Search NASA⌕ Search

SEARCH · Search NASA

Results for “Powder”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,261 records · Page 70

Influence of Braking Conditions on Tribological Performance of Copper-Based Powder Metallurgical Braking Material

High-speed transportation tools demand durable and effective friction materials for practical applications. In this work, we developed a copper-based powder metallurgical friction material via spark plasma sintering, and studied its tribological performances subjected to different braking conditions. Using inertial braking test bench and temperature measuring instrument, average friction coefficient, instantaneous friction coefficient and temperature near friction surface of the material in braking process were tested at two initial speeds (28, 69 m/s) and three contact pressures (0.4, 0.6 and 0.8 MPa). The wear rate of materials was calculated accordingly. Results show that under the same exerted pressure, the average friction coefficient and wear rate at the high speed are smaller than those at the low speed. At the high test speed, the high friction temperature leads to an obvious decrease in instantaneous friction coefficient when the braking process reaches a certain stage. Based on the friction surface morphology analysis, the adhesive wear on the surface has been reduced because of the formation of oxide films at the high speed and surface oxidation wear gradually increases as the pressure increases.

36 MATERIALS SCIENCE↗

Build Rate Optimization for Powder Bed Fusion

The authors previously proposed a geometrically based model to predict the volume fraction of lack-of-fusion porosity in parts produced by powder bed fusion. To test this model, AlSi10Mg cubes with varying hatch spacing and layer thickness were printed in this work. Bulk densities of samples were measured with the Archimedes method and agree well with model predictions. The model was also validated by results from the literature on additively manufactured PA-12 polymer parts. Quantitative prediction of conditions that lead to part porosity allows considerable improvement in the volumetric build rate, compared with the default processing parameters provided by the equipment supplier. Nearly fully dense AlSi10Mg parts (> 99.5% dense) were fabricated with a build rate double that for standard conditions. Some melt-pool variability and large changes in hatch rotation angle do not affect the overall volume fraction of residual porosity.

36 MATERIALS SCIENCE↗

Analyzing the Effect of CeB{sub 6} on Microstructure and Mechanical Properties of High-Speed Steel Consolidated by Powder Metallurgy

By adding various amounts of CeB{sub 6}, high-speed steel (M3:2) was consolidated by powder metallurgy in the form of sintering. The addition of CeB{sub 6} improved the density of the sintered steel and the formation of M{sub 6}C phase in microstructure. It is speculated that CeB{sub 6} was decomposed into boron and cerium. Boron atoms were enriched in M{sub 6}C carbide phases, but cerium atoms were mainly clustered on grain boundary while they were converted to oxides, whereby the mechanical properties were improved. For example, upon the sintering at 1210 °C, relative density ~ 98.5% and average grain size ~ 18 μm were obtained with CeB{sub 6} content at 0.3 wt.%. Excellent mechanical properties, e.g., the Rockwell hardness ~ 52 HRC, flexural strength ~ 3.05 GPa, and fracture toughness ~ 40.92 MPa m{sup 1/2}, were achieved in the sample containing 0.3 wt.% CeB{sub 6}, which implies accordingly remarkable increases by 23.5, 38.1, and 23.7%, of the properties compared with those in the sample free of CeB{sub 6}.

36 MATERIALS SCIENCE↗

Mechanical and Tribological Behavior of Multiwalled Carbon Nanotubes-Reinforced AA7075 Composites Prepared by Powder Metallurgy and Hot Extrusion

Carbon nanotubes (CNT) are synthesized using arc discharge method in an open air. Various amounts of carbon nanotubes-reinforced AA7075 composites are prepared by powder metallurgy route and then hot extrusion at 450 °C. Hot-extruded composites are characterized, and mechanical properties are measured. Dry sliding wear properties of hot-extruded samples were evaluated using a pin-on-disk method for various loads (5-20 N) at room temperature and for various temperatures (100-400 °C) at the applied load 10 N as a function of CNT amount. Grain size of the composites is decreased compared with Al alloy matrix. Transmission electron microscopy of the composites revealed that the CNT are uniformly distributed in the composites. Mechanical properties of the hot-extruded composites are enhanced with an increase in CNT content. The wear performance is improved with an increased CNT amount, but decreases with an increase in the applied load and temperature as well. The wear damage is mild at lower applied loads and temperatures, whereas the damage is severe at 400 °C. The wear mechanism was plowing in the initial stages which is transformed to severe sliding and chipping with increasing load and temperature. The enhanced wear behavior of composites is attributed to self-lubricating nature of carbon nanotubes.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Laser Additive Manufacturing of (Ti-6Al-4V)/10 wt.% Ag Composite Using Spherical Powders to Reduce Wear and Friction

