Search NASA⌕ Search

SEARCH · Search NASA

Results for “Carbides”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,279 records · Page 71

Silicon carbide material sintered bodies manufacturing

A method is described for producing a high density silicon carbide sintering substance which contains aluminum oxide. The sintering is done in CO gas atmosphere, which is kept at 2 to 20 atmospheric pressures.

Suzuki, K.↗

Silicon carbide, a high temperature semiconductor

Electronic applications are described that would benefit from the availability of high temperature semiconductor devices. Comparisons are made among potential materials for these devices and the problems of each are discussed. Recent progress in developing silicon carbide as a high temperature semiconductor is described.

Powell, J. A.↗

Thermogravimetric analysis of silicon carbide-silicon nitride fibers at ambient to 1000 C in air

Thermogravimetric analysis of silicon carbide-silicon nitride fibers was carried out at ambient to 1000 C in air. The weight loss over this temperature range was negligible. In addition, the oxidative stability at high temperature for a short period of time was determined. Fibers heated at 1000 C in air for fifteen minutes showed negligible weight loss (i.e., less than 1 percent).

Daniels, J. G.↗

An improved process for preparing Tris(N-methylamino)methylsilane monomer for use in producing silicon carbide-silicon nitride fibers

A technique is described for the preparation of tris(N-methylamino)methylsilane by a process which may be used for large-scale production. The steps include synthesis, filtration to remove the salt byproduct, and distillation to remove the product from the reaction mixture under anhydrous conditions. Tris(N-methylamino)methylsilane is a precursor used to prepare silicon carbide-silicon nitride fibers that have been shown to have high tensile modulus (29 x 10 to the 6th psi for 0.4 mil diameter), high tensile strength (10.5 x 10 to the 4th psi), and high electrical resistivity (7 x 10 to the 8th ohm-cm).

Penn, B. G.↗

Thermal oxidation of 3C silicon carbide single-crystal layers on silicon

Thermal oxidation of thick single-crystal 3C SiC layers on silicon substrates was studied. The oxidations were conducted in a wet O2 atmosphere at temperatures from 1000 to 1250 C for times from 0.1 to 50 h. Ellipsometry was used to determine the thickness and index of refraction of the oxide films. Auger analysis showed them to be homogeneous with near stoichiometric composition. The oxide growth followed a linear parabolic relationship with time. Activation energy of the parabolic rate constant was found to be 50 kcal/mole, while the linear rate constant was 74 kcal/mole. The latter value corresponds approximately to the energy required to break a Si-C bond. Electrical measurements show an effective density of 4-6 x 10 to the 11th per sq cm for fixed oxide charges at the oxide-carbide interface, and the dielectric strength of the oxide film is aproximately 6 x 10 to the 6th V/cm.

Fung, C. D.↗

Producing Silicon Carbide for Semiconductor Devices

Processes proposed for production of SiC crystals for use in semiconductors operating at temperatures as high as 900 degrees C. Combination of new processes produce silicon carbide chips containing epitaxial layers. Chips of SiC first grown on porous carbon matrices, then placed in fluidized bed, where additional layer of SiC grows. Processes combined to yield complete process. Liquid crystallization process used to make SiC particles or chips for fluidized-bed process.

Hsu, G. C.↗

Sintered silicon carbide molded body and method for its production

Sintered silicon carbide shapes are described. They are produced by using a composition containing an oxide of at least one element chosen from the group: Li, Be, Mg, Si, Ca, Ti, V, Cr, Mn, Fe, Co, Ni, Zn, Nb, Mo, Ba, Tc, Ta, W and Th as a supplement to known sintering aids.

Omori, M.↗

Environmental effects on the tensile strength of chemically vapor deposited silicon carbide fibers

The room temperature and elevated temperature tensile strengths of commercially available chemically vapor-deposited (CVD) silicon carbide fibers were measured after 15 min heat treatment to 1600 C in various environments. These environments included oxygen, air, argon and nitrogen at one atmosphere and vacuum at 10/9 atmosphere. Two types of fibers were examined which differed in the SiC content of their carbon-rich coatings. Threshold temperature for fiber strength degradation was observed to be dependent on the as-received fiber-flaw structure, on the environment and on the coating. Fractographic analyses and flexural strength measurements indicate that tensile strength losses were caused by surface degradation. Oxidation of the surface coating is suggested as one possible degradation mechanism. The SiC fibers containing the higher percentage of SiC near the surface of the carbon-rich coating show better strength retention and higher elevated temperature strength.

