Preparation, microstructure and properties of AlN/CBC composites

Highlights: • AlN/CBC composites can be prepared by gelcasting and pressureless sintering method. • Suitable sintering additive content and increasing sintering temperature help to improve properties of composite. • Relative density, C content and microstructure et al. have effect on properties of composite. - Abstract: Gelcasting method with nontoxic biopolymer as gel former can be used to prepare ceramics with complex shape. AlN ceramic bonded carbon (AlN/CBC) composites with light weight were fabricated by gelcasting and pressureless sintering method using nontoxic agarose as gel former with Y{sub 2}O{sub 3} + CaF{sub 2} as sintering additive. The effect of sintering additive content and sintering temperature on the microstructure, flexural strength and thermal conductivity of composites was investigated. The results reveal that, as the temperature decreases, the raw powders solidify into three-dimensional net structures through abundant hydrogen bonds in the agarose. High sintering temperature facilitates densification and improves mechanical and thermal properties of the composites. Increasing sintering additive content can also tune the density and raise flexural strength. The AlN/CBC composite containing 7 wt% sintering additive content, which was sintered at 2000 °C, exhibits the highest thermal conductivity. Relative density, C content and microstructure uniformity have effects on properties of AlN/CBC composite.

36 MATERIALS SCIENCE↗

SEM and TEM characterization of microstructure of stainless steel composites reinforced with TiB{sub 2}

Steel-8TiB{sub 2} composites were produced by two new sintering techniques, i.e. Spark Plasma Sintering (SPS) and High Pressure-High Temperature (HP-HT) sintering. This study discusses the impact of these sintering methods on the microstructure of steel composites reinforced with TiB{sub 2} particles. Scanning electron microscopy (SEM), wavelength dispersive spectroscopy (WDS), X-ray diffraction, electron backscatter diffraction (EBSD) and transmission electron microscopy (TEM) were used to analyze the microstructure evolution in steel matrix composites. The results of microscopic examinations revealed a close relationship between the composite microstructure and the methods and conditions of sintering. Substantial differences were observed in the grain size of materials sintered by HP-HT and SPS. It has been demonstrated that the composites sintered by HP-HT tend to form a chromium-iron-nickel phase in the steel matrix. In contrast, the microstructure of the composites sintered by SPS is characterized by the presence of complex borides and chromium-iron phase. - Highlights: •The steel-8TiB{sub 2} composites were fabricated by Spark Plasma Sintering (SPS) and High Pressure-High Temperature (HP-HT). •Sintering techniques has an important effect on changes in the microstructure of steel-8TiB{sub 2} composites. •New phases of different size and morphology were identified.

36 MATERIALS SCIENCE↗

Metal Fused Filament Fabrication of Titanium Alloy for In Space Manufacturing

NASA is developing materials and processes for the in-space manufacturing of many items for the International Space Station (ISS) and future exploration platforms. These new manufacturing processes will require the further development of current 3D printing processes to achieve high-performance metal parts within the power and space constraints of the ISS. Manufacturing Ti-6Al-4V alloy parts with 3D printing using a metal fused filament fabrication (MF3) process is an alternative process to the Direct Metal Laser Sintering (DMLS) of the metal powders additive manufacturing process. Our initial work fabricating Ti-6Al-4V parts from Ti-6Al-4V powder-binder feedstock and processed with the MF3 process has resulted in 95-97% sintered densities. The current development work of optimized sintered properties investigates the effects of variation in sintering time, temperature, and vacuum on the sintered properties of Ti-6Al-4V MF3 printed tensile bars. Sintered properties such as density, hardness, and tensile properties were characterized followed by microstructural and chemical (O/C/N) analysis to understand the role of sintering process on the ensuing material properties. Future development of the MF3 process will also involve investigation of the effects of micro-milling the Ti-64Al-4V powder to nanometer particle sizes and the investigation of laser sintering of the 3D printed devices. This new micro-milling technique will have broad application to other areas that require particle size reduction of hard metallic materials, such as Nuclear Thermal Propulsion and other NASA technologies. Laser sintering in lieu of high temperature thermal sintering should allow for significant power reduction and improved processing speeds.

