Influence of grain size on α' Cr precipitation in an isothermally aged Fe-21Cr-5Al alloy

Cr-rich α' precipitation during aging typically leads to hardening and accordingly embrittlement of FeCrAl alloys, which needs to be suppressed. The influence of grain size on α' precipitation was studied by aging coarse-grained (CG), ultra-fine grained (UFG), and nanocrystalline (NC) ferritic Kanthal-D [KD; Fe-21Cr-5Al (wt.%) alloy] at 450, 500 and 550 °C for 500 h. After aging at 450 and 500 °C, less hardening was observed in the UFG KD than in CG KD. Atom probe tomography indicated a lower number density and larger sized intragranular α' in the UFG versus the CG alloy. The smaller grain size and higher defect (vacancy and dislocation) density in the UFG KD facilitated diffusion and accordingly enhanced precipitation kinetics, leading to coarsening of precipitates, as well as saturation of precipitation at lower temperatures, as compared to those in CG KD. No hardening occurred in UFG and CG KD after aging at 550 °C, indicating that the miscibility gap is between 500 and 550 °C. NC KD exhibited softening after aging owing to grain growth. α' precipitation occurred in NC KD aged at 450 °C but not at 500 °C, indicating that miscibility gap is between 450 and 500 °C. Thus, the significantly smaller grain size in NC KD decreased the miscibility gap, as compared to that in CG and UFG KD. Finally, this is attributed to the absorption of vacancies by migrating grain boundaries during aging, suppressing α' nucleation and enhancing Cr solubility.

36 MATERIALS SCIENCE↗

Surface excitons on a ZnO (000-1) thin film

Elementary excitations at the polar (000-1) surface of a 20 nm pseudomorphically grown ZnO thin film are examined by steady state and time-resolved photoluminescence spectroscopy at low temperature. We control the density of emission centers through the deposition of prototypical organic molecules with a carboxylic acid anchor group by the Langmuir-Blodgett technique. Knowledge of the precise film thickness, defect concentrations and number density of deposited molecules leads us to associate the surface exciton emission to defect-related localization centers that are generated through a photochemical process.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Laser Powder Bed Fusion Manufactured Alloys 625 and 282 and Properties Relevant to Advanced Nuclear Components

Under the Advanced Materials and Manufacturing Technologies program, two Ni-based alloys fabricated by laser powder bed fusion (LPBF) have been evaluated: γ′-strengthened Haynes 282 and solution-strengthened Inconel 625. Large printing defects were observed in the LPBF 282 alloy fabricated using a Renishaw AM250 machine, likely due to particle spattering during printing. Annealing at 1,180°C for 1 h followed by 4 h at 800°C in a high density of 50 nm γ′-strengthening precipitates as well as partial recrystallization resulted in a bimodal grain distribution. Creep testing performed at 750°C revealed lower creep life and ductility for the LPBF 282 compared with wrought 282. X-ray computed tomography combined with optical and scanning electron microscopy microstructural characterization revealed crack formation during creep testing, initiated either from printing defects or from creep cavitation at grain boundaries. Printing defects were the likely reason for the lower creep performance of LPBF 282 and could be suppressed by optimizing the build configuration. Printing 625 on an EOS M290 machine using the recommended EOS parameters resulted in a very low defect density. Superior creep strength at 725°C was observed for the as-printed LPBF 625 along the build direction when compared with wrought 625. No defect larger than ~50 µm could be detected by X-ray computed tomography in the as-printed conditions and after creep testing for 1,000 h at 725°C and 150 MPa. Small, needle-like δ-phase precipitates were observed after creep testing for 100 h at 725°C and 200 MPa. The rapid formation of the γ phase is directly related to the initial Nb and Mo segregation in the LPBF 625 cell walls, and its effect on the alloy’s high-temperature performance will be evaluated. Solution annealing was carried out at 1,150°C for 1 h and led to full recrystallization of the alloy. A decrease in strength and increase in ductility were observed after solution annealing, and the alloy recrystallization resulted in isotropic tensile properties at room temperature, contrary to what was observed for the as-printed LPBF 625.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Defect engineering in atomically-thin bismuth oxychloride towards photocatalytic oxygen evolution

