Characterization of SDU 6 Sump Water Samples

This report details results from characterization of the Saltstone Disposal Unit 6 (SDU 6) East Sump water samples. In March of 2022, Saltstone Radiation Protection Department (RPD) personnel reported SDU 6 East Sump beta/gamma radiation levels at ~ 33 dpm/mL (~ 15 pCi/mL) beta/gamma in excess of the water sampling limit of 16 dpm/mL (7.2 pCi/mL). Replicate samples obtained from the SDU 6 East Sump were sent to the Savannah River National Laboratory (SRNL) for analysis to include pH, limited anions, toxic metals and radionuclides. Subsequent sump samples associated with SDU 7 that has not yet been filled with any radioactive material were also analyzed at SRNL for both nitrate and nitrite.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Pyrolysis of Radioactive Spent Resins in the PRIME Installation - 20190

Montair and Belgoprocess developed the pilot PRIME (Pyrolysis Resins In Mobile Electric) Installation for treatment of spent resins in one single reactor without pre-treatment and without intermixing of other waste, allowing for easy traceability and isotopic characterization of the end product. Both low level waste (LLW, < 2 mSv/h) and medium level waste (MLW, > 2 mSv/h) can be treated in the installation. The PRIME pilot installation is designed to treat 2 batches of 100 liter of saturated ion exchange resins over a period of 24 hours. A dosing unit with screw feeder is used for the dosing of the saturated ion exchange resins to the pyrolysis reactor. This completely new developed innovative pyrolysis reactor contains a special design mechanical stirrer and can operate at a temperature of up to 600 deg. C under inert conditions. As a result, the organic molecules will decompose at an accelerated rate until only the mineralized material remains. The lower temperature and the absence of oxygen also prevent the breakdown of ion exchange resins into (powdery) ash, which is a considerable advantage during further handling. Gases that are released during drying and pyrolysis are treated in an also newly developed thermal oxidizer, which uses an innovative, electrically heated design instead of a traditional natural gas- or fuel oil secondary combustion chamber design. After passing through the thermal oxidizer, the gases are cooled down to saturation temperature and treated in the wet scrubbing system. An extraction fan keeps the system under negative pressure to prevent the possibility of any off-gas leakage out of the system. A series of tests were performed successfully with wet cationic resins, anionic resins and a mixture of both. The results of these tests are described in the presentation. For intellectual property protection, the system and process of pyrolysis of organic waste and the system of thermal oxidation of pyrolysis gases described in this paper are patent pending. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Effect of thermal aging on microstructure and crack growth response of Alloy 152 weld

Nickel-based Alloy 690 and the associated weld Alloys 52 and 152 are typically used for nozzle penetrations in replacement heads for pressurized water reactor (PWR) vessels, because of their excellent overall resistance to general corrosion and environmental degradation, primarily stress corrosion cracking (SCC). However, many of the existing PWRs are expected to operate for 40-80 years. Likewise, advanced water-cooled small modular reactors (SMRs) will use Ni-Cr alloys and are expected to receive initial operating licenses for 60 years. Hence, the thermal stability of Ni-Cr alloys is a potential concern for the long-term performance of both existing and advanced nuclear power plants, and possibly spent fuel storage containers. The objective of this research is to understand the microstructural changes occurring in high-Cr, Ni-based Alloy 152 weldments during long time exposure to the reactor operating temperatures, and the effect of these changes on the service performance. One area of particular concern is the potential for long range ordering (LRO), i.e. formation of the intermetallic Ni2Cr phase under prolonged exposure to reactor temperatures and/or irradiation, which can increase strength, decrease ductility, and cause dimensional changes or lead to in-service embrittlement of components made with these alloys. Hence, this research focused on the microstructural evolution and the SCC response of Alloy 152 under accelerated thermal aging. The materials studied involved three heats of Alloy 152 used to produce a dissimilar metal weld (DMW) joining an Alloy 690 plate to an Alloy 533 low alloy steel (LAS) plate, thermally aged at three different temperatures (370°C, 400°C and 450°C) for up to 75,000h (equivalent to 60 years of service). The microstructural characterization by means of synchrotron X-ray did not find evidence of LRO in any of the three heats aged to an equivalent of 60 years of service. Testing in a primary water environment of a heat of Alloy 152 aged at 370°C to a 60-year service equivalent revealed a fatigue and corrosion fatigue crack growth responses similar to those measured on the un-aged alloy. However, the SCC CGR response of the aged sample appears to show a deterioration in performance.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Characterization of Tank 9H Salt Dissolution Batch 2A in Support of Tank Closure Cesium Removal (TCCR) 1A Batch 2 Preparations