sintering, alloys, 3D printing↗

Developing Cost-Effective Dense Continuous SDC Barrier Layers for SOFCs

Significantly improved performance during electrochemical testing of a cell with a dense continuous pulsed laser deposited (PLD) samarium doped ceria (SDC) layer spurred investigations into the fabrication of dense continuous SDC barrier layers by means of cost-effective deposition using screen printing which is amenable to industrial production of SOFCs. Many approaches to improve the SDC density have been explored including the use of powder with reduced particle sizes, inks with increased solids loading, and doping with sintering aids (1). In terms of sintering aids, dopants like Mo or binary systems of Mo+Cu or Fe+Co greatly enhance SDC sinterability. In fact, adding dopants to a screen printed, prefired, porous SDC layer made it possible to achieve a dense continuous barrier layer atop the YSZ electrolyte without sintering above 1200°C. Although the objective of fabricating a dense continuous layer was achieved, additional studies have been initiated to improve the cell performance. Underlying issues with constrained sintering and dopant-enhanced ceria-zirconia solid solubility are also addressed in this paper.

Nguyen, Hoang Viet P.↗

Lightweight Aluminum/Nano composites for Automotive Drive Train Applications

During Phase I, we successfully processed air atomized aluminum powders via Dynamic Magnetic Compaction (DMC) pressing and subsequent sintering to produce parts with properties similar to wrought aluminum. We have also showed for the first time that aluminum powders can be processed without lubes via press and sintering to 100 % density. This will preclude a delube cycle in sintering and promote environmentally friendly P/M processing. Processing aluminum powders via press and sintering with minimum shrinkage will enable net shape fabrication. Aluminum powders processed via a conventional powder metallurgy process produce too large a shrinkage. Because of this, sinter parts have to be machined into specific net shape. This results in increased scrap and cost. Fully sintered aluminum alloy under this Phase I project has shown good particle-to-particle bonding and mechanical properties. We have also shown the feasibility of preparing nano composite powders and processing via pressing and sintering. This was accomplished by dispersing nano silicon carbide (SiC) powders into aluminum matrix comprising micron-sized powders (<100 microns) using a proprietary process. These composite powders of Al with nano SiC were processed using DMC press and sinter process to sinter density of 85-90%. The process optimization along with sintering needs to be carried out to produce full density composites.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Microwave Structure Construction Capability Year One Accomplishments

The Microwave Structure Construction Capability (MSCC) element, part of the Moon to Mars Planetary Autonomous Construction Project (MMPACT) was initiated in 2020. MSCC is responsible for creating horizontal and vertical infrastructure on the moon using microwave energy. Microwave energy was selected since it is the only method to volumetrically heat the regolith. All other sintering/melting methods rely on thermal conduction through the very low conductivity surface, resulting in an inefficient process. Advances were achieved in materials characterization and understanding, microwave sintering in vacuum, and microwave design and analyses. Two dielectric property testing systems have been developed at Radiance Technologies and JPL. These will examine dielectric properties at cryogenic temperatures and over a broad frequency range. Permittivity and permeability testing at -60 ̊C in vacuum from 0.05 to 3 GHz has been generated at JPL. Additional modifications will be made to go to -190 ̊C (LN2). Radiance Technologies created a test system to measure dielectric properties at greater than 10 GHz and initiated work on developing a vacuum capable, portable test system to measure dielectric properties of Apollo regolith and simulants from 100 MHz to 18 GHz. These tests are to identify optimal heating frequencies and protocols. During microwave sintering at about 1100 ̊C, volatiles were creating difficulty in achieving a reasonably dense specimen. Due to processing in vacuum and the nature of the lunar regolith, some volatiles and porosity are expected. However, the Earth produced simulants have non-lunar materials in them that create volatiles that aren’t representative of lunar regolith. Therefore, a five month effort was conducted to establish a heat treat method to remove these non-lunar materials. Tests were conducted using TGA mass spectrometry, heating in vacuum and conducting mass spectrometry, dielectric and DTA, Raman, BET, particle size analysis, morphological analysis, carbon and sulfur chemical content determination and microscopy. The process has been scaled-up to 6 kg batch size and undergoing evaluation. A 36 kg batch size is the target for JSC-1A and other limited availability simulants. These calcining protocols will be standard for NASA and beyond. MSCC has also created scalable processes for fabricating synthetic lunar materials. Processes to fabricate Anorthite (plagioclase CaAl2Si2O8), Diopside (pyroxene CaMgSi₂O₆), and Enstatite (pyroxene Mg2Si2O6) have been generated. These materials will enable generation of microwave sintering models to bound various composition ranges anticipated on the Moon, therefore mitigating the need for a precise simulant with respect to location on the Moon. Successful microwave sintering in air using a horn applicator was demonstrated. All previous microwave vacuum sintering in the literature was at small scale and in a contained enclosure thus taking advantage of reflections. This is the first to use a lunar like microwave applicator to sinter ceramic in a bed as it would be done on the Moon. Small scale and inert sintering were conducted to assist in developing protocols with quicker turnaround times than larger scale testing. Testing has anchored thermal analysis predicting heat flow in vacuum during microwave sintering. Thermal conductivity testing was also initiated. Microwave coupling to the regolith has been modeled by multiple organizations and with different software packages. At least six horn designs and applicator configurations for both magnetron and solid state sources are being examined. Optimal simulant container designs for microwaves have also been generated. The power and electronics design for the solid state microwave system has been initiated. Concept designs for a lander based microwave sintering have been evaluated.

