Preparation and Dynamic Mechanical Properties at Elevated Temperatures of a Tungsten/Glass Composite

Experiments were conducted to prepare a borosilicate glass matrix composite containing 50 vol.% tungsten and examine its dynamic compressive behavior at elevated temperatures in the range of 450-775 °C. The results show that the homogenous microstructure of the tungsten/glass composite with relative density of ~ 97% can be obtained by hot-pressing sintering at 800 °C for 1 h under pressure of 30 MPa. Dynamic compressive testing was carried out by a separate Hopkinson pressure bar system with a synchronous device. The results show that the peak stress decreases and the composite transforms from brittle to ductile in nature with testing temperature increasing from 450 to 750 °C. The brittle–ductile transition temperature is about 500 °C. Over 775 °C, the composite loses load-bearing capacity totally because of the excessive softening of the glass phase. In addition, the deformation and failure mechanism were analyzed.

36 MATERIALS SCIENCE↗

The Prediction of Microstructure Evolution of 6005A Aluminum Alloy in a P-ECAP Extrusion Study

Finite element modeling (FEM) was applied for predicting the recrystallized structure in extruded 6005 aluminum alloy, and simulated results were experimentally validated. First, microstructure evolution of 6005 aluminum alloy during deformation was studied by means of isothermal compression test, where the processing parameters were chosen to reproduce the typical industrial conditions. Second, microstructure evolution was analyzed, and the obtained information was used to fit a dynamic recrystallization model implementing inside the DEFORM-3D FEM code environment. FEM of deformation of 6005 aluminum has been established and validated by microstructure comparison. Finally, the obtained dynamic recrystallization model was applied to tube extrusion by using a portholes-equal channel angular pressing die. The finite element analysis results showed that coarse DRX grains occur in the extruded tube at higher temperature and in the extruded tube at the faster speed of the stem. The test results showed material from the front end of the extruded tube has coarse grains (60 μm) and other extruded tube has finer grains (20 μm).

36 MATERIALS SCIENCE↗

Densification, Microstructural Evolution, Mechanical Properties and Oxidation Study of CrB{sub 2} + EuB{sub 6} Composite

This paper reports the results of investigation on densification, microstructural evolution, mechanical properties and oxidation study of CrB{sub 2} + EuB{sub 6} composite. CrB{sub 2} + EuB{sub 6} (10 and 20 wt.%) composites have been fabricated by hot pressing at a temperature of 1700 °C and 35 MPa pressure. The hardness and flexural strength were measured in the range of 21.25-24.48 GPa and 171-199 MPa, respectively. The fracture toughness increased from 3.3 to 4.01 MPa m{sup 1/2} by the addition of 20% EuB{sub 6}. Microstructural evolution revealed the uniform distribution of EuB{sub 6} and absence of any reaction product. Fracture surface analysis confirmed the presence of transgranular mode of fracture. Oxidation study at 1200 °C revealed that the developed composites have good oxidation resistance and followed the parabolic rate of oxidation.

36 MATERIALS SCIENCE↗

Control of Carbon Content in Ultrafine Cemented Carbide by Heat Treatment in Reducing Atmospheres Containing Carbon Oxides

In this work, the method of control of carbon content in the ultrafine-grained cemented carbide alloy was proposed. The treating of the WC-8Co-0.4VC-0.4Cr{sub 3}C{sub 2} compacts was made in a CO + CO{sub 2} gas mixture at CO concentrations from 0 to 80 vol.% during 50 min at the initial stage of the conventional sintering at a temperature of 700 °C. Conditions for increasing and decreasing the carbon content are CO concentrations of CO in gas mix more than 65 vol.% and less than 35 vol.%, respectively. It is shown that even a small deviation from the stoichiometric carbon content (0.3 wt.%) leads to an increase in porosity and a multiple decrease in the strength of the ultrafine-grained cemented carbide. A comparative analysis with literature data showed that the obtained ultrafine-grained solid alloy WC-8Co-0.4VC-0.4Cr{sub 3}C{sub 2} with stoichiometric composition is not inferior in hardness and toughness to the analogs obtained by hot pressing and electrospark sintering.

