Search NASA⌕ Search

SEARCH · Search NASA

Results for “Cladding”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,261 records · Page 70

Elongate SiC fuel elements

An elongate fuel element is described that has a silicon carbide cladding enclosing a fuel, such as UO 2 , wherein the fuel is dimensioned relative to the cladding to define gaps at each lateral end of the enclosure sufficiently large such that upon swelling in use, the fuel does not increase the strain on the cladding beyond the limits of the claddings strain tolerance. The lateral gaps at the ends of the fuel allow lateral expansion during swelling that reduces the strain on the cladding.

Long, Yun-Bo↗

Hydride Reprecipitation in Prototypical 17x17 PWR Fuel Rods after Simulated Vacuum Drying Conditions

Light water reactor (LWR) fuel rod cladding picks up hydrogen as it oxidizes in reactor. Once the hydrogen concentration exceeds the solubility limit, zirconium hydride platelets precipitate, generally in the circumferential direction. In preparation for dry storage, elevated temperatures can dissolve some of the circumferential hydrides, which during cooling can then reprecipitate in a direction perpendicular to the hoop stress (radially). From 2019 to 2024, ORNL published a series of reports that included metallographic observations of cladding after a thermal transient to 400°C followed by slow cooling. The simulated dry storage process was performed on three full-length 17x17 PWR fuel rods at their as-discharged rod internal pressure. There were two important observations from the metallographic examinations of these heat-treated rods: (1) the propensity for hydride reorientation is strongly influenced by nearby as-discharged precipitated hydrides, (2) the radial hydrides observed near the cladding inner diameter were often associated with cracks in the pellet. Subsequent modeling using the BISON fuel performance code that considered the effects of pellet cracks and pellet-cladding bonding observed in high-burnup fuel support the conclusion that pellet cracks enhance the local hoop stress in the cladding creating preferential sites for hydride reorientation, and that the influence of the pellet cannot be ignored in accurate fuel rod performance predictions.

Montgomery, Rose [ORNL] (ORCID:0000000286038936)↗

MARVEL Reactor Fuel Performance Report

The Microreactor Applications Research Validation and EvaLuation (MARVEL) project is producing a high temperature liquid metal-cooled nuclear test bed at Idaho National Laboratory (INL) to ultimately improve the integration of microreactors to end-user applications. This ambitious effort seeks to design, authorize, construct, test, and operate the reactor within five years. In order to construct and operate the MARVEL reactor in a timely manner, the system will utilize materials and component designs which have already been used, qualified, or licensed from previous reactors. The MARVEL reactor will be located at the INL Transient Reactor Test (TREAT) facility in the north high-bay equipment pit and will use the existing 304 stainless steel-clad U-ZrH1.6 pin-type fuel system developed by General Atomics and purchased from TRIGA International. This fuel has been previously qualified under the United States Department of Energy’s (US DOE) Reduced Enrichment for Research and Test Reactors (RERTR) Program. Even though the regulator of the MARVEL reactor is the US DOE, the standards and overall approach recommended by the Nuclear Regulatory Commission is well-defined and utilized here. Following NUREG-1537 regulatory guidance, this report documents the authorization case for the MARVEL fuel system’s application to MARVEL and establishes stable and predictable fuel performance during the most thermophysically unfavorable conditions achievable in the MARVEL reactor. To that end, this report provides a comprehensive survey of the known thermophysical properties, performance, and quantitative relationships associated with the MARVEL reactor fuel element and uses this information to determine its mechanical integrity and risk of reaching unacceptable conditions during the most extreme accident scenarios predicted for the reactor using the most conservative assumptions available. The information contained herein is compiled from a combination of historical reports and peer reviewed scientific publication manuscripts. Known mechanisms under which the fuel is susceptible to failure are highlighted and compared to conditions that could exist in the MARVEL reactor during an unanticipated transient or accident scenario. The two scenarios considered for analysis in this report are (1) an unprotected loss of flow accident and (2) a hypothetical unprotected loss of coolant accident during the loss of flow accident. Preliminary 2D steady-state analyses herein indicate that both fuel-cladding chemical interactions and fuel-cladding mechanical interactions are negligible throughout the fuel’s operational cycle under both normal and high temperature accident scenario conditions. Although higher fidelity 3D time-dependent modeling and simulations are planned, the following may be concluded presently. The MARVEL fuel element maintains its geometric stability and structural integrity during the most extreme accident scenarios predicted for the MARVEL reactor. The hoop stress during the unprotected loss of flow accident reaches about -1.27 MPa; this negative stress indicates that it is compressive rather than tensile. The compressive stress is a result of the NaK pressure on the outside of the fuel element, caused by the restricted thermal expansion of the NaK coolant, exceeding the internal pressures generated inside of the fuel element. The hoop stress generated in the cladding during the unprotected loss of coolant accident reaches a maximum of about approximately 10 MPa, which is nearly an order of magnitude less than the predicted yield strength of the cladding under high-temperature accident scenario conditions. Calculations were compared with results from high performance computational simulations using BISON and are in very close agreement. A conservative MARVEL fuel meat peak temperature limit of 900 °C is recommended presently, which is about 180 °C higher than the peak fuel temperature predicted to occur during the most extreme accident. Based on the known properties and behavior of the MARVEL fuel element, the fuel successfully meets its design and safety requirements under normal and most extreme accident conditions with a large safety margin.