microwave↗

W-ZrC composites prepared by reactive melt infiltration of Zr 2 Cu alloy into binder jet 3D printed WC preforms

W-ZrC composites were successfully prepared by reactive melt infiltration (RMI) of stoichiometric and excess amounts of Zr 2 Cu into sintered and un-sintered WC preforms made from binder jet 3D printing. The focus of this work was to study the conversion of reactant powders and liquid infiltrant with varying preform density and infiltrant amount by controlling the processing time to reach high conversion yield while understanding the phase composition, microstructure, and hardness. To investigate the effect of time, the reactive melt infiltration was conducted at 1400 °C for 2, 4 and 8 h in a furnace with 96% Ar - 4% H2 gas atmosphere. The increase in reaction time from 2 to 8 h increased the W and W 2 C phase contents and decreased the ZrC phase content when using sintered WC preforms. Samples prepared from un-sintered WC preforms exhibited improved reactive melt infiltration compared to sintered samples, and there was no detectable W 2 C phase and nearly full consumption of WC. Similar to sintered WC samples, the content of W and ZrC phases increased with the increase in time from 2 to 8 h. The interfaces and phases at reaction interfaces were investigated using electron diffraction analysis and S/TEM-EDS to understand material stability; the phases were identified and consistent with XRD analysis. Additionally, there was no Cu present at the interfaces. Increasing the amount of infiltrant led to better reactive melt infiltration. In general, the hardness increased with reaction time and the highest Vickers hardness was found in the W-ZrC sample formed from sintered WC reacted with excess Zr 2 Cu. Finally, this research addresses the critical comparison of sintering and RMI time and shows that by using un-sintered samples for 8 h we are able to achieve W-ZrC composites with fewer undesired phases.

36 MATERIALS SCIENCE↗

Power factor improvement in hydrothermally synthesized Bi{sub 2-x}Sb{sub x}Te{sub 3} (x=1.5) - carbon sphere composites

We report fabrication of compacted Bi{sub 0.5}Sb{sub 1.5}Te{sub 3} composites by adding 1 wt% of carbon spheres in the hydrothermal synthesis. The processing parameter of sintering temperature is investigated in order to optimize the thermoelectric power factor of pressed Bi{sub 0.5}Sb{sub 1.5}Te{sub 3} composites. As a result, we find that the composite sintered at 360 Degree-Sign C shows the best power factor performance among the composites and has a largest power factor of 15.4 {mu}W/cm K{sup 2} at 205 K and 13.5 {mu}W/cm K{sup 2} at 290 K. When compared with the samples without addition of carbon sphere in the hydrothermal synthesis, the composites sintered at 340 Degree-Sign C and 360 Degree-Sign C both surpass the largest power factor of 12.1 {mu}W/cm K{sup 2} at 280 K and 11.9 {mu}W/cm K{sup 2} at 290 K for the 340 Degree-Sign C-sintered counterpart. - Graphical abstract: Compacted Bi{sub 0.5}Sb{sub 1.5}Te{sub 3-{delta}} composites obtained by adding 1 wt% of carbon spheres in the hydrothermal synthesis. The composites sintered at 340 Degree-Sign C and 360 Degree-Sign C both surpass the largest power factor of 12.1 {mu}W/cm K{sup 2} at 280 K and 11.9 {mu}W/cm K{sup 2} at 290 K for the 340 Degree-Sign C-sintered counterpart. Highlights: Black-Right-Pointing-Pointer Fabrication of Bi{sub 0.5}Sb{sub 1.5}Te{sub 3-{delta}} composites. Black-Right-Pointing-Pointer Addition of 1 wt% carbon spheres in the hydrothermal synthesis. Black-Right-Pointing-Pointer Investigation of sintering temperature using encapsulating-and-sintering techniques. Black-Right-Pointing-Pointer 360 Degree-Sign C-sintered composite showing the largest power factor of 15.4 {mu}W/cm K{sup 2} at 205 K. Black-Right-Pointing-Pointer 10-60% improvement over the counterpart without adding carbon spheres.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Powder Metallurgy of Uranium Alloy Fuels for TRU-Burning Reactors Final Technical Report

