At least 1,297 records · Page 72

Evolution of mechanical properties of ultrafine grained 1050 alloy annealing with electric current

The tensile properties and microstructures of 1050 aluminum alloy prepared by equal channel angular pressing at cryogenic temperature (cryoECAP) after electric current annealing at 90–210 °C for 3 h were investigated by tensile test, electron back scattering diffraction (EBSD) and transmission electron microscopy (TEM). An unexpected annealing-induced strengthening phenomenon occurs at 90–210 °C, due to a significant decrease in the density of mobile dislocations after annealing, and thus a higher yield stress is required to nucleate alternative dislocation sources during tensile test. The electric current can enhance the motion of dislocations, lead to a lower dislocation density at 90–150 °C, and thus shift the peak annealing temperature from 150 °C to 120 °C. Moreover, the electric current can promote the migration of grain boundaries at 150–210 °C, result in a larger grain size at 150 °C and 210 °C, and thus causes a lower yield stress. The sample annealed with electric current has a lower uniform elongation at 90–120 °C, and the deviation in the uniform elongation between samples annealed without and with electric current becomes smaller at 150–210 °C. - Highlights: • An unexpected annealing-induced strengthening phenomenon occurs at 90–210 °C. • The d. c. current can enhance the motion of dislocations at 90–150 °C, and thus shift the peak annealing temperature from 150 °C to 120 °C. • The d. c. current can promote the grain growth at 150–210 °C, and thus cause a lower yield stress. • The DC annealed sample has a lower uniform elongation at 90–120 °C.

36 MATERIALS SCIENCE↗

Microstructure and mechanical properties of aluminium matrix composites reinforced by Al{sub 62}Cu{sub 25.5}Fe{sub 12.5} melt spun ribbon

Aluminium matrix composites containing 15, 30 and 50 vol.% of pulverized Al{sub 62}Cu{sub 25.5}Fe{sub 12.5} (in at.%) melt spun ribbons have been prepared by a vacuum hot pressing (T = 673 K, P = 600 MPa). The microstructure of the initial ribbon and the composites was investigated using X-ray, scanning and transmission electron microscopy. In the as-spun ribbon the quasicrystalline icosahedral phase (i-phase) coexisted with the cubic copper rich β-Al(Cu, Fe) intermetallic compound. The phase composition of Al-Cu-Fe particles changed after consolidation process and the i-phase transformed partially to the ω-Al{sub 70}Cu{sub 20}Fe{sub 10} phase. Additionally, the Θ-Al{sub 2}Cu phase formed at the α(Al)/Al-Cu-Fe particle interfaces. With an increase in volume fraction of the reinforcement the hardness of the composites increased up to HV = 180 for the highest amount of added particles. The ultimate compression strength of the same sample reached the value of 545 MPa. - Highlights: • Al and 15, 30, 50% of pulverized Al{sub 62}Cu{sub 25.5}Fe{sub 12.5} melt spun ribbon were consolidated. • The initial ribbon consisted of the icosahedral i-phase and copper rich β-Al(Cu, Fe). • The i-phase partially transforms to ω-Al{sub 7}Cu{sub 2}Fe phase in all composites. • Increase of microhardness and compressive strength with content of reinforcement • Ultimate compression strength 545 MPa for 50% of added particles.

36 MATERIALS SCIENCE↗

Influence of severe plastic deformation on intermetallic particles in Mg-12 wt.%Zn alloy investigated using transmission electron microscopy