36 MATERIALS SCIENCE↗

Effect of Different Post-treatments on the Microstructure of EBM-Built Alloy 718

Electron beam melting (EBM) of Alloy 718 is of rapidly growing interest as it allows cost-effective production of complex components. However, the inherent flaws in the component in as-built state are of concern in view of the severe working conditions in which Alloy 718 components typically operate. The present work entails an investigation of changes in microstructure that accompany some post-treatments that are being widely considered to address defects in EBM processed Alloy 718. The effect of two different post-treatments, namely hot isostatic pressing (HIP) and a combined HIP + heat treatment (HT) carried out inside the HIP vessel, have been studied and results from as-built and post-treated specimens were compared in terms of porosity/lack-of-fusion, microstructure, phase constitution (NbC content, δ-phase) and micro-hardness. Post-treatment resulted in reduction in defect content by more than an order of magnitude. HIPing led to complete dissolution of δ phase. In comparison to as-built material, HIPed specimens exhibited significant drop in hardness. However, a sharp ‘recovery’ of hardness to yield values higher than in as-built condition was observed after HIP + HT and can be attributed to precipitation of γ′′ phase.

36 MATERIALS SCIENCE↗

Tribological Behavior of Solid-State Processed Al-1100/GNP Surface Nanocomposites

Graphene nanoplatelets (GNPs) were infused onto aluminum alloy (Al-1100) surface by a solid-state processing technique to form surface nanocomposites which enrich the mechanical and tribological properties of the aluminum (Al) surface. Electrical resistance heating which locally softens the Al surface, followed by hot pressing, mechanically impregnates and embeds GNPs onto the Al substrate. It was observed that the GNPs mainly occupy the grain boundaries in the matrix during subsequent solidification which leads to strengthening of the matrix through various mechanisms. A detailed tribological study was carried out, and it was found that the wear rate and coefficient of friction decreases by > 85%. Least wear depth in nanoscratch testing was obtained at processing parameters 2200 A and 0.5 s, which could be identified as the optimum current/time combination. The microhardness and Young’s modulus results also show an improvement > 200%, corroborating the tribological studies.

36 MATERIALS SCIENCE↗

Effect of Sintering Atmosphere on the Synthesis Process, Electrical and Mechanical Properties of NiFe{sub 2}O{sub 4}/Nano-TiN Ceramics

NiFe{sub 2}O{sub 4}/nano-TiN ceramics were fabricated by a two-step cold-pressing sintering process. Effect of sintering atmosphere (air, nitrogen, argon) on the synthesis process of NiFe{sub 2}O{sub 4}/nano-TiN ceramics was investigated. The DSC-TG and XRD analysis results indicated that besides principal phases of NiO and NiFe{sub 2}O{sub 4}, new-phase Ni{sub 3}TiO{sub 5} formed in the sintered ceramics under the three sintering atmospheres, and metallic phase including iron and nickel appeared in the sintered samples with inert gas (nitrogen, argon) sintering condition. Microstructure analysis results showed that considerable quantity of micropores appeared in the ceramic samples sintered under inert gases (argon, nitrogen), but lower porosity (3.0, 3.6%) and higher densities (4.78 g/cm{sup 3}, 4.51 g/cm{sup 3}) can be obtained, comparing to the both values (14.4%, 4.17 g/cm{sup 3}) for the ceramic samples sintered under air atmosphere. Besides, the average bending strength and elastic modulus of the samples sintered under argon is 113.75 MPa and 7.13GPa, which is higher than that of 75.12 MPa, 5.42GPa and 91.96 MPa, 6.26GPa for the samples synthesized under air and nitrogen, separately. When changing sintering atmosphere from air to inert gases (argon, nitrogen), the fracture model of the 4 wt.%nano-TiN/NiFe{sub 2}O{sub 4} ceramics synthesized at 1400 °C for 4 h transformed from intergranular fracture to intergranular-transgranular fracture.

