Control of the optical and crystalline properties of TiO{sub 2} in visible-light active TiO{sub 2}/TiN bi-layer thin-film stacks

Multi-layered thin films of TiO{sub 2} and TiN were created by rf reactive magnetron sputtering, and their crystalline, optical, and photoelectrochemical properties were measured. The overall composition of the films (TiO{sub 2}-to-TiN ratio) was kept constant with the height of each film. The number of layers and thickness of each layer was controlled to create bi-layer thin films that were composed of: 9 bi-layers, 18 bi-layers, 27 bi-layers, 36 bi-layers, and 45 bi-layers. XRD patterns were observed for each film after annealing to measure the grain size and composition of anatase and rutile as a function of temperature. It was found that the phase-transition temperature is able to be substantially controlled (between 550 deg. C and 850 deg. C) for the anatase to rutile transition by varying the number of layers/thickness of each layer. In addition, bi-layer stacking significantly affected the film's optical properties by lowering the bandgap into the visible-light region, and also showed up to three times the improvement in photoelectrochemical performance under uv and visible irradiation. Overall, bi-layer stacking of TiO{sub 2}/TiN films has shown a unique and highly desirable control over several important physical characteristics that can be beneficial for many applications, such as high-temperature sensors and optoelectronic devices.

36 MATERIALS SCIENCE↗

Iron and nitrogen self-diffusion in non-magnetic iron nitrides

The self-diffusion of iron and nitrogen is measured in nm range non-magnetic iron nitride thin films. Two non-magnetic iron nitrides, Fe{sub 2.23}N and FeN, were studied using neutron reflectivity. Neutron reflectivity with a depth resolution in the sub-nm range has a different scattering cross section for isotopes, providing a unique opportunity to measure very small diffusivities. The isotope heterostructure in thin film multilayers [Fe-N/{sup 57}Fe-N]{sub 10} and [Fe-N/Fe-{sup 15}N]{sub 10} were prepared using magnetron sputtering. It was observed that nitrogen diffuses slower than iron although the atomic size of iron is larger than that of nitrogen. It was found that a significantly larger group of N atoms participates in the diffusion process than of Fe, making N diffusion slower than that of Fe.

36 MATERIALS SCIENCE↗

Dual phase transformation and resultant magnetic properties in Fe{sub 3}Pt thin films

Fifty-nm-thick Fe{sub 75}Pt{sub 25} thin films have been made on glass substrates by rf magnetron sputtering at room temperature, and subsequently annealed at 300 -700 deg. C (T{sub a}) for 1 h. The as-deposited Fe{sub 3}Pt film exhibits high magnetization of 1530 emu/cm{sup 3} and a disordered bcc structure, confirmed by high-resolution synchrotron radiation x-ray diffractometry. First-phase transformation from the bcc to disorder fcc structure occurs for samples annealed at 300 deg. C. With increasing of T{sub a} up to 375 deg. C, the film displays a nearly disordered fcc phase with low magnetization of 1083 emu/cm{sup 3}. The fcc phase changes to ordered L1{sub 2} structure for samples with T{sub a} {>=} 400 deg. C. The highly ordered L1{sub 2} phase with magnetization of 1270 emu/cm{sup 3} and coercivity of 66 Oe was obtained in Fe{sub 3}Pt film at 700 deg. C-annealing.

36 MATERIALS SCIENCE↗

Effect of the number of interfaces on the magnetic properties of [SnO{sub 2}/Cu-Zn ferrite] multilayer

The [SnO{sub 2}/Cu-Zn ferrite (CZF)]{sub n} (n = 5, 10, 15, and 20) multilayer (ML) were deposited by rf-magnetron sputtering to study their magnetic properties. The magnetization and ferromagnetic resonance (FMR) measurements were undertaken to understand the effect of interfaces on the magnetic properties of these ML. FMR signal line shape changes from asymmetric to symmetric as n increases. The FMR signal peak to peak intensity, FMR linewidth, effective and saturation magnetization and coercivity exhibit oscillations as a function of n. In the parallel configuration the resonance field increases with increase in n, presumably due to the decrease in the active layer to dead layer thickness ratio. The interlayer coupling is strong in the ML with n = 5 leading to the formation of spin waves. The ML interlayer coupling and anisotropy decreases with increasing n. The oscillatory behavior of the magnetic properties can be ascribed to the nonmonotonic variations in the structure and the geometry of the interfaces.