The in-depth microstructural characterization of intermetallic particles in an Mg-12 wt.%Zn binary alloy subjected to a severe plastic deformation is presented. The alloy was processed by four passes via equal channel angular pressing with an applied back pressure at a gradually decreasing temperature and analyzed using transmission electron microscopy techniques to observe the influence of processing on intermetallic particles. The results are compared with the initial state of the material prior to severe plastic deformation. The microstructural evolution of the α-Mg matrix and the Mg{sub 21}Zn{sub 25}, Mg{sub 51}Zn{sub 20} and MgZn{sub 2} was analyzed using bright field imaging, selected area electron diffraction, high-resolution transmission electron microscopy and high-angle annular dark field imaging in scanning mode. The plastic deformation process influenced the α-Mg matrix and each type of intermetallic particle. The α-Mg matrix consisted of two types of areas. The first type of area had a highly deformed structure, and the second type of area had a partially recrystallized structure with an average grain size of approximately 250 nm. The Mg{sub 21}Zn{sub 25} microparticles exhibited distinct forms in the α-Mg matrix that were characterized as a single-crystalline form, a nano-crystalline form and a broken up form. No evidence of Mg{sub 51}Zn{sub 20} nanoparticles within the α-Mg matrix was found in the microstructure, which indicates their dissolution or phase transformation during the deformation process. MgZn{sub 2} nanoparticles exhibited different behavior in both types of α-Mg matrix. Two orientation relationships toward the highly deformed α-Mg matrix were observed; however, there was no relationship toward the partially recrystallized α-Mg matrix. Additionally, the growth of the MgZn{sub 2} nanoparticles was different in the two types of α-Mg matrix. The Mg{sub 51}Zn{sub 20} nanoparticles inside Mg{sub 21}Zn{sub 25} microparticles exhibited a distinct behavior within the single-crystalline or nano-crystalline form of the parent Mg{sub 21}Zn{sub 25} microparticles. The Mg{sub 21}Zn{sub 25} + Mg{sub 51}Zn{sub 20} eutectic compound was confirmed for both forms of the parent Mg{sub 21}Zn{sub 25} microparticles, and the growth of Mg{sub 51}Zn{sub 20} nanoparticles is discussed. - Highlights: •Comprehensive microstructure characterization of Mg-12 wt.%Zn alloy after ECAP-BP •TEM analysis of changes of intermetallic phases caused by SPD •Mg{sub 21}Zn{sub 25} particles exhibit nano-crystalline regions with grain size below 100 nm. •MgZn{sub 2} preserved its orientation relationship toward highly deformed α-Mg after SPD. •Existence of Mg{sub 21}Zn{sub 25} + Mg{sub 51}Zn{sub 20} eutectic remained for each Mg{sub 21}Zn{sub 25} particle form.

36 MATERIALS SCIENCE↗

Microstructure evolution and properties of graphene nanoplatelets reinforced aluminum matrix composites

Highlights: • Lamellar structure of GNPs fibers and Al matrix was obtained in the rolling direction. • Stacking faults were observed in Al grains due to greatly increased GNPs/Al interfaces. • Strength of Al-0.2 wt% GNPs increased 36.8% with negligible electrical conductivity loss. - Abstract: Aluminum matrix composites reinforced with graphene nanoplatelets (GNPs) were prepared by continuous casting and subsequent rolling. Al-GNPs master alloy, prepared by ball milling and cold pressing, was added into Al melts to fabricate the composites. Microstructure evolution of the composites were observed using scanning electron microscopy (SEM), transmission electron microscopy (TEM) and electron back scattered diffraction (EBSD). GNPs distributed uniformly in the as-cast specimen and then transformed into fibers in the rolling direction after deformation and finally a lamellar structure formed in the composites. Raman spectra showed that the structural damage of GNPs mainly came from ball milling. The interface between GNPs and Al was well combined in general while a few microcracks were observed, which reduced the ductility of the composites and no adverse aluminum carbide (Al{sub 4}C{sub 3}) was detected at the interface. Stacking faults were observed interior of the aluminum grain, which may due to the existence of plentiful interface introduced by GNPs. Fracture observation revealed that the load transferred from Al matrix to GNPs. The ultimate tensile strength of Al-0.2 wt% GNPs composites was about 36.8% higher than that of pure Al with the same casting and rolling process, which should result from the lamellar structure and load transfer, while the conductivity of the composites decreased slightly, indicating that interface scattering between Al and GNPs is very limited. The investigation results show that Al-GNPs composite is potential for high strength and high conductivity application.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Research on the interfacial structure and property improvement of the Cfiber/2Si-B-3C-N ceramic matrix composite