Savannah River Remediation (SRR) is currently preparing the second batch of material to be processed through the Tank Closure Cesium Removal (TCCR) 1A system. The feed for TCCR 1A consists of dissolved saltcake from Tank 9H. The first batch of salt to make up Batch 2 (Batch 2A) has been dissolved in Tank 9H and will later be transferred to Tank 10H. Savannah River National Laboratory (SRNL) received samples from the batch of dissolved salt for characterization.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Adsorption of molecular iodine and alkyl iodides from spent-nuclear-fuel-reprocessing off-gas using reduced silver mordenite

Radioactive iodine is a hazardous byproduct of spent-nuclear-fuel reprocessing that must be removed from the off-gas stream before it can be discharged. Reduced silver mordenite (Ag 0 Z) is currently the baseline material for iodine capture in the U.S. Although the performance characteristics and capture mechanisms of I 2 and CH 3 I have been established, similar investigations into long-chain organic iodides have yet to be performed. In this study, thin beds of Ag 0 Z were loaded with I 2 , CH 3 I, C 4 H 9 I, and C 12 H 25 I (5 ppm to 50 ppm) carried in a dry air stream at 150°C. The maximum iodine capacity was 105 ± 5 mg I/g Ag 0 Z for all species. Saturated Ag 0 Z samples were characterized using scanning electron microscopy, X-ray fluorescence, X-ray photoelectron spectroscopy, diffuse reflectance UV–visible spectroscopy, pair distribution function analysis, and thermogravimetric analysis. Further, near-complete Ag utilization and similar physical/chemical properties were observed for all samples. Through a comparison with previous studies and an investigation of aged Ag 0 Z, we propose that iodine species react with Ag + at exchange sites, forming α-AgI within the mordenite channels, and with surface Ag 0 nanoparticles, yielding β-/γ-AgI. The available Ag sites in the interior (Ag + ) and exterior (Ag 0 ) of mordenite determine the adsorption capacity since α-AgI formation is limited by the total pore volume. Potential iodine uptake routes were summarized for aging and non-aging environments. A scalable predictive model was implemented for deep-bed iodine removal, and predictions were in good agreement with experimental data. Sensitivity analysis suggests that iodine uptake kinetics is governed by pore diffusion.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

LAW Glass Formulation to Support Melter Runs with Simulants

The major objective of this work was to prepare and characterize glass formulations in order to develop and select formulations that are compliant with contractual and processing requirements to support melter tests with each of the LAW Sub-Envelopes. Glasses that cover composition ranges of interest were prepared and characterized to ensure that selected glass compositions can tolerate expected composition variations resulting from process errors without adversely affecting processing characteristics or product quality. Glass compositions that are expected to result during transitions from one waste stream to another were also prepared and characterized. Other objectives of the work included preparation and characterization of glasses with respect to the properties of interest, optimization of sulfate loading in the glasses, evaluation of ability to achieve waste loading limits, testing to demonstrate compatibility of glass melts with melter materials of construction, and identification of glass formulation issues with respect to contract specifications and processing requirements.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Modeling Interfaces to Support Low-Level Waste Disposal System Performance Assessments - 20366