Photocatalytic solar energy conversion is a clean technology for producing renewable energy sources, but its efficiency is greatly hindered by the kinetically sluggish oxygen evolution reaction. Herein, confined defects in atomically-thin BiOCl nanosheets were created to serve as a remarkable platform to explore the relationship between defects and photocatalytic activity. Surface defects can be clearly observed on atomically-thin BiOCl nanosheets from scanning transmission electron microscopy images. Theoretical/experimental results suggest that defect engineering increased states of density and narrowed the band gap. With combined effects from defect induced shortened hole migratory paths and creation of coordination-unsaturated active atoms with dangling bonds, defect-rich BiOCl nanosheets displayed 3 and 8 times higher photocatalytic activity towards oxygen evolution compared with atomically-thin BiOCl nanosheets and bulk BiOCl, respectively. As a result, this successful application of defect engineering will pave a new pathway for improving photocatalytic oxygen evolution activity of other materials.

36 MATERIALS SCIENCE↗

p- to n-type conductivity transition in 1.0 eV GaInNAs solar cells controlled by the V/III ratio

In this work, we report a p- to n-type conductivity transition of GaInNAs (1.0 eV bandgap) layers in p-i-n dilute nitride solar cells continuously controlled by the V/III ratio during growth. Near the transition region, we were able to produce GaInNAs layers with very low effective electrically active doping concentrations resulting in wide depleted areas. We obtained internal quantum efficiencies (IQEs) up to 85% at 0.2 eV above the bandgap. However, the high IQE comes along with an increased dark current density resulting in a decreased open circuit voltage of about 0.2 V. This indicates the formation of non-radiant defect centers related to the p-type to n-type transition. Rapid-thermal annealing of the solar cells on the one hand helps to anneal some of these defects but on the other hand increases the effective doping concentrations.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Influence of Irradiation-induced Microstructural Defects on Thermal Transport in Single Crystal Thorium Dioxide

Microstructural defects formed as a result of fission fragment damage are known to drastically alter thermal conductivity, a fuel property that governs the efficiency of a nuclear reactor. A fundamental understanding of radiation-induced effects on thermal transport is critical for the development of advanced fuels. Ion-irradiation has widely been used to simulate the effects of neutron-irradiation by seeding atomic-to-nanoscale defects of controllable size and density. In this work, we investigate the influence of microstructural defects, induced by ion-irradiation, on the thermal properties of single crystal thorium dioxide samples grown using the hydrothermal technique. The samples were irradiated using 2 MeV protons at room temperature. A laser-based modulated thermoreflectance technique was used to measure the thermal diffusivity and conductivity within the damaged ThO2 region. The experimentally measured thermal properties were compared with Boltzmann Transport Equation predictions, to determine the impact of various defect types on the thermal properties of ThO2.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Engineering Nanocolumnar Defect Configurations for Optimized Vortex Pinning in High Temperature Superconducting Nanocomposite Wires

High temperature superconducting (HTS), coated conductor wires based on nanocomposite films containing self-assembled, insulating BaZrO3 (BZO) nanocolumnar defects have previously been reported to exhibit enhanced vortex pinning. Here, we report on microstructural design via control of BZO nanocolumns density in YBa2Cu3O7- (YBCO)+BZO nancomposite films to achieve the highest critical current density, Jc(H, ,T). X-ray diffraction and microstructural examination shows increasing number density of epitaxial BZO nanocolumns in the highly cube-textured YBCO matrix with increasing nominal BZO additions. Transport property measurement reveals that an increase in BZO content upto 4 vol% is required to sustain the highest pinning and Jc performance as the magnetic field increases. By growing thicker, single-layer nanocomposite films (~4 m) with controlled density of BZO columnar defects, the critical current (Ic) of ~1000 A/cm at 77 K, self-field and the minimum Ic of 455 A/cm at 65 K and 3 T for all magnetic field orientations were obtained. This is the highest Ic reported to date for films on metallic templates which are the basis for the 2nd generation, coated conductor-based HTS wires.

