Search NASA⌕ Search

SEARCH · Search NASA

Results for “microstructural properties”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,261 records · Page 70

The microstructure effects on irradiation response of ferritic – martensitic steels

Microstructural optimization to achieve greater mechanical strength has been one of the focuses in ferritic–martensitic steels development. However, these optimized microstructures’ effects on the radiation response are not well known. In this work, two ferritic–martensitic steels (9Cr-NbMo and 9Cr-Ta) underwent neutron irradiation in the High Flux Isotope Reactor, and their room-temperature post-irradiation tensile properties and microstructure evolutions were investigated and compared. These two steels exhibit similar pre-irradiation tensile behavior, and their yield strengths are higher than that of other ferritic–martensitic steels by about 200–250 MPa. Microstructural characterization on pre-irradiated materials reveals a smaller grain size in 9Cr-Ta (2.8 ± 0.3 μm in 9Cr-Ta versus 4.3 ± 0.5 μm in 9Cr-NbMo) but higher dislocation density and precipitate density in 9Cr-NbMo. As is common for ferritic–martensitic steels at low irradiation temperatures (less than about 0.45T m ), irradiation-induced hardening at 400 °C was observed for both alloys. Irradiation at 490 °C causes the two alloys to exhibit different tensile behavior: 9Cr-Ta softens by 208 MPa in yield stress, whereas 9Cr-NbMo maintains strength. Additionally, microstructural characterizations were performed, including precipitate growth, dislocation, and defect formation. Using the barrier hardening model for microstructure–property correlation, the softening in irradiated 9Cr-Ta is primarily attributed to the significant dislocation recovery, while the strength lost from the slight dislocation recovery in 9Cr-NbMo was compensated by the additional strength from the irradiation-induced cavities. The microstructure effect (primarily precipitate, dislocation and boundary) on the radiation response is discussed herein.

36 MATERIALS SCIENCE↗

Investigation on Microstructural Evolutions and Mechanical Properties of P92 Steel During Thermal Processing

The evolution of the microstructure of P92 steel during heat processing has a significant effect on the final performance of steel products and is thus an area of critical interest. Accordingly, the grain growth behavior of austenite and δ-ferrite changes in P92 steel is comprehensively investigated in this study through thermodynamic calculations and physical simulation. The results show that the A{sub C1}, A{sub C3} and γ–δ transformation temperatures of P92 steel are 841 °C, 878 °C and 1095 °C, respectively, which are comparable to the measured values of 850 °C, 879 °C and 1175 °C, respectively. When the temperature exceeds the A{sub C1} temperature, the austenite grain size increases with increasing temperature and longer holding times, and the growth rate of austenite grains increases with higher temperatures but decreases with holding time at a certain temperature. A model that shows the austenite grain growth kinetics is established: D{sup n} − D{sub 0}{sup n} = 2.03 × 10{sup 16}exp(− 498,770/RT)t, in which the time exponent n decreases from 4.52 to 2.11 with an increase in temperature from 1000 °C to 1200 °C due to the reduced pinning effect resultant of the dissolution of precipitates, M{sub 23}C{sub 6}, VX and NbX at 887 °C, 1073 °C and 1200 °C, respectively. The formation of δ-ferrite at 1200 °C when held for 600 s and 1300 °C when held for 60 ~ 600 s causes a smaller austenite grain size. The relationship between the evolution of the microstructure of P92 steel and the mechanical properties is also studied. The results show that the prior austenite grain size has an inverse relationship with impact energy and ultimate tensile strength at 620 °C, while the presence of soft δ-ferrite leads to a reduction in the microhardness, impact energy and ultimate tensile strength at 620 °C.

36 MATERIALS SCIENCE↗

Microstructure, Texture, and Mechanical Properties of Ni-W Alloy After Accumulative Roll Bonding

In this study, the microstructure, texture, and mechanical properties evolution of Ni-14W (wt.%) alloy processed up to four cycles of accumulative roll-bonding (ARB) were investigated using electron backscatter diffraction, microhardness measurements, and tensile tests. The initial equiaxed grains, with an average size of 10 μm, underwent a strong refinement after ARB processing. The elongated ultrafine grains were parallel to the rolling direction, with a grain thickness of 0.2 µm. The texture after ARB processing was characterized by the typical rolling components (Copper, S and Brass), which showed a tendency toward stabilization after four cycles. The microhardness increased substantially (+ 86%) and seemed to saturate after three cycles. The tensile tests demonstrated that Ni-14W samples subjected to ARB processing exhibited high strength (> 1200 MPa after three ARB cycles) and very poor ductility.

