Search NASA⌕ Search

SEARCH · Search NASA

Results for “Powder”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,315 records · Page 73

High-pressure powder x-ray diffraction study of EuVO{sub 4}

The high-pressure structural behavior of europium orthovanadate has been studied using in-situ, synchrotron based, high-pressure x-ray powder diffraction technique. Angle-dispersive x-ray diffraction measurements were carried out at room temperature up to 34.7 GPa using a diamond-anvil cell, extending the pressure range reported in previous experiments. We confirmed the occurrence of zircon–scheelite phase transition at 6.8 GPa and the coexistence of low- and high-pressure phases up to 10.1 GPa. In addition, clear evidence of a scheelite–fregusonite transition is found at 23.4 GPa. The fergusonite structure remains stable up to 34.7 GPa, the highest pressure reached in the present measurements. A partial decomposition of EuVO{sub 4} was also observed from 8.1 to 12.8 GPa; however, this fact did not preclude the identification of the different crystal structures of EuVO{sub 4}. The crystal structures of the different phases have been Rietveld refined and their equations of state (EOS) have been determined. The results are compared with the previous experimental data and theoretical calculations. - Graphical abstract: The high-pressure structural sequence of EuVO{sub 4}. - Highlights: • EuVO{sub 4} is studied under pressure up to 35 GPa using synchrotron XRD. • The zircón–scheelite–fergusonite structural sequence is observed. • Crystal structures are refined and equations of state determined.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Sol–gel method as a way of carbonyl iron powder surface modification for interaction improvement

This article presents a method for modification of carbonyl iron particles’ surface (CIP), (d{sub 50}=4–9 µm) by silica coatings obtained using the sol–gel method. Reaction parameters were determined to obtain dry magnetic powder with homogeneous silica coatings without further processing and without any by-product in the solid or liquid phase. This approach is new among the commonly used methods of silica coating of iron particles. No attempt has been made to cover a carbonyl iron surface by silica in a waste-free method, up to date. In the current work two different silica core/shell structures were made by the sol–gel process, based on different silica precursors: tetraethoxy-silane (TEOS) and tetramethoxy-silane (TMOS). The dependence between the synthesis procedure and thickness of silica shell covering carbonyl iron particles has been described. Surface morphology of the modified magnetic particles and the coating thickness were characterized with the use of scanning electron microscopy (SEM) and transmission electron microscopy (TEM). Determination of the physicochemical structure of the obtained materials was performed by the energy-dispersive X-ray spectroscope (EDS), and the infrared technique (IR). The surface composition was analyzed using X-ray photoelectron spectroscopy (XPS). Additionally, distribution of particle size was measured using light microscopy. The new, efficient process of covering micro-size CIP with a nanometric silica layer was shown. Results of a performed analysis confirm the effectiveness of the presented method. - Highlights: • Proper covering CIP by sol–gel silica layer avoids agglomeration. • A new solid waste-free method of CIP coating is proposed. • Examination of the properties of modified CIP in depends on washing process. • Coatings on CIP particles doesn’t change the magnetic properties of particles.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Preparation of Mo-Re-C samples containing Mo{sub 7}Re{sub 13}C with the β-Mn-type structure by solid state reaction of planetary-ball-milled powder mixtures of Mo, Re and C, and their crystal structures and superconductivity

Mo-Re-C compounds containing Mo{sub 7}Re{sub 13}C with the β-Mn structure were synthesized with high-melting-temperature metals Mo, Re, and C powders using a conventional solid state method with a planetary ball milling machine instead of the arc melting method. Use of the ball milling machine was necessary to obtain Mo{sub 7}Re{sub 13}C with the β-Mn structure using the solid state method. Almost single-phase Mo{sub 7}Re{sub 13}C with a trace of impurity were obtained using the synthesis method. By XRF and lattice parameter measurements on the samples, Fe element existed in the compound synthesized using the planetary ball milling machine with a pot and balls made of steel, though Fe element was not detected in the compound synthesized using a pot and balls made of tungsten carbide. The former compound containg the Fe atom did not show superconductivity but the latter compound without the Fe atom showed superconductivity at 6.1 K. - Graphical abstract: Temperature dependence of the magnetic susceptibility measured under 10 Oe for the superconducting PBM-T samples without Fe element and non-superconducting PBM-S with Fe element. The inset is the enlarged view of the data for the PBM-S sample.