11 - NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

FeCrAl fuel/clad chemical interaction in light water reactor environments

This article investigates the fuel-cladding chemical interaction (FCCI) behavior of two commercial FeCrAl alloys, APMT composition (Fe-21Cr-5Al-3Mo wt.%) and C35M (Fe-13Cr-5Al-2Mo-0.2Si-0.03Y wt.%), after neutron irradiation. “H-cup” diffusion multiples of FeCrAl alloys and ceramic UO 2 fuel were irradiated at a temperature of ~300 °C to a total estimated burnup of 26 GWd/tHM. Post-irradiation Examination results demonstrate the excellent degradation resistance of FeCrAl alloys as accident tolerant fuel (ATF) cladding materials in light water reactor conditions. The study concludes that there was no irradiation-induced defects observed in either of the two commercial FeCrAl claddings. The formation of amorphous Al/U mixed oxide was observed at the fuel-clad interface, which can serve as a tritium permeation barrier and protect against potential chemical attack from the fuel. Finally, the study attributed the formation of amorphous Al/U mixed oxide to the low temperature and limited time of neutron irradiation. APMT forms more distinct Cr and Cr-Fe intermetallic at the FeCrAl-UO 2 interface than C35M due to the higher bulk Cr:Al ratio.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Annealing of (DU-10Mo)-Zr Co-Rolled Foils

Producing uranium-10wt% molybdenum (DU-10Mo) foils to clad with Al first requires initial bonding of the DU-10Mo foil to zirconium (Zr) by hot rolling, followed by cold rolling to final thickness. Rolling often produces wavy (DU-10Mo)-Zr foils that should be flattened before further processing, as any distortions could affect the final alignment and bonding of the Al cladding to the Zr co-rolled surface layer; this bonding is achieved by a hot isostatic pressing (HIP) process. Distortions in the (DU-10Mo)-Zr foil may cause the fuel foil to press against the Al cladding and thus create thinner or thicker areas in the Al cladding layer during the HIP cycle. Post machining is difficult and risky at this stage in the process since there is a chance of hitting the DU-10Mo. Therefore, it is very important to establish a process to flatten and remove any waviness. This study was conducted to determine if a simple annealing treatment could flatten wavy foils. Using the same starting material (i.e. DU-10Mo coupons of the same thickness), five different levels of hot rolling and cold rolling, combined with five different annealing treatments, were performed to determine the effect of these processing variables on flatness, bonding of layers, annealing response, microstructure, and hardness. The same final thickness was reached in all cases. Micrographs, textures, and hardness measurements were obtained for the various processing combinations. Based on these results, it was concluded that annealing at 650°C or higher is an effective treatment to appreciably reduce foil waviness.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Review of fuel/cladding eutectic formation in metallic SFR fuel pins