Overview Fast reactors were evaluated to enable the transmutation of transuranic isotopes generated by nuclear energy systems. The motivation for this was that TRU isotopes have high radiotoxicity and relatively long half-lives, making them unattractive for disposal in a long-term geologic repository. Fast reactors provide an efficient means to utilize the energy content of the TRUs while destroying them. An enabling technology that requires research and development is the fabrication metallic fuel containing TRU isotopes using powder metallurgy methods. This project focused upon developing a powder metallurgical fabrication method to produce U-Zr-transuranic (TRU) alloys at relatively low processing temperatures (500ºC to 600ºC) using either hot extrusion or alpha-phase sintering for charecterization. Researchers quantified the fundamental aspects of both processing methods using surrogate metals to simulate the TRU elements. The process produced novel solutions to some of the issues relating to metallic fuels, such as fuel-cladding chemical interactions, fuel swelling, volatility losses during casting, and casting mold material losses. Workscope There were two primary tasks associated with this project: 1. Hot working fabrication using mechanical alloying and extrusion • Design, fabricate, and assemble extrusion equipment • Extrusion database on DU metal • Extrusion database on U-10Zr alloys • Extrusion database on U-20xx-10Zr alloys • Evaluation and testing of tube sheath metals 2. Low-temperature sintering of U alloys • Design, fabricate, and assemble equipment • Sintering database on DU metal • Sintering database on U-10Zr alloys • Liquid assisted phase sintering on U-20xx-10Zr alloys Appendices Outline Appendix A contains a Fuel Cycle Research & Development (FCR&D) poster and contact presentation where TAMU made primary contributions. Appendix B contains MSNE theses and final defense presentations by David Garnetti and Grant Helmreich outlining the beginning of the materials processing setup. Also included within this section is a thesis proposal by Jeff Hausaman. Appendix C contains the public papers and presentations introduced at the 2010 American Nuclear Society Winter Meeting. Appendix A—MSNE theses of David Garnetti and Grant Helmreich and proposal by Jeff Hausaman A.1 December 2009 Thesis by David Garnetti entitled “Uranium Powder Production Via Hydride Formation and Alpha Phase Sintering of Uranium and Uranium-Zirconium Alloys for Advanced Nuclear Fuel Applications” A.2 September 2009 Presentation by David Garnetti (same title as document in Appendix B.1) A.3 December 2010 Thesis by Grant Helmreich entitled “Characterization of Alpha-Phase Sintering of Uranium and Uranium-Zirconium Alloys for Advanced Nuclear Fuel Applications” A.4 October 2010 Presentation by Grant Helmreich (same title as document in Appendix B.3) A.5 Thesis Proposal by Jeffrey Hausaman entitled “Hot Extrusion of Alpha Phase Uranium-Zirconium Alloys for TRU Burning Fast Reactors” Appendix B—External presentations introduced at the 2010 ANS Winter Meeting B.1 J.S. Hausaman, D.J. Garnetti, and S.M. McDeavitt, “Powder Metallurgy of Alpha Phase Uranium Alloys for TRU Burning Fast Reactors,” Proceedings of 2010 ANS Winter Meeting, Las Vegas, Nevada, USA, November 7-10, 2010 B.2 PowerPoint Presentation Slides from C.1 B.3 G.W. Helmreich, W.J. Sames, D.J. Garnetti, and S.M. McDeavitt, “Uranium Powder Production Using a Hydride-Dehydride Process,” Proceedings of 2010 ANS Winter Meeting, Las Vegas, Nevada, USA, November 7-10, 2010 B.4. PowerPoint Presentation Slides from C.3 B.5 Poster Presentation from C.3 Appendix C—Fuel cycle research and development undergraduate materials and poster presentation C.1 Poster entitled “Characterization of Alpha-Phase Sintering of Uranium and Uranium-Zirconium Alloys” presented at the Fuel Cycle Technologies Program Annual Meeting C.2 April 2011 Honors Undergraduate Thesis by William Sames, Research Fellow, entitled “Uranium Metal Powder Production, Particle Distribution Analysis, and Reaction Rate Studies of a Hydride-Dehydride Process"