36 MATERIALS SCIENCE↗

Coherent 3D nanostructure of γ-Al{sub 2}O{sub 3}: Simulation of whole X-ray powder diffraction pattern

The structure and nanostructure features of nanocrystalline γ-Al{sub 2}O{sub 3} obtained by dehydration of boehmite with anisotropic platelet-shaped particles were investigated. The original models of 3D coherent nanostructure of γ-Al{sub 2}O{sub 3} were constructed. The models of nanostructured γ-Al{sub 2}O{sub 3} particles were first confirmed by a direct simulation of powder X–Ray diffraction (XRD) patterns using the Debye Scattering Equation (DSE) with assistance of high-resolution transmission electron microscopy (HRTEM) study. The average crystal structure of γ-Al{sub 2}O{sub 3} was shown to be tetragonally distorted. The experimental results revealed that thin γ-Al{sub 2}O{sub 3} platelets were heterogeneous on a nanometer scale and nanometer-sized building blocks were separated by partially coherent interfaces. The XRD simulation results showed that a specific packing of the primary crystalline blocks in the nanostructured γ-Al{sub 2}O{sub 3} particles with formation of planar defects on (001), (100), and (101) planes nicely accounted for pronounced diffuse scattering, anisotropic peak broadening and peak shifts in the experimental XRD pattern. The identified planar defects in cation sublattice seem to be described as filling cation non-spinel sites in existing crystallographic models of γ-Al{sub 2}O{sub 3} structure. The overall findings provided an insight into the complex nanostructure, which is intrinsic to the metastable γ-Al{sub 2}O{sub 3} oxide. - Highlights: • Thin plate-like crystallites of γ-Al{sub 2}O{sub 3} were obtained. • Models of 3D coherent nanostructure of γ-Al{sub 2}O{sub 3} were constructed. • Models were verified by simulating XRD patterns using the Debye Scattering Equation. • Specific broadening of XRD peaks was explained in terms of planar defects. • Primary crystalline blocks in γ-Al{sub 2}O{sub 3} are separated by partially coherent interfaces.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Characterization of the carbides and the martensite phase in powder-metallurgy high-speed steel

A microstructural characterization of the powder-metallurgy high-speed-steel S390 Microclean was performed based on an elemental distribution of the carbide phase as well as crystallographic analyses. The results showed that there were two types of carbides present: vanadium-rich carbides, which were not chemically homogeneous and exhibited a tungsten-enriched or tungsten-depleted central area; and chemically homogeneous tungsten-rich M{sub 6}C-type carbides. Despite the possibility of chemical inhomogenities, the crystallographic orientation of each of the carbides was shown to be uniform. Using electron backscatter diffraction the vanadium-rich carbides were determined to be either cubic VC or hexagonal V{sub 6}C{sub 5}, while the tungsten-rich carbides were M{sub 6}C. The electron backscatter diffraction results were also verified using X-ray diffraction. Several electron backscatter diffraction pattern maps were acquired in order to define the fraction of each carbide phase as well as the amount of martensite phase. The fraction of martensite was estimated using band-contrast images, while the fraction of carbides was calculated using the crystallographic data.

36 MATERIALS SCIENCE↗

Studies of microstructural imperfections of powdered Zirconium-based alloys

Different model based approaches of X-ray diffraction line profile analysis have been applied on the heavily deformed zirconium-based alloys in the powdered form to characterize the microstructural parameters like domain size, microstrain and dislocation density. In characterizing the microstructure of the material, these methods are complimentary to each other. Though the parameters obtained by different techniques are differently defined and thus not necessarily comparable, the values of domain size and microstrain obtained from the different techniques show similar trends.

36 MATERIALS SCIENCE↗

Electrochemical study of Aluminum-Fly Ash composites obtained by powder metallurgy