Sodium-cooled Fast Reactors (SFRs) remain a strong contender amongst the Generation IV reactor concepts. Metallic fuel has been a primary fuel option for SFR designers in the US and was used extensively in the first generation of SFRs. One of the benefits of metallic fuel is its chemical compatibility with the coolant; unfortunately this compatibility does not extend to steel cladding at elevated temperatures. It has been known that uranium, plutonium, and rare earths diffuse with cladding constituents to form a low melting point fuel/cladding eutectic which acts to thin the cladding once the interfacial temperature rises above the system liquidus temperature. Since the 1960's, many experiments have been performed and published to evaluate the rate of fuel/cladding eutectic formation and the temperature above which melting will begin as a function of fuel/cladding interfacial temperature, time at temperature, fuel constituents (uranium, fissium or uranium (plutonium) zirconium), cladding type (stainless steel 316, stainless steel 306, D9 or HT9), beginning of life linear power, plutonium enrichment and burnup. The results of these tests, however, remain scattered across conference and journal papers spanning 50 years. The tests used to collect this data also varied in experimental procedure throughout the years. This paper will consolidate the experimental data into four groups of similar test conditions and expand upon the testing performed for each group in detail. A companion paper in PSA 2011 will discuss predictive correlations formulated from this database. (authors)

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Influence of Alloying Elements and Effect of Stress on Anisotropic Hydrogen Diffusion in Zr-Based Alloys Predicted by Accelerated Kinetic Monte Carlo Simulations

The formation of hydrides degrades the toughness of Zr-based claddings, and thus is one of the primary concerns regarding cladding integrity during fuel operation and used fuel storage. However, the formation mechanism of hydrides, particularly the nucleation mechanism, is yet to be fully understood. To explore the nucleation process, atomic scale studies including density functional theory, molecular dynamics and kinetic Monte Carlo have been used to investigate H diffusion, segregation, and the possible nucleation paths of hydrides. Here, density functional theory calculations are used to parameterize a kinetic Monte Carlo model, which can accurately predict the effective H diffusivity in various Zr-based claddings including Zircaloy, Zirlo and Zr-2.5Nb. Assisted by density functional theory calculations, a recently developed charge-optimized-many-body potential is further improved and used to investigate the possible nucleation paths of hydrides. It’s shown that the formation of face-centered hydrides starts with coherent zeta-phase, shearing of which in the basal plane changes the hcp stacking into fcc and leads to the formation of gamma-hydride nuclei. The shearing involves a negligible barrier and negligible strain accumulation in the matrix by adopting three equivalent shear partials. The results obtained at the atomic scale are consistent with previous theory and experiments, and improves the current understanding on how and how fast hydride forms in Zr based cladding.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Development of New Corrosion-Resistant Bimetals with Increased Corrosion Resistance Prepared by Electroslag Surfacing Technology

Results are presented for research in the development of new grades of corrosion-resistant steels for a bimetal cladding layer prepared by electroslag surfacing technology. It is shown that steel of transition martensiticaustenitic class may surpass martensitic steels both with respect to reliability characteristics and wear resistance. In this case, these steels have a more economic alloying system, and correspondingly low cost compared with austenitic chromium-nickel steels. Based on thermodynamic modeling of regions for phase existence optimum steel alloying systems are determined for new grades as a bimetal cladding layer. Results are presented for research in the development of new grades of corrosion-resistant steels for a bimetal cladding layer prepared by electroslag surfacing technology. It is shown that steel of transition martensiticaustenitic class may surpass martensitic steels both with respect to reliability characteristics and wear resistance. In this case, these steels have a more economic alloying system, and correspondingly low cost compared with austenitic chromium-nickel steels. Based on thermodynamic modeling of regions for phase existence optimum steel alloying systems are determined for new grades as a bimetal cladding layer.

36 MATERIALS SCIENCE↗

Accelerated Testing of HT-9 with Zirconia Coatings Containing Gallium using Raman Spectroscopy and XPS