Highlights: • The C{sub fiber}/2Si-B-3C-N composite with nice properties was successfully prepared. • ZrO{sub 2} promotes the densification process, homogeneous nucleation and grain growth. • The interface reaction in the composite was well controlled by the addition of ZrO{sub 2}. • The damage to carbon fiber was largely avoided by the addition of ZrO{sub 2}. - Abstract: A mixture of the mechanically alloyed 2Si-B-3C-N powder and short carbon fiber was hot pressed at 1800 °C for 30 mins in nitrogen. Careful investigation to the prepared C{sub fiber}/2Si-B-3C-N ceramic matrix composite revealed that the composite was very difficult to be densified. Heterogeneous nucleation, abnormal grain growth and severe interface reaction occurred on the fiber surface or between the fiber and the ceramic matrix, leading to a small density and weak mechanical properties of the composite. For the prepared composite without any additive, the relative density, flexural strength, elastic modulus and fracture toughness is 71.7%, 64.6 MPa, 14.7 GPa and 1.47 MPa·m{sup 1/2}, respectively. The average size of the SiC grains close to and far away from the carbon fiber is 249.10 nm and 50.45 nm, respectively. However, with the addition of ZrO{sub 2} (7.5 mol%), the above mentioned phenomenons are changed noticeably, and those properties are significantly increased to 88.5%, 112.4 MPa, 111.1 GPa and 2.94 MPa·m{sup 1/2}, respectively. At the same time, the SiC grains close to or far away from the carbon fiber almost have the same average size of about 448.21 nm, and almost no interface reaction occurs. It shows that the addition of ZrO{sub 2} not only facilitates the sintering and densification process, but also depresses the interface reaction, promotes the homogeneous nucleation and grain growth, and hence significantly improves the mechanical properties of the C{sub fiber}/2Si-B-3C-N composite. This interesting finding is favorable for the preparation of carbon fiber reinforced ceramic matrix composite, which requires both a large relative density and well controlled interface reaction.

36 MATERIALS SCIENCE↗

Synthesis of porous Ti–50Ta alloy by powder metallurgy

Highlights: • The proposed preview milling with the next sintering enables the homogeneous porous Ti50Ta (wt).% alloy to be obtained • The α and β nanocrystalline phases were prepared by ball milling. • For the longest sintering time there is complete diffusion of preview milled initial powders • The press and sinter route is proved to be a promising alternative for melted Ti-based biomaterials. - Abstract: The aim of the present study was to assess the possibility of producing porous Ti50Ta (wt%) alloys using powder metallurgy by characterizing the material properties. The influence of the sintering time on the microstructure, mechanical properties, and corrosion behaviour of the produced alloy was investigated. The samples were examined using scanning electron microscopy (SEM), transmission electron microscopy (TEM), optic microscopy, X-ray diffraction (XRD) and nanoindentation methods. The XRD results confirmed that nanocrystalline α and β phases were formed during high-energy ball milling. A longer sintering time of 72 h allowed complete interdiffusion of the elements in the pre-milled initial powders. The sintering time significantly influenced the microstructure and porosity. Additionally, the corrosion resistance of the Ti-Ta samples in Ringer's solution was characterized and differences were observed between the samples sintered at different temperatures. The open-circuit potential (E{sub OCP}) and the corrosion potential (E{sub CORR}) of all samples were similar. The sintered Ti50Ta (wt%) alloy showed better corrosion resistance than equivalent Ti or Ta reference samples. We concluded that these alloys had suitable properties for medical implant applications in the future.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Mechanical properties of Al/ω-Al-Cu-Fe composites synthesized by the SPS technique

