At least 1,261 records · Page 70

Microstructure and mechanical properties of resistance-spot-welded joints for A5052 aluminum alloy and DP 600 steel

The microstructure and mechanical properties of resistance-spot-welded A5052 aluminum alloy and DP 600 dual-phase steel joint were studied. The fusion zone (FZ) and heat-affected zone (HAZ) of DP 600 exhibited lath martensite and ferrite-martensite structures, respectively. The microstructure of FZ and HAZ in the A5052 side was composed of cellular crystals and the boundary region of FZ exhibited a columnar crystal morphology. A Fe{sub 2}Al{sub 5} intermetallic compound (IMC) layer with 3.3 μm thickness was found adjacent to the DP 600 side, whereas a needle-shaped Fe{sub 4}Al{sub 13} IMC layer with length of 0.67 μm to 15.8 μm was found adjacent to the aluminum alloy side. The maximum tensile shear load of the A5052/DP 600 joint was 5.5 KN, with a corresponding molten nugget diameter of 6.3 mm. The fracture morphology of the optimized A5052/DP 600 joint was mainly an elongated dimple fracture accompanied by cleavage fracture. - Highlights: •A5052 and DP 600 with large gaps in properties were investigated by RSW. •The microstructures of RSW joints in DP 600/A5052 were examined detailedly. •The micro/macro-characteristics and strength relations of joints were analyzed.

36 MATERIALS SCIENCE↗

Microstructure of a safe-end dissimilar metal weld joint (SA508-52-316L) prepared by narrow-gap GTAW

The microstructure, residual strain and interfacial chemical composition distribution of a safe-end dissimilar metal weld joint (DMWJ, SA508-52-316L) prepared by narrow-gap gas-tungsten arc welding (NG-GTAW) were studied by optical microscope (OM) and scanning electron microscope equipped with an energy dispersive X-ray microanalysis (SEM/EDX) and an electron back scattering diffraction (EBSD) system. Complex microstructure and chemical composition distribution are found, especially at the SA508-52 interface and the 52-316L interface. In brief, a complicated microstructure transition exists within the SA508 heat affected zone (HAZ); the residual strain, the fraction of high angle random grain boundaries and low angle boundaries decrease with increasing the distance from the fusion boundary in 316L HAZ; neither typical type II boundary nor obvious carbon-depleted zone is found near the SA508-52 interface; dramatic and complicated changes of the contents of the main elements, Fe, Cr and Ni, are observed at the distinct interfaces, especially at the SA508-52 interface. No carbon concentration is found at the SA508-52 interface. - Highlights: •Residual strain and GBCD change as a function of the distance from FB in 316L HAZ. •Neither type II boundary nor obvious carbon-depleted zone is found in SA508 HAZ. •No carbon concentration is found at the SA508-52 interface. •The middle part of the DMWJ has the highest residual strain.

36 MATERIALS SCIENCE↗

Microstructures of chemical vapor deposited high-purity tungsten achieved by two different precursors

Highlights: • CVD tungsten used as electron emitters of thermionic fuel elements was investigated. • Microstructures were characterized with metallography analysis. • The preferred orientation was determined with XRD and EBSD. • The surface morphology was observed with SEM and WLI. • Tungsten via thermolysis of WCl{sub 6} is better for thermionic fuel elements. - Abstract: Chemical vapor deposited (CVD) high-purity tungsten can be manufactured as electron emitters in thermionic fuel elements. Exposed surface planes of the emitter emit electrons and affect the efficiency and load capacity of the thermionic fuel element. In order to determine the electron emission planes of the emitter, the metallurgic structures, the preferred orientation and the as-deposited surface morphology of CVD tungsten have been investigated. In this work, high-purity (over 99.99%) tungsten was achieved by two different precursors: hydrogen reduction of tungsten hexafluoride (WF{sub 6}) and thermolysis of tungsten hexachloride (WCl{sub 6}). The microstructures of CVD tungsten were characterized by metallography analysis, X-ray diffraction (XRD), electron backscattered diffraction (EBSD), and white light interference (WLI). Tungsten fabricated by hydrogen reduction of WF{sub 6} and thermolysis of WCl{sub 6} has <100>-preferred columnar microstructures. However, the latter exhibits larger columnar grains and preferred <100> less. The preferred orientation is caused by the higher growth rate of the <100> orientation and competition between the <100> orientations of different grains. The as-deposited surface consists of tiny pyramids, with <100> axis and {111} side faces. In contrast to tungsten produced by hydrogen reduction of WF{sub 6}, the pyramid on tungsten synthesized via thermolysis of WCl{sub 6} contains small {110} facets on the four edges. Therefore, tungsten made via thermolysis of WCl{sub 6} is a better candidate for thermionic fuel elements, because the higher work function of {110} planes enables better output efficiency.