Laser Raman spectroscopy and x-ray photoelectron spectroscopy were used to study the evolution of composition of oxide films in the presence of zirconia coatings on miniature HT-9 alloy specimens subjected to elevated temperature in air. The experiments expanded on previous efforts to develop a quick-screening technique for candidate alloys for cladding materials (HT-9) and actinide-based mixed oxide fuel mixtures (represented by the zirconia coating) by investigating the effect of both coating composition and alloy pretreatment conditions on the high temperature reactions. In particular, the presence of the element Ga (a potential impurity in mixed oxide fuel) in the initial zirconia coating was found to accelerate the rate of oxide growth relative to that of yttria-stabilized zirconia studied previously. In addition, HT-9 samples that were subjected to different thermal pretreatments gave different results. The results suggest that the presence of Ga in a mixed oxide fuel will enhance the corrosion of HT-9 cladding under the conditions of this study, although the extent of enhancement is influenced by thermal pretreatment of the cladding material. The results also demonstrate the need to combine Raman spectroscopy with other techniques, particularly photoelectron spectroscopy, for optimizing composition and/or fabrication conditions of both cladding and oxide fuels for advanced nuclear reactors.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Experimental design and analysis for irradiation of SiC/SiC composite tubes under a prototypic high heat flux

The purpose of this work is to design an irradiation vehicle for testing silicon carbide (SiC) fiber-reinforced SiC matrix composite cladding materials under conditions representative of a light water reactor in order to validate thermo-mechanical models of stress states in these materials due to irradiation swelling and differential thermal expansion. The design allows for a constant tube outer surface temperature in the range of 300–350 °C under a representative high heat flux (~0.66 MW/m 2 ) during one cycle of irradiation in an un-instrumented “rabbit” capsule in the High Flux Isotope Reactor. An engineered aluminum foil was developed to absorb the expansion of the cladding tubes, due to irradiation swelling, without changing the thermal resistance of the gap between the cladding and irradiation capsule. Finite-element analyses of the capsule were performed, and the models used to calculate thermal contact resistance were validated by out-of-pile testing and post-irradiation examination of the foils and passive SiC thermometry. Six irradiated cladding tubes (both monoliths and composites) were irradiated and subsequently disassembled in a hot cell. The calculated temperatures of passive SiC thermometry inside the capsules showed good agreement with temperatures measured post-irradiation, with two calculated temperatures falling within 10 °C of experimental measurements. Furthermore, the success of this design could lead to new opportunities for irradiation applications with materials that suffer from irradiation swelling, creep, or other dimensional changes that can affect the specimen temperature during irradiation.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Out-of-pile and postirradiated examination of lanthanide and lanthanide-palladium interactions for metallic fuel

Palladium is being investigated as a fuel additive to bind with and potentially immobilize lanthanide fission products. A primary cause of fuel-cladding chemical interaction (FCCI) is the lanthanide fission products migrating to the fuel periphery and interacting with the cladding. This interaction will lead to wastage of the cladding and eventually to a cladding breach. Palladium has previously been identified as a promising additive used to prevent or decrease FCCI by reacting with the lanthanide fission products. In the current study, an alloy cast from the four highest abundant lanthanides found in irradiated metallic fuel, Nd, Ce, Pr, and La, with and without Pd, has been characterized using neutron diffraction, scanning electron microscopy, and electron probe microanalysis. In the lanthanide-Pd intermetallic compounds, all of the constituent compounds, i.e. Nd-Pd, Ce-Pd, La-Pd and Pr-Pd are known. There is very good agreement, both structurally and compositionally, between the out-of-pile lanthanide alloy and lanthanide fission products characterized in irradiated fuels. In both cases, the lanthanide elements form a solid solution in a hexagonal crystal structure. The out-of-pile lanthanide alloy follows Vegard's Law, with the measured and calculated (weighted average of constituents) lattice parameters being within 1% for both the a and c parameters. Pd bonds with the lanthanides (Ln) forming the phases LnPd and Ln7Pd3. The results indicate the properties of lanthanide compounds in irradiated metallic fuel can be reliably simulated in out-of-pile experiments.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Quantifying deformation during Zry-4 burst testing: a comparison of BISON and a combined in-situ digital image correlation and infrared thermography method

The development and verification of nuclear fuel-cladding performance codes require extensive testing to establish empirical correlations, necessitating more accelerated testing methods that can replace large validation studies. Here, in the present work, a technique was developed and implemented to experimentally quantify the relationship between temperature, cladding internal pressure, and strain in-situ during a burst test, with the specific aim of generating data for code validation and model refinement. Digital image correlation was used to measure hoop, axial, and radial strain, and infrared thermography to quantify axial temperature gradients. Several key experimental modifications to traditional LOCA burst testing were necessary, but are shown to effectively have little impact on burst temperatures. The time/temperature dependent pressure and time/spatially dependent thermal gradient data were used with BISON to simulate cladding burst and strain rates. Although the measured DIC strains reach appreciable amounts at slightly lower temperatures than BISON simulated strains, there is good agreement between the measured and simulated strains in terms of magnitude and rates leading up to burst. However, in the few seconds prior to and during burst, the BISON simulated strains are significantly lower than the measured strains, indicating the potential for model improvement. The combined experiment and simulation technique may be applied to any new cladding concept to accelerate fuel qualification.