Highlights: • For the first time, Al/ω-Al-Cu-Fe composites are produced by Spark Plasma Sintering. • Cu diffusion in Al matrix leads to precipitation of θ′-Al{sub 2}Cu. • The σ{sub 0.2%} drop at around 523 K is due to coarsening of θ′-Al{sub 2}Cu precipitates. • At high temperature, load transfer is the main strengthening mechanism. • At low temperature, SPS Al/ω composites have higher σ{sub 0.2%} than HIP Al/ω composites. - Abstract: Al/40 vol%ω-Al-Cu-Fe composites were produced from Al powder and i-Al-Cu-Fe quasi-crystalline particles using spark plasma sintering (SPS) technique. The mechanical properties of the composite were evaluated over the temperature range 293 K–823 K by performing compression tests at constant strain rate. The temperature dependence of the σ{sub 0,2%} yield stress gives evidence of two temperature regimes with a transition in the range 473 K–523 K. The decrease of σ{sub 0,2%} with increasing temperature, more pronounced in the low temperature regime, indicates that the two temperature regimes correspond to two different thermally activated deformation mechanisms. Based on microstructural analyses of the Al matrix, where plastic deformation takes place, the different strengthening contributions are discussed and the results are finally compared to those obtained for composites produced by hot isostatic pressing (HIP), for which the σ{sub 0,2%} temperature dependence is similar. In the low temperature regime, the σ{sub 0.2%} stress of the SPS composites is higher than that of the HIP composites. In this temperature regime, the stress difference is mainly ascribed to the different reinforcement phases present in the Al matrix. In the high temperature regime, the temperature dependence of σ{sub 0.2%} is comparable for the two composites whatever the processing route: load transfer is thus the main strengthening mechanism, which is similar for the two Al/ω-Al-Cu-Fe composites, the temperature dependence being ascribed to cross slip and climb processes.

36 MATERIALS SCIENCE↗

Influence of fabrication on microstructure and heat affected zone width in weldments of nuclear reactor pressure vessel steel

Advanced manufacturing routes such as electron beam welding and powder metallurgy with hot isostatic pressing are increasingly used across energy and aerospace industries, where the reliable prediction of weld behavior and heat affected zone (HAZ) evolution is critical. This study examines how fabrication routes and post-weld heat treatments influence phase distribution, crystallite size, microstrain, and dislocation density in nuclear reactor pressure vessel steels using synchrotron X-ray diffraction (SXRD). Retained austenite occurs only in samples that did not undergo austenitization, whereas an austenitizing heat treatment fully eliminates retained austenite and produces a more uniform microstructure across the weldment in terms of phase fraction, dislocation density, and microstrain. The Rosenthal solution underestimates the HAZ width for powder metallurgy samples. A newly proposed modified Rosenthal solution, reducing density by accounting for porosity, matches the SXRD-measured HAZ width with a 0.65% error. Structure–property correlations reveal that dislocation density correlates strongly with nanohardness in homogenous microstructures, while in heterogenous weldments nanohardness is further influenced by the presence of dissimilar phase boundaries. These findings provide new insight into the thermal and microstructural response of powder metallurgy fabricated steels and offer a framework for optimizing welding procedures and heat treatments in advanced manufacturing applications.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Preparation and microwave characterization of BaNd{sub 2-x}Sm{sub x}Ti{sub 4}O{sub 12} (0 {<=} x {<=} 2) ceramics and their effect on the temperature coefficient of dielectric constant in polytetrafluoroethylene composites

High dielectric and temperature-stable ceramic compositions have been prepared through solid-state ceramic route. The structure and microstructure of the ceramics have been studied using powder X-ray diffraction and scanning electron microscopic techniques. The dielectric properties of well-sintered ceramics are studied in the microwave frequency region using Hakki and Coleman post-resonator technique. The samples exhibited high dielectric constant (>77), relatively high quality factor (>1500) and near zero temperature coefficient of resonant frequency. Phase pure calcined ceramic materials are incorporated in the polytetrafluoroethylene matrix through a proprietary process comprising of sigma mixing, extrusion, calendering followed by hot pressing for the fabrication of planar circuit laminates. The effect of temperature coefficient of dielectric constant of the resultant polytetrafluoroethylene/ceramic composite materials is studied with respect to compositional variation of the filler materials.