In order to extend the service lifetime of Ti-6Al-4V-based components, friction and wear behaviors of Ti-6Al-4V alloys needed to be further improved. Laser additive manufacturing with a moving laser beam was used to prepare (Ti-6Al-4V)/10 wt.% Ag samples, on a three-dimensional RC-SLM400 printer with laser powers of 2-10 kW. (Ti-6Al-4V)/10 wt.% Ag samples were successfully printed using spherical powders prepared by gas atomization process (SPGAP) and combustion reaction (SP-CR). The tribological properties of the as-prepared samples sliding against Si{sub 3}N{sub 4} balls were examined using a ball-on-disk tribometer. The results showed that the tribological behavior of (Ti-6Al-4V)/10 wt.% Ag printed by SP-CR was better than that of the sample printed by SPGAP. The low friction and reduced wear were mainly attributed to the formation of the lubrication layer containing large amounts of silver, which can exhibit an excellent deformation and plastic ductility. It effectively reduced the friction resistance and material loss and provided the good lubrication for 0-80 min, resulting in low friction and reduced wear of the samples prepared by SP-CR.

36 MATERIALS SCIENCE↗

Experimental and Numerical Analyses of the Consolidation Process of AA 7075–2 wt.% ZrO{sub 2} Powders by Equal Channel Angular Pressing

AA7075 matrix composite was obtained by mechanical alloying using ZrO{sub 2} particles as reinforcement. After that, the powders were cold-compacted into an aluminum tube and consolidated by equal channel angular pressing at 220 °C. The temperature influence was analyzed, and it was found by scanning electron microscopy that this route gave the minimum pore percentage. Besides, it was noticeable that the hardness was wide superior in comparison with the AA 7075 aged bulk alloy. In addition, there was no evidence of any chemical reaction between ZrO{sub 2} and alloying elements at the temperature employed. On the other hand, it was numerically and experimentally demonstrated that the more strained regions exhibited a higher relative density values.

36 MATERIALS SCIENCE↗

Effect of Heat Treatment on Microstructure and Mechanical Properties of Ti-6Al-4V-1.5Mn Fabricated by Powder Metallurgy

Ti-6Al-4V-1.5Mn alloy was prepared by powder metallurgy and solid solution aging treatment. Effect of composition segregation on properties of the titanium alloy was eliminated, and microstructure and the mechanical properties of the alloy were studied. Results show that the microstructure of Ti-6Al-4V-1.5Mn is composed of homogeneous α + β phase, and the optimal mechanical properties of the alloy are obtained when the solution temperature is 950 °C and the aging temperature is 460 °C. Analysis of the fracture illustrates that a small amount of dimple was found in the section and the fracture of the material was quasi-cleavage fracture.

36 MATERIALS SCIENCE↗

Mechanical Behavior of Titanium-Based Layered Structures Fabricated Using Blended Elemental Powder Metallurgy