critical current density↗

Mitigating Structural Defects in Droop-Minimizing InGaN/GaN Quantum Well Heterostructures

Modern commercial InGaN/GaN blue LEDs continue to suffer from efficiency droop, a reduction in efficiency with increasing drive current. External quantum efficiency (EQE) typically peaks at low drive currents (< 10 A cm 2 ) and drops monotonically at higher current densities, falling to <85% of the peak EQE at a drive current of 100 A cm 2 . Mitigating droop-related losses will yield tremendous gains in both luminous efficacy (lumens/W) and cost (lumens/$). Such improvements are critical for continued large-scale market penetration of LED technologies, particularly in high-power and high flux per unit area applications. However, device structures that reduce droop typically require higher indium content and are accompanied by a corresponding degradation in material quality which negates the droop improvement via enhanced Shockley-Read-Hall (SRH) recombination. In this work, we use advanced characterization techniques to identify and classify structural defects in InGaN/GaN quantum well (QW) heterostructures that share features with low-droop designs. Using aberration-corrected scanning transmission electron microscopy (C s -STEM), we find the presence of severe well width fluctuations (WWFs) in a number of low droop device architectures. However, the presence of WWFs does not correlate strongly with external quantum efficiency nor defect densities measured via deep level optical spectroscopy (DLOS). Hence, performance losses in the heterostructures of interest are likely dominated by nanoscale point or interfacial defects rather than large-scale extended defects.

36 MATERIALS SCIENCE↗

A mechanism-based quantitative multi-scale framework for investigating irradiation hardening of tungsten at low temperature

We present the development and validation of a mechanism-based multi-scale modeling framework to quantitatively link the irradiation defect evolution kinetics at the microscopic scale to the macroscopic yield strength and flow stress evolution of tungsten irradiated at low temperature (0.08 < T/T m < 0.18, where T m is the melting point and is equal to 3673 K). The mechanism-based strength model, proposed as the superposition of thermal softening and modified dispersed barrier hardening, is developed to understand the underlying strengthening mechanisms. The thermal softening exponent as defined in the Johnson-Cook model is obtained by fitting unirradiated yield strength at different temperatures. A set of irradiation-induced defect kinetics equations with the thermodynamics parameters derived from the atomic calculations reported in the literature is used to determine the densities and sizes of defect clusters at the meso-scale, and the predicted irradiation damage characteristics are in reasonable quantitative agreement with experimental data from literature. The effects of irradiation condition (temperature and irradiation dose) and test temperature on yield strength are quantitatively predicted and compared with experimental measurements from the literature. Here, the predicted irradiation hardening and strain hardening are compared with experimental data as model validation.

36 MATERIALS SCIENCE↗

Defect control strategies for Al 1- x Gd x N alloys

Tetrahedrally bonded III-N and related alloys are useful for a wide range of applications from optoelectronics to dielectric electromechanics. Heterostructural AlN-based alloys offer unique properties for piezoelectrics, ferroelectrics, and other emerging applications. Atomic-scale point defects and impurities can strongly affect the functional properties of materials, and therefore, it is crucial to understand the nature of these defects and the mechanisms through which their concentrations may be controlled in AlN-based alloys. In this study, we employ density functional theory with alloy modeling and point defect calculations to investigate native point defects and unintentional impurities in Al 1-x Gd x N alloys. Among the native defects that introduce deep midgap states, nitrogen vacancies (V N ⁠) are predicted to be in the highest concentration, especially under N-poor growth conditions. We predict and experimentally demonstrate that V N formation can be suppressed in thin films through growth in N-rich environments. We also find that Al 1-x Gd x N alloys are prone to high levels of unintentional O incorporation, which indirectly leads to even higher concentrations of deep defects. Growth under N-rich/reducing conditions is predicted to minimize and partially alleviate the effects of O incorporation. The results of this study provide valuable insights into the defect behavior in wurtzite nitride-based alloys, which can guide their design and optimization for various applications.