36 MATERIALS SCIENCE↗

Synthesis and thermoelectric properties of Bi{sub 2}O{sub 2}Se nanosheets

Graphical abstract: Sheet-like Bi{sub 2}O{sub 2}Se is synthesized by composite-molten-salt (CMS) method. The film made from the as-synthesized Bi{sub 2}O{sub 2}Se nanosheets show very low thermal conductivity and high electrical conductivity. - Highlights: • Bi{sub 2}O{sub 2}Se nanosheets are synthesized by the composite-molten-salt approach. • Thermoelectric properties of a film consisting of Bi{sub 2}O{sub 2}Se are investigated. • The film shows very low thermal conductivity and high electrical conductivity. - Abstract: The pure tetragonal bismuth oxiselenide nanosheets are synthesized by the composite-molten-salt approach at 200 °C. Field emission scanning electron microscopy, X-ray diffraction, and energy dispersive X-ray spectroscopy are used to characterize the structure, morphology, and composition of the sample. The results show that the thickness of the nanosheets is about 120 nm. The sample for thermoelectric property measurements is prepared using cold pressing method. Thermoelectric properties, including electrical conductivity, Seebeck coefficient and thermal conductivity, are measured from room temperature to 470 K. The results show that the sample exhibits n-type semiconductor behavior with low thermal conductivity (κ{sub 300} = 0.346 Wm{sup −1} K{sup −1}, and κ{sub 470} = 0.458 Wm{sup −1} K{sup −1}). Although the obtained figure of merit is small, it would be enhanced with increase in temperature.

36 MATERIALS SCIENCE↗

Silver nanowire/polyaniline composite transparent electrode with improved surface properties

Highlights: • AgNWs/PANI transparent electrode was prepared by layer-by-layer coating method. • The surface roughness of the electrode reached to 6.5 nm (root mean square). • The electrode had reasonable sheet resistance (25 Ω/□) and transmittance (83.5%). - Abstract: Silver nanowires (AgNWs) are as potential candidates to replace indium tin oxide (ITO) in transparent electrodes because of their preferred conducting and optical properties. However, their rough surface properties are not favorable for the fabrication of optoelectronic devices, such as displays and thin-film solar cells. In the present investigation, AgNWs/polyaniline composite transparent electrodes with better surface properties were successfully prepared. AgNWs were incorporated into polyaniline:polystyrene sulfonate (PANI:PSS) by layer-by-layer coating and mechanical pressing. PANI:PSS decreased the surface roughness of the AgNWs electrode by filling the gap of the random AgNWs network. The transparent composite electrode had decreased surface roughness (root mean square 6.5 nm) with reasonable sheet resistance (25 Ω/□) and transmittance (83.5%)

36 MATERIALS SCIENCE↗

Influence of sintering conditions on the microstructure and optical properties of Eu: CaF{sub 2} transparent ceramic

Highlights: • Eu: CaF2 ceramics sintering at different conditions were fabricated by HP method. • The results show that the temperatures have great effect on the microstructure. • The ceramic sintered at 600 °C/30 MPa has high transmittance and pore-free structure. • The diffusion and densification process mainly occurs between 350 °C and 500 °C. • The optical losses in ceramic were caused by structure defects and polishing damage. - Abstract: Nanopowders of the 5 at.% Eu doped CaF{sub 2} have been synthesized by co-precipitated method. X-ray diffraction (XRD) indicated that the samples corresponds to the cubic CaF{sub 2} phase and scanning electron microscopy (SEM) showed that the morphology of nanopowders were approximately spherical. The Eu: CaF{sub 2} transparent ceramics were fabricated by hot-pressing (HP) method at different P-T conditions in a vacuum environment. The fracture surface, the relative density, average grain size and shrinkage displacements were also studied to analysis the influence of sintering conditions on Eu: CaF{sub 2} ceramic. In comparison with other samples, the proper sintering temperature and pressure was 600 °C/30 MPa. The transmittance of ceramic was up to 79.7% and 88.85% at the wavelength of 760 nm and 2400 nm. Furthermore, the emission spectra of Eu: CaF{sub 2} transparent ceramics under 393.5 nm excitation was also discussed.