36 MATERIALS SCIENCE↗

Microstructural characterization and comparison of Ti-6Al-4V manufactured with different additive manufacturing processes

In this work, the microstructures of Ti-6Al-4V manufactured by different additive manufacturing (AM) processes have been characterized and compared. The microstructural features that were characterized are the α lath thickness, grain boundary α (GB-α) thickness, prior β grain size and α colony size. In addition, the microhardnesses were also measured and compared. The microstructure of shaped metal deposited (SMD) Ti-6Al-4V material showed the smallest variations in α lath size, whereas the material manufactured with laser metal wire deposition-0 (LMwD-0) showed the largest variation. The prior β grain size was found to be smaller in material manufactured with powder bed fusion (PBF) as compared with corresponding material manufactured with the directed energy deposition (DED) processes. Parallel bands were only observed in materials manufactured with DED processes while being non-present in material manufactured with PBF processes.

36 MATERIALS SCIENCE↗

Creep-induced microstructural evolution in a nickel-based superalloy designed for advanced ultra-supercritical boilers

Highlights: • Microstructural evolution of a nickel-based superalloy during long-term creep was investigated. • Precipitate-free zones (PFZs) widely arose near the grain boundary under stress. • The coarsened and elongated particles in the PFZs were identified as γ′ precipitates. • The boundary movement plays a role in evolution of grain boundary precipitates. - Abstract: Long-term microstructural stability is a major concern for candidate materials used in advanced ultra-supercritical (A-USC) power plants. In the present work, precipitation behavior of a nickel based superalloy designed for A-USC boilers, with a base composition of Ni-25Cr-20Co, was investigated during long-term thermal exposure under different stresses at 1043 K. The results showed that the coarsening of γ′ precipitates in the grain interior had occurred during thermal exposure in the presence and absence of stress. The microstructure around grain boundary was altered remarkably under stress. The precipitate-free zones (PFZs) commonly existed near the grain boundary in the gauge sections of specimens after long-term creep. Coarsened and elongated particles in the PFZs were identified as γ′-Ni{sub 3} (Ti, Al) precipitates by chemical composition analysis and diffraction pattern. Furthermore, the morphology and distribution of MC-type carbides have no significant changes observed due to their good stability, but discontinuous M{sub 23}C{sub 6} appeared under stress, due to formation of PFZs resulting in dissolution of the adjacent M{sub 23}C{sub 6}. Besides, the creep-rupture mechanism was discussed to explore a potential approach for improving creep properties.

36 MATERIALS SCIENCE↗

Effect of build geometry on the microstructural development of 316L parts produced by additive manufacturing