In low-level waste (LLW) disposal sites, interfaces between cementitious materials, used as waste forms and/or engineered barriers, and the surrounding soil or backfill material are often encountered. Reactions across these interfaces may lead to chemical and structural alteration of the cementitious and backfill materials that may ultimately affect long-term performance. For example, the ingress of carbon dioxide from soil gas into a waste tank concrete shell at the Hanford Site or Savannah River Site (SRS) or a low-level waste disposal vault at SRS leads to carbonation of cement hydration products (e.g. portlandite, calcium-silicate hydrate or C-S-H, and ettringite). The result of carbonation is a decrease in pH in the cement paste portion of the tank wall or vault concrete structure that could ultimately lead to de-passivation of the embedded structural steel and, eventually, to cracking. Cracking can lead to increased ingress of water into the structure, corresponding increased release of constituents of concern, and to subsequent increased transport of these constituents to the surrounding environment. The mobility of trace constituents (e.g., radionuclides of concern) in waste forms may increase in response to changes in pH, pore structure, and mineralogical gradients. Depletion of portlandite results in subsequent decalcification of C-S-H that leads to changes in the cement strength and may lead to structural failure. At the boundary between waste forms and concrete vaults, the migration of sulfate ions from the salt waste form (e.g., the saltstone waste form used for LLW disposal at the Savannah River Site in Saltstone Disposal Units, or SDUs) into the barrier or vault concrete has been predicted to result in expansive mineral phase formation (or 'sulfate attack'). Expansive mineral formation could result in cracking and potential loss of structural integrity in the vault concrete. In the performance assessment (PA) for the SRS SDUs, prediction of both the carbonation and sulfate attack fronts are critical to assessing the long-term performance of these LLW disposal vaults. A general purpose geochemical reactive transport model has been developed in LeachXS/ORCHESTRA to evaluate typical interfaces for LLW disposal environments, including SDUs at SRS. The model may be used to predict the long-term performance of interfaces between cementitious materials and saltstone or backfill materials with respect to primary phases by considering mass transport, cement chemistry, geochemical speciation, and multi-ionic diffusion over interfaces between different materials. The present study compares the performance and interactions between vault concrete and saltstone waste form for a representative SDU scenario. The materials were characterized using pH-dependence leaching test (EPA 1313) and semi-dynamic transport tests (EPA 1315) with test results used to parameterize the interface model. The development of a credible inter model provides an important basis for supporting future PAs where carbonation and sulfate attack are important aging and degradation mechanisms. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Synthesizing, Compounding, and Characterizing a Heat Labile Polyurethane Foam

ABSTRACT A need exists for a packaging foam material that can be converted from solid to gaseous degradation products at reasonably low energy levels or temperatures, such as 100O C. This paper will primarily discuss the approaches currently being used to synthesize and characterize such a material. These approaches include the incorporation of novel polyols such as azo containing diols, polycarbonate diols, and polypropylene carbonate polyols into polyurethane foams. Characterization methods include NMR, FTIR, TGA, finite element analysis, impact strength, and others. This project will be funded for a duration of three years. Year 1 focused on developing the proposed test methods and producing an initial rigid polyurethane foam. Year 2 focuses on refining the materials and test methods. If appropriate, design of experiment (doe) techniques will be used to optimize components, component levels, density and other variables to attain required final material properties (TGA weight loss, impact strength, etc.). Year 3 focuses on scaling up to larger engineering quantities. The application for this material is in load securement for transportation of low level radioactive waste materials within the US Department of Energy (DOE) complex. Foam in place process equipment and operators will be shielded using this novel method over current practice. Current practice can involve time consuming methods of load securement in low level radiation environments. This new technique would eliminate exposure time securing the load and greatly improve the As Low As Reasonably Attainable (ALARA) conditions. The objective is to progress to higher Technical Readiness Levels (TRL) and larger pilot scale quantities. This paper discusses methodologies and presents current results to date.

Kranjc, Mark D.↗

Summary of Chloride-induced Stress Corrosion Cracking Experiments with a Spent Fuel Storage Canister Large Plate

This report provides a comprehensive summary of the crack growth rate testing and the experiments to evaluate the corrosion behavior of welded plate material taken from the Sandia National Laboratories’ full-size mockup of a spent nuclear fuel (SNF) dry storage canister. The information includes that previously reported, and new work on detailed surface characterization of the corrosion attack from the large plate experiment. The work and the results inform aging management programs for the SNF canisters.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Sodium Extraction from Full-Length Fermi-1 Blanket Assembly

Enrico Fermi Nuclear Generating Station is a nuclear power plant on the shore of Lake Erie. On October 5, 1966, Fermi 1, a prototype fast breeder reactor, suffered a partial fuel meltdown (no radioactive material was released). As a result, 34 metric tons of sodium-bonded blanket material from the decommissioned Fermi-1 reactor were shipped to and are currently stored at the Idaho Nation Lab (INL). This material is currently awaiting removal from the state of Idaho by 2035. In its current state, the Fermi-1 material is not suitable for disposal due to the reactive characteristic of its bond sodium. This work demonstrates removal of bond sodium from an entire full-length unirradiated Fermi-1 outer radial blanket assembly using a gravity assisted melt-drain-evaporate (MEDE) treatment process. Quantitative and qualitative analyses were performed to characterize the extent of sodium removal from the blanket material following MEDE treatment.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Aging of Concrete for the Evaluation of Repair Materials to Protect the Walls of the HCAEX Tunnel at Savannah River - 20301