36 MATERIALS SCIENCE↗

Strong photoluminescence emission at low dopant amount in YAG:Ce and YAG:Eu phosphors

Highlights: • YAG:Ce and YAG:Eu materials were prepared by solid state reaction. • Pure YAG phase can be obtained at 1300 °C. • High density materials were synthesized at 1600 °C for 10 h. • The highest PL emission was observed for the YAG:Ce{sub 0.01} and YAG:Eu{sub 0.1} samples. - Abstract: YAG:Ce and YAG:Eu phosphors have been prepared by solid state reaction. The use of submicrometric powders allows preparing pellets with high density, enhancing the photoluminescence (PL) properties. Pellets were prepared by uniaxial pressing and the influence of the thermal treatment on the microstructural and optical properties were also studied. Pure YAG phase was obtained at 1400 °C during 1 h and high density pellets (97%) after sintering at 1600 °C for 10 h. The highest PL emission was achieved for the sintered YAG:Ce and YAG:Eu pellets doped with low dopant concentrations (0.01 mol% for Ce and 0.1 mol% for Eu). Finally, increasing the Ce and Eu concentration the PL intensity decreases and the dopants occupy different positions than the Y one in the YAG lattice.

36 MATERIALS SCIENCE↗

Fractal nature structure reconstruction method in designing microstructure properties

Highlights: • Structure and material’s properties, within the material’s consolidation triad: Synthesis – Structure – Properties. • The grain prediction methods is based on the measurements of the solid Euclidean geometric fractal characteristics. • The intergranular contacts inside the BaTiO3 -ceramic are responsible for intergranular capacities. • The inner complex geometry of intergrain contacts imposes fractal correction factor for permeability. - Abstract: In the process of predicting materials properties, it is necessary to predict microstructures. This is important for ceramic materials, for the purpose of miniaturization and for a higher level of integration. Although the method of material structure reconstruction is for the first time used on BaTiO{sub 3}-ceramics by these authors, it can also be used for silicate, refractory and other ceramics, and, for any powder-based material. The reconstruction is based on the grain perimeter fractal analysis and the Richardson method. The main contribution of this paper is establishing the relationship between the electronic properties of BaTiO{sub 3}-ceramics and its microstructural fractal nature. Similar relations can be used for any ceramics or even any materials. The samples consolidation includes both powder pressing (cold sintering phase) and sintering in a furnace (hot sintering phase). The fractal nature characterization has a very important role from the powder phase up to the final microstructure, through which structures it directly impacts electro-physical and other ceramics properties. Thereby, the new possibilities in the microstructure characterization applications are directly introduced to an engineering system, providing the new solutions related to computer aided support. This creates new industrial production and application possibilities, especially in the process of ceramics material consolidation, now based on microstructural properties, which is providing a basis for “fractal electronics’’ development.

36 MATERIALS SCIENCE↗

Low loss polypropylene-silicon composites for millimetre wave applications

Highlights: • Developed polypropylene-silicon composite. • The composite shows a decrease in loss tangent with increasing frequency. • The composite is useful for high frequency applications such as Internet of Things and 5th Generation wireless communication. - Abstract: Polypropylene-silicon composite laminates were fabricated via hot pressing and their dielectric properties up to 35 GHz were studied. The loss tangent was found to decrease with increasing frequency whereas an increasing trend of loss tangent has previously been reported in the literature for such composites. The decreasing trend of the loss tangent with frequency is due to the decreasing conductor loss of silicon (Si) and indicates the possibility for use in high frequency applications such as the Internet Of Things and 5 t h generation wireless communication. The composite containing 25 vol% of Si had a relative permittivity of 3.5 and a loss tangent of 0.001 at 35 GHz. The coefficient of thermal expansion and the thermal conductivity of 40 vol% Si loaded composites were 51 ppm/{sup o}C and 2.23 W/mK, respectively. The thermal conductivity of the composite increased by 163% and 913% for 25 and 40 vol% Si addition, respectively.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Synthesis and Characterization of Zr2SC Ceramics

