Two-dimensional antiferromagnetic correlations in an La{sub 1.4}Sr{sub 1.6}(Mn{sub 0.9}Co{sub 0.1}){sub 2}O{sub 7} single crystal
The temperature and field dependences of the magnetization, the electrical resistivity, and the magnetostriction of bilayer lanthanum manganite La{sub 1.4}Sr{sub 1.6}Mn{sub 2}O{sub 7} single crystals and cobalt-doped La{sub 1.4}Sr{sub 1.6}(Mn{sub 0.9}Cu{sub 0.1}){sub 2}O{sub 7} are measured. The magnetostriction of the cobalt-doped compound increases as compared to the initial La{sub 1.4}Sr{sub 1.6}Mn{sub 2}O{sub 7} compound, and the magnetization and the magnetoresistance of the former compound change substantially. Powder and single-crystal neutron diffraction patterns are used to detect ferromagnetic ordering in La{sub 1.4}Sr{sub 1.6}(Mn{sub 0.9}Co{sub 0.1}){sub 2}O{sub 7} at a temperature below T{sub C} ~ 45(2) K, and this ordering coexists with antiferromagnetic correlations, which develop at temperatures below T{sub C} ~ 80(5) K.