In this paper, two different ASTM C 618 Class C fly ashes (FA) were used for the production of aluminum metal matrix composites (MMCs) using powder metallurgy (PM) technology. Calcareous FAs were sampled from the electrostatic precipitators of two different lignite-fired power stations: from Megalopolis, Southern Greece (MFA) and from Kardia, Northen Greece (KFA), under maximum electricity load. FAs were milled in order to reduce the mean particle diameter and Aluminum-FA composites containing 10% and 20% of FA were then prepared and compacted. The green products were sintered for 2 h at 600 Degree-Sign C. Sintered Al-FA MMCs showed increased hardness and wear resistance suggesting their possible use in industrial applications for example in covers, casings, brake rotors or engine blocks. As most possible industrial applications of MMCs not only require wear resistance, but also corrosion resistance in different mild aggressive medias, this paper aims to study the electrochemical behavior of FA MMCs in order to evaluate their corrosion resistance. The morphology and chemical composition of the phases in the Aluminum-FA composite samples were investigated using Scanning Electron Microscopy (SEM) and Energy Dispersive X-ray Spectroscopy (EDXS). Moreover, topographic and Volta potential maps were acquired by Scanning Kelvin Probe Force Microscopy (SKP-FM). Volta potential maps provide information about the electrochemical behavior of the different phases in absence of electrolyte. The electrochemical behavior was investigated by Open Circuit Potential measurements and potentiodynamic polarization, while the corrosion mechanisms were studied by SEM observations after different times of immersion in a mild corrosive medium. In all cases it could be stated that the addition of the FA particles into the Al matrix might cause an increase of the hardness and mechanical properties of the pure aluminum but deteriorates the corrosion resistance. The degradation phenomena occurring on the FA containing samples might be related to the following mechanisms: 1) Partial detachment or dissolution of the FA soluble phases, in particular based on Si, Fe and Ca; 2) dissolution of the Al matrix surrounding the FA particles due to crevice corrosion; 3) Al localized dissolution due to galvanic coupling between the Fe-rich intermetallics and the matrix. - Highlights: Black-Right-Pointing-Pointer Aluminum metal matrix composites containing two types of fly ashes have been characterized. Black-Right-Pointing-Pointer The microstructure and the electrochemical behavior have been studied using different techniques. Black-Right-Pointing-Pointer The addition of FA deteriorates the corrosion resistance of the aluminum. Black-Right-Pointing-Pointer Degradation mechanisms: galvanic coupling, crevice corrosion, detachment of FA particles.

36 MATERIALS SCIENCE↗

Characterisation of titanium-titanium boride composites processed by powder metallurgy techniques

In this work, a detailed characterisation of titanium-titanium boride composites processed by three powder metallurgy techniques, namely, hot isostatic pressing, spark plasma sintering and vacuum sintering, was conducted. Two composites with different volume percents of titanium boride reinforcement were used for the investigation. One was titanium with 20% titanium boride, and the other was titanium with 40% titanium boride (by volume). Characterisation was performed using X-ray diffraction, electron probe micro analysis - energy dispersive spectroscopy and wavelength dispersive spectroscopy, image analysis and scanning electron microscopy. The characterisation results confirm the completion of the titanium boride reaction. The results reveal the presence of titanium boride reinforcement in different morphologies such as needle-shaped whiskers, short agglomerated whiskers and fine plates. The paper also discusses how mechanical properties such as microhardness, elastic modulus and Poisson's ratio are influenced by the processing techniques as well as the volume fraction of the titanium boride reinforcement. - Highlights: Black-Right-Pointing-Pointer Ti-TiB composites were processed by HIP, SPS and vacuum sintering. Black-Right-Pointing-Pointer The completion of Ti-TiB{sub 2} reaction was confirmed by XRD, SEM and EPMA studies. Black-Right-Pointing-Pointer Hardness and elastic properties of Ti-TiB composites were discussed. Black-Right-Pointing-Pointer Processing techniques were compared with respect to their microstructure.

36 MATERIALS SCIENCE↗

Friction stir processing of an aluminum-magnesium alloy with pre-placing elemental titanium powder: In-situ formation of an Al{sub 3}Ti-reinforced nanocomposite and materials characterization