36 MATERIALS SCIENCE↗

Impact Behavior of Polyetheretherketone/Nickel Foam Co-continuous Composites

In this study, we prepared eight types of polyetheretherketone/nickel (PEEK/Ni) foam co-continuous phase composites (named “PEEK-Nis”) in which virgin PEEK was infiltrated into homologous hollow Ni structures by using hot pressing. Their Charpy impact behavior was investigated in accordance with ISO: 179-1, and the effect of the structure of the foam Ni on the impact properties of the PEEK-Nis was also studied. Compared with unfilled PEEK, the Ni prisms can effectively disperse, transfer, and absorb the energy of the pendulum, further improve the impact toughness of the PEEK-Nis and eventually lead to different fracture modes. The impact toughness of PEEK-Nis was mainly affected by Ni volume fraction, coating thickness, and pores per inch (PPI) value, which are mutually restricted. When the Ni content was less than 8.5%, the impact toughness of PEEK-Nis increased with an increase in PPI value. When the Ni content was between 8.5 and 18%, the impact toughness of PEEK-Nis increased with the coating thickness. When the Ni content exceeded 18%, the impact toughness decreased dramatically possibly because of the mechanical mismatch of the two-phase materials in PEEK-Nis. For further optimization, PEEK-NiB-2 was fabricated and had the most reasonable structure of the reinforcing phase. Among all PEEK-Nis, PEEK-NiB-2 exhibited the best impact toughness, with a value over two times that of unfilled PEEK.

36 MATERIALS SCIENCE↗

Powder Metallurgy HIP Process Study and Mechanical Property Evaluations for IN740H

The effects of hot isostatic pressing (HIP) parameters and powder size distribution (PSD) on the resulting microstructure and properties of powder metallurgy (P/M) IN740H have been investigated. Properties can be substantially tailored through the appropriate management of these parameters. Applying a thermal presoak to the input powder prior to the sintering stage of HIP can significantly increase average grain size and coarse grain fraction, enabling a trade for improved creep resistance at the expense of tensile strength. Here, powder thermal presoak was found to have a larger impact on microstructure and properties than the use of a coarser PSD alone. Additionally, substantial grain growth and grain boundary migration is observed in P/M IN740H at HIP temperatures above 1260°C. Given its inherently finer grain size, P/M HIP IN740H typically outperforms its cast and wrought counterparts in tensile response. Creep life at 700–800°C was inferior to wrought due to PPBs coincident with grain boundaries which served as cavity nucleation sites, leading to lower creep ductility. The ability to adjust the microstructure toward a more balanced creep and tensile behavior allows P/M HIP IN740H to be considered for high-temperature applications in advanced ultra-supercritical steam and supercritical carbon dioxide power cycles.

36 MATERIALS SCIENCE↗

On the efficacy of post-build thermomechanical treatments to improve properties of Zirconium fabricated using ultrasonic additive manufacturing

Here, hot-isostatic pressing has been applied to Zirconium plate fabricated using the ultrasonic additive manufacturing (UAM) technique to enhance interfacial bond quality. Specimens heated to 800 C for 1 h at 100 MPa pressure showed grain growth across many prior foil-to-foil interfaces, thereby increasing foil adhesion. In addition to the material softening induced by a loss of Hall-Petch strengthening, premature failure of specimens loaded parallel to the build direction was observed. Premature specimen failure was attributed to the local delamination at prior foil-to-foil boundaries where grain growth was pinned by Ti impurities introduced during the UAM process via the interaction between a Ti-alloy buffer foil and the welded Zr-foils underneath. In addition, the presence of Ti along select foil interfaces resulted in the nucleation and growth of secondary (Zr,Ti)(Fe,Cr) laves phases during higher-temperature thermomechanical processing. Using a combination of micro-scale X-ray computed tomography, fractography, and in-situ digital image correlation, the effect of defects along prior foil-to-foil boundaries was revealed as delamination-assisted plasticity accelerated specimen failure in preferred tensile orientations. These findings underscore the importance of impurity control when optimizing weld quality of higher-strength material systems using ultrasonic welding.

36 MATERIALS SCIENCE↗

Laboratory synthesis of C3S on the kilogram scale

An optimized process using amorphous silica for efficient C{sub 3}S synthesis in the laboratory is reported: an estimated production capacity of ~2 kg C{sub 3}S within a week is possible. Amorphous silica (fumed silica) was used as raw material and inter-ground with CaCO{sub 3} and water for C{sub 3}S synthesis, the dried raw mixture has sufficient green strength to be self-supporting, which allows large cylinders to be placed in Platinum crucibles. The mineral composition of the sintered sample was quantified with X-ray powder diffraction using Rietveld analysis. C{sub 3}S with 3 S synthesis was dramatically enhanced because of 1) increased burnability of the raw mix due to amorphous silica and very fine CaCO{sub 3} particles after grinding, 2) simplified sample preparation process avoiding pressing discs and 3) improved capacities of the crucible and furnace.