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Optimization of the dissolution of molybdenum disks. FY-16 results

Argonne National Laboratory is providing technical development assistance to NorthStar Medical Technologies LLC in its pursuit of two pathways for production of molybdenum-99: the 98 Mo(n,γ) 99 Mo reaction and the photonuclear reaction, 100 Mo(γ,n) 99 Mo. Processing of irradiated targets, from either production mode, requires dissolution of the target material in H 2 O 2 followed by a concentration step, addition of ferric ion to precipitate impurities, and conversion of the final solution to 5M potassium hydroxide solution of potassium molybdate. Currently, NorthStar is using pressed and sintered Mo disks as targets. Several options are being considered for the design of Mo targets for the production of 99 Mo using the (γ,n) reaction. In the current design, the target holder contains a series of sintered Mo disks lined up perpendicular to two incident electron beams, one entering from each side of the target stack. In this configuration, the front-most disks absorb most of the heat from the electron beam and need to be thinner to allow for better cooling, while the middle of the target can be thicker. Distribution of the total mass of Mo allows for larger masses of Mo material and thus larger production batches of 99 Mo. A limitation of the sintering approach is the production of very thin disks. Recent advances in 3D printing allow for much thinner target components can be achieved than when the traditional press-and-sinter approach is used. We have demonstrated that several factors can play important roles in dissolution behavior: particle size of Mo metal used for production of targets, sintering conditions, degree of open porosity, and thickness of the sintered Mo targets. Here we report experimental results from studies of small-scale dissolution of sintered Mo disks fabricated from various recycled and commercial Mo materials, and dissolution of 3D-printed Mo disks that were fabricated by Oak Ridge National Laboratory (ORNL). We also report on large-scale dissolution studies with 600 g batches of sintered Mo disks.

38 RADIATION CHEMISTRY, RADIOCHEMISTRY, AND NUCLEA↗

Preparation and thermoelectric properties of ternary superionic conductor CuCrS{sub 2}

Transition metal chalcogenide CuCrS{sub 2} powder was synthesized by mechanical alloying (MA) and then consolidated by spark plasma sintering (SPS) technique at 673-1073 K. The phase structure, microstructure and thermoelectric properties of samples were characterized by X-ray diffraction (XRD), field emission scanning electron microscopy (FESEM) and Seebeck coefficient/electrical conductivity measuring system, respectively. All the bulks indicated a single phase CuCrS{sub 2}, while the high relative density over 90% were attained for the samples sintered at 873-1073 K. The electrical conductivity of bulk samples displayed a typical characteristic of semiconductor. With increasing measuring temperature, the conductive behaviour of bulk samples sintered over 973 K showed a semiconductor transformation from n-type to p-type due to the changes of main carrier type. The sample obtained by applying SPS at 873 K got the highest power factor 83.2 {mu}W m{sup -1} K{sup -2}, and the largest ZT value 0.11 at 673 K. - Graphical abstract: The samples sintered above 873 K, both of the Seebeck coefficient and electrical conductivity exhibit an increase tendency with increasing temperature, which is due to the mechanism of mix-conduction for CuCrS{sub 2}. Highlights: Black-Right-Pointing-Pointer Single phase CuCrS{sub 2} powder was synthesized by ball-milling at 425 rpm for 40 h. Black-Right-Pointing-Pointer Dense CuCrS{sub 2} bulks were fabricated using SPS techniques at sintering temperature 873-1073 K. Black-Right-Pointing-Pointer Seebeck coefficient of CuCrS{sub 2} samples sintered over 973 K change the signs. Black-Right-Pointing-Pointer Highest power factor reached 83.2 {mu}W m{sup -1} K{sup -2} at 673 K for the sample sintered at 873 K. Black-Right-Pointing-Pointer ZT value was 0.11 at 673 K for the sample sintered at 873 K.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Fabrication and characterization of powder metallurgy tantalum components prepared by high compaction pressure technique