A fine-grained Al–Mg/Al{sub 3}Ti nanocomposite was fabricated by friction stir processing (FSP) of an aluminum-magnesium (AA5052) alloy with pre-placed titanium powder in the stirred zone. Microstructural evolutions and formation of intermetallic phases were analyzed by optical and electron microscopic techniques across the thickness section of the processed sheets. The microstructure of the nanocomposite consisted of a fine-grained aluminum matrix (1.5 µm), un-reacted titanium particles (<40 µm) and reinforcement particles of Al{sub 3}Ti (<100 nm) and Mg{sub 2}Si (<100 nm). Detailed microstructural analysis indicated solid-state interfacial reactions between the aluminum matrix and micro-sized titanium particles to form Al{sub 3}Ti intermetallic phase. The hard inclusions were then fractured and re-distributed in the metal matrix by the severe thermo-mechanical conditions imposed by FSP. Evaluation of mechanical properties by hardness measurement and uniaxial tensile test determined significant enhancement in the mechanical strength (by 2.5 order of magnetite) with a high ductility (~22%). Based on a dislocation-based model analysis, it was suggested that the strength enhancement was governed by grain refinement and the presence of hard inclusions (4 vol%) in the metal matrix. Fractographic studies also showed a ductile-brittle fracture mode for the nanocomposite compared with fully ductile rupture of the annealed alloy as well as the FSPed specimen without pre-placing titanium particles. - Highlights: • FSP was employed to fabricate in situ nanocomposite. • The AA5052 Al alloy with pre-placed micro-sized Ti particles were utilized. • The structural analysis was revealed that the in situ formation of Al{sub 3}Ti nanophase. • The SZ grain structure was refined by PSN and ZHP mechanisms during DRX. • Hardness and tensile strength were improved up to ~2.5 times with a good ductility.

36 MATERIALS SCIENCE↗

Phase identification in boron-containing powder metallurgy steel using EBSD in combination with EPMA

Boron (B) is extensively used to induce liquid phase sintering (LPS) in powder metallurgy (PM) steels and thereby increase the densification. The alloying elements in B-containing PM steels affect the boride phase, stability of the boride, the temperature of liquid formation, and the progress of LPS. However, the boride phase has not been systematically identified yet. The main objective of this study was to clarify the influences of alloying elements, including C, Cr, and Ni, on the boride phases using electron backscatter diffraction (EBSD) in combination with electron probe microanalysis (EPMA). Network structures consisting of ferrite, Fe{sub 2}B boride, and Fe{sub 3}C carbide were extensively observed in the Fe–0.4B–0.5C steel. The portions of Fe{sub 2}B were sufficiently larger than those of Fe{sub 3}C, and Fe{sub 3}C was mostly distributed at the interfaces between ferrite and Fe{sub 2}B. Adding 1.5 wt.% Cr or 1.8 wt.% Ni to Fe–0.4B–0.5C steel completely changes the Fe{sub 2}B and Fe{sub 3}C phases to a M{sub 3}(B,C) phase, where M represents the metallic elements, including Fe, Cr, Mo, and Ni. Furthermore, Cr, Mo, B, and C atoms tend to concentrate on the M{sub 3}(B,C) phase, but Ni atoms do not. - Highlights: • Network structures consisting of ferrite, Fe{sub 2}B boride, and Fe{sub 3}C carbide were extensively observed in the Fe–0.4B–0.5C steel. • Adding 1.5 wt.% Cr or 1.8 wt.% Ni to Fe–0.4B–0.5C steel completely transforms the Fe{sub 2}B and Fe{sub 3}C phases to a M{sub 3}(B,C) phase. • Cr, Mo, B, and C atoms tend to concentrate on the M{sub 3}(B,C) phase, but Ni atoms do not.

36 MATERIALS SCIENCE↗

Microstructure evolution and dynamic recrystallization behavior of a powder metallurgy Ti-22Al-25Nb alloy during hot compression

The flow behavior of a powder metallurgy (P/M) Ti-22Al-25Nb alloy during hot compression tests has been investigated at a strain rate of 0.01 s{sup −1} and a temperature range of 980–1100 °C up to various true strains from 0.1 to 0.9. The effects of deformation temperature and strain on microstructure characterization and nucleation mechanisms of dynamic recrystallization (DRX) were assessed by means of Optical microscope (OM), electron backscatter diffraction (EBSD) and transmission electron microscope (TEM) techniques, respectively. The results indicated that the process of DRX was promoted by increasing deformation temperature and strain. By regression analysis, a power exponent relationship between peak stresses and sizes of stable DRX grains was developed. In addition, it is suggested that the discontinuous dynamic recrystallization (DDRX) and continuous dynamic recrystallization (CDRX) controlled nucleation mechanisms for DRX grains operated simultaneously during the whole hot process, and which played the leading role varied with hot process parameters of temperature and strain. It was further demonstrated that the CDRX featured by progressive subgrain rotation was weakened by elevating deformation temperatures. - Highlights: •Flow behavior of a P/M Ti-22Al-25Nb is studied by hot compression tests. •Microstructure evolution of alloy is affected by deformation temperature and strain. •The relationship between peak stress and stable DRX grain size was developed. •The process of DRX was promoted by increasing deformation temperature and strain. •Nucleation mechanisms of DRX were identified by EBSD analysis and TEM observation.