H-Canyon, located in the Savannah River site, is a unique facility for chemical reprocessing of plutonium, highly-enriched uranium, and other radioactive materials. The exhaust gases of the H-Canyon are sent through the H-Canyon Exhaust (HCAEX) tunnel for contamination removal. Robotic inspections of the tunnel revealed significant degradation of the reinforced concrete structure that was associated with acid attack, and could compromise the structural stability of the tunnel. Thus, the identification and evaluation of potential repair materials that could be applied on the degraded walls to mitigate and prevent further degradation is of significant interest to the Department of Energy and the Savannah River representatives. This research effort has been divided into two phases: 1) Development and evaluation of aged concrete under accelerated aging conditions (which is the focus of this paper) and 2) Evaluation of potential repair materials applied on aged and non-aged concrete under simulated aggressive conditions. In order to develop and evaluate concrete samples exposed to accelerated aging conditions in simulated aggressive environments, a literature review of the HCAEX tunnel was conducted that included 1) characterization and extent of the concrete damage, 2) environmental conditions inside the tunnel and 3) primary deterioration mechanisms. In addition, potential coatings and/or repair materials for degraded concrete surfaces exposed to aggressive environments (primarily acidic) were selected from the literature review and the most common testing and measurements for evaluating acid attack phenomena, erosion, etc. were reviewed. From the literature review findings, a preliminary bench-scale test plan for the concrete aging was developed, including accelerated aging tests with aggressive conditions (acid fumes, humidity, etc.). Concrete samples were exposed to the aging accelerated conditions (e.g. immersion in acid solutions) and visual inspection, mass loss and pH change (acid solution) were recorded over time. Correlations between the visual inspection, mass loss and pH changes results and the aging time or the aging conditions were developed. Specimens submitted to the highest acid concentration showed the fastest and most intense degradation. The type of coarse aggregate (limestone) used for the concrete seemed to be the cause of the fastest aging observed, compared to the cement paste. The research findings created the foundation for the ongoing investigation, in which new concrete samples with a mix design similar to the HCAEX tunnel will be tested and will serve as the substrate for testing the selected coatings and /or repair materials. In this paper, the literature review and preliminary results from the aging tests are provided. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Aluminophosphate Waste Forms for Immobilizing Cations from Electrochemical Salt Wastes

This report provides experimental details and results of evaluating aluminophosphate waste forms for treating and immobilizing the salt cations from salt wastes generated during electrochemical reprocessing of used nuclear fuel. In the waste form process for these materials, chloride salt streams are reacted with NH 4 H 2 PO 4 , the chlorine is removed from the salts and driven off as NH 4 Cl (a solid condensate that can be captured), and then the product can be vitrified in conjunction with glass-forming chemicals (e.g., Fe 2 O 3 , Al 2 O 3 ) to create a high-durability waste form. This study was initiated with some literature review on aluminophosphates containing high alkali oxide content and some of this information is summarized in this report. Following literature review, three new samples were synthesized where two contained Fe 2 O 3 +Al 2 O 3 (i.e., samples G3 and G5 ) and one was only Al 2 O 3 (Fe 2 O 3 -free) (i.e., sample G6 ). In addition to these samples, G1 was also made, which is the baseline reference waste form referred to as DPF5-336 (made without Al 2 O 3 ). Samples G1, G3, G5, and G6 had phases of Li 3 Fe 2 (PO 4 ) 3 (likely), monazite (below XRD detection limits), AlPO 4 , and AlPO 4 , respectively. Characterizations on these materials included optical images, scanning electron microscopy, energy dispersive X-ray spectroscopy, and X-ray diffraction. These samples were shipped to Argonne National Laboratory for chemical durability testing. Depending on how the samples perform in these tests, an additional phase of aluminophosphate formulations could be designed and tested. This report completes the milestone M4FT-23PN030104041 with details provided in Appendix B.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Constraining Inputs to Realistic Kilonova Simulations through Comparison to Observed r -process Abundances