The present study has investigated the consolidation behaviors of tantalum powders during compaction and sintering, and the characteristics of sintered components. For die compaction, the densification behaviors of the powders are simulated by finite element analyses based on the yield function proposed by Shima and Oyane. Accordingly, the green density distribution for coarser particles is predicted to be more uniform because they exhibits higher initial relative tap density owing to lower interparticle friction. It is also found that cold isostatic pressing is capable of producing higher dense compacts compared to the die pressing. However, unlike the compaction behavior, the sintered density of smaller particles is found to be higher than those of coarser ones owing to their higher specific surface area. The maximum sintered density was found to be 0.96 of theoretical density where smaller particles were pressed isostatically at 400 MPa followed by sintering at 2000 °C. Moreover, the effects of processing conditions on grain size and texture were also investigated. The average grain size of the sintered specimen is 30.29 μm and its texture is less than 2 times random intensity. Consequently, it is concluded that the higher pressure compaction technique is beneficial to produce high dense and texture-free tantalum components compared to hot pressing and spark plasma sintering. - Highlights: • Higher Ta density is obtained from higher pressure and sintering temperature. • High compaction method enables P/M Ta to achieve the density of 16.00 g·cm{sup −3}. • A P/M Ta component with fine microstructure and random orientation is developed.

36 MATERIALS SCIENCE↗

Synthesis of porous Ti–50Ta alloy by powder metallurgy

Highlights: • The proposed preview milling with the next sintering enables the homogeneous porous Ti50Ta (wt).% alloy to be obtained • The α and β nanocrystalline phases were prepared by ball milling. • For the longest sintering time there is complete diffusion of preview milled initial powders • The press and sinter route is proved to be a promising alternative for melted Ti-based biomaterials. - Abstract: The aim of the present study was to assess the possibility of producing porous Ti50Ta (wt%) alloys using powder metallurgy by characterizing the material properties. The influence of the sintering time on the microstructure, mechanical properties, and corrosion behaviour of the produced alloy was investigated. The samples were examined using scanning electron microscopy (SEM), transmission electron microscopy (TEM), optic microscopy, X-ray diffraction (XRD) and nanoindentation methods. The XRD results confirmed that nanocrystalline α and β phases were formed during high-energy ball milling. A longer sintering time of 72 h allowed complete interdiffusion of the elements in the pre-milled initial powders. The sintering time significantly influenced the microstructure and porosity. Additionally, the corrosion resistance of the Ti-Ta samples in Ringer's solution was characterized and differences were observed between the samples sintered at different temperatures. The open-circuit potential (E{sub OCP}) and the corrosion potential (E{sub CORR}) of all samples were similar. The sintered Ti50Ta (wt%) alloy showed better corrosion resistance than equivalent Ti or Ta reference samples. We concluded that these alloys had suitable properties for medical implant applications in the future.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Mechanical characterization of fine-grain dispersion-strengthened tungsten as a plasma facing material

