High-Throughput In-Line Deposition of Silicon Oxide for Polycrystalline Silicon Passivating Contacts

Polycrystalline silicon passivating contacts rely on an ultrathin (1–2 nm) silicon oxide layer to minimize recombination at the wafer/oxide interface and regulate dopant diffusion. Traditionally formed by thermal or chemical oxidation, this oxide is herein replaced by silicon oxide deposited via aerosol impact-driven assembly (AIDA), enabling high wafer-per-hour throughput and precise thickness control. In this study, we show that AIDA coatings conformally cover planar or textured substrates and achieve a SiO x /poly-Si(n) structure with an implied open-circuit voltage (iV oc = 726 mV) and contact saturation current density (J 0 = 8.8 fA/cm 2 ). Furthermore, annealing AIDA SiO x films at elevated temperatures desorbs hydroxyl groups while the stoichiometry transitions toward SiO 2 , improving passivation quality. Together, these results highlight AIDA’s potential for scalable, high-throughput manufacturing of advanced passivating contacts, offering a cost-effective alternative to conventional low-pressure chemical vapor deposition and plasma-enhanced chemical vapor deposition-based silicon and oxide processes.

TOPcon↗

Field‐Relevant Degradation Mechanisms in Metal Halide Perovskite Modules

Field testing, failure analysis, and understanding of degradation mechanisms are essential to advancing metal halide perovskite (MHP) photovoltaic (PV) technology toward commercialization. Here, we present performance data from up to 1 year of outdoor testing of MHP modules in Golden, Colorado. The module encapsulation architecture and encapsulant materials have a significant impact on module reliability, with modules containing a polyolefin elastomer (POE) in addition to a desiccated polyisobutylene (PIB) edge seal outlasting modules with only a PIB edge seal or PIB blanket. Nondestructive and destructive characterization of the field-tested modules points to module scribes and interfaces as areas of potential mechanical weakness and chemical migration, resulting in shunt pathways and increased series resistance. Finally, indoor accelerated stress testing with light and elevated temperatures is performed, demonstrating failure with similar scribe degradation signatures as compared to the field-tested modules. In conclusion, under both outdoor testing and light and elevated temperature conditions, electrochemical corrosion between the copper electrode and the mobile iodine ions appeared dominant, with a significant progression at the scribes that is speculated to result from an interplay between the initial laser damage and joule heating from enhanced ion diffusion under bias.

14 SOLAR ENERGY↗

Enhancing lifetime, forecasting, and economic benefits of photovoltaic technologies undergoing UV-induced degradation with optical filtering

Ultraviolet-induced degradation (UV-ID) of various PV cell types was analyzed under optical UV filters with different cutoff wavelengths. Cell types studied included interdigitated back contact (IBC), passivated emitter and rear totally diffused (PERT), and heterojunction technology (HJT) based on crystalline Si (c-Si), and metal halide perovskite (MHP) cells. Analyzing degradation rates in two distinct regimes proved beneficial for all cell types. We used empirical linearizing functions ln(t) for c-Si technologies and 2 √t for MHP samples where t is time. These were applied to extrapolate UV-induced degradation over the lifetime of PV modules under various levels of optical UV filtering and used to predict the relative economic benefits for PV power plants. Degradation rates for all technologies were generally faster under the long pass optical filters having shorter cutoff wavelengths transmitting more UV irradiation and at elevated temperatures when testing MHP samples in the range between 60 °C and 90 °C.

14 SOLAR ENERGY↗

UV + Damp Heat Induced Power Losses in Fielded Utility N-Type Si PV Modules

A recent trend in commercial PV modules is a transition to n-type silicon cells, including passivated emitter rear totally diffused (n-PERT), tunnel oxide passivated contact (TOPCon), and silicon heterojunction (SHJ). There is evidence via lab studies that some of these cells are more susceptible to UV induced degradation (UVID), yet there is a lack of confirmation that such degradation occurs in the field. Current IEC standards designed to screen for early module failures require only minimal UV exposure (15 kWh/m2 280-400 nm, ~2-3 months equivalent outdoor exposure). Here, we investigate fielded n-PERT silicon (Si) modules from a commercial utility that show power losses of ~2%/year. We present a comprehensive picture of the physics and chemistry of degradation supported by both module and cell electronic characterization (EL, PL, IV, EQE, and DLIT) and materials-level morphological and chemical analysis (SEM, EDS, XPS, FTIR, and HPLC). All sampled site modules show short circuit current (Isc) and open circuit voltage (Voc) losses when compared to unfielded spares, with the most severely degraded also having losses in fill factor (FF). We identify two different degradation modes contributing to overall power loss: (1) external quantum efficiency (EQE) measurements show losses in the blue range of the spectra, indicative of cell surface recombination losses, and (2) variations in high series resistance (Rs) at the cell level that are correlated with compositional differences in cell metallization. Using unfielded spares, we were able to reproduce Voc, Isc, and EQE losses via a minimum UV stress of 67.5 kWh/m2 (280-400 nm), 4.5x the exposure currently required in IEC 61215-2 (MQT 10). Degradation continued with additional UV dosage equivalent to the fielded modules (405 kWh/m2 total), with power loss leveling out at an average of 6.1%. Subsequent 1000 h of 85% RH/85degrees C damp heat testing showed that cells exposed to UV underwent additional severe series resistance degradation, even those without the susceptible paste composition seen in the field, whereas non-UV exposed cells saw little change. We attribute this to higher concentrations of acetic acid generated on the UV exposed area of the module, leading to degradation of the gridline/cell interface and high Rs. This study is unique in that it reproduces field observed utility scale UVID with an accelerated test and supports the need for standards development for longer UV exposure combined with other stress factors to catch materials interplay within a module package.

14 SOLAR ENERGY↗