36 MATERIALS SCIENCE↗

Shell particles, trials, tribulations and triumphs

The concept of pellicular particles was imagined by Horvath and Lipsky fifty years ago. They were initially intended for the analysis of macromolecules. Later, shell particles were prepared. The rational behind this concept was to improve column efficiency by shortening the pathways that analyte molecules must travel and, so doing, to improve their mass transfer kinetics. Several brands of superficially porous particles were developed and became popular in the 1970s. However, the major improvements in the manufacturing of high-quality, fully porous particles, that took place in the same time, particularly by making them finer and more homogeneous, hampered the success of shell particles, which eventually disappeared. Recently, the pressing needs to improve analytical throughputs forced particle manufacturers to find a better compromise between the demands for higher column efficiency that require short diffusion paths of analyte molecules in columns and the need for columns that can be operated with the conventional instruments for liquid chromatography, which operate with moderate column back-pressures. This lead to the apparition of a new generation of columns packed with shell particles, which bring chromatographic columns to a level of efficiency undreamed of a few years ago. This evolution is reviewed, the reason that motivated it, and the consequences of their success are discussed.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Consolidation of cubic and hexagonal boron nitride composites

When we Consolidate cubic boron nitride (cBN) it typically requires either a matrix of metal bearing materials that are undesirable for certain applications, or very high pressures within the cBN phase stability field that are prohibitive to manufacturing size and cost. We present new methodology for consolidating high stiffness cBN composites within a hexagonal boron nitride (hBN) matrix (15–25 vol%) with the aid of a binder phase (0–6 vol%) at moderate pressures (0.5–1.0 GPa) and temperatures (900–1300 °C). The composites are demonstrated to be highly tailorable with a range of compositions and resulting physical/mechanical properties. Ultrasonic measurements indicate that in some cases these composites have elastic mechanical properties that exceed those of the highest strength steel alloys. Moreover, two methods were identified to prevent phase transformation of the metastable cBN phase into hBN during consolidation: 1. removal of hydrocarbons, and 2. increased cBN particle size. Lithium tetraborate worked better as a binder than boron oxide, aiding consolidation without enhancing cBN to hBN phase transformation kinetics. These powder mixtures consolidated within error of their full theoretical mass densities at 1 GPa, and had only slightly lower densities at 0.5 GPa. This shows potential for consolidation of these composites into larger parts, in a variety of shapes, at even lower pressures using more conventional manufacturing methods, such as hot-pressing.

36 MATERIALS SCIENCE↗

Influence of ionomer content on the structure and performance of PEFC membrane electrode assemblies

Nafion ionomer content of the cathode catalyst-layer of a polymer electrolyte fuel cell (PEFC), made by the decal hot pressing method, has been investigated for its effect on performance and structure of the membrane electrode assembly (MEA). Varying Nafion content was shown to have an effect on performance within the entire range of polarization curves (i.e. kinetic, ohmic, and mass-transport regions) as well as on the structure. AFM analysis shows the effect of Nafion on the dispersion of carbon aggregates. Further analysis using TEM demonstrates the effect of Nafion on both the dispersion of carbon aggregates and the distribution and thickness of the Nafion ionomer films surrounding the catalyst/carbon aggregates. The MEA structure change correlates well with the MEA performance on both kinetics and mass-transport region. The determining factors on the performance of MEA are the interfacial zone (between the ionomer and catalyst particle), the dispersion of catalyst/carbon aggregates and the distribution/thickness of Nafion films. An optimized Nafion content in the range of 27 6 wt.% for the cathode was determined for an E-TEK 20% Pt3Cr/C catalyst at a loading of 0.20mg Pt/cm2.