Field-Assisted Sintering Technology (FAST) was used to produce fine-grained, dispersion-strengthened tungsten (W) materials. Investigated materials 4138, 4353, and 4355 composed of 3 wt% ZrC sintered at 1800 °C, 5 wt% ZrC sintered at 1800 °C, and 3 wt% ZrC sintered at 2000 °C, respectively. They were compared against ITER-grade W. A series of mechanical and thermal property testing and microstructure studies were conducted to study them as a potential plasma facing material (PFM) for fusion reactors. Hardness testing showed that manufacturing conditions substantially altered hardness. Material 4355 had an average HV10 value of 497.2 ± 16.8, slightly higher than ITER-grade at 378.5 ± 40.3. However, material 4353 was substantially higher with an HV10 value of 738.9 ± 31.7 over the investigated temperature range. Electron Backscatter Diffraction (EBSD) analysis showed that FAST produced substantially smaller grains than the hot-rolled ITER-grade W material, offering notable control over grain size. Materials 4353 and 4355 had grain sizes of 0.44 ± 0.20 µm and 3.67 ± 0.89 µm, respectively, whereas ITER-grade 27.14 ± 19.76 µm at room temperature. The fine grain structures showed no net coarsening after 1 hr. anneals up to 1800 °C, several hundred degrees above the 1100 – 1500 °C recrystallization range reported for conventional W. Inverse application of the Zener pinning relationship to the measured grain sizes indicates that these two FAST sintering conditions produce markedly different effective dispersoid populations, with effective particle diameters of approximately 90 nm at a peak sintering temperature of 1800 °C and approximately 460 nm at 2000 °C, respectively. This result demonstrates that the FAST thermal condition itself, and not the nominal ZrC content alone, governs the pinning effectiveness of the dispersion. Thermal diffusivity measurements support this finding independently. Materials of identical composition sintered at different temperatures differ by approximately 19% in measured thermal diffusivity with statistically indistinguishable density, while materials of different composition and sintering temperature converge to within approximately 2%. At a representative divertor heat flux of 10 MW/m², the lower thermal conductivity of the fine-grained materials corresponds to approximately 28 to 33 °C per millimeter of armor thickness relative to ITER-grade W, traded against a substantially larger margin to recrystallization-driven degradation. While high temperature tensile testing revealed likely contamination that motivates refinement of the manufacturing process, FAST-produced, fine-grained, dispersion-strengthened W offers process-controlled microstructural stability well above the operating temperatures of conventional W and supports its continued development as a PFM for economically viable commercial fusion power.

Parker, Gabe [ORNL] (ORCID:0000000190394100)↗

Magnesia tuned multi-walled carbon nanotubes–reinforced alumina nanocomposites

Magnesia tuned alumina ceramic nanocomposites, reinforced with multi-walled carbon nanotubes, were condensed using pressureless and hot-press sintering processes. Densification, microstructure and mechanical properties of the produced nanocomposites were meticulously investigated. Electron microscopy studies revealed the homogenous carbon nanotube dispersion within the alumina matrix and confirmed the retention of carbon nanotubes' distinctive tubular morphology and nanoscale features during the extreme mixing/sintering processes. Pressureless sintered nanocomposites showed meagre mechanical responses due to the poorly-integrated microstructures with a slight improvement upon magnesia addition. Conversely, both the magnesia addition and application of hot-press sintering technique resulted in the nanocomposite formation with near-theoretical densities (~ 99%), well-integrated microstructures and superior mechanical properties. Hot-press sintered nanocomposites incorporating 300 and 600 ppm magnesia exhibited an increase in hardness (10 and 11%), flexural strength (5 and 10%) and fracture toughness (15 and 20%) with respect to similar magnesia-free samples. Compared to monolithic alumina, a decent rise in fracture toughness (37%), flexural strength (22%) and hardness (20%) was observed in the hot-press sintered nanocomposites tuned with merely 600 ppm magnesia. Mechanically superior hot-press sintered magnesia tailored nanocomposites are attractive for several load-bearing structural applications. - Highlights: • MgO tailored Al{sub 2}O{sub 3}–2 wt.% CNT nanocomposites are presented. • The role of MgO and sintering on nanocomposite structures and properties was studied. • Well-dispersed CNTs maintained their morphology/structure after harsh sintering. • Hot-pressing and MgO led nanocomposites to higher properties/unified structures. • MgO tuned composites showed higher toughness (37%) and strength (22%) than Al{sub 2}O{sub 3}.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Structure and microwave dielectric characteristics of lithium-excess Ca{sub 0.6}Nd{sub 0.8/3}TiO{sub 3}/(Li{sub 0.5}Nd{sub 0.5})TiO{sub 3} ceramics