36 MATERIALS SCIENCE↗

Low temperature recovery of OFF-state stress induced degradation of AlGaN/GaN high electron mobility transistors

Thermal annealing is a widely used strategy to enhance semiconductor device performance. However, the process is complex for multi-material multi-layered semiconductor devices, where thermoelastic stresses from lattice constant and thermal expansion coefficient mismatch may create more defects than those annealed. We propose an alternate low temperature annealing technique, which utilizes the electron wind force (EWF) induced by small duty cycle high density pulsed current. To demonstrate its effectiveness, we intentionally degrade AlGaN/GaN high electron mobility transistors (HEMTs) with accelerated OFF-state stressing to increase ON-resistance ∼182.08% and reduce drain saturation current ∼85.82% of pristine condition at a gate voltage of 0 V. We then performed the EWF annealing to recover the corresponding values back to ∼122.21% and ∼93.10%, respectively. The peak transconductance, degraded to ∼76.58% of pristine at the drain voltage of 3 V, was also recovered back to ∼92.38%. This recovery of previously degraded transport properties is attributed to approximately 80% recovery of carrier mobility, which occurs during EWF annealing. We performed synchrotron differential aperture x-ray microscopy measurements to correlate these annealing effects with the lattice structural changes. We found a reduction of lattice plane spacing of (001) planes and stress within the GaN layer under the gate region after EWF annealing, suggesting a corresponding decrease in defect density. Application of this low-temperature annealing technique for in-operando recovery of degraded electronic devices is discussed.

Physics↗

pymatgen-analysis-defects: A Python package for analyzing point defects in crystalline materials

Point defects can often determine the properties of semiconductor and optoelectronic materials. Due to the large simulation cell and the higher-cost density functionals required for defect simulations, the computational cost of defect calculations is often orders of magnitude higher than that of bulk calculations. As such, managing and curating the results of the defect calculations generated by a single user has the potential to save a significant amount of computational resources. Moreover, eventually building a high-quality, persistent defects database will significantly reduce the computational cost of defect calculations for the entire community.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Influence of in situ applied ultrasound during Si{sup +} implantation in SiO{sub 2} on paramagnetic defect generation

Electron spin resonance (ESR) results are presented on the influence of in situ ultrasound treatment (UST) during implantation at 300 K of Si{sup +} ions into thermal SiO{sub 2} on (100)Si before and after subsequent high-temperature (T) annealing (1100 deg. C) intended to promote the formation of embedded Si nanoparticles. The as-implanted state exhibits high densities of three prominent types of point defects, including the SiO{sub 2}-specific S and E{sup '}{sub {gamma}} O-vacancy type centers, and an unknown broad ({approx_equal}20 G) signal at g{approx_equal}2.0026 denoted IS. The high-intensity S signal shows demagnetization shape effects, pointing to a distribution of high local density of defects over a thin layer. UST is observed to effectuate a drastic reduction in S and E{sup '}{sub {gamma}} centers, and elimination of IS beyond detection. This reveals a strong healing influence of in situ transferred ultrasound (US) energy on implantation-induced damage, here quantified and identified on atomic level in terms of mainly intrinsic paramagnetic point defects elimination, viz., Frenkel pair elimination, while all three initial signals disappear. Other types of defects surface after annealing of the non-US treated sample, including the SiO{sub 2}-specific EX defect signal and P{sub b}-type Si/SiO{sub 2} interface centers, the appearance of the latter providing direct ESR evidence for crystallization of the excess Si nanoparticles. The influence of the UST healing effect is kept up after subsequent annealing, now resulting in the absence of virtually all ESR-active centers. The drop in P{sub b}-type centers below the detection level in the UST annealed sample indicates improvement of the nanocrystalline-Si/SiO{sub 2} interface quality. The combination of UST with high-T annealing emerges as a highly efficient means to eradicate ion implantation damage in terms of intrinsic point defects.