Highlights: • Stainless steel ribs were created via direct metal laser sintering to investigate microstructural effect of part design. • EBSD confirmed the presence of large elongated grains in the center of the part, with preferred orientation. • Small grains at the rib surface were found to grow towards the center of the rib with random orientation. • By changing rib thickness and build angle varying texture was observed in the final products. • Large intragranular misorientations were observed in all samples. - Abstract: Additive manufacturing (AM) technology has shown great potential in manufacturing complex products, such as lattice structures without extensive tooling. The focus of this study was to understand the effect of the part geometry on the resulting microstructure. Direct metal laser sintering was used for fabrication of ribs with thicknesses varying between 0.2 and 3.0 mm as well as inclined ribs the with build angles of 30° and 45°. The investigation showed that grains were growing in an epitaxial manner parallel to the building direction. The large elongated grains had a preferential orientation, resulting from the temperature gradient. Additionally, it was found that small grains had formed close to the part surface which were inclined towards the center of the rib. In contrast to the elongated grains, they had a random orientations. The results also indicated that at build angles below 45°, the formed microstructure consisted of the large grains elongated in the building direction. For the used process parameters, the critical part thickness to avoid large elongated grains was found to be about 0.4 mm. These findings allowed us to establish the basics for design rules when it comes to thin wall structures.

36 MATERIALS SCIENCE↗

Non-equilibrium approach to prediction of microstructure evolution for metals undergoing severe plastic deformation

Highlights: • New consistent physically-based model of dynamic recrystallization. • The model is based on evolution of fraction of high-angle grain boundaries. • Possibility to predict the evolution of dislocation cells and grain boundaries. • The model is implemented for FEM simulations. • Results demonstrate inhomogeneous distribution of strain within the sample. - Abstract: Available models of dynamic recrystallization have a number of disadvantages that in most cases make them inapplicable for practical predictions of material microstructure evolution. Both the microstructural and the empirically based approaches do not reflect physical processes leading to evolution of material defect structure in the process of plastic deformation. This work presents an attempt to develop a consistent physically-based model of dynamic recrystallization. This model, accounting for physical nature of processes of material defect structure evolution, should provide a possibility to predict evolution of several different experimentally measurable parameters of material microstructure without introduction of big number of fitting parameters. It is suggested that such a model should be based on equation for evolution of fraction of high-angle grain boundaries (HAGBs) in the process of deformation. It is shown, that the new model gives a possibility to predict the evolution of dislocation cells and grain boundaries in copper-based alloys providing good coincidence with experimental observations. Full 3-dimensional numerical simulation of multidirectional forging of copper is performed utilizing the developed dynamic recrystallization model. The same 3D simulations demonstrate new noteworthy effects connected to inhomogeneous distribution of plastic strain within the bulk of the material and material strain hardening.

36 MATERIALS SCIENCE↗

Influence of rapid heating and cooling combined with deformation at ultrahigh strain rates on the microstructure evolution of pure titanium shaped charge liner

Highlights: • A slug prepared from pure titanium SCL was recovered after detonation deformation at an ultrahigh strain rate over 10{sup 5} s{sup −1}. • The α → β → α phase transformation occurred in Ti SCL during the ultrahigh-strain -rate deformation. • The microstructures of the recovered slug included lamellar α grains, equiaxed α grains, and jagged α grains. - Abstract: A slug prepared from pure titanium shaped charge liners was recovered after detonation deformation at an ultrahigh strain rate over 10{sup 5} s{sup −1} and high strain over 500%. Optical microscopy, electron backscattered diffraction (EBSD), and transmission electron microscopy (TEM) were employed to investigate the microstructure of the Ti shaped charged liner before and after the detonation deformation. The microstructures of the recovered slug include lamellar α grains, equiaxed α grains within localized shear bands, and jagged α grains. EBSD results indicated that the grain orientation distribution is random and no texture was observed in the slug. TEM observation revealed that the α → β → α phase transformation occurred owing to the rapid heating and cooling combined with deformation at ultrahigh strain rates in the Ti shaped charge liner. No melting phenomenon was observed during the deformation process. The deformation process consisted of the explosive detonation stage combined with rapid heating and the subsequent penetration stage combined with rapid cooling. In the explosive detonation stage, the α → β phase transformation instantaneously occurred via a martensitic mechanism. In the penetration stage, the high-temperature slug in β state was cooled rapidly and showed different deformation behaviors in three different areas.