Graphical abstract: - Highlights: • Dense ceramics were fabricated by the conventional solid-state route. • Excess-Li addition lowers sintering temperature. • Excess-Li addition improves the relative density and microwave dielectric properties. - Abstract: Compositions based on (1−x)Ca{sub 0.6}Nd{sub 8/3}TiO{sub 3}−x(Li{sub 1/2}Nd{sub 1/2})TiO{sub 3} + yLi (CNLNTx + yLi, x = 0.30–0.60, y = 0–0.05), suitable for microwave applications have been developed by systematically adding excess lithium in order to tune the microwave dielectric properties and lower sintering temperature. Addition of 0.03 excess-Li simultaneously reduced the sintering temperature and improved the relative density of sintered CNLNTx ceramics. The excess Li addition can compensate the evaporation of Li during sintering process and decrease the secondary phase content. The CNLNTx (x = 0.45) ceramics with 0.03 Li excess sintered at 1190 °C have single phase orthorhombic perovskite structure, together with the optimum combination of microwave dielectric properties of ε{sub r} = 129, Q × f = 3600 GHz, τ{sub f} = 38 ppm/°C. Obviously, excess-Li addition can efficiently decrease the sintering temperature and improve the microwave dielectric properties. The high permittivity and relatively low sintering temperatures of lithium-excess Ca{sub 0.6}Nd{sub 0.8/3}TiO{sub 3}/(Li{sub 0.5}Nd{sub 0.5})TiO{sub 3} ceramics are ideal for the development of low cost ultra-small dielectric loaded antenna.

36 MATERIALS SCIENCE↗

Performance and Reliability of Bonded Interfaces for High-Temperature Packaging. Annual Report

Current generation automotive power electronics packages utilize silicon devices and lead-free solder alloys. To meet stringent technical targets for 2020 and beyond (for cost, power density, specific power, efficiency and reliability), wide-bandgap devices are being considered since they offer advantages such as operation at higher frequencies, voltages, and temperatures. Traditional power electronics packages must be redesigned to utilize the full potential of wide-bandgap devices, and the die- and substrate-attach layers are key areas where new material development and validation is required. Present solder alloys do not meet the performance requirements for these new package designs while also meeting cost and hazardous substance restrictions. Sintered silver (Ag) promises to meet the needs for die- and substrate-attach interfaces but synthesis optimization and reliability evaluation must be completed. Sintered Ag material was proposed as an alternative solution in power electronics packages almost 20 years back. However, synthesis pressure requirements up 40 MPa caused a higher complexity in the production process and more stringent flatness specifications for the substrates. Recently, several manufacturers have developed sintered Ag materials that require lower (3-5 MPa) or even no bonding pressures. Degradation mechanisms for these sintered Ag materials are not well known and need to be addressed. We are addressing these aspects to some extent in this project. We are developing generalized (i.e., independent of geometry) stress intensity factor versus cycles-to-failure relations for sintered Ag. Because sintered Ag is a relatively new material for automotive power electronics, the industry currently does not have a good understanding of recommended synthesis parameters or expected reliability under prescribed conditions. It is an important deliverable of this project to transfer findings to industry to eliminate barriers to using sintered Ag as a viable and commercialized die- and substrate-attach material. Only a few manufacturers produce sintered Ag pastes and may consider some processing conditions as proprietary. It is the goal of this project to openly explore and define best practices in order to impact the maximum number of power electronics module manufacturers and suppliers.

30 DIRECT ENERGY CONVERSION↗

Acetabular Cup with a Trabecular Coating: A Novel Approach to a Monolithic Cup Made of One High-Strength Ceramic Material

An advanced monolithic cup comprising a thin liner and a trabecular coating is a promising alternative to the current modular ceramic cups for hip replacements because it can be anchored directly to the human bone and features larger femoral heads allowing a greater range of motion. In this study, the authors propose a fabrication route for an advanced monolithic cup of only one high-strength ceramic material by joining a partially sintered liner and a coating with a ceramic paste as an intermediate layer and subsequent sintering. Therefore, the challenge here is to avoid the formation of defects at the coating/intermediate layer interfaces during classical sintering which is due to compressive tension constrained coating sintering in the initial sintering stages. In this study, the defect formation is minimized by sintering at constant low shrinkage rates, as this results in favorable compressive stresses in the coating in the initial sintering stages and a decrease in the differences in the densification rates. For the first time, by using the proposed route, the authors prepare an advanced monolithic cup of only alumina-toughened zirconia (ATZ) that contains a coating with a porosity of 50 vol% and interconnected pores between 150 and 450 μm, as required for bone-ingrowth.

36 MATERIALS SCIENCE↗