36 MATERIALS SCIENCE↗

Role of the junction voltage on the overflow current in light-emitting diodes

Quantum-well (QW)-based light emitters, such as light-emitting diodes (LEDs) and lasers, of various semiconductor materials experience a reduction in their efficiency when operating at higher temperatures, a phenomenon referred to as “thermal droop.” Among the various claims on the origins of thermal droop, an increased overflow current with increasing temperatures is a common contender. Since overflow of carriers can only occur when the junction voltage 𝑉 Junction approaches the built-in voltage 𝑉 BI of any diodes, we develop a simple method relating the difference between 𝑉 Junction and 𝑉 BI to approximate the upper limit of overflow occurring in QW-based light-emitting diodes. The measured difference between 𝑉 Junction and 𝑉 BI of state-of-the-art commercial blue and green In⁢Ga⁢N-based LEDs at temperatures up to ∼450 K suggests negligible overflow. To further experimentally verify the absence of overflow, we perform temperature-dependent electron emission spectroscopy on the same commercial blue and green LEDs and find no evidence of thermally enhanced overflow carriers up to ∼450 K. In agreement with our claims that 𝑉 Junction must approach 𝑉 BI for overflow to occur, two-dimensional temperature-dependent electrical simulations of violet, blue, and green LEDs including alloy disorder and V-defects demonstrate that overflow can be significant in violet LEDs, where the small band offset between the In⁢Ga⁢N QW and Ga⁢N cladding layers due to the larger QW bandgap requires larger 𝑉 Junction to reach standard operating current densities, thereby approaching 𝑉 BI . By contrast, simulations indicate that overflow is negligible in blue and green LEDs, whose smaller QW bandgaps result in smaller quasi-Fermi levels difference to reach significant carrier injection, resulting in a 𝑉 Junction much smaller than 𝑉 BI up to large operating current densities. Considering that overflow is negligible in blue and longer-wavelength LEDs, and our observations of the large thermal droop occurring at low current densities, where Shockley-Read-Hall (SRH) recombination dominates, we conclude that thermally enhanced SRH processes are the most significant contributor to thermal droop. Finally, we also simulate the carrier densities in the different QWs of a multiple-QW LED and observe a reduction in the total carrier density at a given operating current density, which results in a decrease in the total Auger-Meitner current of the LED from just the thermally enhanced carrier redistribution among QWs without taking any possible additional temperature dependence of their recombination coefficients. Taking all this into account, minimizing thermal droop effects in LEDs can be achieved by a reduction in defect density, using wider band gap p-n junction-defining cladding layers, and operating at higher currents.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Automated Quantitative Analysis of Extended Irradiation Defects - Dislocations, Voids and Precipitates in Neutron Irradiated HT-9 Steel