MAX-phase Zr{sub 2}SC ceramics were synthesized by hot pressing mixtures containing ZrH{sub 2}, carbon or ZrC, and ZrS{sub 2}, WS{sub 2}, or FeS{sub 2} as sulfur sources. The Zr{sub 2}SC synthesized with FeS{sub 2} had a typical MAX-phase laminated structure, good thermal shock resistance, thermal stability to 2100 C, and were readily machineable. The flexural strength was about 250 MPa up to 800 C. The thermal expansion coefficient was 8.8 x 10{sup -6}/C in the 25-2000 C-temperature range, thermal conductivity was 38 W/m-K at 100 C and about 30 W/m-K at 1100 C, and specific heat at temperatures from 100 to 1100 C ranged from 0.4 to 0.5 kJ/kg C. Load-deflection curves exhibited plastic deformation from RT to 2066 C. The sample deflection at fracture demonstrated significant dependence on temperature with a minimum at 1510 C. In arc heater testing at 2150 C for 23 s, the material developed an adherent, protective scale.

36 MATERIALS SCIENCE↗

Mechanical behavior of post-processed Inconel 718 manufactured through the electron beam melting process

Here, the electron beam melting (EBM) process was used to fabricate Inconel 718. The microstructure and tensile properties were characterized in both the as-fabricated and post-processed state transverse (T-orientation) and longitudinal (L-orientation) to the build direction. Post-processing involved both a hot isostatic pressing (HIP) and solution treatment and aging (STA) to homogenize the microstructure. In the as-fabricated state, EBM Inconel 718 exhibits a spatially dependent microstructure that is a function of build height. Spanning the last few layers is a cored dendritic structure comprised of the products (carbides and Laves phase) predicted under equilibrium solidification conditions. With increasing distance from the build's top surface, the cored dendritic structure becomes increasingly homogeneous with complete dissolution of the secondary dendrite arms. Further, temporal phase kinetics are observed to lead to the dissolution of the strengthening γ"γ" and precipitation of networks of fine δ needles that span the grains. Microstructurally, post-processing resulted in dissolution of the δ networks and homogeneous precipitation of γ'"γ'" throughout the height of the build. In the as-fabricated state, the monotonic tensile behavior exhibits a height sensitivity within the T-orientation at both 20 and 650 °C. Along the L-orientation, the tensile behavior exhibits strength values comparable to the reference wrought material in the fully heat-treated state. After post-processing, the yield strength, ultimate strength, and elongation at failure for the EBM Inconel 718 were observed to have beneficially increased compared to the as-fabricated material. Further, as a result of post-processing the spatial variance of the ultimate yield strength and elongation at failure within the transverse direction decreased by 4 and 3× respectively.

36 MATERIALS SCIENCE↗

Effect of preheat temperature and post-process treatment on the microstructure and mechanical properties of stainless steel 410 made via ultrasonic additive manufacturing

Ultrasonic additive manufacturing (UAM) is a solid-state manufacturing technology for producing near-net shape metallic parts combining additive ultrasonic metal welding and subtractive machining. Even though UAM has been demonstrated to produce robust metal builds in Al–Al, Al–Ti, Al-steel, Cu–Cu, Al–Cu, and other material systems, UAM welding of high strength steels has proven challenging. This study investigates process and post-processing methods to improve UAM steel weld quality and demonstrates the UAM fabrication of stainless steel 410 (SS 410) builds which possess, after post-processing, mechanical properties comparable with bulk material. Unlike UAM fabrication of softer metals, this study shows that increasing the baseplate temperature from 38°C (100°F) to 204°C (400°F) improves interfacial strength and structural homogeneity of the UAM steel samples. Further improvement in strength is achieved through post-processing. The hot isostatic pressing (HIP) post treatment improves the shear strength of UAM samples to 344 MPa from 154 MPa for as-welded samples. Microstructural analyses with SEM and EBSD show no evidence of body centered cubic (BCC) ferrite to face centered cubic (FCC) austenite transformation taking place during UAM welding of SS 410. The weld quality improvement of UAM steel at higher baseplate temperatures is believed to be caused by the reduction of the yield strength of SS 410 at elevated temperature. Finaly, HIP treatment is shown to increase the overall hardness of UAM SS 410 from 204 ± 7 HV to 240 ± 16 HV due to the formation of local pockets of martensite. Nanohardness tests show that the top of layer n is harder than the bottom of layer n+1 due to grain boundary strengthening.

36 MATERIALS SCIENCE↗