Mechanical behavior of bilayered structures composed of the layer of Ti-6Al-4 V (wt.%) (Ti-64) alloy and metal matrix composite (MMC) on the base of this alloy reinforced with 5 and 10% (vol.) of either TiB or TiC particles has been studied. Structures were fabricated using blended elemental powder metallurgy and studied by tensile and three-point flexural tests. Mechanical tests were performed on uniform single-layer samples of the alloy as well as individual MMCs. In addition, bilayered structures were also tested in three-point flexural experiment. Posttest fractographic inspections were made using the SEM. The deformation energy was measured based on engineering stress–strain curves obtained on tensile test. The results were compared with the data previously reported on Ti-64 alloy fabricated using cast and wrought technique. The presence of TiB and TiC reinforcement particles in the alloy causes substantial drop in strength and ductility of MMCs as compared to uniform sintered Ti-64 alloy, since those particles provide additional sites for the cracks and pores nucleation and promote the embrittlement of material. However, when MMC layers are used in bilayered structures with Ti-64 alloy layers, the three-point flexural test demonstrates significant increase in flexure stress compared to uniform Ti-64 alloy and uniform structures of MMCs. The suitability of studied structures for antiballistic impact application is discussed.

36 MATERIALS SCIENCE↗

A New Approach for Consolidation of Pure Magnesium Powder Using an Integrated Severe Plastic Deformation Route

In this paper, a new approach using a novel severe plastic deformation route is presented for consolidation and processing of a high-density and ultrafine-grained pure magnesium. Pure magnesium particles were successfully consolidated at 400 °C into a sufficiently dense bulk material using a new combined method including cyclic extrusion compression, equal channel angular pressing (ECAP) and conventional extrusion. The grain refinement, consolidation behavior and mechanical properties were deeply investigated. Results showed that the as-consolidated material had a fine grain structure with excellent tensile strength and ductility compared to as-cast and as-ECAPed specimens. Vickers microhardness increased from 38.75 to 52.58 during the process. Porosity also reduced considerably from 12.55 to 1.2% during the process which led to a dense bulk material. Results indicate that the introduced method is a promising and effective process for producing strong bulk materials from metal powders.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of B{sub 4}C-Blended M3:2 High-Speed Steel Powders Consolidated by Sintering and Heat Treatment

Water-atomized powders of M3:2 high-speed steel (HSS) were blended with B{sub 4}C and consolidated by cold press sintering. With the addition of B{sub 4}C (~ 0.2 vol.%), satisfactory mechanical properties were achieved for HSS by sintering at a temperature as low as 1190 °C [e.g., 53.2 ± 0.2 in the Rockwell hardness (HRC) and 3074 ± 56 MPa in bending strength]. High relative density (98.5%) and good strength were attributed to the mechanism described as follows: First, the atoms of boron and carbon escaped after the reaction between B{sub 4}C and iron matrix. Then, the sintered HSS was strengthened by boron atoms while they were distributed in M{sub 6}C or MC carbides and iron matrix. Second, a plenty of M{sub 6}C carbides were formed due to the release of carbon atoms. As a result, the value of solidus temperature was reduced. In addition, mechanical properties were greatly improved by heat treatment (quenching and tempering) (e.g., 61.2 ± 0.3 in HRC, 4356 ± 64 MPa in bending strength, and 42.3 ± 0.5 MPa m{sup 1/2} in fracture toughness, respectively).

36 MATERIALS SCIENCE↗

Dust and powder in fusion plasmas: recent developments in theory, modeling, and experiments

Abstract In this paper, we present a brief historic overview of the research on dust in fusion devices with carbon plasma-facing components and then highlight the most recent developments in the post-carbon era of the field. In particular, we consider how the metallic dust form, mobilize, and interact with fusion plasmas and plasma facing components. Achievements in wall conditioning and associated anomalous plasma transport modification, including ELM suppression, with the powder injection technique is another focus of the paper. Capabilities of the state-of-art simulation tools to describe different aspects of dust in fusion devices are exemplified and new directions for future dust studies are brought forward.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

High temperature high strength austenitic steel fabricated by laser powder-bed fusion

Extremely fast cooling rates during laser powder-bed fusion (LPBF) can result in materials with unique microstructures. For LPBF 316L stainless steel, the formation of sub-grain cellular structures with high dislocation density has been linked to superior tensile properties at room temperature. This cellular structure offers also a new route for the development of high temperature LPBF steels with the nucleation of nano-size strengthening carbides in the cell walls. HK30Nb steel (Fe-25Cr-20Ni-Nb-C) was, therefore, fabricated by LPBF to evaluate its potential for high temperature applications. Optimization of the fabrication parameters yielded material with density greater than 99.7%, with nano Nb-rich precipitates in the cell walls. Annealing at 800 °C for 5h resulted in the nucleation and growth of additional precipitates mainly in the cell walls and at grain boundaries. Furthermore, the high dislocation density led to yield strength at 20–900 °C two to three times higher than yield strength for cast HK30Nb and the nano carbides in the cell walls significantly improved the cellular structure stability at 800 °C.