30 DIRECT ENERGY CONVERSION↗

Synthesis and Structural Stability of Ti2GeC

In this paper we report the synthesis of a ternary-layered ceramic, Ti2GeC, a 211 Mn+1AXn compound by hot-pressing. X-ray analysis confirmed the hexagonal crystal symmetry. Using a synchrotron radiation and a diamond anvil cell, we measured the pressure dependencies of the lattice parameters. The phase is structurally stable up to the 49 GPa-the maximum experimental pressure reached. The bulk modulus of Ti2GeC calculated using the Birch-Murnaghan equation of state is 211 {+-} 4 GPa with K? = 3.9 {+-} 0.2. Surprisingly the bulk modulus was found to be greater than both Ti2AlC and Ti2SC by 13% and 10%. Also, Ti2GeC has the highest bulk modulus among M2GeC phases where M = Ti, V, Cr.

43 PARTICLE ACCELERATORS↗

Synthesis of a New MAX Compound (Cr0.5V0.5)2GeC and its Compressive Behavior up to 49 GPa

In this paper we report for the first time the synthesis of a new ternary layered ceramic (Cr0.5V0.5)2GeC, a 211 Mn+1AXn compound by hot-pressing. Scanning electron microscopy and X-ray diffraction were used to characterize and confirm the hexagonal crystal structure of this ternary layered ceramic. The calculated lattice parameters are a = 2.9773 A and c = 12.1619 A. Using a diamond anvil cell and synchrotron radiation we also report the pressure dependencies of the lattice parameters. No phase transformation was observed and the phase is stable up to 49 GPa. The bulk modulus of (Cr0.5V0.5)2GeC calculated using the Birch-Murnaghan equation of state is 219 {+-} 5 GPa with K? = 4.1 {+-} 0.3, which is higher than the end members V2GeC and Cr2GeC.

36 MATERIALS SCIENCE↗

Synergistic cellulase–xylanase formulations for enhanced dewatering and fiber bonding toward energy-efficient and sustainable paper and packaging production

A mechanistic understanding of the synergistic effects of enzymes on cellulosic fibers dewatering and fiber bonding is essential for advancing energy-efficiency and lightweight production of paper and packaging materials. This study investigates the impact of varying cellulase and xylanase formulations on equilibrium moisture content (EMC) after pressing and tensile strength of cellulosic fiber webs using a factorial experimental design. Nine custom enzyme formulations were evaluated at controlled dosages ranging from ∼20 to 76 FPU/mL cellulase and ∼500–1130 IU/mL xylanase. Response surface modeling revealed a significant synergy, particularly at 20–40 FPU/mL cellulase combined with ≥ 1000 IU/mL xylanase. Under these conditions, EMC decreased by up to 3.6% compared with the untreated refined control, while tensile index gains of up to 16% were statistically significant for optimized blends (p < 0.05). The interaction between cellulase and xylanase was also significant for the tensile response (p = 0.010). Protein efficiency analysis showed that optimized formulations containing 30–40% less protein outperformed the commercial benchmark. The nonlinear synergy between cellulase and xylanase is attributed to their complementary substrate specificities. Endoglucanase- and β‑glucosidase‑rich cellulases hydrolyze internal β‑1,4‑glycosidic bonds in amorphous cellulose, loosening fiber walls and increasing flexibility, while xylanases target hemicellulose, primarily xylan-rich domains, enhancing porosity and improve cellulase accessibility. Tailoring enzyme formulations at low loadings overcomes traditional trade-offs between strength and dewatering, enabling cost-effective, energy-efficient, low-carbon solutions for sustainable packaging and hygiene products.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Ultrasonic additive manufacturing of steel: Method, post-processing treatments and properties

In this study, ultrasonic additive manufacturing (UAM) was applied to fabricate laminated carbon steel structures. The feasibility of UAM to manufacture low-alloy carbon steel samples was proven. Interface investigation of the UAM parts was conducted by SEM, EBSD and TEM analysis. Multiple defects at the interfaces of the as-printed parts were observed. In order to improve the structural homogeneity and mechanical properties of the parts, spark plasma sintering (SPS) and hot isostatic pressing (HIP) post-treatments were applied. As a result, after both treatments, interface defects were healed and the shear strength of the welding interfaces was significantly improved. Lastly, treatment by SPS apparatus showed higher shear strength improvements as compared to the HIP-treated specimens.

36 MATERIALS SCIENCE↗