36 MATERIALS SCIENCE↗

Effect of annealing after strip casting on microstructure, precipitates and texture in non-oriented silicon steel produced by twin-roll strip casting

Highlights: • Non-oriented silicon steel with superior magnetic properties was produced by twin-roll strip casting. • The effect of annealing after strip casting on microstructure, precipitates and texture was investigated. • Role of precipitates in microstructure and texture evolution along the entire route was explored. • High magnetic induction and strong λ-fiber texture was obtained by optimizing strip annealing process. - Abstract: A 3.1 mm thick non-oriented Fe-1.0% Si steel as-cast strip was produced by twin-roll strip casting. Samples with/without strip annealing were cold rolled to 0.5 mm and then annealed. The development of microstructure, precipitate and texture was characterized along the entire processing route. It was found that annealing after strip casting had a minor influence on the average grain size and texture of the as-cast strip. A large number of particles precipitated and coarsened during the strip annealing process. Meanwhile, precipitates hindered dislocation slip and crystal rotation such that more significant in-grain shear bands were formed in cold rolled sheets. During recrystallization annealing process, the newly formed fine precipitates in directly cold-rolled sheets consumed stored strain energy and also hindered grain growth. But the initial precipitates in the annealed strip grew further and the effect of pinning of dislocations and grain boundary was lost. Therefore, annealed sheets with strip annealing process showed homogeneous equiaxed grains and the recrystallization texture was characterized by strong λ-fiber texture, which led to high permeability.

36 MATERIALS SCIENCE↗

Microstructure characterization by X-ray tomography and EBSD of porous FeCr produced by liquid metal dealloying

Highlights: • FeCr-Ni precursors were dealloyed in a Mg bath to give FeCr-Mg bicontinuous structure. • FeCr-Mg bicontinuous structure was immersed in HNO{sub 3} solution to get porous FeCr. • (FeCr){sub x}-Ni{sub 1−x} precursors are fully FCC phase while porous FeCr are fully BCC phase. • Composition & dealloying parameters are key parameters for controlling microstructure - Abstract: Liquid metal dealloying is a promising technique to get nanoporous materials which are attractive for their excellent functional properties. From a (FeCr){sub x}-Ni{sub 1−x} precursor, it is possible to get porous FeCr with this technique. While immersing precursors in a molten Mg bath, Ni atoms selectively migrate into the Mg bath. After cooling down to room temperature, the resulting microstructure is a bi-continuous structure of FeCr and Mg (with Ni in solid solution). A final etching step removes the Mg solid-state solution phase. Precursors with different compositions were dealloyed and imaged in 3D. From X-ray tomography images, porous FeCr characteristics as solid fraction, phase size, specific surface were extracted. EBSD maps were acquired on samples before and after dealloying. We will show that precursor composition is a key parameter to control pores and grains size while dealloying parameters (time and temperature) are key parameters to control ligaments size and in fine specific surface. By controlling precursor composition and dealloying parameters it is now possible to get dealloyed nanoporous metals with desired grain and porous microstructure by liquid metal dealloying.

36 MATERIALS SCIENCE↗

Microstructural evolution and electrical resistivity of nanocrystalline W thin films grown by sputtering

Highlights: • W thin films with thicknesses of 5–40 nm were deposited by sputtering and annealed up to 400°C. • Grain size of the beta (β)-W was about 5 nm, whereas that of the alpha (α)-W was about 130 nm. • Thickness dependent electrical resistivity variations as a function of annealing temperature were presented. - Abstract: Tungsten (W) thin films and nanostructures, particularly those having a beta (β)-phase, have attracted a large amount of attention lately because an ultrathin β-phase W film attached to a ferromagnetic layer can reverse the direction of magnetization upon current injection. However, in-depth microstructural studies including the phase transformation in W films as a function of thickness and post-deposition heat treatment temperature are rare. Here, we report the microstructural evolution and the change in the electrical resistivity of W films with thicknesses of 5–40 nm. Microstructural analyses indicate that the β-W is nanocrystalline with a small grain size of about 5 nm, while the alpha (α)-W has a grain size larger than 130 nm with random crystal orientation. We present a state diagram showing the phase of the W film as functions of film thickness and annealing temperature.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Local residual stresses and microstructure within recrystallizing grains in iron