36 MATERIALS SCIENCE↗

Long-term thermal aging behavior and strength reduction in a laser powder bed fusion 316H stainless steel

The long-term thermal stability of structural alloys is essential for ensuring the safe and reliable operation of nuclear reactors and other power plants. While extensive research has explored the effects of thermal aging on conventional stainless steels, the behavior of additively manufactured (AM) alloys remains less understood. This study examines the thermal aging response of laser powder bed fusion (LPBF) 316H stainless steel (SS) at temperatures ranging from 550 °C to 750 °C over durations of up to 10,000 h (approximately 1.14 years). Advanced characterization techniques, including electron microscopy and synchrotron X-ray diffraction, were used to investigate dislocation recovery and phase evolution. Based on these findings, a time-temperature-precipitation (TTP) diagram was developed for LPBF 316H SS, revealing a 10- to100-fold acceleration in precipitation kinetics compared to wrought 316H SS. A physics-informed model was calibrated using the short-term experimental data, enabling predictions of average precipitate sizes, volume fractions of M 23 C 6 and Laves phases, and changes in molybdenum solute concentration for aging up to 1 × 10⁶ h (114 years). These microstructural insights were further utilized to estimate yield strength and extrapolate strength reduction factors over the extended aging period. Despite the accelerated aging kinetics, LPBF 316H SS demonstrated superior yield strength retention compared to its wrought counterpart. In conclusion, this study establishes a framework for evaluating long-term performance using short-term experimental data and supports the accelerated qualification of AM materials for high-temperature structural applications.

Laser powder bed fusion↗

Mitigating keyhole pore formation by nanoparticles during laser powder bed fusion additive manufacturing

Keyhole pore formation is one of the most detrimental subsurface defects in the laser metal additive manufacturing process. However, effective ways to mitigate keyhole pore formation beyond tuning laser processing conditions during keyhole mode laser melting are still lacking. Here we report a novel approach to mitigate keyhole pore formation during laser powder bed fusion (LPBF) process by using stable nanoparticles. The critical keyhole depth for keyhole pore generation (i.e., the largest keyhole depth without keyhole pore formation) during LPBF of Al6061 increases from 246 µm to 454 µm (85% increase) after adding TiC nanoparticles. In-depth x-ray imaging studies and thermo-fluid dynamics simulation enable us to identify that two mechanisms work together to mitigate keyhole pore generation: (1) adding nanoparticles prevents the keyhole from collapsing by increasing the liquid viscosity to impede the protrusion development; (2) adding nanoparticles slows down the keyhole pore movement by increasing the liquid viscosity, resulting in the recapturing of the pore by the keyhole. We further demonstrate that adding TiC nanoparticles can also eliminate the keyhole fluctuation induced keyhole pore during LPBF of Al6061. Our research provides a potential way to mitigate keyhole pore formation for defect lean metal additive manufacturing.

36 MATERIALS SCIENCE↗

Characterization of topology optimized Ti-6Al-4V components using electron beam powder bed fusion

The use of manufacturing to generate topology optimized components shows promise for designers. However, designers who assume that additive manufacturing follows traditional manufacturing techniques may be misled due to the nuances in specific techniques. Since commercial topology optimization software tools are neither designed to consider orientation of the parts nor large variations in properties, the goal of this research is to evaluate the limitations of an existing commercial topology optimization software (i.e. Inspire®) using electron beam powder bed fusion (i.e. Arcam®) to produce optimized Ti-6Al-4V alloy components. Emerging qualification tools from Oak Ridge National Laboratory including in-situ near-infrared imaging and log file data analysis were used to rationalize the final performance of components. While the weight savings of each optimized part exceeded the initial criteria, the failure loads and locations proved instrumental in providing insight to additive manufacturing with topology optimization. In conclusion, this research has shown the need for a comprehensive understanding of correlations between geometry, additive manufacturing processing conditions, defect generation, and microstructure for characterization of complex components such as those designed by topology optimization.