36 MATERIALS SCIENCE↗

Control of magnetic properties of MnBi and MnBiCu thin films by Kr{sup +} ion irradiation

Mn{sub 52}Bi{sub 48} (15 nm) and Mn{sub 54}Bi{sub 24}Cu{sub 21} (15 nm) thin films were prepared by the magnetron sputtering and vacuum annealing at 350 deg. C, and the variations of their structures and magnetic properties with 30 keV Kr{sup +} ion irradiation were studied. The MnBi and MnBiCu films exhibited saturation magnetizations M{sub s} of 180 emu/cc and 210 emu/cc, the coercivities H{sub c} of 10 kOe and 3.4 kOe, respectively. The M{sub s} and H{sub c} of the MnBi abruptly vanished by the irradiation of ion dose at 3 x 10{sup 14} ions/cm{sup 2}, while those of the MnBiCu film gradually decreased with increasing the ion dose and became zero at 5 x 10{sup 13} ions/cm{sup 2}. The different trend on the ion irradiation between MnBi and MnBiCu films is understood by the surface structure of the film, i.e., the MnBi has convex islands on its surface, which protect the underneath NiAs-type MnBi from the irradiation, while the MnBiCu has rather flat surface, and its crystal structure was uniformly modified by the irradiation. From the surface flatness and the uniformity of the MnBiCu film, as well as the low annealing temperature of 350 deg. C, it was concluded that the MnBiCu film is one of the attractive materials for high-density ion irradiation bit patterned media.

36 MATERIALS SCIENCE↗

One-step fabrication of L1{sub 0} FePt nanocubes and rods by cluster beam deposition

In this work, single crystal L1{sub 0} FePt nanocubes have been successfully produced by a cluster beam deposition technique without the need of post annealing. Particles have been deposited by dc magnetron sputtering using high Ar pressures on both single crystal Si substrates and Au grids for the measurement of magnetic and structural properties, respectively. The nanocubes have a uniform size distribution with an average size of 5 nm. At 1 Torr, the particles have the L1{sub 0} structure with an order parameter of 0.5 and a RT coercivity of 2 kOe with high switching fields observed in the hysteresis loop. Further annealing increased the particle size to 20 nm and the RT coercivity to 10.2 kOe with perfect chemical ordering. In addition to these nanocubes, micron size rods with the L1{sub 0} structure have been observed near the cluster gun. SEM analysis showed that these rods consist of nanoparticles with 20 nm average size. Surfactant assisted high-energy ball milling has been used to separate the nanoparticles from the rods. After one hour of milling, these 20 nm particles showed a room temperature coercivity of 9 kOe with an order parameter of 0.85. These FePt nanocubes have a potential for use in the development of future high-density magnetic recording media because of their high coercivity, good shape and very narrow size distribution.

36 MATERIALS SCIENCE↗

Polycrystalline magnetic garnet films comprising weakly coupled crystallites for piezoelectrically-driven magneto-optic spatial light modulators

We have investigated the magnetization process of the polycrystalline magnetic garnet films in order to determine the most suitable composition of garnet films for piezoelectrically-driven magneto-optic spatial light modulators (MOSLMs). For experiment, the bismuth-dysprosium-aluminum-substituted yttrium iron (Bi{sub 1.3}Dy{sub 0.7}Y{sub 1.0}Fe{sub 3.1}Al{sub 1.9}O{sub 12}) garnet films were deposited by an RF magnetron sputter and annealed at 700 deg. C in air. The annealing time was varied in a range of several minutes to control the grain size. The saturation magnetization, the remanent magnetization and the composition of the fabricated garnet films slightly changed versus the annealing time. Experiments showed that the coercivity and the grain size increased at longer annealing; the coercivity was larger for films with bigger grains. This work shows that garnet films with smaller coercivity are most suitable for controlling the magnetization of garnet and, correspondingly, the magneto-optical rotation of MOSLM pixels driven by piezoelectrics.