36 MATERIALS SCIENCE↗

Microstructure, mechanical and electrical properties of nanocrystalline W-Mo thin films

The effect of sputtering pressure on the surface/interface microstructure, crystal phase, mechanical properties and electrical characteristics of nanocrystalline W-Mo films is reported. The W-Mo films (≈300 nm) with variable microstructure were deposited under variable argon (Ar) sputtering pressure (P Ar ), which is varied in the range of 3-19 mTorr. X-ray diffraction analyses indicate that the W-Mo films crystallize in thermodynamically stable α-phase of W. However, the crystal-quality degradation occurs for W-Mo films deposited at higher P Ar due to difference in the adatom mobilities. The average grain size (d) of the W-Mo films was in the range of 11-24 nm; grain size decreases with increasing P Ar . The effect of P Ar and associated microstructure are significant on the mechanical characteristics; the hardness (H) and modulus of elasticity (E r ) of W-Mo films deposited at lower P Ar were higher but decreases continuously with increasing P Ar . The W-Mo films deposited under optimum sputtering pressure exhibit superior mechanical characteristics: H=40 GPa, E r =275 GPa, H/E r =0.8, and H 3 /E r 2 =0.145 GPa, which are higher compared to pure, α-phase W-films. The W-Mo films deposited at P Ar =3-9 mTorr exhibit high resistivity≈350-400 μΩ-cm, which decreases to 150-200 μΩ-cm for films deposited at higher P Ar . Based on the results, structure-mechanical-electrical property correlation in W-Mo films is established.

36 MATERIALS SCIENCE↗

Microstructural Evolution and Mechanical Properties of Cold-deformed Al-5Cu Alloy Samples After Isothermal Heat Treatments

Abstract.In this paper, the microscopic morphology of a semi solid Al5Cu alloy by strain induced melt activated (SIMA) process were investigated, and the effects of predeformation, microstructural evolution, aging response and hardness changes were determined. The microstructural observation shows that while the grain boundaries started to appear after 620 deg. C, globular grains surrounded wet boundaries needed for SSP were obtained at 650 deg. C. The grain sizes exhibited ununiformity from the outer surface to the center of the sample because of ununiform predeformation. Although isothermal heat treatments reduced hardness, age hardening gave back the hardness loss.

36 MATERIALS SCIENCE↗

Microstructure, Texture, and Mechanical Properties of AM60 Magnesium Alloy Processed by Extrusion and Multidirectional Forging

In the present paper, multidirectional forging (MDF), as a severe plastic deformation process, was carried out on an extruded AM60 magnesium alloy. The microstructure, texture, and mechanical properties of the MDFed samples were examined. Microstructural findings indicated that the grain size of the alloy decreased from 10.2 to 3.7 µm after six MDF passes, carried out at a constant temperature of 220 °C. Textural studies revealed that after six MDF passes, the fiber texture of the extruded material was transformed to another texture, in which the basal planes tend to rotate toward 45{sup o} to the transverse direction. Shear punch testing (SPT) was employed to assess the shear yield stress (SYS) and ultimate shear strength (USS) at room temperature. Both SYS and USS were enhanced after two MDF passes, but decreased in the next pressing stages, despite developing finer grains at higher levels of imposed strain. The observed drop in strength is ascribed to texture softening that counterbalances the grain refinement strengthening effects. The variation in average microhardness values after different passes of MDF showed the trend that was in concurrence with the rise and fall of the SPT results. Finally, the changes in mechanical properties were discussed, based on the microstructural and textural findings.

36 MATERIALS SCIENCE↗

An efficient algorithm for generating diverse microstructure sets and delineating properties closures

Properties closures delineate the theoretical objective space for materials design problems, allowing designers to make informed trade-offs between competing constraints and target properties. In this paper, we present a new algorithm called hierarchical simplex sampling (HSS) that approximates properties closures more efficiently and faithfully than traditional optimization based approaches. By construction, HSS generates samples of microstructure statistics that span the corresponding microstructure hull. As a result, we also find that HSS can be coupled with synthetic polycrystal generation software to generate diverse sets of microstructures for subsequent mesoscale simulations. Finally, by more broadly sampling the space of possible microstructures, it is anticipated that such diverse microstructure sets will expand our understanding of the influence of microstructure on macroscale effective properties and inform the construction of higher-fidelity mesoscale structure-property models.