The intragranular strains and the microstructure within recrystallizing grains in single phase pure iron have been systematically studied in 3D using synchrotron micro-diffraction. In contradiction to common knowledge we observe that residual elastic strains of up to 1–2 × 10 –3 are present in the recrystallizing grains. The local strain variations within individual grains can be similar in magnitude to those between different grains. The effects of processing parameters, including rolling reduction, recrystallized volume fraction, and cooling rate, as well as microstructural parameters, including grain size, orientation and internal misorientation, on the development of local residual elastic strains and microstructure have been quantified. It is suggested that the difference in local defect density between recrystallized grains and the surrounding deformed matrix, as well as the redistribution of medium to long-range residual stresses in the deformed grains, are the main reasons for the development of such strains in the recrystallized grains. The local residual stress levels are calculated and their possible impact on the mechanical properties and recrystallization processes are discussed.

36 MATERIALS SCIENCE↗

Influence of fabrication on microstructure and heat affected zone width in weldments of nuclear reactor pressure vessel steel

Advanced manufacturing routes such as electron beam welding and powder metallurgy with hot isostatic pressing are increasingly used across energy and aerospace industries, where the reliable prediction of weld behavior and heat affected zone (HAZ) evolution is critical. This study examines how fabrication routes and post-weld heat treatments influence phase distribution, crystallite size, microstrain, and dislocation density in nuclear reactor pressure vessel steels using synchrotron X-ray diffraction (SXRD). Retained austenite occurs only in samples that did not undergo austenitization, whereas an austenitizing heat treatment fully eliminates retained austenite and produces a more uniform microstructure across the weldment in terms of phase fraction, dislocation density, and microstrain. The Rosenthal solution underestimates the HAZ width for powder metallurgy samples. A newly proposed modified Rosenthal solution, reducing density by accounting for porosity, matches the SXRD-measured HAZ width with a 0.65% error. Structure–property correlations reveal that dislocation density correlates strongly with nanohardness in homogenous microstructures, while in heterogenous weldments nanohardness is further influenced by the presence of dissimilar phase boundaries. These findings provide new insight into the thermal and microstructural response of powder metallurgy fabricated steels and offer a framework for optimizing welding procedures and heat treatments in advanced manufacturing applications.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Controlling homogenization length scales and microstructure in additively manufactured Ti-Ta functionally graded materials

Materials with smooth compositional gradients or functionally grade materials (FGMs) produced via additive manufacturing (AM), enables joining dissimilar materials and optimizing multiple properties in advanced engineering applications. However, as-printed AM microstructures exhibit micro-segregation and solidification defects which, when combined with controlling macroscale gradient properties, complicates necessary post-processing. Here, we use CALPHAD-informed diffusion modelling to design post-processing heat treatments for lightweight to refractory FGMs. Ti-Ta (0 to 85 at. % Ta) FGMs were fabricated using laser-based directed energy deposition AM. Post-processing heat treatments at 1000° C and 1500° C were designed to promote homogenization across specific length scales and experimentally validated. Investigation of chemical segregation and microstructures demonstrated that the length scale of homogenization is controlled as a function of time, temperature, and local composition. Ta-rich regions exhibited incomplete homogenization compared to Ti-rich layers. Unmelted Ta particles were found to completely dissolve at 1500 °C. By controlling cooling rate (200 °C/min), martensitic structures were produced between 14–36 at. % Ta, consistent with martensite-start temperatures calculations, while furnace cooling (2 °C/min) produced α+β morphologies. This work establishes a validated predictive framework for designing post-processing to tailor microstructure and chemical architecture in AM FGMs, facilitating their deployment in demanding environments.