36 MATERIALS SCIENCE↗

Breakdown by magnetic field in a La{sub 0.7}Sr{sub 0.3}MnO{sub 3}/MgO/Fe spin valve

A La{sub 0.7}Sr{sub 0.3}MnO{sub 3}/MgO/Fe spin valve with inverse tunneling magnetoresistance (TMR) was fabricated on a (100) SrTiO{sub 3} substrate by radio frequency magnetron sputtering. Giant TMR ratios up to 540% were obtained. The breakdown of the spin valve was observed at high magnetic field, which was attributed to the joint action of the invalidation of MgO barrier and the shift of Fermi energy in La{sub 0.7}Sr{sub 0.3}MnO{sub 3} at high magnetic field.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Designing interlayers to improve the mechanical reliability of transparent conductive oxide coatings on flexible substrates

In this study, we investigate the effect of interlayers on the mechanical properties of transparent conductive oxide (TCO) on flexible polymer substrates. Indium tin oxide (ITO), which is the most widely used TCO film, and Ti, which is the most widely used adhesive interlayer, are selected as the coating and the interlayer, respectively. These films are deposited on the polymer substrates using dc-magnetron sputtering to achieve varying thicknesses. The changes in the following critical factors for film cracking and delamination are analyzed: the internal stress ({sigma}{sup i}) induced in the coatings during deposition using a white light interferometer, the crystallinity using a transmission electron microscope, and the surface roughness of ITO caused by the interlayer using an atomic force microscope. The resistances to the cracking and delamination of ITO are evaluated using a fragmentation test. Our tests and analyses reveal the important role of the interlayers, which significantly reduce the compressive {sigma}{sup i} that is induced in the ITO and increase the resistance to the buckling delamination of the ITO. However, the relaxation of {sigma}{sup i} is not beneficial to cracking because there is less compensation for the external tension as {sigma}{sup i} further decreases. Based on these results, the microstructural control is revealed as a more influential factor than {sigma}{sup i} for improving crack resistance.

36 MATERIALS SCIENCE↗

Optical and electronic properties of Ti{sub 1-x}Nb{sub x}N thin films

Ti{sub 1-x}Nb{sub x}N thin films with x=0, 0.26, 0.41, 0.58 and 1 were deposited on silicon (311) substrate by RF magnetron sputtering. The dielectric functions of these films were calculated by fitting measured reflectance spectra to the Drude-Lorentz model. The measured reflectance spectra exhibits a minimum in the visible region and this feature shifts to higher energy (shorter wavelength) with increase in x. The observed behavior can be modeled as the response of four Lorentz oscillators. The real part of the dielectric function is characterized by a screened plasma energy of 2.26 eV for x=0 which increased to 2.80 eV for x=0.58 in the Ti{sub 1-x}Nb{sub x}N film.

36 MATERIALS SCIENCE↗

Optimization of Ti addition in Fe for Fe-Ti-N thin films

In this work we studied the magnetic and structural properties of Fe{sub 1-x}Ti{sub x}(x=0, 0.02, 0.05, 0.07) thin films prepared with dc-magnetron sputtering. It was found that the inter-atomic spacing increases as the amount of Ti is increased indicating that Ti is getting dissolved substitutionally in Fe lattice. We found that the addition of 5% Ti is best suited for its usage in Fe-Ti-N alloys.