36 MATERIALS SCIENCE↗

Linking Initial Microstructure to ORR Related Property Degradation in SOFC Cathode: A Phase Field Simulation

Microstructure evolution driven by thermal coarsening is an important factor for the loss of oxygen reduction reaction rates in SOFC cathode. In this work, the effect of an initial microstructure on the microstructure evolution in SOFC cathode is investigated using a recently developed phase field model. Specifically, we tune the phase fraction, the average grain size, the standard deviation of the grain size and the grain shape in the initial microstructure, and explore their effect on the evolution of the grain size, the density of triple phase boundary, the specific surface area and the effective conductivity in LSM-YSZ cathodes. It is found that the degradation rate of TPB density and SSA of LSM is lower with less LSM phase fraction (with constant porosity assumed) and greater average grain size, while the degradation rate of effective conductivity can also be tuned by adjusting the standard deviation of grain size distribution and grain aspect ratio. The implication of this study on the designing of an optimal initial microstructure of SOFC cathodes is discussed.

25 ENERGY STORAGE↗

Characterization of microstructure, texture and magnetic properties in twin-roll casting high silicon non-oriented electrical steel

An Fe-6.5 wt.% Si-0.3 wt.% Al as-cast sheet was produced by twin-roll strip casting process, then treated with hot rolling, warm rolling and annealing. A detailed study of the microstructure and texture evolution at different processing stages was carried out by optical microscopy, X-ray diffraction and electron backscattered diffraction analysis. The initial as-cast strip showed strong columnar grains and pronounced < 001 >//ND texture. The hot rolled and warm rolled sheets were characterized by large amounts of shear bands distributed through the thickness together with strong < 110 >//RD texture and weak < 111 >//ND texture. After annealing, detrimental < 111 >//ND texture almost disappeared while beneficial (001)<210 >, (001)<010 >, (115)<5 − 10 1 > and (410) < 001 > recrystallization textures were formed, thus the magnetic induction of the annealed sheet was significantly improved. The recrystallization texture in the present study could be explained by preferred nucleation and grain growth mechanism. - Highlights: • A high silicon as-cast strip with columnar structure was produced. • A thin warm rolled sheet without large edge cracks was obtained. • Microstructure and texture evolution at each stage were investigated. • Beneficial (001)<210 >, (001)<010 >, (410)<001 > recrystallization textures were formed. • The magnetic induction of annealed sheet was significantly improved.

36 MATERIALS SCIENCE↗

Microstructure Evolution and Mechanical Properties of the AZ91 Magnesium Alloy with Sr and Ti Additions in the As-Cast and As-Aged Conditions

Effect of different amounts of Sr and Ti additions with T6 heat treatment on microstructure and mechanical properties of the AZ91 alloy was investigated. The microstructure of the AZ91 alloy is consisted of the α-Mg phase surrounded by the semicontinuous network of β-Mg{sub 17}Al{sub 12} intermetallics. The average grain size and volume fraction of β phase decreased up to 1 wt.% Sr and 0.1 wt.% Ti additions. Exceeding Ti additions led to increase in both grain size and volume fraction. It was found that the grain refinement mechanism of AZ91 alloys with Sr additions was grain restriction factor. Also, 0.1 wt.% Ti addition could refine the grain structure of the AZ91 alloy by the formation of Al{sub 3}Ti particles that act as nucleation sites for the α-Mg phase. Furthermore, adding 1 wt.% Sr and 0.1 wt.% Ti enhanced the hardness values for both cast and aged AZ91 alloy. Moreover, ultimate tensile strength and tensile elongation values reached their maximum amounts with the 0.5 wt.% Sr and 0.1 wt.% Ti additions and more Sr and Ti additions deteriorated the mechanical properties of cast and aged AZ91 alloys. The fracture surface characterizations had good relations with the tensile properties. The fracture modes were cleavage and quasi-cleavage in the cast and aged AZ91 alloys. Furthermore, the optimum levels of Sr and Ti additions altered the fracture modes to more quasi-cleavage fractures.

36 MATERIALS SCIENCE↗

Microstructure, texture and mechanical properties of AA 1060 aluminum alloy processed by cryogenic accumulative roll bonding