36 MATERIALS SCIENCE↗

Morphology evolution of γ′ precipitates in a powder metallurgy Ni-base superalloy

Highlights: • The 3-D morphology of the γ′ precipitate for the Ni-base superalloy was characterized using the electronic etching. • Various morphologies of the γ′ precipitates, including cuboids, octet and dendritic shape, were observed. • Cooling rate has a significant influence on the morphology of the γ′ precipitate. • When the cooling rate was lower than 6 °C/min, the dendritic shape γ′ with eight-primary-branch pattern was observed. - Abstract: Effect of the cooling rate on the morphological evolution of the γ′ precipitate in a powder metallurgy Ni-base superalloy FGH96 was studied. Results showed that as the cooling rate decreased from 600 °C/min to 2 °C/min, the precipitate morphology transformed from sphere to cuboid, octet and dendrite. As the cooling rate increased, the mean size of the γ′ precipitates decreased while the nucleation density increased. When the cooling rate was lower than 6 °C/min, the precipitate would evolve from a sphere to cuboids with concave faces, octets, dendrite to final split-off branches. The morphological transition was driven by energy balance between coherent strain induced by the γ′/γ lattice misfit and interface energy. The dendritic shape γ′ exhibited an eight-primary-branch pattern with preferred growth direction along <111>, and secondary arms along <100>.

36 MATERIALS SCIENCE↗

Effect of homogenization heat treatment on the evolution of carbonitrides in powder bed fusion processed INCONEL 718

Inconel 718 fabricated using laser powder-bed fusion, contains precipitates in the as-built condition that can be coarsened by high-temperature heat treatments. In this study, two homogenization heat treatment regimens were applied to discern the impact of heat treatment conditions on the growth of complex M(C, N) carbonitrides. In the first heat treatment, the samples underwent heat treatment between 1050 °C and 1200 °C for 0.5 h. In the second heat treatment, the samples were held at a constant temperature of 1150 °C, with varied holding times from 0.5 h to 8 h. Heat treatments dissolved the unstable Laves phase, but the carbonitrides persisted in the structure regardless of temperature and duration. Changes in the compositions, lattice parameters, and sizes of M(C, N) carbonitrides were measured using transmission electron microscopy and high-energy synchrotron X-ray diffraction. The results show an Nb enrichment at carbonitrides while Nb loss at the matrix with increased homogenization temperature. The findings suggest the optimum heat treatment conditions to achieve a homogeneous structure and controlled carbonitride size are between 1000 and 1050 °C for up to 2 h.

IN178↗

Cooling dynamics of two titanium alloys during laser powder bed fusion probed with in situ X-ray imaging and diffraction

Metal parts produced by laser powder bed fusion (LPBF) additive manufacturing exhibit characteristic microstructures comparable to those observed in laser welding. The primary cause of this characteristic microstructure is rapid, localized heating and cooling cycles, which result in extreme thermal gradients where material solidification is followed by fast cooling in the solid state. The final microstructure and mechanical performance are also influenced by pore formation caused by melt pool fluid dynamics. Here, we use high speed, in situ X-ray diffraction to probe the kinetics of cooling and solid-solid phase transitions after laser melting in two aerospace titanium alloys: Ti-6Al-4V, an α + β alloy; and Ti-5Al-5V-5Mo-3Cr, a near-β alloy. We complement these diffraction studies with in situ X-ray imaging to probe melt pool dynamics and pore formation. From these two complementary probes, we quantify pore formation during melting and the subsequent microstructural evolution as the material rapidly cools after solidification. These results are critical for understanding defect formation and residual stress development in different titanium alloys under LPBF conditions and can help inform process models to predict final part performance.