Kilonovae, one source of electromagnetic emission associated with neutron star mergers, are powered by the decay of radioactive isotopes in the neutron-rich merger ejecta. Models for kilonova emission consistent with the electromagnetic counterpart to GW170817 predict characteristic abundance patterns, determined by the relative balance of different types of material in the outflow. Assuming that the observed source is prototypical, this inferred abundance pattern in turn must match r -process abundances deduced by other means, such as what is observed in the solar system. We report on analysis comparing the input mass-weighted elemental compositions adopted in our radiative transfer simulations to the mass fractions of elements in the Sun, as a practical prototype for the potentially universal abundance signature from neutron star mergers. We characterize the extent to which our parameter inference results depend on our assumed composition for the dynamical and wind ejecta and examine how the new results compare to previous work. We find that a dynamical ejecta composition calculated using the FRDM2012 nuclear mass and FRLDM fission models with extremely neutron-rich ejecta ($Y_e$ = 0.035) along with moderately neutron-rich ($Y_e$ = 0.27) wind ejecta composition yields a wind-to-dynamical mass ratio of $M_w$/$M_d$ = 0.47, which best matches the observed AT2017gfo kilonova light curves while also producing the bestmatching abundance of neutron capture elements in the solar system, though, allowing for systematics, the ratio may be as high as of order unity.

79 ASTRONOMY AND ASTROPHYSICS↗

Advanced high-performance large diameter Cs 2 HfCl 6 (CHC) and mixed halides scintillator

This paper reports on successful growth and performance evaluation of two large diameter Cs 2 HfCl 6 (CHC) and Cs 2 HfCl 4 Br 2 (CHCB), both recently developed scintillator crystals. The discovery of Cs 2 HfCl 6 (CHC) as a scintillator has lately generated much interest in this material and its family, which belongs to the K 2 PtCl 6 cubic crystal structure. CHC is an intrinsic scintillator that is non-hygroscopic (slightly deliquescent, i.e., slightly moisture sensitive but does not deteriorate much when left in air), has no self-radioactivity, provides excellent energy resolution, and has excellent non-proportionality. CHC has a moderate density of 3.9 g/cm 3 and an effective atomic number of 58. Reported in this paper are transparent crack-free single crystal CHC and CHCB boules of one inch in diameter, both grown using the vertical Bridgman method. Samples retrieved from the boules, sized 23 mm × 30 mm and 23 mm × 26 mm, respectively, are characterized for their optical and scintillation properties. Energy resolutions of 3.5% and 3.7% (FWHM) at 662 keV, respectively, are reported. Light yields of 23,000 ph/MeV and 20,000 ph/MeV have been calculated for the large diameter CHC and CHCB crystals, respectively. Results comparable to previously reported results for smaller crystals have been obtained. Studies on decay time, non-proportionality, as well as detector characterization are also reported.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Characterization of Tank 22 Demister Solids Responsible for Preventing Adequate Purge Ventilation Flow (U)

In December 2020, about 2.5 grams of the solid material from the Tank 22 purge ventilation demister, responsible for preventing adequate purge ventilation flow, were delivered to Savannah River National Laboratory (SRNL) by Savannah River Remediation (SRR) for analysis to identify the chemical nature of the solids and possibly address why fresh water and caustic flushes with 50 wt. % sodium hydroxide solution are essentially ineffective in dissolving or dislodging the accumulated solids from the Tank 22 demister at low ambient temperature conditions.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Remote detection of radioactive material using a short-pulse CO 2 laser

Detection of radioactive material at distances greater than the radiated particle range is an important goal with applications in areas such as national defense and disaster response. Here, we demonstrate avalanche-breakdown-based remote detection of a 3.6 mCi α-particle source at a standoff distance of 10 m, using 70 ps, long-wave infrared (λ = 9.2 µm) CO 2 laser pulses. This is ∼10 times longer than our previous results using a mid-IR laser. The primary detection method is direct backscatter from microplasmas generated in the laser focal volume. The backscatter signal is amplified as it propagates back through the CO 2 laser chain, enhancing sensitivity by >100 times. Here we also characterize breakdown plasmas with fluorescence imaging, and present a simple model to estimate backscattered signals as a function of the seed density profile in the laser focal volume. All of this is achieved with a relatively long-drive laser focal geometry (f/200) that is readily scalable to >100 m.