36 MATERIALS SCIENCE↗

Realization of low resistive p-ZnO thin film by Al-As codoping

Al-As codoping into ZnO has been proposed to realize low resistive and stable p-ZnO thin film by RF magnetron sputtering. Al-As codoping has been achieved by As back diffusion from GaAs substrate and sputtering Al doped ZnO target. Hall measurements showed that the hole concentration increases with the increase of Al concentration from 10{sup 15} to 10{sup 20} cm{sup -3}. Among the grown films, 1 at% Al doped ZnO: As showed low resistivity (3.5x10{sup -2}{Omega}cm) with high hole concentration. X-ray diffraction shows that all the films are crystallized in wurtzite structure with (002) preferential orientation. The diffusion of As atoms from the substrate and the presence of dopants in the film have been confirmed by Rutherford ford back scattering and energy dispersive spectroscopy analysis, respectively.

36 MATERIALS SCIENCE↗

Structural, electrical and optical properties of GaP codoped ZnO thin films

The GaP codoped ZnO (GPZO) thin films of different concentrations (0, 1, 2 and 4 mol%) have been grown by RF magnetron sputtering to realize p-ZnO. The grown films on sapphire substrates have been characterized by X-ray diffraction (XRD), Hall measurement, photoluminescence (PL), and Energy dispersive spectroscopy (EDS). XRD studies reveal that all the films are preferentially oriented along (002) plane. Hall measurement shows that 2% GPZO film shows low resistivity (2.17 {Omega} cm) and high hole concentration (1.8 x 10{sup 18} cm{sup -3} due to optimum amount of P incorporation. EDS spectra confirms the presence of Ga and P in 2 mol% GPZO film.

36 MATERIALS SCIENCE↗

Atomic scale observation of phase separation and formation of silicon clusters in Hf higk-{kappa} silicates

Hafnium silicate films were fabricated by RF reactive magnetron sputtering technique. Fine microstructural analyses of the films were performed by means of high-resolution transmission electron microscopy and atom probe tomography. A thermal treatment of as-grown homogeneous films leads to a phase separation process. The formation of SiO{sub 2} and HfO{sub 2} phases as well as pure Si one was revealed. This latter was found to be amorphous Si nanoclusters, distributed uniformly in the film volume. Their mean diameter and density were estimated to be about 2.8 nm and (2.9 {+-} 0.4) x 10{sup 17} Si-ncs/cm{sup 3}, respectively. The mechanism of the decomposition process was proposed. The obtained results pave the way for future microelectronic and photonic applications of Hf-based high-{kappa} dielectrics with embedded Si nanoclusters.

36 MATERIALS SCIENCE↗

B{sub 4}C thin films for neutron detection

Due to the very limited availability of {sup 3}He, new kinds of neutron detectors, not based on {sup 3}He, are urgently needed. Here, we present a method to produce thin films of {sup 10}B{sub 4}C, with maximized detection efficiency, intended to be part of a new generation of large area neutron detectors. B{sub 4}C thin films have been deposited onto Al-blade and Si wafer substrates by dc magnetron sputtering from {sup nat}B{sub 4}C and {sup 10}B{sub 4}C targets in an Ar discharge, using an industrial deposition system. The films were characterized with scanning electron microscopy, elastic recoil detection analysis, x-ray reflectivity, and neutron radiography. We show that the film-substrate adhesion and film purity are improved by increased substrate temperature and deposition rate. A deposition rate of 3.8 A/s and substrate temperature of 400 deg. C result in films with a density close to bulk values and good adhesion to film thickness above 3 {mu}m. Boron-10 contents of almost 80 at. % are obtained in 6.3 m{sup 2} of 1 {mu}m thick {sup 10}B{sub 4}C thin films coated on Al-blades. Initial neutron absorption measurements agree with Monte Carlo simulations and show that the layer thickness, number of layers, neutron wavelength, and amount of impurities are determining factors. The study also shows the importance of having uniform layer thicknesses over large areas, which for a full-scale detector could be in total {approx}1000 m{sup 2} of two-side coated Al-blades with {approx}1 {mu}m thick {sup 10}B{sub 4}C films.