36 MATERIALS SCIENCE↗

Multi phenomena melt pool sensor data fusion for enhanced process monitoring of laser powder bed fusion additive manufacturing

Finding actionable trends in laser-based metal additive manufacturing process monitoring data is challenging owing to the diversity and complexity of the underlying physical interactions. A single monitoring solution that captures a particular process phenomenon, such as a photodiode that tracks melt pool intensity, is not alone capable of evaluating process stability or detecting flaw formation with sufficient precision for routine application in industry. In this work, to improve flaw detection performance, we adopted a data fusion approach that captures multiple process phenomena. To demonstrate this, we acquired data from laser powder bed fusion (LPBF) builds of cylindrical specimens produced with different laser spot sizes, emulating defocusing due to process faults such as thermal lensing. The resulting specimens had porosity of varying types and severity, quantified by post-build non-destructive X-ray computed tomography, Archimedes density measurements, and destructive metallographic characterization. During the build, the melt pool state was monitored with two coaxial high-speed video cameras and a temperature field imaging system. Physically intuitive low-level melt pool signatures, such as melt pool temperature, shape and size, and spatter intensity were extracted from this high-dimensional, image-based sensor data. These process signatures were subsequently used as input features in relatively simple machine learning models, such as a support vector machine, which were trained to detect laser defocusing, and in addition, predict porosity type and severity. The results show that the data fusion approach significantly enhanced system performance by reducing the overall false positive rate from ~ 0.1 to ~ 0.001 without sacrificing the true positive rate (~0.90). These results were at par with a black-box, deep machine learning approach (convolutional neural network).

36 MATERIALS SCIENCE↗

Multimodal and multiscale strengthening mechanisms in Al-Ni-Zr-Ti-Mn alloy processed by laser powder bed fusion additive manufacturing

The unique thermokinetics of laser-powder bed fusion additive manufacturing (L-PBFAM) has been exploited for development of a novel high-strength Al-Ni-Ti-Zr-Mn alloy. The addition of 0.5 wt% Mn leads to extraordinary improvement in ultimate tensile strength (502 MPa) and work hardening due to the activation of two Mn-induced strengthening mechanisms. First, by a bimodal particle strengthening effect due to Al 31 Mn 6 Ni 12 nano-quasi-crystal particles rejected in inter-dendritic spaces and fibrous Al 3 Ni eutectic dendritic channels, which predominately contributes to the strength improvement, and second by solid solution strengthening from remaining Mn entrapped in Al. These mechanisms supplement the particle strengthening effect imparted by coherent and incoherent Al 3 (Ti,Zr) co-precipitates present at melt pool boundaries, dislocation strengthening due to solidification induced strain, and Hall-Petch and backstress strengthening effect due to heterogenous grain size distribution occurring at various length scales. In conclusion, the solidification dynamics and hierarchical heat distribution that are associated with L-PBFAM resulted in complex spatial variations in these strengthening phenomena and were investigated via a high-throughput multiscale structure–property correlation that involved thermokinetic simulation, X-ray diffraction, high-resolution nanoindentation mapping, and site-specific transmission electron microscopy of the alloy.

36 MATERIALS SCIENCE↗

Quantification of solution annealing effects on microstructure and property in a laser powder bed fusion 316H stainless steel

Solution annealing (SA) is an effective way to mitigate microstructural heterogeneity and to optimize mechanical performance of alloys manufactured by laser powder bed fusion (LPBF). In this study, a comprehensive and quantitative understanding of the recovery and recrystallization processes in the SA temperature range of LPBF 316H stainless steel is provided using results from analytical electron microscopy and in-situ high-energy synchrotron x-ray scattering. The profound effect of dislocation structures and secondary phase particles on mechanical performance, particularly under tension and creep conditions, is rationalized using deformation models that incorporate microstructural inputs. This study, for the first time, quantifies the broad effect of nano oxide inclusions on dislocation recovery kinetics, on grain growth and recrystallization kinetics, and on tension strength and creep resistance. The fundamental differences between the LPBF and the conventional wrought materials are revealed. The findings address critical questions in post-build processing of AM materials and pave the way for their rapid qualification for high temperature applications.

In-situ X-ray diffraction↗

Activated combustion features in the Mo-Si-C-promoter system and synthesis of MoSi{sub 2}-SiC composite powders

Opportunities on combustion synthesizing the MoSi{sub 2}-SiC ceramic composites in a wide range of compositions under the chemical activated mode were studied. Molybdenum, silicon powders and carbon black were used as initial reagents, and Teflon was used as an activating additive. It was established that Teflon displays a dual (kinetic and thermal) impact on the interaction between reagents. The phasic character of the combustion process evolution, being characterized by low- and high-temperature regimes, was revealed. The end-products were subjected to SEM, XRD and chemical analyses.

36 MATERIALS SCIENCE↗