43 PARTICLE ACCELERATORS↗

EPC-ES WIPP WAC Appendix A Equivalence Support Measurements 2019-2020

Characterization of low-level waste (LLW) at Los Alamos National Laboratory (LANL) is primarily performed by the Environmental Protection and Compliance - Environmental Stewardship (EPC-ES) Characterization Services team and/or the Nuclear Process Infrastructure (NPI--9) Nuclear Material Support Services team (hereafter referred to as the gamma spectroscopy teams). The gamma spectroscopy teams use portable high-purity germanium (HPGe) detector systems for the nondestructive assay (NDA) characterization of LLW. Controlled-approved procedures and processes for the use of such systems to assay LLW items are currently in place. Additionally, a number of performance studies have been conducted by the gamma spectroscopy teams to support the efficacy and quality of assay results generated by the established NDA process.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

GeoMelt{sup R} In-Container Vitrification (ICV){sup TM} for Fukushima Daiichi Water Treatment Secondary Wastes - 20212

The Japanese government is supporting development work implemented jointly by Veolia subsidiaries Kurion Japan, K.K., Veolia Nuclear Solutions (VNS), Inc., and Veolia Nuclear Solutions Federal Services, LLC for treating radioactive waste generated from Fukushima Daiichi Nuclear Power Station (NPS) water treatment using the GeoMelt{sup TM} In-Container Vitrification (ICV){sup TM} technology. The initial work consisted of glass formulation and engineering-scale testing which was completed in 2018, in the frame of an IRID (International Research Institute for Nuclear Decommissioning) program as part of a project subsidized by Japan's Ministry of Economy, Trade and Industry (METI). The Fukushima Daiichi NPS Mid- and Long-Term Road-map requires investigation of methods to stabilize solid wastes (and to immobilize radioisotopes in the wastes) generated as a result of emergency response and decommissioning activities. Cooling water treatment has resulted in a significant amount of solid and slurry secondary wastes (mostly adsorbents and ion-exchange materials) which will require processing at some point. GeoMelt{sup R} ICV{sup TM} is a joule-heated melter technology which uses a refractory-lined single-use container combining the melter and disposal container. There is no pouring required nor concerns with refractory corrosion which allows the process to accommodate a wide range of waste chemistries and high waste loadings. The testing described here consisted of three engineering-scale melts, each processing between 212 kg and 240 kg of waste simulants, glass formers, and non-radioactive cesium (Cs) and strontium (Sr) tracers. Continuous isokinetic stack sampling of off-gas emissions was performed for each test in order to calculate Cs and Sr retention in the glass wasteform. Single-pass retention of Cs in the final glass wasteform ranged from 91.46 to 99.30%, and single-pass retention of Sr ranged from 99.76 to 100%. Planned particulate recycle will increase these retention levels. Melt 1 processed a mixture of KUR-EH (a zeolite-based ion-exchange material), simulated Advanced Liquid Processing System (ALPS) Carbonate and Iron Slurries, and glass additives. Melt 2 processed a mixture of KUR-EH, KUR-TSG (a titanate-based adsorbent), and glass additives. Melt 3 processed a mixture of KUR-EH, simulated barium sulfate/iron ferrocyanide sludge (AREVA sludge), and glass additives. Waste loadings for these melts ranged from 70 weight percent (wt%) to 82 wt%. Vitrification produces a waste form much denser than the stored water treatment secondary waste wastes, resulting in significant volume reduction. Volume reductions for the three tests ranged from 74 to 79 vol%. Vitrification produces a chemically durable wasteform. Pacific Northwest National Laboratory (PNNL) tested three glass samples from each engineering-scale melt) by the Materials Characterization Center 1 (MCC-1) test, an international standard leach test of the chemical durability of nuclear waste glasses. PNNL also obtained one U.S. reference glass (EA Glass) and two Japan reference glasses P0798) and tested these under the same MCC-1 conditions (90 deg. C, 10 m-1, DIW, and 7, 14, 28-day) as the GeoMelt{sup R} ICV{sup TM} glasses. The GeoMelt{sup R} ICV{sup TM} glasses exhibited lower total normalized releases and 14- to 28-day normalized release rates than the three reference glasses. These results suggest that the GeoMelt{sup R} ICV{sup TM} glasses have durabilities on par with high-level waste glasses under standard test conditions. Post-melt process sampling and analysis indicated no Cs migration into the melter refractory materials and very little deposition of Cs or Sr onto the melter hood or off-gas piping internals. The results of the testing indicated good Cs retention in the glass, high volume reduction and waste loadings, and excellent chemical durability. These factors are important to minimize treatment costs and to protect workers and the environment. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