36 MATERIALS SCIENCE↗

Structural and electrical studies of ultrathin layers with Si{sub 0.7}Ge{sub 0.3} nanocrystals confined in a SiGe/SiO{sub 2} superlattice

In this work, SiGe/SiO{sub 2} multi-layer (ML) films with layer thickness in the range of a few nanometers were successfully fabricated by conventional RF-magnetron sputtering at 350 deg. C. The influence of the annealing treatment on SiGe nanocrystals (NCs) formation and crystalline properties were investigated by Raman spectroscopy and grazing incidence x-ray diffraction. At the annealing temperature of 800 deg. C, where well defined SiGe NCs were observed, a thorough structural investigation of the whole ML structure has been undertaken by Rutherford backscattering spectroscopy, grazing incidence small angle x-ray scattering, high resolution transmission electron microscopy, and annular dark field scanning transmission electron microscopy. Our results show that the onset of local modifications to the ML composition takes place at this temperature for annealing times of the order of a few tens of minutes with the formation of defective regions in the upper portion of the ML structure. Only the very first layers over the Si substrate appear immune to this problem. This finding has been exploited for the fabrication of a defect free metal-oxide-semiconductor structure with a well-defined single layer of SiGe NCs. A memory effect attributed to the presence of the SiGe NCs has been demonstrated by high frequency capacitance-voltage measurements.

36 MATERIALS SCIENCE↗

Nanostructured multilayered thin film barriers for Mg{sub 2}Si thermoelectric materials

The Mg{sub 2}Si-based alloys are promising candidates for thermoelectric energy conversion in the middle-high temperature range in order to replace lead compounds. The main advantages of silicide-based thermoelectrics are the nontoxicity and the abundance of their constituent elements in the earth crust. The drawback of such kind of materials is their oxygen sensitivity at high temperature that entails their use under vacuum or inert atmosphere. In order to limit the corrosion phenomena, nanostructured multilayered molybdenum silicide-based materials were deposited via RF magnetron sputtering onto stainless steel, alumina and silicon (100) to set up the deposition process and then onto Mg{sub 2}Si pellets. XRD, EDS, FE-SEM and electrical measurements at high temperature were carried out in order to obtain, respectively, the structural, compositional, morphological and electrical characterization of the deposited coatings. At the end, the mechanical behavior of the system thin film/Mg{sub 2}Si-substrate as a function of temperature and the barrier properties for oxygen protection after thermal treatment in air at high temperature were qualitatively evaluated by FE-SEM.

36 MATERIALS SCIENCE↗

Nanocrystallization of amorphous M-Si thin film composites (M=Cr, Mn) and their thermoelectric properties

We report on electrical resistivity and thermoelectric power of Cr-Si and Mn-Si composite films at temperatures from 300 K to 1000 K. The films were deposited on unheated Si/SiO{sub 2} substrates by magnetron sputtering from composite targets. The as-deposited films have amorphous structure. We use annealing with in-situ transport properties measurements to transform the films into nanocrystalline state with continuous monitoring their state. Nanocrystallization is considered as a promising way to improve thermoelectric efficiency, primarily due to reduction of lattice thermal conductivity {kappa}. Among variety of methods for fabrication of NC materials, crystallization from amorphous state has features which are crucially important with respect to their electronic transport properties: since the crystallites and their interfaces are formed in this method via solid state reaction, the NC samples are dense and the interfaces are clean. This removes additional factors affecting properties of a nanocrystalline composite, such as contamination of nanocrystal interfaces by elements from environment or nanocrystal lattice distortion during nanocrystallization. Depending on the initial film composition, the films are transformed during annealing into single phase or multi-phase nanocrystalline composites with average grain size of 10 nm to 20 nm. We study the crystallization kinetics, stability of amorphous and nanocrystalline state and relation between electronic transport properties and structural state of the composites.

36 MATERIALS SCIENCE↗