Bhatt, R. T.↗

Preparation of silicon carbide-silicon nitride fibers by the pyrolysis of polycarbosilazane precursors

The development of silicon carbide-silicon nitride fibers (SiC-Si3N4) by the pyrolysis of polycarbosilazane precursors is reviewed. Precursor resin, which was prepared by heating tris(N-methylamino)methylsilane or tris(N-methylamino)phenylsilane to about 520 C, was drawn into fibers from the melt and then made unmeltable by humidity conditioning at 100 C and 95 percent relative humidity. The humidity treated precursor fibers were pyrolyzed to ceramic fibers with good mechanical properties and electrical resistivity. For example, SiC-Si3N4 fibers derived from tris(N-methylamino)methylsilane had a tensile rupture modulus of 29 million psi and electrical resistivity of 6.9 x ten to the 8th power omega-cm, which is ten to the twelfth power times greater than that obtained for graphite fibers.

Penn, B. G.↗

Thermogravimetric analysis of silicon carbide-silicon nitride polycarbosilazane precursor during pyrolysis from ambient to 1000 C

Thermogravimetric analysis data are presented on the unmeltable polycarbosilazane precursor of silicon carbide-silicon nitride fibers, over the room temperature-1000 C range in a nitrogen atmosphere, in order to establish the weight loss at various temperatures during the precursor's pyrolysis to the fiber material. The fibers obtained by this method are excellent candidates for use in applications where the oxidation of carbon fibers (above 400 C) renders them unsuitable.

Ledbetter, F. E., III↗

Conduction mechanism in boron carbide

Electrical conductivity, Seebeck-coefficient, and Hall-effect measurements have been made on single-phase boron carbides, B(1-x)C(x), in the compositional range from 0.1 to 0.2 X, and between room temperature and 1273 K. The results indicate that the predominant conduction mechanism is small-polaron hopping between carbon atoms at geometrically inequivalent sites.

Wood, C.↗

Silicon carbide filaments - Microstructure

The microstructure of chemically vapor deposited silicon carbide filaments has been examined using transmission electron microscopy. The filament bulk consisted of heavily faulted columnar subgrains of beta-SiC which were preferentially oriented such that 1 1 1 planes were parallel to the surface of the carbon fiber substrate. The protective coating on the filament surface was characterized by several microstructurally distinct layers, all of which consisted primarily of carbon. The first layers of the coating contained small crystallites of SiC in addition to turbostratic carbon, while the outer layers showed no evidence of SiC. Implications of the filament microstructure with respect to mechanical properties are discussed.

Nutt, S. R.↗

Effect of hot isostatic pressing on the properties of sintered alpha silicon carbide

Two lots of alpha silicon carbide were isostatically hot-pressed under 138 MPa for 2 h in Ar at temperatures up to 2200 C. Nearly theoretically dense specimens resulted. Hot isostatic pressing increased both room-temperature strength and 1200 C strength, and resulted in improved reliability. One lot of material which was pressed at 2200 C showed increases of about 20 percent in room-temperature strength and about 50 percent in 1200 C flexural strength; the Weibull modulus improved about 100 percent.

Watson, G. K.↗

Continuous Fiberization of Silicon-Carbide-Nitride Precursor Resin

The objective of this project is to design and build a laboratory scale extruder and with it to fiberize 5000 continuous feet of silicon-carbide-nitride precursor resin. Subsequently the objective is extended to include the cross-linking and pyrolysis of approximately 100 feet of the resin fiber. The extruder is designed to accommodate approximately 1 cubic centimeter samples at accurately controllable rates corresponding to take-up from a single orifice of a 25 micron fiber at speeds in the 1000 feet/minute region. Positive feed delivery is achieved with a cylinder and piston driven by a geared down electric motor. Gear reduction is achieved primarily with off-the-shelf parts. Over 5000 feet of fiber, 20 to 30 micron diameter, are spun from precursor resin samples. The formation of continuous silicon carbide/silicon nitride fiber appears to be feasible.

Dunn, S. A.↗

Development of a continuous spinning process for producing silicon carbide - silicon nitride precursor fibers

An apparatus was designed for the continuous production of silicon carbide - silicon nitride precursor fibers. The precursor polymer can be fiberized, crosslined and pyrolyzed. The product is a metallic black fiber with the composition of the type C sub x Si sub y n sub z. Little, other than the tensile strength and modulus of elasticity, is known of the physical properties.

Source record↗

Improved consolidation of silicon carbide

Alpha silicon carbide powder was consolidated by both dry and wet methods. Dry pressing in a double acting steel die yielded sintered test bars with an average flexural strength of 235.6 MPa with a critical flaw size of approximately 100 micro m. An aqueous slurry pressing technique produced sintered test bars with an average flexural strength of 440.8 MPa with a critical flaw size of approximately 25 micro m. Image analysis revealed a reduction in both pore area and pore size distribution in the slurry pressed sintered test bars. The improvements in the slurry pressed material properties are discussed in terms of reduced agglomeration and improved particle packing during consolidation.

Freedman, M. R.↗