Materials science↗

TiO2 nanotubes grown on Ti substrates with different microstructure

Highlights: • TiO{sub 2} nanotube layers were grown on four different Ti substrates by anodization. • Ti substrates with completely different microstructures were used. • The grain size of the substrates ranged from nanocrystalline to single-crystalline. • Differences between the nanotubes grown on these substrates were evaluated. • Similar nanotube dimensions were received on all Ti substrates. - Abstract: Four Ti substrates with various microstructures were investigated for the anodic growth of TiO{sub 2} nanotube layers: nanocrystalline and single-crystalline ingots as well as microcrystalline thick Ti sheets and microcrystalline thin Ti foils. All substrates were anodized in a conventional ethylene glycol based electrolyte under identical conditions. The resulting TiO{sub 2} nanotube layers were compared in dimensions and the consumption of Ti required for their growth. Unexpectedly, the results showed that on all substrates nanotube layers with a similar thickness and nanotube diameter, as well as a similar degree of ordering and after annealing the same crystallographic orientation of anatase were received, regardless the microstructures. However, the nanotube layers grown on a Ti sheet revealed a slightly higher thickness compared to the other substrates which were assigned to slower field-assisted dissolution rates due to different impurities found in this substrate compared to other ones.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Heterogeneous microstructural evolution during hydrodynamic penetration of a high-velocity copper microparticle impacting copper

Microparticle hydrodynamic penetration (HDP) may be associated with the erosion regime in cold spray processing and other high-velocity impact events. Here, in an experimental approach where we can individually launch particles and study the impact sites, we explore copper microparticles impacted on copper substrates at velocities above 900 m/s where HDP begins. We lift cross-sectional lamellae from the impact sites with a focused-ion beam for further microstructural characterization using electron backscatter diffraction and scanning transmission electron microscopy. Due to the gradients of strain, strain rate, and temperature associated with HDP, heterogeneous microstructures result. The structural evolution processes observed include deformation twinning and multiple dislocation-mediated grain recrystallization mechanisms—geometric dynamic recrystallization (gDRX), discontinuous DRX (dDRX), and meta DRX (mDRX). The higher strains at the interface lead to the most significant structural changes and complex mechanisms. In contrast, there is a gradient to more conventional dislocation plasticity away from the interface (on either the particle or substrate side). Here, these microstructural observations are consistent with the deformation map for copper and extend the observations of impact-induced recrystallization across new regimes of behavior.

Cold spray process↗

Microstructure and mechanical properties of Ti–6Al–4V: Mill-annealed versus direct metal laser melted alloys

Additive manufacturing processes such as direct metal laser melting (DMLM) are known to produce highly anisotropic microstructures. The present work compares the microstructure and mechanical properties of DMLM Ti–6Al–4V with that of mill-annealed alloys. Results show that the yield and hardening response of DMLM Ti–6Al–4V does not depend on the testing direction relative to the build direction, while the response of mill-annealed Ti–6Al–4V strongly depends on the testing direction. In conclusion, these results are discussed in light of the microstructure, texture, and polycrystal plasticity modeling.

36 MATERIALS SCIENCE↗

The effects of microstructural stability on the compressive response of two cast aluminum alloys up to 300 °C

Here in this study, the high temperature compressive response of cast aluminum alloys 319 and RR350 is compared in light of their microstructures. The 319 alloy is widely used in thermally critical automotive applications and provides a baseline for comparison with the RR350 alloy, whose microstructural stability at high homologous temperatures was recently reported. Cylindrical compression samples from each alloy were tested at four temperatures up to 300 °C at a constant true strain rate that was varied over four orders of magnitude. Although both alloys are strengthened by metastable precipitates (nominally Al 2 Cu) in the as-aged condition, their mechanical response diverges at temperatures greater than 250 °C as the strengthening precipitates evolve in the 319 alloy and retain their as-aged morphology in the RR350 alloy. Deformation mechanisms of each alloy are examined using microstructural analysis and empirical activation energy calculations. The stability of the θ' phase in the RR350 alloy leads to effective precipitation hardening at homologous temperatures up to 0.6 and an extensive regime of grain boundary controlled deformation.

36 MATERIALS SCIENCE↗