36 MATERIALS SCIENCE↗

Thermal effects on transducer material for heat assisted magnetic recording application

Heat Assisted Magnetic Recording (HAMR) is a promising technology for next generation hard disk drives with significantly increased data recording capacities. In HAMR, an optical near-field transducer (NFT) is used to concentrate laser energy on a magnetic recording medium to fulfill the heat assist function. The key components of a NFT are transducer material, cladding material, and adhesion material between the cladding and the transducer materials. Since transducer materials and cladding materials have been widely reported, this paper focuses on the adhesion materials between the Au transducer and the Al{sub 2}O{sub 3} cladding material. A comparative study for two kinds of adhesion material, Ta and Cr, has been conducted. We found that Ta provides better thermal stability to the whole transducer than Cr. This is because after thermal annealing, chromium forms oxide material at interfaces and chromium atoms diffuse remarkably into the Au layer and react with Au to form Au alloy. This study also provides insights on the selection of adhesion material for HAMR transducer.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Single-polarization hollow-core square photonic bandgap waveguide

Materials with a periodic structure have photonic bandgaps (PBGs), in which light can not be guided within certain wavelength ranges; thus light can be confined within a low-index region by the bandgap effect. In this paper, rectangular-shaped hollow waveguides having waveguide-walls (claddings) using the PBG have been discussed. The design principle for HE modes of hollow-core rectangular PBG waveguides with a Bragg cladding consisting of alternating high- and low-index layers, based on a 1D periodic multilayer approximation for the Bragg cladding, is established and then a novel single-polarization hollow-core square PBG waveguide using the bandgap difference between two polarized waves is proposed. Our results demonstrated that a single-polarization guiding can be achieved by using the square Bragg cladding structure with different layer thickness ratios in the mutually orthogonal directions and the transmission loss of the guided mode in a designed hollow-core square PBG waveguide is numerically estimated to be 0.04 dB/cm.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Estimation of carbon 14 inventory in hull and end-piece wastes from Japanese commercial reprocessing operation

Hull and end-piece wastes generated from reprocessing plant operations are expected to be disposed of in a deep underground repository as Group 2 TRU wastes under the Japanese classification system. The activated metals that compose the spent fuel assemblies such as Zircaloy claddings and stainless steel nozzles are mixed and compressed after fuel dissolution, and then stuffed into stainless steel canisters. Carbon 14 is a typical activated product in the hulls and end-pieces and is mainly generated by the {sup 14}N(n,p){sup 14}C reaction. In the previous safety assessment of the TRU waste in Japan, the radionuclides inventory was calculated by ORIGEN-2 code. Some conservative assumptions and preliminary estimates were used in this calculation. For example, total radionuclides generated from a single type of fuel assembly (45 GWd/tU for a PWR unit), and the thickness of the Zircaloy oxide film on the hulls (80 μm) were both overestimated. The second assumption in particular has a large effect on exposure dose evaluation. Therefore, it is essential to have a realistic source term evaluation regarding such items as the C-14 inventory and its distribution to waste parts. In the present study, a C-14 inventory of the hull and end-piece wastes from the operation of a commercial reprocessing plant in Japan corresponding to 32,000 tU (16,000 tU in each BWR and PWR) was calculated. Analysis using individual irradiation conditions and fuel characteristics was conducted on 6 types of fuel assemblies for BWRs and 12 types for PWRs (4 pile types x 3 burnup limits). The oxide film thickness data for each fuel type cladding were obtained from the published literature. Activation calculations were performed by using ORIGEN-2 code. For the amount of spent assembly and other waste characteristics, representative values were assumed based on the published literature. As a preliminary experiment, C-14 in irradiated BWR claddings was measured and found to be consistent with the calculated activation. The total C-14 inventory was estimated as 4.46x10{sup 14} Bq, consisting of 2.58x10{sup 14} Bq for BWRs and 1.87x10{sup 14} Bq for PWRs, and is consistent with the safety assessment of 4.4x10{sup 14} Bq. However, the distribution of the C-14 inventory to hull oxide, which was estimated under the assumption of instantaneous radionuclide release in the safety assessment, decreased from 5.72x10{sup 13} Bq (13% of the total) in the previous assessment to 1.30x10{sup 13} Bq (2.9% of the total; consisting of 1.48x10{sup 12} for BWRs and 1.15x10{sup 13} for PWRs). In other words, the exposure dose peak is reduced to approximate 25% of its previous value due to the use of detailed oxide film data that the BWR cladding has a thin oxide film. Other instantaneous release components for C-14 such as the fuel residual were negligible. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Confirmatory Survey Results for Portions of the Materials and Equipment from Units 1 and 2 at the Humboldt Bay Power Plant, Eureka, California