Structural alloys that make up the core components of nuclear reactors are exposed to radiation that can substantially alter the microstructure and mechanical properties of the material. Irradiation can cause the formation of extended defects including dislocation line and loops, voids and various types of precipitates. To understand the irradiation effects, it is critical to characterize these defects individually and collectively to quantify how they evolve throughout irradiation stages. Transmission electron microscopy (TEM) is a standard tool for providing extensive size, number density and spatial distribution of extended irradiation defects, however, manual measurement of defect size and number density requires time-intensive effort to analyze enough defects that provide a statistically meaningful result and are prone to errors of subjectivity. In this work, we developed a set of MATLAB algorithms offering robust and automated identification and quantification of extended irradiation defects like dislocation lines, voids and precipitates commonly observed in neutron irradiated cladding alloys [1]. Using a neutron-irradiated HT-9 martensitic alloy irradiated at 412°C to 111.8 dpa, we demonstrate the capability of these algorithms for quantitative defect analysis. Figure 1 presents defect images of the HT-9 using an advanced diffraction contrast imaging scanning transmission electron microscopy (DCI STEM) that suppresses bend contours and provides better defect contrast compared to conventional TEM [2]. The first step of defect analysis is defect identification, a process that can be digitally achieved by contrast thresholding (for simple defect contrast) and by machine learning computer vision for defect semantic segmentation [3]. Here, labeled binary defect images (Figures 2a and 2c) were used. For dislocation density quantification, we employed an optimized circular-grid intersection method first introduced by Dr. John Steeds [4]. This method is shown in Figures 2a and 2b, where the number of intersections of dislocation lines with circular traces was measured. This produces an unbiased sampling of dislocation lines, regardless of their orientation. This process was optimized with automated digital intersection number and grid length registration. Interestingly, it was found that a relatively large number of circles in a set circular gird is was needed to produce an invariant result (Figure 2b), with a low systematic measurement error. This demonstrates the main advantage of computer-based defect analysis, in performing repetitive operations quickly with a reduced systematic error. For the quantitative analysis of voids and precipitates a challenge encountered with automated defect analysis is feature overlap, particularly when the density of voids/precipitates is high. To mitigate this problem, as shown in Figure 2d, we modified the popular circular Hough transformation and treated ‘circular shape’ as the particle descriptor for voids/precipitates, efficiently resolving the overlapping particles. In summary, this automated digital quantification together with machine learning enabled defect identification [3] opens new opportunities for standardizing the characterization workflow for quantitative analysis of extended irradiation defects.

Sainju, Rajat↗

Large bandgap observed on the surfaces of EuZn 2 As 2 single crystals

EuM 2 As 2 (M = Zn, Cd, In, Sn etc.) is an excellent material system for studying magnetism-tuned topological properties. However, discrepancies exist between experimental data and theoretical calculations regarding the bulk and surface bandgaps. In this work, cleaved EuZn 2 As 2 crystals are studied using scanning tunneling microscopy/spectroscopy and density functional theory calculations. Triangular-shaped defect-induced modifications in the local density of states help distinguish between Eu-terminated and AsZn-terminated surfaces. While large bandgaps (~1.5 eV at 77 K) are observed on both pristine surfaces, the bandgap size is found to be highly sensitive to local heterogeneity, tending to decrease. By combining experimental observations with theoretical simulations, we conclude that the reduced bandgap in heterogeneous regions arises from Zn vacancies and/or substitution by As atoms, both impacting greater in the Eu surface electronic properties than those in the AsZn surface. This demonstrates the intimate relationship between the electronic structure and magnetism in EuZn 2 As 2 .

interfaces↗

Impact of dislocations and dangling bond defects on the electrical performance of crystalline silicon thin films

A wide variety of liquid and solid phase crystallized silicon films are investigated in order to determine the performance limiting defect types in crystalline silicon thin-film solar cells. Complementary characterization methods, such as electron spin resonance, photoluminescence, and electron microscopy, yield the densities of dangling bond defects and dislocations which are correlated with the electronic material quality in terms of solar cell open circuit voltage. The results indicate that the strongly differing performance of small-grained solid and large-grain liquid phase crystallized silicon can be explained by intra-grain defects like dislocations rather than grain boundary dangling bonds. A numerical model is developed containing both defect types, dislocations and dangling bonds, describing the experimental results.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

The Influence of the InAlAs Layer Surface Morphology on the Temperature Dependence of Parameters of Au/Ti/n-InAlAs(001) Schottky Diodes

Growth-related structural defects present on the surface of InAlAs layers grown by molecular beam epitaxy on InP(001) substrates influence the temperature dependences of the current–voltage characteristics of Au/Ti/InAlAs Schottky barriers. It is established that these defects in the form of pits cause the appearance of regions with reduced barrier height. At a surface density of ≥10{sup 7} cm{sup –2}, these defects significantly influence the parameters of the Schottky barriers at temperatures below 200 K.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