42 ENGINEERING↗

Towards improved speed and accuracy of laser powder bed fusion simulations via representation of multiple time scales

Here, we report the result of investigations into alternative representations of the temporal evolution of the laser powder bed fusion (LPBF) process. In order to provide the reader with sufficient context for the following discussion, the modeling challenge and its underlying cause, as well as current attempts to provide a satisfactory solution, will be discussed. Next, the author will describe two numerical methods (multirate time integration and parallel-in-time) to better represent the temporal scales of the problem. Finally, the results of applying these methods to a two-dimensional version of the heat transfer portion of the LPBF problem will be presented, reporting on both convergence and performance behavior, which indicate the possibility of significant speedup of solution calculations (40–100 times), along with well-characterized effects on solution accuracy.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Elucidating the effect of preheating temperature on melt pool morphology variation in Inconel 718 laser powder bed fusion via simulation and experiment

In laser powder bed fusion (L-PBF) additive manufacturing, the mechanical performance, microstructure and defects of fabricated parts are closely associated with the melt pool morphology, e.g., its dimension and shape through the building process. Past studies have largely focused on how the process parameters such as laser power and scan speed affect melt pool characteristics. In this study, the melt pool morphology variation as a function of preheating temperature in the conduction, transition, and keyhole regimes and the underlying mechanisms in each regime are investigated through ex-situ sample characterization and computation thermal fluid dynamics (CtFD) simulation. Single tracks with different combinations of laser power and scan speed are deposited on an Inconel 718 bare plate preheated to a temperature range of 100–500 °C in the experiment. Significant changes are observed in melt pool morphology as a function of preheating temperature from optical measurements of melt track cross sections. The depth of melt pool in the three regimes increases monotonically with preheating temperature, e.g., at 500 °C, the experimental melt pool depth is increased by 49% in conduction regime, 34% in transition regime and 33% in keyhole regime, respectively, while the variation of melt pool width in each regime does not all follow an increasing trend but depends on the melt pool regimes. Melt pool width variation in the conduction and transition regimes is found to depend on the enhanced heat conduction directly related to temperature dependent thermal properties. Through validated CtFD simulations, it is found that in the keyhole regime the evaporation mass, recoil pressure, and laser drilling effect is enhanced with higher preheating temperature, which gives rise to a deeper melt pool. The simulations also reveal that preheating temperature significantly elongates the melt track length due to the increased flow rate and strong recoil pressure that accelerates the backward flow.

36 MATERIALS SCIENCE↗

Effects of spatial energy distribution-induced porosity on mechanical properties of laser powder bed fusion 316L stainless steel

Laser powder bed fusion (LPBF) additive manufacturing (AM) offers a variety of advantages over traditional manufacturing, however its usefulness for manufacturing of high-performance components is currently hampered by internal defects (porosity) created during the LPBF process that have an unknown impact on global mechanical performance. By inducing porosity distributions through variations in print energy density and inspecting the resulting tensile samples using computed tomography, nearly 50,000 pores across 75 samples were identified. Porosity characteristics were quantitatively extracted from inspection data and compared with mechanical properties to understand the strength of relationships between porosity and global tensile performance. Useful porosity characteristics were identified for prediction of part performance. Results indicate that ductility and strain at ultimate tensile strength are the global tensile properties most significantly impacted by porosity and can be predicted with reasonable accuracy using simple porosity shape descriptors such as volume, diameter, and surface area. Moreover, it was found that the largest pores influenced behavior most significantly. Specifically, pores in excess of 125 µm in diameter were found to be a sufficient threshold for property estimation. These results establish an initial understanding of the complex defect-performance relationship in AM 316L stainless steel and can be leveraged to develop certification standards and improve confidence in part quality and reliability for the broader set of engineering alloys.

36 MATERIALS SCIENCE↗