Highlights: • The Al sheets were accumulative roll bonded to five cycles at cryogenic temperature. • The microstructure, texture and mechanical properties of ARB sheets were investigated. • The texture evolution at surface layer was quantified by mathematical formulae. • The strength of the β fiber at center layer was affected by the initial texture and the strain. - Abstract: AA 1060 aluminum alloy sheet was processed to five accumulative roll bonding (ARB) cycles at cryogenic temperature. The microstructure, texture and mechanical properties of the ARB processed sheets were investigated. The results show that the surface layer of the ARB processed sheets exhibits a significant r-cube shear texture. Initial cube orientation at the surface layer was gradually rotated to the r-cube orientation during the ARB process, leading to the increase in the strength of the r-cube shear texture with ARB cycles. The texture evolution at the surface layer was quantified in terms of a simple relation between the texture volume fractions and accumulated true strain. The strength of the β fiber rolling texture and the distribution of orientation intensities along the β fiber at the center layer were strongly affected by the initial texture. As the ARB cycles increased, the initial texture was changed from the cube texture to the r-cube texture, leading to a continuous increase in the strength of the β fiber rolling texture dominated by the C orientation. The yield and ultimate tensile strength of the ARB processed sheets increased markedly after the first ARB cycle and then increased slowly with increasing ARB cycles, while the elongation decreased accordingly.

36 MATERIALS SCIENCE↗

Effects of the microstructure and porosity on properties of Ti-6Al-4V ELI alloy fabricated by electron beam melting (EBM)

Electron Beam Melting (EBM) is a metal powder bed-based Additive Manufacturing (AM) technology that makes possible the fabrication of three dimensional near-net-shaped parts directly from computer models. EBM technology has been in continuously updating, obtaining optimized properties of the processed alloys. Ti-6Al-4V titanium alloy is the most widely used and studied alloy for this technology and is the focus of this work. Several research works have been completed to study the mechanisms of microstructure formation as well as its influence on mechanical properties. However, the relationship is not completely understood, and more systematic research work is necessary in order to attain a better understanding of these features. In this work, samples fabricated at different locations, orientations, and distances from the build platform have been characterized, studying the relationship of these variables with the resulting material intrinsic characteristics and properties (surface topography, microstructure, porosity, micro-hardness and static mechanical properties). This study has revealed that porosity is the main factor controlling mechanical properties relative to the other studied variables. Therefore, in future process developments, decreasing of the porosity should be considered as the primary goal in order to improve mechanical properties.

36 MATERIALS SCIENCE↗

Microstructural evolution and mechanical properties of maraging steel produced by wire + arc additive manufacture process

Highlights: • Wire + arc additive manufacture (WAAM) was applied to produce maraging steel structures. • Microstructure evolution of WAAM alloy was characterized and correlated with the layer-by-layer building manner. • Mechanical properties of WAAM alloy were tested and correlated with the aging response of WAAM microstructure. • Retained austenite content was measured and correlated with the tensile strength loss. - Abstract: Wire + arc additive manufacture is developed for producing large-scale metallic components. In this paper, maraging steel parts were produced, and the microstructure and mechanical properties were investigated. The microhardness and tensile strength of the as deposited alloy reduced from the bottom to the top due to the transient thermal cycling, which resulted in partial aging and non-uniform formation of intermetallic compounds along the building direction. Solutionizing, followed by 3 h aging, significantly reduced the microstructural heterogeneity and increased the mechanical properties by 24.7% through the formation of large amounts of finely distributed precipitates. The as deposited alloy possessed superior strength to the wrought alloy in solutionized condition but inferior to the later in aged condition, which was attributed to the less pronounced aging response of the low-angle columnar grains characterized microstructure and the presence of retained and reverted austenite.

36 MATERIALS SCIENCE↗

Microstructural stability and creep properties of die casting Mg-4Al-4RE magnesium alloy

The AE44 (Mg-4Al-4RE) alloy was prepared by a hot-chamber die casting method. The microstructure, microstructural stability and creep properties at 175 deg. C were investigated. The microstructure was analyzed by scanning electron microscopy (SEM), transmission electron microscopy (TEM), X-ray diffraction (XRD) and the Rietveld method. The results show that die cast AE44 magnesium alloy consists of {alpha}-Mg, Al{sub 11}RE{sub 3}, Al{sub 2}RE and Al{sub 2.12}RE{sub 0.88} phases. The Al{sub 11}RE{sub 3} phase is thermally stable at 175 deg. C whereas the metastable Al{sub 2.12}RE{sub 0.88} phase undergoes a transition into the equilibrium Al{sub 2}RE phase. The alloy investigated is characterized by good creep properties at temperatures of 175 deg. C and 200 {sup o}C.