The Pacific Gas & Electric Company (PG&E) operated the Humboldt Bay Power Plant (HBPP) Unit 3 nuclear reactor near Eureka, California under Atomic Energy Commission (AEC) provisional license number DPR-7. HBPP Unit 3 achieved initial criticality in February 1963 and began commercial operations in August 1963. Unit 3 was a natural circulation boiling water reactor with a direct-cycle design. This design eliminated the need for heat transfer loops and large containment structures. Also, the pressure suppression containment design permitted below-ground construction. Stainless steel fuel claddings were used from startup until cladding failures resulted in plant system contamination—zircaloy-clad fuel was used exclusively starting in 1965 eliminating cladding-related contamination. A number of spills and gaseous releases were reported during operations resulting in a range of mitigative activities (see ESI 2008 for details).

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Neutron Diffraction Measurement of Residual Stresses, Dislocation Density and Texture in Zr-bonded U-10Mo ''Mini'' Fuel Foils and Plates

Aluminum clad monolithic uranium 10 weight percent molybdenum (U-10Mo) fuel plates are being considered for conversion of several research and test nuclear reactors from high-enriched to low-enriched uranium fuel due to the inherently high density of fissile material. Comprehensive neutron diffraction measurements of the evolution of the textures, residual phase stresses, and dislocation densities in the individual phases of the mini-foils throughout several processing steps and following hot-isostatic pressing to the Al cladding, have been completed. Recovery and recrystallization of the bare U-10Mo fuel foil, as indicated by the dislocation density and texture, are observed depending on the state of the material prior to annealing and the duration and temperature of the annealing process. In general, the HIP procedure significantly reduces the dislocation density, but the final state of the clad plate, both texture and dislocation density, depends strongly on the final processing step of the fuel foil. In contrast, the residual stresses in the clad fuel plate do not depend strongly on the final processing step of the bare foil prior to HIP bonding. Rather, the residual stresses are dominated by the thermal expansion mismatch of the constituent materials of the fuel plate.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Severe Accident Test Station (SATS) Activity Report

Enhancing safety margins in light water reactor (LWR) severe accidents is currently the focus of a number of international R&D programs. The current UO 2 /Zr-based alloy fuel system is particularly susceptible since the Zr-based cladding experiences rapid oxidation kinetics in steam at elevated temperatures. Therefore, alternative cladding materials that offer slower oxidation kinetics and a smaller enthalpy of oxidation can significantly reduce the rate of heat and hydrogen generation in the core during a coolant-limited severe accident. In the U.S. program, the high temperature steam oxidation performance of accident tolerant fuel (ATF) cladding solutions has been evaluated in the Severe Accident Test Station (SATS) at Oak Ridge National Laboratory (ORNL) since 2012. This report summarizes the capabilities of the SATS and provides an overview of the oxidation kinetics of several candidate cladding materials. A suggested baseline for evaluating ATF candidates is a two order of magnitude reduction in the steam oxidation resistance above 1000°C compared to Zr-based alloys. The ATF candidates are categorized based on the protective external oxide or scale that forms during exposure to steam at high temperature: chromia, alumina, and silica. Comparisons are made to literature and SATS data for Zr-based alloys and other less-protective materials.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