating a cascading propagation effect through the entire system. This work examines the response of modules of stacked pouch cells after thermal runaway is induced in a single cell. The prevention of cascading propagation is explored on cells with reduced states of charge and stacks with metal plates between cells. Reduced states of charge and metal plates both reduce the energy stored relative to the heat capacity, and the results show how cascading propagation may be slowed and mitigated as this varies. These propagation limits are correlated with the stored energy density. Results show significant delays between thermal runaway in adjacent cells, which are analyzed to determine intercell contact resistances and to assess how much heat energy is transmitted to cells before they undergo thermal runaway. A propagating failure of even a small pack may stretch over several minutes including delays as each cell is heated to the point of thermal runaway. This delay is described with two new parameters in the form of gap-crossing and cell-crossing time to grade the propensity of propagation from cell to cell.

25 ENERGY STORAGE↗

Li + (ionophore) nanoclusters engineered aqueous/non-aqueous biphasic electrolyte solutions for high-potential lithium-based batteries

The use of aqueous/non-aqueous biphasic electrolyte solutions in Li-based battery systems circumvents the limitations of poor reductive stability of aqueous electrolyte solutions, broadening their electrochemical stability window. However, aqueous/non-aqueous electrolytes suffer from biphasic mixing and high impedance when Li ions cross the biphasic interface. Here we propose the use of 12-crown-4 (12C4) and tetraglyme (G4) as lithium ionophores to form Li + (ionophore) nanoclusters in both non-aqueous and aqueous phases to overcome the interface challenges in biphasic electrolytes. The Li + (ionophore) nanoclusters have the H 2 O-excluding inner Li + solvation structure in non-polar 1,1,2,2-tetrafluoroethyl 2,2,3,3-tetrafluoropropyl ether (TTE), allowing fast charge transport across the biphasic interface without solvent mixing or water shuttling. Further, a tailored electrolyte formulation comprising the lithium bis(trifluoromethanesulfonyl)imide (LiTFSI) salt, 12C4, TTE and H 2 O solvents (labelled LiTFSI-12C4@TTE/H 2 O) demonstrates low impedance (2.7 Ω cm -2 ) at the TTE/H 2 O interface and enabling 2,000 cycles of prelithiated graphite||LiFePO 4 coin cells at 850 mA g -1 with an average Coulombic efficiency of 99.8%. Single-layer 22.5 mAh Li||LiMn 2 O 4 pouch cells using LiTFSI-12C4@TTE/H 2 O electrolyte with G4 delivered a stable discharge capacity of about 1.3 mAh cm -2 for 80 cycles at 0.5 mA cm -2 .

25 ENERGY STORAGE↗