36 MATERIALS SCIENCE↗

Effect of Zn on microstructure, texture and mechanical properties of Al-Mg-Si-Cu alloys with a medium number of Fe-rich phase particles

Highlights: • Zn has a negligible influence on the final recrystallization microstructure and texture of Al-Mg-Si-Cu alloys. • By adding Fe-rich phase particles to refine the recrystallization grain sizes could control the texture. • The deep drawability of Al-Mg-Si-Cu alloys could be affected by solute Zn atom besides the microstructure and texture. - Abstract: The effect of Zn on the microstructure, texture evolution and mechanical properties of Al-Mg-Si-Cu alloys with a medium number of Fe-rich phase particles was investigated using tensile testing machine, optical microscopy (OM), scanning electron microscope (SEM), transmission electron microscope (TEM) and X-ray diffractometer (XRD) in the present study. The results show that Zn addition has a significant influence on the final mechanical properties, but a slight effect on microstructure and final recrystallization texture. Zn addition is favorable to increase yield strength, ultimate tensile strength and elongation, however it is detrimental to improve r value and reduce Δr value. During the thermomechanical processing, the microstructure almost has nothing to do with Zn addition. However, Zn could prevent the secondary phase particles from precipitating during intermediate annealing. In contrast to the alloy sheet without Zn, the alloy sheet with 1.0 wt% Zn always has weaker textures before final cold rolling, but a stronger texture after experiencing final cold rolling. After solution treatment, they almost possess the same recrystallization texture. Finally, the effect of Zn addition on the recrystallization texture was discussed. Their similar recrystallization texture can be attributed to the similar microstructure, which was caused by the medium number of Fe-rich phase particles.

36 MATERIALS SCIENCE↗

Magnetic properties, phase evolution, and microstructure of melt-spun (Sm{sub 1-x}Pr{sub x})Co{sub 7-y}Hf{sub y}C{sub z} (x=0-1; y=0.1-0.3; z=0-0.14) ribbons

Magnetic properties, phase evolution, and microstructure of melt-spun (Sm{sub 1-x}Pr{sub x})Co{sub 7-y}Hf{sub y}C{sub z} ribbons have been investigated. For (Sm{sub 1-x}Pr{sub x})Co{sub 7-y}Hf{sub y} (x=0-1; y=0.1-0.3) ribbons, the magnetization increases, but coercivity decreases, with increasing Pr content. However, the phase constitution and microstructure have not been influenced by modifying Pr content x. The attractive magnetic properties of B{sub r}=6.5 kG, {sub i}H{sub c}=6.1 kOe, and (BH){sub max}=7.2 MG Oe could be obtained for (Sm{sub 0.8}Pr{sub 0.2})Co{sub 6.9}Hf{sub 0.1} ribbons. A slight addition of C in (Sm{sub 0.8}Pr{sub 0.2})Co{sub 6.9}Hf{sub 0.1}C{sub z} (z=0.06-0.14) ribbon not only refines the microstructure, but also induces nanoscale fcc-Co precipitation in the matrix, leading to the stronger exchange-coupling effect between magnetic grains and the enhancement of remanence and magnetic energy product. As a result, the improved magnetic properties of B{sub r}=7.1 kOe, {sub i}H{sub c}=8.5 kOe, and (BH){sub max}=11.2 MG Oe can be achieved for (Sm{sub 0.8}Pr{sub 0.2})Co{sub 6.9}Hf{sub 0.1}C{sub 0.12} ribbons.

36 MATERIALS SCIENCE↗

Microstructural Characteristics and Mechanical Properties of Friction-Stir-Welded CuSn6 Tin Bronze

Tin bronze is widely applied in various industries for its excellent wear and corrosion resistance. Friction stir welding is a solid-state welding process, which generates less heat and avoids the melting-related defects. CuSn6 tin bronze plates of 4 mm in thickness were friction-stir-welded at welding speeds ranging from 50 to 150 mm/min under a constant rotation speed. The microstructural and mechanical properties of joints were investigated. The microstructure of the stir zone consists of refined equiaxed grains. The grain size decreased from top to bottom of the welds. The mean grain size is increased with increasing welding speed. The largest strength and elongation of welded joints were both obtained at the welding speed of 100 mm/min. During tensile test, all of the joints were fractured at the heat affected zone of retreating side with typical plastic fracture feature, since the grains were coarsened by welding heat.

36 MATERIALS SCIENCE↗

The Effects of Heat Treatment and Microstructure Variations on Disk Superalloy Properties at High Temperature

The effects of heat treatment and resulting microstructure variations on high temperature mechanical properties were assessed for a powder metallurgy disk superalloy LSHR. Blanks were consistently supersolvus solution heat treated and quenched at two cooling rates, than aged at varying temperatures and times. Tensile, creep, and dwell fatigue crack growth tests were then performed at 704 C. Gamma' precipitate microstructures were quantified. Relationships between heat treatment-microstructure, heat treatment-mechanical properties, and microstructure-mechanical properties were assessed.

Gabb, Timothy P.↗